Side view of stacked GB/T 19879 Q390GJE building steel plates at SHH STEEL

GB/T 19879 Q390GJE Building Steel Plate Supplier

GB/T 19879 Q390GJE is high-performance building structure steel plate with 390 MPa minimum yield, a 390 – 510 MPa yield window, yield ratio ≤0.83 and 47 J Charpy impact at −40°C. SHH STEEL supplies Q390GJE mill-direct, 6 mm – 150 mm, with Z15, Z25 or Z35 options and full heat and product analysis.
Keywords
Q390GJE, Q390GJE steel plate, GB/T 19879 Q390GJE, Q390GJ-E, Q390GJEZ15, Q390GJEZ25, Q390GJEZ35, Q390GJ, building structure steel plate, Q390GJE supplier
Equivalent Grades
GB/T 19879 Q390GJE / GB/T 1591 Q390NE or Q390ME (no yield cap) / EN 10025 S420 (next step up; no S390) / ASTM A572 Gr.55 (380 MPa) / JIS G3106 SM520 — Material Specification: GB/T 19879-2023 (supersedes GB/T 19879-2015) — Delivery: CR, NR, N, NT, TMCP or TMCP+T; −40°C impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q390GJE vs Q390NE
Q390GJ vs Q355GJ
Material Comparison
Z15 / Z25 / Z35
Equivalent Material Grades
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 19879 Q390GJE Building Steel Plate?

Q390GJE, also written Q390GJ-E or Q390 GJE, is hot-rolled steel plate for building structures under GB/T 19879. Q means yield, 390 is the minimum yield in MPa, GJ (gao jian) marks high-performance building steel, and E is the quality grade: Charpy V-notch at −40°C, at least 47 J.

The GJ rules are what the structural engineer is paying for. Q390GJE sets a maximum yield as well as a minimum, caps the yield ratio, limits carbon equivalent by thickness and delivery route, and keeps P and S low. The frame then yields where the designer expects.

Q390GJE is a made-to-order grade. 390 MPa with 47 J at −40°C needs clean steel, fine grain and a disciplined rolling schedule; most mills route it through normalizing or TMCP rather than plain controlled rolling.

GB/T 19879-2023 replaced GB/T 19879-2015 on 1 April 2024. The yield-ratio cap for Q390GJ is 0.83 in both editions. What changed is the thickness effect: the 2015 edition stepped yield down 10 MPa above 50 mm, while the 2023 edition holds 390–510 MPa (ReH) from 16 mm to 100 mm. Delivery codes now read CR/NR/N/NT and TMCP/TMCP+T. Sister grades are listed under GB/T 19879, including Q390GJB.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q390GJE cut to size with an EN 10204 3.1 or 3.2 certificate.

Material Specification

Specification element Requirement SHH STEEL compliance
Plate standard GB/T 19879-2023 Q390GJE (GB/T 19879-2015 when the drawing names it) Confirmed
Thickness for Q390GJ 6 mm – 150 mm Confirmed
Yield strength 390 MPa min; 390 – 510 MPa for 16–100 mm Confirmed
Tensile strength 510 – 660 MPa (to 100 mm) Confirmed
Yield ratio ≤ 0.83 Printed on MTC
Quality grade E, Charpy V at −40°C, KV2 ≥ 47 J, longitudinal Confirmed
Delivery condition CR, NR, N, NT, TMCP or TMCP+T As ordered
Through-thickness Z15, Z25 or Z35 to GB/T 5313 As ordered
Dimensions GB/T 709-2019, thickness tolerance Class B Confirmed
Chemistry report Heat analysis + CEV; product analysis on request Confirmed
Certificate EN 10204 3.1 or 3.2 As ordered

Grades often confused with it are GB/T 1591 Q390NE and ASTM A572 Gr.55. None of them carries the GJ yield cap or yield-ratio rule.

Chemical Composition: Heat Analysis and Product Analysis

Two chemistry numbers exist for every Q390GJE plate. The mill reports the heat (ladle) analysis, which must sit inside Table 1. A check analysis drilled from the plate is the product analysis; clause 7.1.4 of GB/T 19879 lets it differ from Table 1 by the GB/T 222 deviations.

Table 1 below is the heat analysis for Q390GJE. The columns on the right show the quality-grade groups at Q390GJ.

Table 1. Heat (ladle) analysis, GB/T 19879-2023 Table 1, %

Element Q390GJE heat analysis (%) Q390GJ B / C Q390GJ D / E
C, max 0.18 0.20 0.18
Si, max 0.55 0.55 0.55
Mn, max 1.70 1.70 1.70
P, max 0.020 0.025 0.020
S, max 0.010 0.015 0.010
V, max 0.200 0.200 0.200
Nb, max 0.070 0.070 0.070
Ti, max 0.030 0.030 0.030
Als, min 0.015 0.015 0.015
Cr, max 0.30 0.30 0.30
Cu, max 0.30 0.30 0.30
Ni, max 0.70 0.70 0.70
Mo, max 0.50 0.50 0.50
V + Nb + Ti, max (if combined) 0.22 0.22 0.22

Notes to Table 1. Total aluminium (Alt ≥ 0.020%) may replace acid-soluble aluminium. If Al, V, Nb or Ti is added alone or together at 0.015% or more, the minimum aluminium does not apply. V + Nb + Ti, when combined, is limited to 0.22%. These limits are the same in the 2015 and 2023 editions.

B and C grades share one chemistry column. D and E grades tighten carbon to 0.18%, phosphorus to 0.020% and sulfur to 0.010%, because they are tested at −20°C and −40°C.

Table 2. Product analysis limits for Q390GJE, GB/T 19879 clause 7.1.4 with GB/T 222-2025, %

Element Heat limit (%) Permitted deviation, GB/T 222-2025 Table 1 Q390GJE product analysis limit (%)
C ≤ 0.18 +0.02 ≤ 0.20
Si ≤ 0.55 +0.05 ≤ 0.60
Mn ≤ 1.70 +0.06 ≤ 1.76
P ≤ 0.020 +0.005 ≤ 0.025
S ≤ 0.010 +0.005 ≤ 0.015
V ≤ 0.200 +0.02 ≤ 0.220
Nb ≤ 0.070 ±0.005 ≤ 0.075 (Table 1 lists Nb to 0.060%; agree above that)
Ti ≤ 0.030 +0.02 ≤ 0.050
Als ≥ 0.015 −0.003 ≥ 0.012
Cr ≤ 0.30 +0.05 ≤ 0.35
Cu ≤ 0.30 +0.05 ≤ 0.35
Ni ≤ 0.70 +0.05 ≤ 0.75
Mo ≤ 0.50 Not listed in Table 1 Agree in contract (alloy-steel Table 2 would give ≤ 0.52)

How to read Table 2. The band is chosen by the Table 1 upper limit. Si ≤0.55% is above 0.37%, so +0.05% applies; Mn ≤1.70% falls in the 0.80–1.70% band, so +0.06%. For one heat an element may deviate in one direction only.

GB/T 222-2025 replaced GB/T 222-2006 on 1 December 2025. One more rule from it matters to buyers: if no reliable heat analysis exists, the product analysis must meet the heat limits with no deviation at all (clause 5.6).

Z-grade plate is cleaner still. GB/T 5313-2023 limits sulfur by heat analysis:

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

CEV and Pcm are always worked out from the heat analysis, not the product analysis. SHH STEEL prints the heat values used and adds a product-analysis column on request. This is building steel, not boiler chemistry such as GB/T 713 Q345R in GB/T 713.

Mechanical Properties

Values below follow Table 3 and Table 5 of GB/T 19879-2023 for Q390GJ. Tensile specimens are transverse; Charpy specimens are longitudinal.

Thickness Upper yield ReH (MPa) Tensile Rm (MPa) Yield ratio, max Elongation A, min
6 – 16 mm ≥ 390 510 – 660 0.83 20%
> 16 – 100 mm 390 – 510 510 – 660 0.83 20%
> 100 – 150 mm 370 – 490 490 – 640 0.83 20%

The 2015 edition used lower yield ReL and stepped yield down 10 MPa above 50 mm. Write the edition on the order so the mill tests to the right table.

Test Q390GJE requirement
Charpy V-notch, longitudinal −40°C, KV2 ≥ 47 J, average of 3
Single value One value may fall below the average requirement, not below 70% of it (GB/T 17505)
Sub-size specimens 7.5 mm or 5 mm wide when plate is too thin: 75% or 50% of the required energy
180° bend Per Table 6 to GB/T 232; may be omitted when the mill guarantees it (7.4.3.2)
Through-thickness (≥ 15 mm) Z15, Z25 or Z35 to GB/T 5313, when ordered

Density for theoretical weight is 7.85 g/cm³.

Q390GJE vs Q390NE / Q390ME (GB/T 1591): Same 390 MPa, Different Job

Q390 under GB/T 1591 and Q390GJE share a number and little else. Q390 steps yield down as plate gets thicker: by 40–63 mm the minimum is 360 MPa. Q390GJE holds 390 MPa to 100 mm, then caps it at 510 MPa.

That matters most in thick column plate, which is exactly where 390 MPa gets specified. A 60 mm flange in GB/T 1591 Q390 is really a 360 MPa flange.

Property Q390NE / Q390ME (GB/T 1591-2018) Q390GJE (GB/T 19879-2023)
Yield at 16 mm 390 MPa 390 MPa
Yield at 16–40 mm 380 MPa min 390 – 510 MPa
Yield at 40–63 mm 360 MPa min 390 – 510 MPa
Yield upper limit None 510 MPa to 100 mm
Yield ratio No limit ≤ 0.83
Tensile to 100 mm 490 – 650 MPa 510 – 660 MPa
Impact −40°C, lower energy than 47 J −40°C, 47 J
C / P / S, max Per GB/T 1591 grade 0.18 / 0.020 / 0.010%
Ni, max Per GB/T 1591 grade 0.70%
CEV ≤ 50 mm Per GB/T 1591 route 0.45% (CR/N), 0.40% (TMCP)

GB/T 1591-2018 hot-rolled Q390 stops at D. For −40°C the general-steel options are GB/T 1591 Q390NE and GB/T 1591 Q390ME. Q390GJE is the building-steel option.

Q390GJE vs Q355GJE: When to Step Up a Strength Level

Check Q355GJE Q390GJE
Yield, 16–100 mm 355 – 475 MPa 390 – 510 MPa
Tensile, to 100 mm 490 – 610 MPa 510 – 660 MPa
Yield ratio ≤ 0.83 ≤ 0.83
CEV ≤ 50 mm 0.43% (AR/N) 0.45% (CR/N)
CEV TMCP ≤ 50 mm 0.38% 0.40%
Max thickness 200 mm 150 mm
Ni / Mo, max 0.30 / 0.20% 0.70 / 0.50%

The yield gain is 35 MPa, about 10%. In a strength-governed column that is roughly a 9% cut in plate thickness and weld volume. CEV rises only 0.02 points on CR/N plate.

Above 150 mm Q390GJ is not available, so very heavy sections stay at Q355GJ. Below that, compare tonnage, weld time and plate price, not plate price alone. See Q345GJE for the 355 MPa plate.

Q390GJB, Q390GJC, Q390GJD or Q390GJE: Which Quality Grade?

Grade Impact temperature Energy, min C / P / S max (%) Typical use
Q390GJB +20°C 47 J 0.20 / 0.025 / 0.015 Heated interiors, mild climates
Q390GJC 0°C 47 J 0.20 / 0.025 / 0.015 Cold regions, exposed frames
Q390GJD −20°C 47 J 0.18 / 0.020 / 0.010 Severe winters, thick welded nodes
Q390GJE −40°C 47 J 0.18 / 0.020 / 0.010 Arctic and low-temperature sites

Strength, yield ratio and CEV do not change from B to E. Only the impact temperature and the D/E chemistry move. The letter should follow the coldest temperature the steel will see, during erection as well as in service.

Q390GJE is the coldest letter in GB/T 19879; there is no F grade in this standard. For the same letter at another strength level: one level up, Q420GJE; one level down, Q345GJE.

Q390GJEZ15, Q390GJEZ25 and Q390GJEZ35: Through-Thickness Plate

Lamellar tearing starts inside the plate, parallel to the surface, when a large weld pulls on it through the thickness. Box-column diaphragms and T-joints on thick flanges are the classic cases. A Z grade is the guarantee against it.

The designation adds the Z level to the grade, for example Q390GJEZ25. Z tests apply to plate 15 mm and thicker and follow GB/T 5313-2023.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

The E melt already caps S at 0.010%, the Z15 limit, so Z25 and Z35 are the levels that change the steelmaking.

GB/T 19879-2023 clause 7.6 requires every Z plate to be ultrasonic tested one by one to GB/T 2970, acceptance level III. Z35 costs most: lowest sulfur, more rejects, and a Z test on each plate.

Our advice: mark Z25 or Z35 on the cutting list by member, not on the whole order. Stiffeners and webs rarely need it.

Equivalent Material Grades

EN 10025 has no 390 MPa grade, so European reviewers usually check Q390GJ against S420 and accept it on the yield floor, or against S355 with a strength upgrade. Neither has the GJ ratio cap.

Designation Region Standard Notes
Q390GJE China GB/T 19879-2023 Grade on this page
GB/T 1591 Q390NE China GB/T 1591-2018 Normalized; no yield cap
GB/T 1591 Q390ME China GB/T 1591-2018 TMCP; no yield cap
EN 10025-3 S420NL Europe EN 10025-3/-4 Next step up (no S390 in EN); strength only
EN 10025-2 S355K2 Europe EN 10025-2 Next step down
ASTM A572 Gr.55 USA ASTM A572 380 MPa; one step lower
JIS G3106 SM520C Japan JIS G3106 355 MPa class; no ratio rule

For mill-direct supply under the GB family, the normalized and TMCP Q390 grades in GB/T 1591 are the nearest relatives.

Weldability

GB/T 19879 makes the mill calculate CEV from the heat analysis and print it, together with the elements used, on every Q390GJE certificate:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Delivery condition CEV ≤ 50 mm CEV > 50 – 100 mm CEV > 100 – 150 mm Pcm ≤ 50 mm Pcm > 50 – 100 mm Pcm > 100 – 150 mm
CR, NR, N, NT 0.45 0.47 0.49 0.28 0.30 0.31
TMCP, TMCP+T 0.40 0.43 By agreement 0.26 0.27 —

CR/N Q390GJ sits at 0.45% CEV to 50 mm, TMCP plate at 0.40%. The TMCP route is the easier one to weld thick, and we suggest it for column plate above 60 mm.

The E letter helps: carbon is capped at 0.18% and P and S are lower, which reduces hot-cracking and HAZ embrittlement risk.

Typical consumables: E50- or E55-class low-hydrogen electrodes (E5515 types) or matching ER55 wire. Shops work to GB 50661 or AWS D1.1. Write the CEV basis (actual heat, not table maximum) into the WPS.

Heat Treatment and Delivery Condition

Q390GJE may be delivered CR, NR, N or NT, or TMCP / TMCP+T. QT is not listed for Q390GJ in Table 2. Each route has its own CEV and Pcm limits, so the route is part of the specification, not a mill detail.

TMCP gives the lowest CEV and the best weldability. N or NT gives the most uniform through-thickness properties on heavy plate. QT holds strength in the thickest sizes.

Agree the route before price. A mill quoting N where the drawing assumed TMCP CEV is not quoting the same plate. TMCP references: GB/T 1591 Q390ME; normalized: GB/T 1591 Q390NE.

Test lots follow clause 9.2 of GB/T 19879-2023; retests and judgement follow GB/T 17505.

Dimensions

Q390GJE sizes we supply from mill and stock:

  • Thickness: 6 mm – 150 mm; most orders 8 mm – 100 mm
  • Width: 1500 mm – 3000 mm standard; wider by mill confirmation
  • Length: 3000 mm – 12000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, on the mean of maximum and minimum thickness, 7.85 g/cm³

Column flanges, diaphragms, stiffeners and gussets are cut to drawing. Rolled sections for the same frame are under steel beam profiles and steel structural profiles.

Tolerances

Dimensional tolerances for Q390GJE come from GB/T 709-2019, as GB/T 19879 directs. The default is Class B, which fixes the minus side at 0.30 mm. Ask for Class C if the design cannot accept any minus.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Flatness and width follow GB/T 709. EN 10029 or ASTM A6 tolerances are possible if written on the order.

Supplementary Requirements

Q390GJE already fixes strength, yield ratio, CEV and −40°C impact. Anything more goes on the purchase order.

  • Edition: GB/T 19879-2023 or -2015. Never write only Q390.
  • Product analysis: ask for a second chemistry column checked to GB/T 222.
  • Through-thickness: add Z15, Z25 or Z35, e.g. Q390GJEZ25.
  • Delivery condition: name it (CR, NR, N, NT, TMCP or TMCP+T) if the welding procedure depends on it.
  • Ultrasonic testing beyond Z plates: GB/T 2970 class, or EN 10160 / ASTM A578.
  • Impact: extra test positions (e.g. quarter thickness) or transverse tests, if the owner wants them beyond the E letter.
  • Tolerance: Class C for zero minus.
  • Inspection: EN 10204 3.2 with SGS, BV, TÜV or a named inspector.

Q390GJE Price Factors and How to Order

Two Q390GJE quotes can differ by a lot and both be fair. The base price is similar across mills; the extras below are where they part.

Cost driver Effect on price
GJ grade over general Q390 plate Grade extra for cleaner steel, yield control and CEV
Quality letter E Highest letter extra: −40°C testing, cleaner melt, more retest risk
Delivery route TMCP or N; NT adds furnace time
Thickness Thin and very thick plate carry size extras; 10–60 mm is usually cheapest
Z15 / Z25 / Z35 Desulfurization, plate-by-plate Z test and UT; Z35 costs most
Width and length Over 3000 mm wide or 12 m long needs mill confirmation
Quantity per size Mill rolling minimums per size; small lots come from stock or combined rolling
Inspection and cutting 3.2 witness, profile cutting, blasting and priming are quoted per item

To get a firm quote in one round, send:

  • Grade and edition, e.g. Q390GJEZ25 to GB/T 19879-2023
  • Thickness × width × length and pieces or tonnes
  • Delivery route, UT standard and class
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line, so you can compare like with like. Need a different letter? See Q390GJD.

Applications

Sector Typical Q390GJE components
Super-tall towers Column flanges and webs above 60 mm, belt trusses
Long-span roofs Heavy truss chords and supports
Industrial buildings Heavy crane runway girders
Transfer structures Podium transfer girders where plate thickness must drop

E grade is for the coldest sites and for owners who specify −40°C for every primary member.

It is the wrong plate for pressure equipment (pressure vessel steel plates), for bare exposed steel (weathering steel plates) or for ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q390GJE from first-line building-steel mills: Wuyang (Wugang), a drafting mill of GB/T 19879, plus Xinyu, Valin Xiangtan, Shougang, Puyang and Hongchang when size requires.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness
  • Tests: tensile, −40°C Charpy, bend, Z test to GB/T 5313, UT to GB/T 2970, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blast and primer
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill

Q390GJE leaves Shanghai for projects designed to Chinese codes abroad, mostly through EPC contractors in Southeast Asia, the Middle East and Africa. We also ship ASTM, ASME, EN, DIN and JIS plate to Europe and the Americas.

Lead time: stock sizes about 5–7 days; mill rolling about 30–45 days; Z35 or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Singapore and 28–35 days to Rotterdam.

Why Choose SHH STEEL

SHH STEEL works mill-direct as a steel manufacturer and exporter and global steel mill sourcing partner, China origin. With Q390GJE you get the GJ plate the drawing asks for, traced to the heat.

Before shipment we check four lines on every certificate: yield inside the GJ window, yield ratio within the cap, CEV inside the thickness band for the delivery route, and −40°C impact at 47 J or more. If one fails, the plate does not ship as GJ.

We also tell buyers when they are over-specifying. If the plate is under 40 mm and strength is not critical, Q345GJE may be the cheaper answer. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q390GJE steel?
Q390GJE is high-performance building structure steel plate to GB/T 19879. It has 390 MPa minimum yield, a 390–510 MPa yield window from 16 to 100 mm, yield ratio ≤0.83, CEV limits by delivery route and Charpy impact of at least 47 J at −40°C. GJ stands for gao jian, high-performance building steel.
What is the difference between Q390GJE and Q390NE?
Q390NE / Q390ME (GB/T 1591) guarantees 390 MPa only to 16 mm; minimum yield falls to 380 MPa above 16 mm and 360 MPa above 40 mm, with no yield cap or ratio limit. Q390GJE (GB/T 19879) holds 390–510 MPa from 16 to 100 mm, caps the yield ratio at 0.83 and needs 47 J at −40°C.
Is Q390GJE suitable for −40°C service?
Yes. Q390GJE is Charpy tested at −40°C and must average at least 47 J on longitudinal specimens. GB/T 19879 has no colder letter, so for design temperatures below −40°C look at GB/T 1591 Q390 M-route or EN S420ML (−50°C) and check the yield-cap rules separately.
What is the maximum thickness of Q390GJ plate?
Q390GJ is specified from 6 mm to 150 mm. Yield is 390–510 MPa from 16 to 100 mm and 370–490 MPa above 100 mm. Heavier sections stay at Q355GJ, which goes to 200 mm.
What is the CEV limit of Q390GJE?
Under GB/T 19879-2023 Table 2, Q390GJE up to 50 mm is capped at CEV 0.45% (CR, NR, N, NT); TMCP plate at 0.40%. CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15, from the heat analysis.
What is the ASTM or EN equivalent of Q390GJE?
There is no exact equivalent. EN 10025 has no 390 MPa grade, so Q390GJE is compared with S420N/S420M (one step higher) or S355 (one step lower). ASTM A572 Gr.55 is 380 MPa. None of these caps yield or limits the yield ratio, which GB/T 19879 does at 0.83.

Conclusion

Q390GJE steel plate to GB/T 19879 is building structure plate with 390 MPa minimum yield, a capped yield window, a yield-ratio limit and 47 J impact at −40°C. It shares its chemistry with Q390GJB but proves toughness at its own letter. It is not general structural plate under GB/T 1591.

Every Q390GJE plate from SHH STEEL ships with heat analysis, CEV, yield and yield ratio, and Charpy results on an EN 10204 3.1 or 3.2 certificate. Product analysis to GB/T 222, Z15–Z35, UT to GB/T 2970, Class C tolerance and cut-to-size are options.

We ship from Shanghai to buyers worldwide. Browse the full GB/T 19879 range or other carbon steel plates.

Share your size list, Z level, quality letter and the edition on the drawing, and we reply with the mill, delivery route, lead time, test plan and price in one message. Contact SHH STEEL for a mill-direct Q390GJE building steel plate quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *