Product Showcase
EN 10296-2 Stainless Steel Products
SHH STEEL offers EN 10296-2-compliant 304/316 stainless steel tubes. EN 10296-2 specifies welded stainless steel tubes for general purposes, ideal for mechanical, decorative, and structural applications. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
EN 10296-2 1.4435 Welded Stainless Steel Tube
EN 10296-2 1.4435 / X2CrNiMo18-14-3 welded stainless general-purpose tube (316L high-Ni/Mo), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 190 MPa, Rm min 490 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4436 Welded Stainless Steel Tube
EN 10296-2 1.4436 / X3CrNiMo17-13-3 welded stainless general-purpose tube (316 high-Mo), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 205 MPa, Rm min 510 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4429 Welded Stainless Steel Tube
EN 10296-2 1.4429 / X2CrNiMoN17-13-3 welded stainless general-purpose tube (316LN), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 295 MPa, Rm min 580 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4432 Welded Stainless Steel Tube
EN 10296-2 1.4432 / X2CrNiMo17-12-3 welded stainless general-purpose tube (316L high-Mo (2.5–3.0)), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 190 MPa, Rm min 490 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4571 Welded Stainless Steel Tube
EN 10296-2 1.4571 / X6CrNiMoTi17-12-2 welded stainless general-purpose tube (316Ti), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 210 MPa, Rm min 510 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4401 Welded Stainless Steel Tube
EN 10296-2 1.4401 / X5CrNiMo17-12-2 welded stainless general-purpose tube (316), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 205 MPa, Rm min 510 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4404 Welded Stainless Steel Tube
EN 10296-2 1.4404 / X2CrNiMo17-12-2 welded stainless general-purpose tube (316L), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 190 MPa, Rm min 490 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4550 Welded Stainless Steel Tube
EN 10296-2 1.4550 / X6CrNiNb18-10 welded stainless general-purpose tube (347), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 205 MPa, Rm min 510 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4541 Welded Stainless Steel Tube
EN 10296-2 1.4541 / X6CrNiTi18-10 welded stainless general-purpose tube (321), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 200 MPa, Rm min 500 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4301 Welded Stainless Steel Tube
EN 10296-2 1.4301 / X5CrNi18-10 welded stainless general-purpose tube (304), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 195 MPa, Rm min 500 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4311 Welded Stainless Steel Tube
EN 10296-2 1.4311 / X2CrNiN18-10 welded stainless general-purpose tube (304LN), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 270 MPa, Rm min 550 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More -
EN 10296-2 1.4306 Welded Stainless Steel Tube
EN 10296-2 1.4306 / X2CrNi19-11 welded stainless general-purpose tube (304L high-Ni), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 180 MPa, Rm min 460 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.View More
EN 10296-2 Stainless Steel Products
Stainless Steel Pipes and Tubes
SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.
Stainless Steel Pipes and Tubes