EN 10296-2 1.4307 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4307 Welded Stainless Steel Tube

EN 10296-2 1.4307 / X2CrNi18-9 welded stainless general-purpose tube (304L), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 180 MPa, Rm min 470 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4307 / X2CrNi18-9 (304L — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4307 Welded Stainless Steel Tube

EN 10296-2:2005 (BS EN 10296-2:2005) is the European product standard for welded circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10217-7, and not for seamless general-purpose tube under EN 10297-2. Steel number 1.4307 is listed as X2CrNi18-9 in the austenitic corrosion-resisting set. If the purchase file still names only “304L welded tube,” EN 10296-2 1.4307 selects low-carbon X2CrNi18-9 under welded general-purpose acceptance — not PED pressure Part 7. Filler/shop note for 1.4307: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

SHH STEEL can produce and supply X2CrNi18-9 under EN 10296-2 1.4307 as welded tube for mechanical and general engineering — not as a silent dual of EN 10217-7 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Weld thread: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

On the shop floor people still say “304L tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4307, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum. Typical duties include food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”. Design caution: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb Family filing for 1.4307 is austenitic corrosion-resisting.

EN 10296-2 is welded product only for this series. When a seamless general-purpose twin is required, look to EN 10297-2 rather than forcing a seamless claim onto a 10296-2 order. When PED pressure welded acceptance is mandatory, use EN 10217-7 for the same chemistry family where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”.

Inside this welded general-purpose series, compare EN 10296-2 1.4301, EN 10296-2 1.4311, EN 10296-2 1.4306, EN 10296-2 1.4541. Hub: EN 10296-2. Pressure seamless sister (different acceptance): EN 10216-5 1.4307. ASTM/ASME related product pages (not interchangeable by default): A269 TP304L, A213 TP304L, A312 TP304L.

Chemical Composition of EN 10296-2 1.4307

Every 1.4307 heat under EN 10296-2 must meet the cast (ladle) analysis for X2CrNi18-9 in the austenitic corrosion-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Duty thread: low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum.

Use the cast table for 1.4307 as the contractual chemistry window for welded general-purpose duty — role reminder: low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum. Do not substitute a sister analysis from 1.4301, 1.4311, 1.4306, 1.4541 without rewriting the steel number on the order. Primary application sketch: food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”.

Steel C Si Mn P S Cr Ni N
1.4307 / X2CrNi18-9 ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.015 17.5–19.5 8.0–10.5 ≤0.11

Mechanical Properties of EN 10296-2 1.4307

Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4307 order. General-purpose Table values for this number read: Rp0.2 min 180 MPa, Rp1.0 min 215 MPa, Rm min 470 MPa, longitudinal elongation min 40%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Size context for 1.4307: broad welded mechanical and decorative OD×wall, W2A/W2R/WCA common for brighter OD.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 180 215 470 min 40 35 Yes

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4307 / X2CrNi18-9. Guideline solution/anneal band (Annex B): 1000–1100 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4307

EN 10296-2 does not offer a seamless route for 1.4307. Tube in X2CrNi18-9 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. Annex A process-route symbols for welded 1.4307 include W0 (as-welded), W1/W1A/W1R (hot-rolled strip routes), W2/W2A/W2R (cold-rolled strip routes), WCA/WCR (cold-worked recrystallised weld), and WG/WP (ground/polished). Bead-worked conditions append “b” (for example W2Ab). Caution thread: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb.

For austenitic 1.4307, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4307 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1000–1100 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”.

State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4307. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Caution thread: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb.

Dimensions and Tolerances for EN 10296-2 1.4307

Dimensional orders for 1.4307 name OD × wall, length tolerance, delivery condition, and the Annex A finish symbol. Exact cut lengths and special end preparations are by agreement. Broad welded mechanical and decorative od×wall, w2a/w2r/wca common for brighter od. Weld thread: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

Length supply for 1.4307 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Caution thread: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb.

Equivalent Grades for EN 10296-2 1.4307

Equivalence talk for 1.4307 starts with X2CrNi18-9: that is the EN steel name for welded general-purpose tube under this Part 2. Buyers who only write 304L still need the steel number and EN 10296-2 on the PO. Sister grades often quoted alongside this duty: 1.4301, 1.4311, 1.4306, 1.4541. Design caution stays: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb Family filing for 1.4307 is austenitic corrosion-resisting.

Heat Treatment and Delivery Condition for EN 10296-2 1.4307

Austenitic 1.4307 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1000–1100 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Role reminder while setting HT: low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum Filler/shop note for 1.4307: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

Hot-working temperature bands in Annex B for X2CrNi18-9 are guidance during further processing (for example hot bending). Cooling type matters — chase the rapid cool required for austenitic and duplex solution anneal; ferritic anneal practice differs. Duty thread: low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum.

Corrosion Resistance of EN 10296-2 1.4307

Corrosion behaviour of EN 10296-2 1.4307 tracks its austenitic corrosion-resisting balance: low carbon supports as-welded IGC resistance versus 1.4301; chromium-nickel passive film for aqueous and mild chemical media. This standard’s IGC column (where present) refers to EN ISO 3651-2 testing under the tabulated conditions — it is not a blanket warranty for every process medium. Design caution remains: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb Family filing for 1.4307 is austenitic corrosion-resisting.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4307 is filed as austenitic corrosion-resisting — pick tests that match that filing. Weld thread: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

Applications of EN 10296-2 1.4307 Tube

Typical field use for 304L-named welded tube under steel number 1.4307: food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”. Keep pressure seamless talk on EN 10216-5 pages when that standard is the regulatory home. Filler/shop note for 1.4307: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

Skip 1.4307 when the specification locks a different family — for example forcing ferritic 1.4307 into severe chloride process duty, or forcing a heat-resisting number into aqueous chloride service. Sister conversation inside EN 10296-2: 1.4301, 1.4311, 1.4306, 1.4541. Corrosion thread: low carbon supports as-welded IGC resistance versus 1.4301; chromium-nickel passive film for aqueous and mild chemical media.

Weldability of EN 10296-2 1.4307

Weldability of EN 10296-2 1.4307 covers both the mill longitudinal seam and downstream fabricator joints. Practical shop note: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints. Caution that shapes WPS choices: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb Primary application sketch: food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”.

For corrosive service after welding, confirm whether stabilisation, low carbon, duplex ferrite control, or post-weld solution anneal is required. Caution for this number: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb Primary application sketch: food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”.

Surface Finishes for EN 10296-2 1.4307

Interior Ra limits, electropolish, or special protection for X2CrNi18-9 fall under explicit order text. SHH STEEL can produce and supply pickled/descaled, bright-annealed, and polished 1.4307 when the mill can measure and report the finish. Weld thread: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

For 1.4307, export and coastal routes need extra wrap discipline on W*R/WCR/WG/WP finishes. Size context: broad welded mechanical and decorative OD×wall, W2A/W2R/WCA common for brighter OD. SHH STEEL confirms sleeve, paper, or plastic protection against the ordered Annex A symbol before dispatch.

Inspection and Testing for EN 10296-2 1.4307

SHH STEEL EN 10204 3.1 documents for 1.4307 report cast chemistry, tensile results, delivery condition, dimensions, and the Optional tests actually performed. We do not print a leak-test or NDT line unless that Option was executed. Caution thread: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb.

For X2CrNi18-9 under EN 10296-2, technological Options and IGC (where tabulated) belong on the enquiry checklist beside OD × wall. SHH STEEL correlates marking on 1.4307 bundles to the EN 10204 3.1 document so heat identity survives transit. Caution reminder: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb Filler/shop note for 1.4307: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

Packaging and Shipping for EN 10296-2 1.4307

SHH STEEL ships EN 10296-2 1.4307 in end-protected, size-sorted bundles or wooden crates with waterproof wrap on export routes. Descaled W1A/W2A engineering finishes still get caps and separators; carbon-steel strapping never sits bare on the stainless OD. Weld thread: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

For 1.4307, inland trucking may use lighter wrap than ocean freight, but end protection and heat-identity tags remain mandatory. Chloride-bearing road salt exposure on open flats is avoided for bright finishes. Duty thread: low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum.

For 1.4307, packing-list discipline matters when multiple sisters (1.4301, 1.4311, 1.4306, 1.4541) ship on the same vessel — wrong bundle cards create wrong field installs. SHH STEEL can produce and supply photographed mark sets when the EPC file demands them. Duty thread: low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10296-2 1.4307 as welded general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “304L tube” label on whatever is in the rack. We keep pressure talk honest: when PED welded pressure acceptance is required, we point you to EN 10217-7 for the same chemistry family where it exists. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”.

Grade advice for 1.4307 stays practical. If the duty needs a sister chemistry, we point to 1.4301, 1.4311, 1.4306, 1.4541. Design caution for this number: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb Contact the engineering desk with OD × wall, delivery condition, and medium notes before the cast is locked. Filler/shop note for 1.4307: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

Supply Capability

SHH STEEL can make and supply 304L-family chemistry only when the order locks EN 10296-2 and steel number 1.4307. Capability below is an RFQ map for X2CrNi18-9, not a promise that every OD×wall sits in a Shanghai rack tonight. Duty thread: low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4307 / X2CrNi18-9
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

Enquiry-oriented Stock / Available sizes map for EN 10296-2 1.4307 — not a frozen warehouse SKU list with tonnages. Availability tracks mill heats of X2CrNi18-9, strip/plate starting stock, and welding/finishing slots for the ordered Annex A symbol; send the OD × wall list, delivery-condition preference, and any Optional tests tied to food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”. Filler/shop note for 1.4307: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints.

Cut lengths, special ends, IGC Options, and dual enquiries against 1.4301, 1.4311, 1.4306, 1.4541 on the same size list are routine for 1.4307. Peer mill catalogues only sanity-check typical OD × wall bands — acceptance remains EN 10296-2 with dimensional agreements stated on the order. SHH STEEL can produce and supply trial lengths before a production heat when the project schedule allows. Use thread: food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”.

FAQ

What is EN 10296-2 1.4307 welded stainless steel tube used for?
EN 10296-2 1.4307 (X2CrNi18-9) is welded tube for mechanical and general engineering — food and beverage utilities, pharmaceutical water lines, instrumentation, architectural welded tube, and mechanical fabrications that still say “304L welded”. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum.
Is EN 10296-2 1.4307 the same as EN 10216-5 1.4307?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4307 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4307 / X2CrNi18-9?
Delivery framing for 1.4307 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1000–1100 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4307?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4307 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4307 compare with sister grades 1.4301, 1.4311, 1.4306?
1.4307 / X2CrNi18-9 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4301, 1.4311, 1.4306. Design caution: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4307 tube on site?
1.4307 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 308/308L-class fillers; low carbon in the base helps as-welded IGC but fabricator WPS, heat input, and purge still matter on site joints. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4307?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4307?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4307 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: broad welded mechanical and decorative OD×wall, W2A/W2R/WCA common for brighter OD. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 304L belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 304L in body text and BOM notes, but lock EN 10296-2 and 1.4307 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4307?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: Mo-free — chloride pitting remains the outdoor and process limiter; move to 1.4404 or duplex when chlorides and temperature climb Sister pointers: 1.4301, 1.4311, 1.4306. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4307 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4307 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4307 (X2CrNi18-9) is welded stainless tube for mechanical and general engineering — low-carbon 18-8 austenitic welded tube for general engineering where as-welded IGC resistance matters more than molybdenum. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4301, 1.4311, 1.4306. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X