EN 10296-2 1.4318 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4318 Welded Stainless Steel Tube

EN 10296-2 1.4318 / X2CrNiN18-7 welded stainless general-purpose tube (301LN / N-strengthened lean 18-7), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 330 MPa, Rm min 630 MPa, A long. min 45%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
Grade
1.4318 / X2CrNiN18-7 (301LN / N-strengthened lean 18-7 — body alias)
Standard
EN 10296-2
Product form
Welded tube for mechanical and general engineering purposes, delivery +AT as applicable
Size
~6–219 mm OD × ~0.5–12.7 mm wall within family practice; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10296-2 1.4318 Welded Stainless Steel Tube

EN 10296-2 covers welded stainless tube for mechanical and general engineering (i.e. not pressure). Within that scope, 1.4318 is the austenitic corrosion-resisting grade X2CrNiN18-7, commercially discussed as 301LN / N-strengthened lean 18-7. When the stress floor needs more than 1.4307 without jumping to duplex, EN 10296-2 1.4318 puts N-strengthened X2CrNiN18-7 on a welded general-purpose MTC. Filler/shop note for 1.4318: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2.

SHH STEEL can produce and supply X2CrNiN18-7 under EN 10296-2 1.4318 as welded tube for mechanical and general engineering — not as a silent dual of EN 10217-7 pressure acceptance unless that standard is also ordered. Typical supply includes Annex A finish symbols, cut lengths by agreement, and EN 10204 3.1 certification. Duty thread: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum.

On the shop floor people still say “301LN / N-strengthened lean 18-7 tube,” yet that commercial alias does not select cast chemistry, welded process route, delivery-condition heat treatment, or optional tests. The purchase order has to name EN 10296-2, 1.4318, the Annex A process/surface symbol, the delivery condition (+AR / +A / +AT as applicable), and any Options so the mill applies the correct analysis, forming/welding route, heat treatment, mechanical floors, and marking. This number’s job on welded general-purpose duty is: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum. Typical duties include structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7. Design caution: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty Primary application sketch: structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7.

Do not treat an EN 10296-2 1.4318 MTC as automatic clearance for pressure equipment — EN 10217-7 is the welded pressure home. Likewise, seamless pressure tube lives under EN 10216-5 and seamless general-purpose under EN 10297-2. Match the product standard to the duty before dual-marking talk begins. Corrosion thread: nitrogen raises strength and helps austenite stability; aqueous corrosion still tracks Mo-free 18-8 practice.

Inside this welded general-purpose series, compare EN 10296-2 1.4307, EN 10296-2 1.4311, EN 10296-2 1.4301. Hub: EN 10296-2. Related pressure seamless chemistry page: EN 10216-5 1.4307.

Chemical Composition of EN 10296-2 1.4318

Buying 301LN / N-strengthened lean 18-7-family welded tube without locking 1.4318 invites silent chemistry drift. Under EN 10296-2 the cast must satisfy X2CrNiN18-7; highlight elements for this grade include C ≤0.030, Cr 16.5–18.5, Ni 6.0–8.0, N 0.10–0.20, Si ≤1.00, S ≤0.015. Options for product analysis are agreed at enquiry when the purchaser wants them on the certificate. Size context for 1.4318: commodity-to-structural welded OD on W1A/W2A/WCA routes with +AT when purchaser specifies solution anneal.

The table below reproduces public BSSA EN 10296-2 chemical limits for 1.4318 / X2CrNiN18-7, cross-checked against the EN 10296-2:2005 grade list. Values are maximum unless a range is shown. Commercial talk still says 301LN / N-strengthened lean 18-7, but only the steel-number cast windows below belong on the MTC for this austenitic corrosion-resisting welded tube. Caution thread: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty.

Steel C Si Mn P S Cr Ni N
1.4318 / X2CrNiN18-7 ≤0.030 ≤1.00 ≤2.00 ≤0.045 ≤0.015 16.5–18.5 6.0–8.0 0.10–0.20

Mechanical Properties of EN 10296-2 1.4318

Do not borrow EN 10217-7 pressure mechanical rows for an EN 10296-2 1.4318 order. General-purpose Table values for this number read: Rp0.2 min 330 MPa, Rp1.0 min 370 MPa, Rm min 630 MPa, longitudinal elongation min 45%. State +AR versus +A/+AT on the purchase order so marking and the MTC match the tested condition. Size context for 1.4318: commodity-to-structural welded OD on W1A/W2A/WCA routes with +AT when purchaser specifies solution anneal.

Delivery condition Rp0.2 min (MPa) Rp1.0 min (MPa) Rm (MPa) A long. min (%) A trans. min (%) IGC
+AT 330 370 630 min 45 45 Yes

Ambient values from EN 10296-2:2005 Tables 4–5 for 1.4318 / X2CrNiN18-7. Guideline solution/anneal band (Annex B): 1020–1100 °C; cooling: water, air or gas.

Welded Tube Manufacture for EN 10296-2 1.4318

EN 10296-2 does not offer a seamless route for 1.4318. Tube in X2CrNiN18-7 is made by longitudinal automatic welding across abutting strip or plate edges, with or without filler as agreed, on one of the Table A.1 process routes, then heat-treated to the ordered delivery condition. For 1.4318, SHH STEEL aligns the Annex A symbol to the duty: W0 for as-welded economy, W1A/W2A for descaled engineering tube, W2R/WCR for brighter OD, and WG/WP when a measured roughness target is part of the order text. Weld thread: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2.

For austenitic 1.4318, cold-rolled strip routes (W2/W2A/W2R) are the usual path to tighter OD and surface control; hot-rolled strip routes (W1/W1A/W1R) cover other starting stock. WCA/WCR add cold work and recrystallised weld metal when bead appearance matters. Austenitic 1.4318 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1020–1100 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Caution thread: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty.

State leak-tightness, flattening, drift expanding, bend, or NDT Options explicitly for 1.4318. General-purpose welded acceptance is not identical to EN 10217-7 pressure regimes; copy the Options list you need onto the EN 10296-2 order. Duty thread: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum.

Dimensions and Tolerances for EN 10296-2 1.4318

Order EN 10296-2 1.4318 by outside diameter D and wall thickness T for steel name X2CrNiN18-7. Preferred size practice commonly follows EN ISO 1127 classes agreed at enquiry. Mass per unit length uses stainless densities — not the carbon-steel 7.85 kg/dm³ default. Commodity-to-structural welded od on w1a/w2a/wca routes with +at when purchaser specifies solution anneal. Duty thread: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum.

Length supply for 1.4318 may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so bright or polished finishes are not marked in transit. Weld thread: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2.

Equivalent Grades for EN 10296-2 1.4318

Equivalence talk for 1.4318 starts with X2CrNiN18-7: that is the EN steel name for welded general-purpose tube under this Part 2. Buyers who only write 301LN / N-strengthened lean 18-7 still need the steel number and EN 10296-2 on the PO. Sister grades often quoted alongside this duty: 1.4307, 1.4311, 1.4301. Design caution stays: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty Family filing for 1.4318 is austenitic corrosion-resisting.

Heat Treatment and Delivery Condition for EN 10296-2 1.4318

Austenitic 1.4318 is delivered as-welded (+AR) or solution annealed (+AT) as the purchaser specifies. Corrosive and hygienic duties usually lock +AT. Public Annex B guidance places solution annealing near 1020–1100 °C with water, air or gas cooling — fabricator HT after hot work should chase the lower end of the band when further processing applies. Role reminder while setting HT: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum Primary application sketch: structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7.

For 1.4318, purchasers who need verified IGC after fabrication should say so with the applicable Option and method (EN ISO 3651-2 framing). Mill +AT or +A of the tube does not automatically clear a fabricator’s as-welded joint without procedure control. Duty thread: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum.

Corrosion Resistance of EN 10296-2 1.4318

For 1.4318 / X2CrNiN18-7, read corrosion through the austenitic corrosion-resisting lens rather than a generic “stainless” slogan. Plain-language summary: nitrogen raises strength and helps austenite stability; aqueous corrosion still tracks Mo-free 18-8 practice. IGC Options follow EN ISO 3651-2 where the tables say Yes — and still do not replace medium-specific design. Caution: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty Filler/shop note for 1.4318: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2.

For heat-resisting grades, oxidation and carburisation resistance dominate over aqueous IGC talk; for corrosion-resisting grades, aqueous and chemical media dominate. 1.4318 is filed as austenitic corrosion-resisting — pick tests that match that filing. Weld thread: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2.

Applications of EN 10296-2 1.4318 Tube

Applications of EN 10296-2 1.4318 tube centre on mechanical, decorative, and general engineering rather than PED pressure shells: structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7. Role summary: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum. When the same chemistry is required as pressure seamless tube, open the EN 10216-5 sister page where that steel number exists and is live. Primary application sketch: structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7.

Skip 1.4318 when the specification locks a different family — for example forcing ferritic 1.4318 into severe chloride process duty, or forcing a heat-resisting number into aqueous chloride service. Sister conversation inside EN 10296-2: 1.4307, 1.4311, 1.4301. Caution thread: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty.

Weldability of EN 10296-2 1.4318

Weldability of EN 10296-2 1.4318 covers both the mill longitudinal seam and downstream fabricator joints. Practical shop note: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2. Caution that shapes WPS choices: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty Filler/shop note for 1.4318: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2.

Filler selection should match or over-alloy the base X2CrNiN18-7 chemistry as the WPS demands. Heat input, interpass temperature, and shielding practice follow the family — austenitic, ferritic, duplex, or heat-resisting — not a single shop habit. Caution thread: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty.

Surface Finishes for EN 10296-2 1.4318

For 1.4318, pick W2R/WCR when residual scale is unacceptable on visible mechanical or decorative assemblies; pick WG/WP only with a written OD/ID scope and roughness target. Descaled W1A/W2A remains the workhorse engineering finish for many duties. Corrosion thread: nitrogen raises strength and helps austenite stability; aqueous corrosion still tracks Mo-free 18-8 practice.

Special measures to protect 1.4318 / X2CrNiN18-7 during delivery or storage may be agreed at enquiry. Bright and polished tubes take sleeve or paper wrap; descaled engineering finishes still need end caps and dry bundling so chloride-bearing dirt does not sit on the OD in transit — especially important for 301LN / N-strengthened lean 18-7-family decorative or hygienic OD. Size context for 1.4318: commodity-to-structural welded OD on W1A/W2A/WCA routes with +AT when purchaser specifies solution anneal.

Inspection and Testing for EN 10296-2 1.4318

Specific inspection applies to EN 10296-2 1.4318 as agreed on the order. Cast analysis is reported per heat. Room-temperature tensile testing follows the standard’s test-unit rules for the ordered delivery condition. Dimensional checks cover OD, wall, length, and the agreed tolerance class. Use thread: structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7.

Inspection intensity on 1.4318 tracks Options — leak, flattening, drift expanding, bend, NDT, IGC — not a silent EN 10217-7 pressure package. Role context for what those Options protect: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum. Filler/shop note for 1.4318: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2.

Packaging and Shipping for EN 10296-2 1.4318

Finished EN 10296-2 1.4318 (X2CrNiN18-7) welded tube is packed with end caps or plugs matched to the OD, sorted into same-size bundles or crates, and wrapped for weather when the route is ocean freight. Bright-annealed and polished OD (W*R/WCR/WG/WP) take sleeve or paper wrap so handling marks do not become rejectable scratches. Use thread: structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7.

When cut lengths and special ends are part of the 1.4318 order, those pieces are segregated and capped before wrap so warehouse mixing cannot silently swap walls or finishes. Packing lists cross-reference heat numbers to bundle IDs. Duty thread: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum.

Export packing lists for 1.4318 / X2CrNiN18-7 cross-reference heat numbers to bundle IDs so the EN 10204 3.1 document matches without opening every crate. SHH STEEL aligns packaging with the order text before dispatch and can photograph bundle marks on request for project files that still say 301LN / N-strengthened lean 18-7 in the email subject. Weld thread: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2.

Why Choose SHH STEEL

SHH STEEL can produce and supply X2CrNiN18-7 as EN 10296-2 1.4318 welded tube with honest scope boundaries. General engineering welded acceptance is what this page sells; pressure welded, seamless pressure, and seamless general-purpose sisters are separate standards with separate MTCs. Caution thread: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty.

SHH STEEL will not stretch X2CrNiN18-7 into a medium it cannot defend. Typical right-fit duties: structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7. When those duties slip toward a sister, we say so before the quote hardens. Primary application sketch: structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7.

Supply Capability

Supply capability for 1.4318 / X2CrNiN18-7 is enquiry-led: SHH STEEL can produce and supply welded general-purpose tube with the Annex A finish and +AR/+A/+AT condition you name. Size hint: commodity-to-structural welded OD on W1A/W2A/WCA routes with +AT when purchaser specifies solution anneal. Primary application sketch: structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7.

Item Capability
Standard EN 10296-2:2005 welded general-purpose
Steel 1.4318 / X2CrNiN18-7
Product form Welded tube (W0 / W1A / W2A / W2R / WCA / WCR / WG / WP)
Delivery condition +AT
Documents EN 10204 3.1 (Options as ordered)
Typical enquiry OD ~6–219 mm (other by agreement)
Typical enquiry wall ~0.5–12.7 mm within welded family practice (other by agreement)

Stock / Available sizes

For X2CrNiN18-7, tell us which Annex A symbol and whether +AT (or +A/+AR) is locked before we hold strip. Caution that shapes size choice: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty Filler/shop note for 1.4318: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2.

Cut lengths, special ends, IGC Options, and dual enquiries against 1.4307, 1.4311, 1.4301 on the same size list are routine for 1.4318. Peer mill catalogues only sanity-check typical OD × wall bands — acceptance remains EN 10296-2 with dimensional agreements stated on the order. SHH STEEL can produce and supply trial lengths before a production heat when the project schedule allows. Size context for 1.4318: commodity-to-structural welded OD on W1A/W2A/WCA routes with +AT when purchaser specifies solution anneal.

FAQ

What is EN 10296-2 1.4318 welded stainless steel tube used for?
EN 10296-2 1.4318 (X2CrNiN18-7) is welded tube for mechanical and general engineering — structural-adjacent welded mechanical tube, higher-design-stress utility lines, and orders that name 301LN / X2CrNiN18-7. It is not automatically PED pressure tube; when pressure seamless acceptance is mandatory, specify EN 10216-5 for the same chemistry where listed; when pressure welded acceptance is mandatory, specify EN 10217-7 where listed. Role summary: N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum.
Is EN 10296-2 1.4318 the same as EN 10216-5 1.4318?
Chemistry families may overlap, but acceptance differs. EN 10296-2 is welded general-purpose / mechanical engineering; EN 10216-5 is seamless pressure. An EN 10296-2 MTC for 1.4318 does not clear PED pressure duties by itself. Dual orders must satisfy each standard’s mechanical and test regime.
What delivery condition applies to 1.4318 / X2CrNiN18-7?
Delivery framing for 1.4318 is +AT under the EN 10296-2 family tables. Guideline heat-treatment temperatures sit in Annex B near 1020–1100 °C with water, air or gas cooling. State the delivery condition on the purchase order so marking and the MTC match.
What Annex A finishes can SHH STEEL supply for 1.4318?
SHH STEEL can produce and supply W0, W1A, W2A, W2R, WCA, WCR, WG, and WP routes for EN 10296-2 1.4318 when the mill can meet the ordered surface. Descaled HFD/CFD covers most engineering duties; CFA is bright annealed; CFG/CFP need a written OD/ID roughness scope. Carbon-steel strapping never contacts the stainless OD.
How does 1.4318 compare with sister grades 1.4307, 1.4311, 1.4301?
1.4318 / X2CrNiN18-7 is filed as austenitic corrosion-resisting. Typical sisters discussed on the same RFQ are 1.4307, 1.4311, 1.4301. Design caution: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty Pick the sister when the medium or strength floor outgrows this number rather than stretching surface finish alone.
How should fabricators weld EN 10296-2 1.4318 tube on site?
1.4318 already has a mill longitudinal weld; fabricator circumferential and attachment welds still need a WPS. Shop guidance: 308L-class fillers common; control heat input and ferrite balance on fabricator joints; mill longitudinal weld already present under EN 10296-2. Mill heat treatment of the welded tube does not replace qualified procedures on site joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or PWHT as applicable.
What tests should appear on the EN 10204 3.1 document for 1.4318?
Expect cast analysis, room-temperature tensile results for the ordered delivery condition, dimensions, and every Optional test actually performed (leak, hydrostatic, eddy current, ultrasonic, IGC). SHH STEEL does not print surrogate NDT lines. EN 10296-2 Options are not identical to EN 10216-5 TC1/TC2 pressure categories.
What size range can SHH STEEL quote for EN 10296-2 1.4318?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 1.4318 — commonly instrumentation through mid-process sizes, with heavier walls by agreement. Size context: commodity-to-structural welded OD on W1A/W2A/WCA routes with +AT when purchaser specifies solution anneal. Send the OD × wall list, Annex A symbol, and delivery condition for a firm acknowledgement. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
Does commercial alias 301LN / N-strengthened lean 18-7 belong in the purchase-order H1?
No. On steelspecs.com product pages the H1 is the steel number only. Use 301LN / N-strengthened lean 18-7 in body text and BOM notes, but lock EN 10296-2 and 1.4318 on the order line so cast analysis, delivery condition, and Options are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
When should I choose duplex or Mo austenitic instead of 1.4318?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic corrosion-resisting practice can defend for the temperature and stress state. Caution for this number: lean Ni and Mo-free chemistry — chloride pitting and SCC margins sit below 316L and duplex; do not stretch it into seawater process duty Sister pointers: 1.4307, 1.4311, 1.4301. SHH STEEL will not invent PREN marketing digits — bring the medium data and we will map chemistry honestly.
Is EN 10296-2 1.4318 suitable for heat-resisting furnace duty?
Only the heat-resisting grades in Table 9 are first-choice furnace numbers. 1.4318 is filed as austenitic corrosion-resisting. If you need oxidising heat service, confirm whether 1.4828 / 1.4835 / 1.4833 / 1.4845 / 1.4818 / 1.4854 is the intended family before ordering a corrosion-resisting analysis. Conversely, do not force a heat-resisting number into aqueous chloride process duty without review.

Conclusion

EN 10296-2 1.4318 (X2CrNiN18-7) is welded stainless tube for mechanical and general engineering — N-strengthened lean austenitic welded tube for higher proof strength than 304L without adding molybdenum. SHH STEEL can produce and supply it with the Annex A finish, delivery condition, and Optional tests named on your enquiry, documented on EN 10204 3.1 certificates. Sister grades often discussed alongside this number include 1.4307, 1.4311, 1.4301. For pressure seamless acceptance of the same chemistry family, see EN 10216-5 where listed; for pressure welded, see EN 10217-7 when published. Email admin@steelspecs.com with OD × wall, delivery condition, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response