EN 10296-2 1.4462 Welded Stainless Steel Tube
What is EN 10296-2 1.4462 Welded Stainless Steel Tube
EN 10296-2:2005 (BS EN 10296-2:2005) is the European product standard for welded circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10217-7, and not for seamless general-purpose tube under EN 10297-2. Steel number 1.4462 is listed as X2CrNiMoN22-5-3 in the austenitic-ferritic (duplex) set. If the purchase file still names only “2205 welded tube,” EN 10296-2 1.4462 selects X2CrNiMoN22-5-3 under welded general-purpose acceptance — not pressure Part 7 unless ordered. Filler/shop note for 1.4462: 2205/duplex fillers; heat-input and interpass control to hold phase balance; mill seam +AT does not replace fabricator WPS.
SHH STEEL can produce and supply X2CrNiMoN22-5-3 under EN 10296-2 1.4462 as welded tube for mechanical and general engineering — not as a silent dual of EN 10217-7 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Duty thread: workhorse 2205 duplex welded tube for chloride SCC-resistant mechanical and general engineering duty.
On the shop floor people still say “2205 tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4462, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: workhorse 2205 duplex welded tube for chloride SCC-resistant mechanical and general engineering duty. Typical duties include offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”. Design caution: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo Primary application sketch: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”.
Do not treat an EN 10296-2 1.4462 MTC as automatic clearance for pressure equipment — EN 10217-7 is the welded pressure home. Likewise, seamless pressure tube lives under EN 10216-5 and seamless general-purpose under EN 10297-2. Match the product standard to the duty before dual-marking talk begins. Duty thread: workhorse 2205 duplex welded tube for chloride SCC-resistant mechanical and general engineering duty.
Inside this welded general-purpose series, compare EN 10296-2 1.4362, EN 10296-2 1.4410, EN 10296-2 1.4404. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4462. ASTM/ASME related product pages (not interchangeable by default): A789 S32205.
Chemical Composition of EN 10296-2 1.4462
Every 1.4462 heat under EN 10296-2 must meet the cast (ladle) analysis for X2CrNiMoN22-5-3 in the austenitic-ferritic (duplex) chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Use thread: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”.
The table below reproduces public BSSA EN 10296-2 chemical limits for 1.4462 / X2CrNiMoN22-5-3, cross-checked against the EN 10296-2:2005 grade list. Values are maximum unless a range is shown. Commercial talk still says 2205, but only the steel-number cast windows below belong on the MTC for this austenitic-ferritic (duplex) welded tube. Size context for 1.4462: process and structural welded OD common in 2205 catalogues, typically +AT.
| Steel | C | Si | Mn | P | S | Cr | Mo | Ni | N |
|---|---|---|---|---|---|---|---|---|---|
| 1.4462 / X2CrNiMoN22-5-3 | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.015 | 21.0–23.0 | 2.50–3.5 | 4.5–6.5 | 0.10–0.22 |
Mechanical Properties of EN 10296-2 1.4462
Ambient mechanical properties for EN 10296-2 1.4462 follow Tables 4–5 by family (wall thickness ≤30 mm framing for Table 4 corrosion-resisting grades). For this grade the delivery-condition floors to watch are: Rp0.2 min 450 MPa, Rm min 700 MPa, longitudinal elongation min 22%. Intergranular corrosion resistance per EN ISO 3651-2 is tabulated where applicable — see the IGC column on the mechanical table below. Duty thread: workhorse 2205 duplex welded tube for chloride SCC-resistant mechanical and general engineering duty.
| Delivery condition | Rp0.2 min (MPa) | Rp1.0 min (MPa) | Rm (MPa) | A long. min (%) | A trans. min (%) | IGC |
|---|---|---|---|---|---|---|
| +AT | 450 | — | 700 min | 22 | — | Yes |
Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4462 / X2CrNiMoN22-5-3. Guideline solution/anneal band (Annex B): 1020–1100 °C; cooling: water, air or gas.
Welded Tube Manufacture for EN 10296-2 1.4462
EN 10296-2 1.4462 is welded only — formed from strip or plate and longitudinally welded (automatic arc or laser practice as agreed), then heat-treated to the ordered delivery condition. Duplex X2CrNiMoN22-5-3 needs controlled thermomechanical history so the ferrite–austenite balance lands in the ordered window after +AT. Order EN 10296-2 1.4462 with an Annex A surface/process symbol suited to ferritic tube — heat-treated descaled W1A/W2A analogues, WCA/WCR when the weld must be scarcely recognizable, and WG/WP only with a written OD/ID roughness scope. W0/W1/W2 are not applicable to ferritic steels. Weld thread: 2205/duplex fillers; heat-input and interpass control to hold phase balance; mill seam +AT does not replace fabricator WPS.
For duplex 1.4462, solution annealing and rapid cooling are part of the product story whenever +AT is ordered — not an optional cosmetic step. Ferritic 1.4462 under EN 10296-2 may be delivered as-welded (+AR) or annealed (+A) at the manufacturer’s discretion unless the order locks +A. Annex B annealing guidance sits near 1020–1100 °C with water, air or gas cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Optional tests (leak, flattening, drift expanding, bend, NDT) are selected on the order; they are not a substitute for correct duplex heat treatment. Corrosion thread: balanced duplex with Mo and nitrogen for chloride SCC resistance well above 316L in many aqueous duties.
State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4462. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Size context for 1.4462: process and structural welded OD common in 2205 catalogues, typically +AT.
Dimensions and Tolerances for EN 10296-2 1.4462
Order EN 10296-2 1.4462 by outside diameter D and wall thickness T for steel name X2CrNiMoN22-5-3. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Process and structural welded od common in 2205 catalogues, typically +at. Duty thread: workhorse 2205 duplex welded tube for chloride SCC-resistant mechanical and general engineering duty.
For precision mechanical or decorative duty on 1.4462, cold-rolled W2/W2A/W2R and WCA/WCR routes are the usual conversation; heavier walls may start from hot-rolled strip. Agree bead-worked “b” suffixes when smoothed welds are mandatory. Caution thread: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo.
Equivalent Grades for EN 10296-2 1.4462
Equivalence talk for 1.4462 starts with X2CrNiMoN22-5-3: that is the EN steel name for welded general-purpose tube under this Part 2. Buyers who only write 2205 still need the steel number and EN 10296-2 on the PO. Sister grades often quoted alongside this duty: 1.4362, 1.4410, 1.4404. Design caution stays: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo Family filing for 1.4462 is duplex (austenitic-ferritic).
Heat Treatment and Delivery Condition for EN 10296-2 1.4462
Ferritic 1.4462 under EN 10296-2 may be delivered as-welded (+AR) or annealed (+A) at the manufacturer’s discretion unless the order locks +A. Annex B annealing guidance sits near 1020–1100 °C with water, air or gas cooling. Do not expect austenitic elongation floors after cold expansion without a forming trial. Role reminder while setting HT: workhorse 2205 duplex welded tube for chloride SCC-resistant mechanical and general engineering duty Primary application sketch: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”.
Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4462, restore the delivery condition agreed on the order before corrosive or load-bearing service. Use thread: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”.
Corrosion Resistance of EN 10296-2 1.4462
Corrosion behaviour of EN 10296-2 1.4462 tracks its austenitic-ferritic (duplex) balance: balanced duplex with Mo and nitrogen for chloride SCC resistance well above 316L in many aqueous duties. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo Filler/shop note for 1.4462: 2205/duplex fillers; heat-input and interpass control to hold phase balance; mill seam +AT does not replace fabricator WPS.
For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4462 is filed as austenitic-ferritic (duplex) — pick tests that match that filing. Use thread: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”.
Applications of EN 10296-2 1.4462 Tube
Typical field use for 2205-named welded tube under steel number 1.4462: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”. Keep pressure seamless talk on EN 10216-5 pages when that standard is the regulatory home. Primary application sketch: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”.
It is the wrong first choice when a seamless product form is mandatory (use EN 10297-2 or EN 10216-5 as applicable), when PED pressure welded acceptance is locked to EN 10217-7 alone, or when the medium clearly needs a sister such as 1.4362. Use thread: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”.
Weldability of EN 10296-2 1.4462
1.4462 / X2CrNiMoN22-5-3 arrives as a longitudinally welded product under EN 10296-2, and fabricators still add circumferential and attachment welds on mechanical assemblies. Shop guidance: 2205/duplex fillers; heat-input and interpass control to hold phase balance; mill seam +AT does not replace fabricator WPS. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Filler/shop note for 1.4462: 2205/duplex fillers; heat-input and interpass control to hold phase balance; mill seam +AT does not replace fabricator WPS.
For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo Family filing for 1.4462 is duplex (austenitic-ferritic).
Surface Finishes for EN 10296-2 1.4462
For 1.4462, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Weld thread: 2205/duplex fillers; heat-input and interpass control to hold phase balance; mill seam +AT does not replace fabricator WPS.
For 1.4462, export and coastal routes need extra wrap discipline on W*R/WCR/WG/WP finishes. Size context: process and structural welded OD common in 2205 catalogues, typically +AT. SHH STEEL confirms sleeve, paper, or plastic protection against the ordered Annex A symbol before dispatch.
Inspection and Testing for EN 10296-2 1.4462
NDT and technological-test intensity on 1.4462 is Option-driven under EN 10296-2 — leak, flattening, drift expanding, bend, or NDT methods are selected at enquiry. That is a different framing from EN 10217-7 pressure categories; copy the Options you need. Caution thread: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo.
For X2CrNiMoN22-5-3 under EN 10296-2, technological Options and IGC (where tabulated) belong on the enquiry checklist beside OD × wall. SHH STEEL correlates marking on 1.4462 bundles to the EN 10204 3.1 document so heat identity survives transit. Caution reminder: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo Primary application sketch: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”.
Packaging and Shipping for EN 10296-2 1.4462
Export packing for 1.4462 / X2CrNiMoN22-5-3 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavier descaled bundles use spacers to stop fretting in transit. Corrosion thread: balanced duplex with Mo and nitrogen for chloride SCC resistance well above 316L in many aqueous duties.
For 1.4462, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Size context for 1.4462: process and structural welded OD common in 2205 catalogues, typically +AT.
Ocean-freight wrap for X2CrNiMoN22-5-3 repeats cast/code on tags inside and outside the wrap. Duty thread for why identity matters: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”. Primary application sketch: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”.
Why Choose SHH STEEL
SHH STEEL can produce and supply EN 10296-2 1.4462 as welded general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “2205 tube” label on whatever is in the rack. We keep pressure talk honest: when PED welded pressure acceptance is required, we point you to EN 10217-7 for the same chemistry family where it exists. Caution thread: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo.
SHH STEEL will not stretch X2CrNiMoN22-5-3 into a medium it cannot defend. Typical right-fit duties: offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”. When those duties slip toward a sister, we say so before the quote hardens. Family filing for 1.4462 is duplex (austenitic-ferritic).
Supply Capability
SHH STEEL can make and supply 2205-family chemistry only when the order locks EN 10296-2 and steel number 1.4462. Capability below is an RFQ map for X2CrNiMoN22-5-3, not a promise that every OD×wall sits in a Shanghai rack tonight. Size context for 1.4462: process and structural welded OD common in 2205 catalogues, typically +AT.
| Item | Capability |
|---|---|
| Standard | EN 10296-2:2005 welded general-purpose |
| Steel | 1.4462 / X2CrNiMoN22-5-3 |
| Product form | Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP) |
| Delivery condition | +AT |
| Documents | EN 10204 3.1 (Options as ordered) |
| Typical enquiry OD | ~6–219 mm (other by agreement) |
| Typical enquiry wall | ~0.5–12.7 mm within welded family practice (other by agreement) |
Stock / Available sizes
For X2CrNiMoN22-5-3, tell us which Annex A symbol and whether +AT (or +A/+AR) is locked before we hold strip. Caution that shapes size choice: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo Filler/shop note for 1.4462: 2205/duplex fillers; heat-input and interpass control to hold phase balance; mill seam +AT does not replace fabricator WPS.
Trial lengths of 1.4462 / X2CrNiMoN22-5-3 help fabricators prove forming and weld procedures before a production heat. Sisters often sampled on the same RFQ: 1.4362, 1.4410, 1.4404. SHH STEEL can produce and supply those trials when strip slots allow. Size context for 1.4462: process and structural welded OD common in 2205 catalogues, typically +AT.
FAQ
-
What is EN 10296-2 1.4462 welded stainless steel tube used for?
- EN 10296-2 1.4462 (X2CrNiMoN22-5-3) is welded tube for mechanical and general engineering — offshore-adjacent utilities, chemical process mechanical lines, water systems, and fabrications that still say “2205 welded tube”. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: workhorse 2205 duplex welded tube for chloride SCC-resistant mechanical and general engineering duty.
-
Is EN 10296-2 1.4462 the same as EN 10216-5 1.4462?
- Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4462 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
-
What delivery condition applies to 1.4462 / X2CrNiMoN22-5-3?
- Delivery framing for 1.4462 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1020–1100 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
-
What Annex A finishes can SHH STEEL supply for 1.4462?
- SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4462 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
-
How does 1.4462 compare with sister grades 1.4362, 1.4410, 1.4404?
- 1.4462 / X2CrNiMoN22-5-3 is filed as duplex (austenitic-ferritic). Typical sisters discussed on the same RFQ are 1.4362, 1.4410, 1.4404. Design caution: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
-
How should fabricators weld EN 10296-2 1.4462 tube on site?
- 1.4462 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 2205/duplex fillers; heat-input and interpass control to hold phase balance; mill seam +AT does not replace fabricator WPS. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
-
What tests should appear on the EN 10204 3.1 document for 1.4462?
- Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
-
What size range can SHH STEEL quote for EN 10296-2 1.4462?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4462 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: process and structural welded OD common in 2205 catalogues, typically +AT. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
Does commercial alias 2205 belong in the purchase-order H1?
- No. On steelspecs.com product pages the H1 is the steel number only. Use 2205 in body text and BOM notes, but lock EN 10296-2 and 1.4462 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
When should I choose duplex or Mo austenitic instead of 1.4462?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what duplex (austenitic-ferritic) practice can defend for the temperature and stress state. Caution for this number: restore solution anneal after hot work; do not leave duplex in deleterious precipitation windows; severe seawater crevices may still need superduplex or 6Mo Sister pointers: 1.4362, 1.4410, 1.4404. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
-
Is EN 10296-2 1.4462 suitable for heat-resisting furnace duty?
- Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4462 is filed as duplex (austenitic-ferritic). If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.
Conclusion
EN 10296-2 1.4462 (X2CrNiMoN22-5-3) is welded stainless tube for mechanical and general engineering — workhorse 2205 duplex welded tube for chloride SCC-resistant mechanical and general engineering duty. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4362, 1.4410, 1.4404. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.