EN 10296-2 1.4845 Welded Stainless Steel Tube
What is EN 10296-2 1.4845 Welded Stainless Steel Tube
If the purchase file still names only a commercial alias such as 310S without a product standard, the mill cannot know whether general-purpose welded acceptance or pressure-tube acceptance applies. EN 10296-2 plus steel number 1.4845 (X8CrNi25-21) selects welded tube for mechanical and general engineering. EN 10296-2 1.4845 puts X8CrNi25-21 on welded general-purpose tube when 309-class oxidation life is not enough. Filler/shop note for 1.4845: 310-class fillers; high Ni/Cr dilution control on fabricator joints after mill seam.
SHH STEEL can produce and supply EN 10296-2 1.4845 welded stainless steel tube — longitudinal welded from strip or plate on Annex A routes, heat-treated to the ordered delivery condition, with EN 10204 3.1 inspection documents and the optional tests named on your enquiry (leak-tightness, flattening, drift expanding, bend, and non-destructive testing Options). Caution thread: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%).
On the shop floor people still say “310S tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4845, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class. Typical duties include furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product. Design caution: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%) Primary application sketch: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
Do not treat an EN 10296-2 1.4845 MTC as automatic clearance for pressure equipment — EN 10217-7 is the welded pressure home. Likewise, seamless pressure tube lives under EN 10216-5 and seamless general-purpose under EN 10297-2. Match the product standard to the duty before dual-marking talk begins. Corrosion thread: 25Cr-20Ni balance for higher oxidation resistance in severe elevated-temperature oxidising atmospheres.
Inside this welded general-purpose series, compare EN 10296-2 1.4833, EN 10296-2 1.4854, EN 10296-2 1.4835. Hub: EN 10296-2.
Chemical Composition of EN 10296-2 1.4845
Every 1.4845 heat under EN 10296-2 must meet the cast (ladle) analysis for X8CrNi25-21 in the austenitic heat-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Duty thread: 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class.
The table below reproduces public BSSA EN 10296-2 chemical limits for 1.4845 / X8CrNi25-21, cross-checked against the EN 10296-2:2005 grade list. Values are maximum unless a range is shown. Commercial talk still says 310S, but only the steel-number cast windows below belong on the MTC for this austenitic heat-resisting welded tube. Corrosion thread: 25Cr-20Ni balance for higher oxidation resistance in severe elevated-temperature oxidising atmospheres.
| Steel | C | Si | Mn | P | S | Cr | Ni | N |
|---|---|---|---|---|---|---|---|---|
| 1.4845 / X8CrNi25-21 | ≤0.10 | ≤1.50 | ≤2.00 | ≤0.045 | ≤0.015 | 24.0–26.0 | 19.0–22.0 | ≤0.11 |
Mechanical Properties of EN 10296-2 1.4845
Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4845 order. General-purpose Table values for this number read: Rp0.2 min 210 MPa, Rp1.0 min 250 MPa, Rm min 500 MPa, longitudinal elongation min 35%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Duty thread: 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 210 | 250 | 500 min | 35 | 35 | N/A |
Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4845 / X8CrNi25-21. Guideline solution/anneal band (Annex B): 1050–1150 °C; cooling: water, air or gas.
Welded Tube Manufacture for EN 10296-2 1.4845
EN 10296-2 does not offer a seamless route for 1.4845. Tube in X8CrNi25-21 is made by longitudinal welding of strip or plate edges, then solution annealed (+AT) to meet Table 5 heat-resisting mechanical floors. Welded manufacture for 1.4845 finishes through hot- or cold-rolled strip/plate routes in Table A.1. Pick W1/W2 families for descaled engineering surfaces, W*R for bright anneal atmospheres, and WG or WP only when the enquiry states which surface (OD, ID, or both) is ground or polished. Caution thread: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%).
Austenitic heat-resisting 1.4845 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1050–1150 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. High-temperature service still needs fabricator WPS discipline on site joints after the mill seam. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4845. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Caution thread: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%).
Dimensions and Tolerances for EN 10296-2 1.4845
Order EN 10296-2 1.4845 by outside diameter D and wall thickness T for steel name X8CrNi25-21. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. High-temp welded od on +at heat-resisting annex a routes. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
Tolerance classes on diameter and wall follow the EN 10296-2 / referenced dimensional agreements on the order. Out-of-roundness, eccentricity, and straightness limits should be stated when they are tighter than the default product practice. SHH STEEL confirms measurable limits before production. Weld thread: 310-class fillers; high Ni/Cr dilution control on fabricator joints after mill seam.
Equivalent Grades for EN 10296-2 1.4845
Do not treat ASTM welded or seamless pages as drop-in equals for EN 10296-2 1.4845 / X8CrNi25-21. Wall bases, mechanical tables, and optional tests differ. Body alias 310S is fine in BOM notes; H1 and order line stay on the steel number. Compare 1.4833, 1.4854, 1.4835 when the medium outgrows this analysis. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
Heat Treatment and Delivery Condition for EN 10296-2 1.4845
Austenitic heat-resisting 1.4845 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1050–1150 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Apps that usually decide +AT versus +AR for this number: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product. Primary application sketch: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
For 1.4845, purchasers who need verified IGC after fabrication should say so with the applicable Option and method (EN ISO 3651-2 framing). Mill +AT or +A of the tube does not automatically clear a fabricator’s as-welded joint without procedure control. Caution thread: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%).
Corrosion Resistance of EN 10296-2 1.4845
Corrosion behaviour of EN 10296-2 1.4845 tracks its austenitic heat-resisting balance: 25Cr-20Ni balance for higher oxidation resistance in severe elevated-temperature oxidising atmospheres. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%) Primary application sketch: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
Chloride pitting, crevice attack, and stress-corrosion cracking limits depend on temperature, concentration, and tensile stress — move across sisters 1.4833, 1.4854, 1.4835 when the medium outgrows this number rather than hoping surface finish alone will hold. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
Applications of EN 10296-2 1.4845 Tube
Buyers pick EN 10296-2 1.4845 / X8CrNi25-21 when the duty list looks like this: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product. That is welded general-purpose work — not a silent PED pressure shell. Role in one line: 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class. Filler/shop note for 1.4845: 310-class fillers; high Ni/Cr dilution control on fabricator joints after mill seam.
Typical BOM language pairs EN 10296-2 1.4845 with OD × wall, Annex A symbol, and delivery condition. Downstream fabricators should inherit the same steel number on cut lists so informal “310S” substitutions do not creep in. Caution thread: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%).
Weldability of EN 10296-2 1.4845
1.4845 / X8CrNi25-21 arrives as a longitudinally welded product under EN 10296-2, and fabricators still add circumferential and attachment welds on mechanical assemblies. Shop guidance: 310-class fillers; high Ni/Cr dilution control on fabricator joints after mill seam. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Filler/shop note for 1.4845: 310-class fillers; high Ni/Cr dilution control on fabricator joints after mill seam.
For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%) Primary application sketch: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
Surface Finishes for EN 10296-2 1.4845
For 1.4845, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Weld thread: 310-class fillers; high Ni/Cr dilution control on fabricator joints after mill seam.
Descaled 1.4845 engineering finishes still get caps and separators; bright X8CrNi25-21 OD never rides bare under carbon-steel strapping. Packaging notes on the order should repeat the Annex A symbol so warehouse staff do not treat every bundle as the same 310S commodity. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
Inspection and Testing for EN 10296-2 1.4845
NDT and technological-test intensity on 1.4845 is Option-driven under EN 10296-2 — leak, flattening, drift expanding, bend, or NDT methods are selected at enquiry. That is a different framing from EN 10217-7 pressure categories; copy the Options you need. Duty thread: 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class.
Inspection intensity on 1.4845 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class. Primary application sketch: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
Packaging and Shipping for EN 10296-2 1.4845
SHH STEEL ships EN 10296-2 1.4845 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled W1A/W2A engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Use thread: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
For 1.4845, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Caution thread: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%).
For 1.4845, packing-list discipline matters when multiple sisters (1.4833, 1.4854, 1.4835) ship on the same vessel — wrong bundle cards create wrong field installs. SHH STEEL can produce and supply photographed mark sets when the EPC file demands them. Caution thread: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%).
Why Choose SHH STEEL
SHH STEEL can produce and supply EN 10296-2 1.4845 as welded general-purpose tube when you need a mill partner who will not blur EN 10296-2 with EN 10217-7 or EN 10216-5 on the certificate. We can produce and supply the ordered Annex A finish, delivery condition, and Optional tests — and we say so in plain language on the quote. Duty thread: 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class.
Grade advice for 1.4845 stays practical. If the duty needs a sister chemistry, we point to 1.4833, 1.4854, 1.4835. Design caution for this number: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%) Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Family filing for 1.4845 is austenitic heat-resisting.
Supply Capability
SHH STEEL can produce and supply EN 10296-2 1.4845 welded stainless steel tube against the edition, delivery condition, Annex A symbol, and Options named on your enquiry. The capability table and Stock / Available sizes enquiry map below frame a first-pass size list for X8CrNi25-21 — role: 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class. Primary application sketch: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product.
| Item | Capability |
|---|---|
| Standard | EN 10296-2:2005 welded general-purpose |
| Steel | 1.4845 / X8CrNi25-21 |
| Product form | Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–12.7 mm within welded family practice (other by agreement) |
Stock / Available sizes
Enquiry-oriented Stock / Available sizes map for EN 10296-2 1.4845 — not a frozen warehouse SKU list with tonnages. Availability tracks mill heats of X8CrNi25-21, strip/plate starting stock, and welding/finishing slots for the ordered Annex A symbol; send the OD × wall list, delivery-condition preference, and any Optional tests tied to furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product. Filler/shop note for 1.4845: 310-class fillers; high Ni/Cr dilution control on fabricator joints after mill seam.
When the project needs both decorative WP and engineering W2A on 1.4845, say so up front — finishing slots differ. Apps that usually drive the mix: furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product. Family filing for 1.4845 is austenitic heat-resisting.
FAQ
-
What is EN 10296-2 1.4845 welded stainless steel tube used for?
- EN 10296-2 1.4845 (X8CrNi25-21) is welded tube for mechanical and general engineering — furnace tubes adjacent hardware, radiant-section mechanical parts, and high-temp oxidising service naming 310S welded product. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class.
-
Is EN 10296-2 1.4845 the same as EN 10216-5 1.4845?
- Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4845 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4845 / X8CrNi25-21?
- Delivery framing for 1.4845 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1050–1150 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4845?
- SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4845 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4845 compare with sister grades 1.4833, 1.4854, 1.4835?
- 1.4845 / X8CrNi25-21 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4833, 1.4854, 1.4835. Design caution: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%) Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
How should fabricators weld EN 10296-2 1.4845 tube on site?
- 1.4845 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 310-class fillers; high Ni/Cr dilution control on fabricator joints after mill seam. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4845?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10296-2 1.4845?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4845 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: high-temp welded OD on +AT heat-resisting Annex A routes. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 310S belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 310S in body text and BOM notes, but lock EN 10296-2 and 1.4845 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4845?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: heat-resisting first choice — not aqueous process 316L substitute; elongation floors follow Table 5 (PDF 35% long./trans. — see UNCERTAIN vs BSSA 40%) Sister pointers: 1.4833, 1.4854, 1.4835. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10296-2 1.4845 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4845 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10296-2 1.4845 (X8CrNi25-21) is welded stainless tube for mechanical and general engineering — 25Cr-20Ni austenitic heat-resisting welded tube (310S-class) for higher oxidation resistance than 309-class. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4833, 1.4854, 1.4835. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.