EN 10296-2 1.4828 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4828 Welded Stainless Steel Tube

EN 10296-2 1.4828 / X15CrNiSi20-12 welded stainless general-purpose tube (309Si / Si-bearing 20-12), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 230 MPa, Rm min 550 MPa, A long. min 30%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4828 / X15CrNiSi20-12 (309Si / Si-bearing 20-12 — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4828 Welded Stainless Steel Tube

EN 10296-2:2005 (BS EN 10296-2:2005) is the European product standard for welded circular stainless and heat-resisting steel tubes for mechanical and general engineering purposes — not for pressure equipment under EN 10217-7, and not for seamless general-purpose tube under EN 10297-2. Steel number 1.4828 is listed as X15CrNiSi20-12 in the austenitic heat-resisting set. When the duty is oxidising heat — not aqueous process — EN 10296-2 1.4828 puts X15CrNiSi20-12 on welded general-purpose tube. Primary application sketch: furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry.

SHH STEEL can make and supply EN 10296-2 1.4828 / X15CrNiSi20-12 as welded general-purpose tube across furnace-adjacent welded OD on +AT heat-resisting routes, annealed or solution annealed as the grade tables and order require, documented on EN 10204 3.1 MTCs tied to cast analysis and mechanical results. Family filing for 1.4828 is austenitic heat-resisting.

On the shop floor people still say “309Si / Si-bearing 20-12 tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4828, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty. Typical duties include furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry. Design caution: heat-resisting first — not a first choice for aqueous chloride process duty; carbon up to 0.20% means as-welded aqueous IGC talk does not apply the same way as L grades Filler/shop note for 1.4828: heat-resisting austenitic fillers matched to Si/Cr; control restraint on fabricator joints in thick sections.

EN 10296-2 is welded product only for this series. When a seamless general-purpose twin is required, look to EN 10297-2 rather than forcing a seamless claim onto a 10296-2 order. When PED pressure welded acceptance is mandatory, use EN 10217-7 for the same chemistry family where it exists. Preferred dimensions commonly reference EN ISO 1127 practice agreed at enquiry. Use thread: furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry.

Inside this welded general-purpose series, compare EN 10296-2 1.4833, EN 10296-2 1.4818, EN 10296-2 1.4845. Hub: EN 10296-2.

Chemical Composition of EN 10296-2 1.4828

Every 1.4828 heat under EN 10296-2 must meet the cast (ladle) analysis for X15CrNiSi20-12 in the austenitic heat-resisting chemical tables. Product analysis may be agreed as an Option with permissible deviations as tabulated in the standard. SHH STEEL reports actual cast values on the EN 10204 document and does not sell unproven “equivalent” chemistry under this steel number. Use thread: furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry.

Chemical limits for 1.4828 / X15CrNiSi20-12 under EN 10296-2 appear in the table underneath. Source priority is BSSA’s EN 10296-2 article cross-checked to the 2005 grade list. If your client specification cites a different edition footnote for 309Si / Si-bearing 20-12-family welded tube, send it before the heat is melted. Size context for 1.4828: furnace-adjacent welded OD on +AT heat-resisting routes.

Steel C Si Mn P S Cr Ni N
1.4828 / X15CrNiSi20-12 ≤0.20 1.50–2.50 ≤2.00 ≤0.045 ≤0.015 19.0–21.0 11.0–13.0 ≤0.11

Mechanical Properties of EN 10296-2 1.4828

Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4828 order. General-purpose Table values for this number read: Rp0.2 min 230 MPa, Rp1.0 min 270 MPa, Rm min 550 MPa, longitudinal elongation min 30%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Use thread: furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 230 270 550 min 30 30 N/A

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4828 / X15CrNiSi20-12. Guideline solution/anneal band (Annex B): 1050–1150 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4828

EN 10296-2 does not offer a seamless route for 1.4828. Tube in X15CrNiSi20-12 is made by longitudinal welding of strip or plate edges, then solution annealed (+AT) to meet Table 5 heat-resisting mechanical floors. For 1.4828, SHH STEEL aligns the Annex A symbol to the duty: W0 for as-welded economy, W1A/W2A for descaled engineering tube, W2R/WCR for brighter OD, and WG/WP when a measured roughness target is part of the order text. Size context for 1.4828: furnace-adjacent welded OD on +AT heat-resisting routes.

Austenitic heat-resisting 1.4828 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1050–1150 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. High-temperature service still needs fabricator WPS discipline on site joints after the mill seam. Size context for 1.4828: furnace-adjacent welded OD on +AT heat-resisting routes.

When dual documentation against EN 10217-7 is requested for the same 1.4828 chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 1.4828: furnace-adjacent welded OD on +AT heat-resisting routes.

Dimensions and Tolerances for EN 10296-2 1.4828

Order EN 10296-2 1.4828 by outside diameter D and wall thickness T for steel name X15CrNiSi20-12. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Furnace-adjacent welded od on +at heat-resisting routes. Weld thread: heat-resisting austenitic fillers matched to Si/Cr; control restraint on fabricator joints in thick sections.

Length supply for 1.4828 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Weld thread: heat-resisting austenitic fillers matched to Si/Cr; control restraint on fabricator joints in thick sections.

Equivalent Grades for EN 10296-2 1.4828

Do not treat ASTM welded or seamless pages as drop-in equals for EN 10296-2 1.4828 / X15CrNiSi20-12. Wall bases, mechanical tables, and optional tests differ. Body alias 309Si / Si-bearing 20-12 is fine in BOM notes; H1 and order line stay on the steel number. Compare 1.4833, 1.4818, 1.4845 when the medium outgrows this analysis. Duty thread: Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty.

Heat Treatment and Delivery Condition for EN 10296-2 1.4828

Austenitic heat-resisting 1.4828 mechanical floors in Table 5 assume solution-annealed (+AT) delivery. Public Annex B guidance places solution annealing near 1050–1150 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Role reminder while setting HT: Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty Primary application sketch: furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry.

Annex B is informative guidance for heat treatment during fabrication and hot working — it does not rewrite Table mechanical floors. After hot bending or heavy cold work on 1.4828, restore the delivery condition agreed on the order before corrosive or load-bearing service. Weld thread: heat-resisting austenitic fillers matched to Si/Cr; control restraint on fabricator joints in thick sections.

Corrosion Resistance of EN 10296-2 1.4828

309Si / Si-bearing 20-12-family marketing claims do not override EN 10296-2 tabulated IGC notes for 1.4828. Corrosion thread: Si-enhanced oxidation resistance at elevated temperature in oxidising atmospheres; aqueous IGC columns are N/A for this heat-resisting filing. Move to sisters 1.4833, 1.4818, 1.4845 when the medium outgrows this analysis.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4828 is filed as austenitic heat-resisting — pick tests that match that filing. Caution thread: heat-resisting first — not a first choice for aqueous chloride process duty; carbon up to 0.20% means as-welded aqueous IGC talk does not apply the same way as L grades.

Applications of EN 10296-2 1.4828 Tube

Typical field use for 309Si / Si-bearing 20-12-named welded tube under steel number 1.4828: furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry. Keep pressure seamless talk on EN 10216-5 pages when that standard is the regulatory home. Filler/shop note for 1.4828: heat-resisting austenitic fillers matched to Si/Cr; control restraint on fabricator joints in thick sections.

It is the wrong first choice when a seamless product form is mandatory (use EN 10297-2 or EN 10216-5 as applicable), when PED pressure welded acceptance is locked to EN 10217-7 alone, or when the medium clearly needs a sister such as 1.4833. Use thread: furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry.

Weldability of EN 10296-2 1.4828

Even though 1.4828 is already a welded tube product, site joints still need a WPS matched to X15CrNiSi20-12. Filler and heat-input guidance: heat-resisting austenitic fillers matched to Si/Cr; control restraint on fabricator joints in thick sections. Alias on the shop traveler may say 309Si / Si-bearing 20-12; the WPS should cite the steel number. Family filing for 1.4828 is austenitic heat-resisting.

When IGC testing of welded coupons is specified, align the EN ISO 3651-2 method with the grade’s tabulated expectations and the purchaser’s Option list. SHH STEEL can coordinate mill-supplied weld data only when it is part of the agreed scope. Corrosion thread: Si-enhanced oxidation resistance at elevated temperature in oxidising atmospheres; aqueous IGC columns are N/A for this heat-resisting filing.

Surface Finishes for EN 10296-2 1.4828

For 1.4828, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Corrosion thread: Si-enhanced oxidation resistance at elevated temperature in oxidising atmospheres; aqueous IGC columns are N/A for this heat-resisting filing.

Special measures to protect 1.4828 / X15CrNiSi20-12 during delivery or storage may be agreed at enquiry. Bright and polished tubes take sleeve or paper wrap; descaled engineering finishes still need end caps and dry bundling so chloride-bearing dirt does not sit on the OD in transit — especially important for 309Si / Si-bearing 20-12-family decorative or hygienic OD. Duty thread: Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty.

Inspection and Testing for EN 10296-2 1.4828

Specific inspection applies to EN 10296-2 1.4828 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Duty thread: Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty.

For X15CrNiSi20-12 under EN 10296-2, technological Options and IGC (where tabulated) belong on the enquiry checklist beside OD × wall. SHH STEEL correlates marking on 1.4828 bundles to the EN 10204 3.1 document so heat identity survives transit. Caution reminder: heat-resisting first — not a first choice for aqueous chloride process duty; carbon up to 0.20% means as-welded aqueous IGC talk does not apply the same way as L grades Family filing for 1.4828 is austenitic heat-resisting.

Packaging and Shipping for EN 10296-2 1.4828

Export packing for 1.4828 / X15CrNiSi20-12 keeps heat identities intact: tags and bundle cards carry the cast/code that matches the EN 10204 3.1 document. Polished and bright tubes are sleeved; heavier descaled bundles use spacers to stop fretting in transit. Duty thread: Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty.

When cut lengths and special ends are part of the 1.4828 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Size context for 1.4828: furnace-adjacent welded OD on +AT heat-resisting routes.

Ocean-freight wrap for X15CrNiSi20-12 repeats cast/code on tags inside and outside the wrap. Duty thread for why identity matters: furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry. Family filing for 1.4828 is austenitic heat-resisting.

Why Choose SHH STEEL

SHH STEEL can produce and supply EN 10296-2 1.4828 as welded general-purpose tube — heat-treated to the ordered delivery condition, tested to the Options you name, and documented on EN 10204 3.1 certificates — not as a generic “309Si / Si-bearing 20-12 tube” label on whatever is in the rack. We keep pressure talk honest: when PED welded pressure acceptance is required, we point you to EN 10217-7 for the same chemistry family where it exists. Duty thread: Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty.

SHH STEEL will not stretch X15CrNiSi20-12 into a medium it cannot defend. Typical right-fit duties: furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry. When those duties slip toward a sister, we say so before the quote hardens. Family filing for 1.4828 is austenitic heat-resisting.

Supply Capability

SHH STEEL can produce and supply EN 10296-2 1.4828 welded stainless steel tube against the edition, delivery condition, Annex A symbol, and Options named on your enquiry. The capability table and Stock / Available sizes enquiry map below frame a first-pass size list for X15CrNiSi20-12 — role: Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty. Filler/shop note for 1.4828: heat-resisting austenitic fillers matched to Si/Cr; control restraint on fabricator joints in thick sections.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4828 / X15CrNiSi20-12
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

Enquiry-oriented Stock / Available sizes map for EN 10296-2 1.4828 — not a frozen warehouse SKU list with tonnages. Availability tracks mill heats of X15CrNiSi20-12, strip/plate starting stock, and welding/finishing slots for the ordered Annex A symbol; send the OD × wall list, delivery-condition preference, and any Optional tests tied to furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry. Filler/shop note for 1.4828: heat-resisting austenitic fillers matched to Si/Cr; control restraint on fabricator joints in thick sections.

Trial lengths of 1.4828 / X15CrNiSi20-12 help fabricators prove forming and weld procedures before a production heat. Sisters often sampled on the same RFQ: 1.4833, 1.4818, 1.4845. SHH STEEL can produce and supply those trials when strip slots allow. Caution thread: heat-resisting first — not a first choice for aqueous chloride process duty; carbon up to 0.20% means as-welded aqueous IGC talk does not apply the same way as L grades.

FAQ

What is EN 10296-2 1.4828 welded stainless steel tube used for?
EN 10296-2 1.4828 (X15CrNiSi20-12) is welded tube for mechanical and general engineering — furnace parts, heat shields, and high-temperature mechanical welded tubing in oxidising gases naming 309Si-class chemistry. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty.
Is EN 10296-2 1.4828 the same as EN 10216-5 1.4828?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4828 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4828 / X15CrNiSi20-12?
Delivery framing for 1.4828 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1050–1150 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4828?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4828 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4828 compare with sister grades 1.4833, 1.4818, 1.4845?
1.4828 / X15CrNiSi20-12 is filed as austenitic heat-resisting. Typical sisters discussed on the same RFQ are 1.4833, 1.4818, 1.4845. Design caution: heat-resisting first — not a first choice for aqueous chloride process duty; carbon up to 0.20% means as-welded aqueous IGC talk does not apply the same way as L grades Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4828 tube on site?
1.4828 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: heat-resisting austenitic fillers matched to Si/Cr; control restraint on fabricator joints in thick sections. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4828?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4828?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4828 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: furnace-adjacent welded OD on +AT heat-resisting routes. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 309Si / Si-bearing 20-12 belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 309Si / Si-bearing 20-12 in body text and BOM notes, but lock EN 10296-2 and 1.4828 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4828?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic heat-resisting practice can defend for the temperature and stress state. Caution for this number: heat-resisting first — not a first choice for aqueous chloride process duty; carbon up to 0.20% means as-welded aqueous IGC talk does not apply the same way as L grades Sister pointers: 1.4833, 1.4818, 1.4845. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4828 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4828 is filed as austenitic heat-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4828 (X15CrNiSi20-12) is welded stainless tube for mechanical and general engineering — Si-bearing 20Cr-12Ni heat-resisting welded tube for oxidising elevated-temperature mechanical duty. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4833, 1.4818, 1.4845. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X