GB/T 19879 Q500GJD Building Steel Plate Supplier
What is GB/T 19879 Q500GJD Building Steel Plate?
Q500GJD, also written Q500GJ-D or Q500 GJD, is high-strength plate for building structures under GB/T 19879-2023. Q means yield, 500 is the minimum yield in MPa, GJ (gao jian) marks high-performance building steel, and D is the quality grade: Charpy V-notch at −20°C, at least 47 J.
The GJ rules still apply at this strength. Q500GJD has a yield ceiling of 640 MPa above 20 mm, a CEV cap of 0.52% for QT plate and low P and S. Unlike Q235GJ–Q460GJ, it is made only by quenching and tempering or TMCP, only from 12 to 50 mm, and its yield ratio is agreed in the contract.
Q500GJD gives 500–640 MPa yield (above 20 mm) with 47 J at −20°C. It is used to shave weight off long-span roof chords and truss members that would otherwise need very thick Q460GJ plate.
GB/T 19879-2023 replaced GB/T 19879-2015 on 1 April 2024. Q500GJ entered GB/T 19879 in the 2015 edition; the 2005 edition stopped at Q460GJ. In 2015 the grade covered 12–40 mm and reported ReL. The 2023 edition keeps the same chemistry, extends the range to 50 mm, reports ReH, and sets 55 J at 0°C for C and 47 J at −20°C / −40°C for D and E. Sister grades are listed under GB/T 19879, including Q500GJC.
SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q500GJD cut to size with an EN 10204 3.1 or 3.2 certificate.
Material Specification
| Specification element | Requirement | SHH STEEL compliance |
|---|---|---|
| Plate standard | GB/T 19879-2023 Q500GJD (GB/T 19879-2015 when the drawing names it) | Confirmed |
| Thickness for Q500GJ | 12 mm – 50 mm | Confirmed |
| Yield strength | 500 MPa min; 500 – 640 MPa above 20 mm | Confirmed |
| Tensile strength | 610 – 770 MPa | Confirmed |
| Yield ratio | By agreement; we print it on the MTC | Printed on MTC |
| Quality grade | D, Charpy V at −20°C, KV2 ≥ 47 J, longitudinal | Confirmed |
| Delivery condition | QT, TMCP or TMCP+T | As ordered |
| Through-thickness | Z15, Z25 or Z35 to GB/T 5313 | As ordered |
| Dimensions | GB/T 709-2019, thickness tolerance Class B | Confirmed |
| Chemistry report | Heat analysis + CEV; product analysis on request | Confirmed |
| Certificate | EN 10204 3.1 or 3.2 | As ordered |
Grades often confused with it are GB/T 16270 Q500D and GB/T 1591 Q500MD. None of them carries the GJ yield cap.
Chemical Composition: Heat Analysis and Product Analysis
Buyers often reject plate because a third-party lab reads 0.02% more carbon than the MTC. That is usually not a failure. Table 1 is the heat (ladle) limit; plate drilled after rolling is judged as product analysis, with the tolerances of GB/T 222 that clause 7.1.4 calls up.
Table 1 below is the heat analysis for Q500GJD. The columns on the right show the quality-grade groups at Q500GJ.
Table 1. Heat (ladle) analysis, GB/T 19879-2023 Table 1, %
| Element | Q500GJD heat analysis (%) | Q500GJ C | Q500GJ D / E |
|---|---|---|---|
| C, max | 0.18 | 0.18 | 0.18 |
| Si, max | 0.60 | 0.60 | 0.60 |
| Mn, max | 1.80 | 1.80 | 1.80 |
| P, max | 0.020 | 0.025 | 0.020 |
| S, max | 0.010 | 0.015 | 0.010 |
| V, max | 0.120 | 0.120 | 0.120 |
| Nb, max | 0.110 | 0.110 | 0.110 |
| Ti, max | 0.030 | 0.030 | 0.030 |
| Als, min | 0.015 | 0.015 | 0.015 |
| Cr, max | 1.20 | 1.20 | 1.20 |
| Cu, max | 0.50 | 0.50 | 0.50 |
| Ni, max | 1.20 | 1.20 | 1.20 |
| Mo, max | 0.60 | 0.60 | 0.60 |
| B, max (if added) | 0.003 | 0.003 | 0.003 |
Notes to Table 1. Total aluminium (Alt ≥ 0.020%) may replace acid-soluble aluminium. If Al, V, Nb or Ti is added alone or together at 0.015% or more, the minimum aluminium does not apply. When boron is added, and for any QT plate, B ≤ 0.003%. These limits are the same in the 2015 and 2023 editions.
The C and D/E columns differ only in P and S: the D and E letters tighten P to 0.020% and S to 0.010%. Carbon stays at 0.18% for every quality letter at this level.
Table 2. Product analysis limits for Q500GJD, GB/T 19879 clause 7.1.4 with GB/T 222-2025, %
| Element | Heat limit (%) | Permitted deviation, GB/T 222-2025 Table 2 (alloy steel) | Q500GJD product analysis limit (%) |
|---|---|---|---|
| C | ≤ 0.18 | +0.01 | ≤ 0.19 |
| Si | ≤ 0.60 | +0.04 | ≤ 0.64 |
| Mn | ≤ 1.80 | +0.04 | ≤ 1.84 |
| P | ≤ 0.020 | +0.005 | ≤ 0.025 |
| S | ≤ 0.010 | +0.005 | ≤ 0.015 |
| V | ≤ 0.120 | +0.03 | ≤ 0.150 |
| Nb | ≤ 0.110 | Agree in contract | Agree in contract |
| Ti | ≤ 0.030 | +0.02 | ≤ 0.050 |
| Als | ≥ 0.015 | ±0.005 band (Al ≤ 0.10%) | Agree in contract |
| Cr | ≤ 1.20 | +0.05 | ≤ 1.25 |
| Cu | ≤ 0.50 | +0.03 | ≤ 0.53 |
| Ni | ≤ 1.20 | +0.05 | ≤ 1.25 |
| Mo | ≤ 0.60 | +0.02 | ≤ 0.62 |
| B (if added) | ≤ 0.003 | Agree in contract | Agree in contract |
How to read Table 2. Q500GJ–Q690GJ heats carry Ni, Cr, Mo and often B for hardenability, which normally classes them as alloy steel, so the alloy-steel table of GB/T 222 applies. For Q500GJD, Mn ≤1.80% sits in the 1.00–2.00% band (±0.04), and Ni ≤1.20% in the 1.00–2.00% band (±0.05). GB/T 222 clause 5.4 says one steel uses one table only, so the certificate should state which table was applied.
GB/T 222-2025 replaced GB/T 222-2006 on 1 December 2025. One more rule from it matters to buyers: if no reliable heat analysis exists, the product analysis must meet the heat limits with no deviation at all (clause 5.6).
Z-grade plate is cleaner still. GB/T 5313-2023 limits sulfur by heat analysis:
| Z grade | Heat sulfur, max (%) | Reduction of area, avg / single (%) |
|---|---|---|
| Z15 | 0.010 | 15 / 10 |
| Z25 | 0.007 | 25 / 15 |
| Z35 | 0.005 | 35 / 25 |
CEV and Pcm are always worked out from the heat analysis, not the product analysis. SHH STEEL prints the heat values used and adds a product-analysis column on request. This is building steel, not boiler chemistry such as GB/T 713 Q345R in GB/T 713.
Mechanical Properties
Values below follow Table 4 and Table 5 of GB/T 19879-2023 for Q500GJ. Tensile specimens are transverse; Charpy specimens are longitudinal.
| Thickness | Upper yield ReH (MPa) | Tensile Rm (MPa) | Yield ratio, max | Elongation A, min |
|---|---|---|---|---|
| 12 – 20 mm | ≥ 500 | 610 – 770 | By agreement | 17% |
| > 20 – 50 mm | 500 – 640 | 610 – 770 | By agreement | 17% |
Below 20 mm only the 500 MPa minimum applies; from 20 to 50 mm the 500 – 640 MPa window applies. Write the yield-ratio limit into the contract; GB/T 19879-2023 leaves it to agreement for this grade.
| Test | Q500GJD requirement |
|---|---|
| Charpy V-notch, longitudinal | −20°C, KV2 ≥ 47 J, average of 3 |
| Single value | One value may fall below the average requirement, not below 70% of it (GB/T 17505) |
| Sub-size specimens | 7.5 mm or 5 mm wide when plate is too thin: 75% or 50% of the required energy |
| 180° bend | Per Table 6 to GB/T 232; may be omitted when the mill guarantees it (7.4.3.2) |
| Through-thickness (≥ 15 mm) | Z15, Z25 or Z35 to GB/T 5313, when ordered |
Density for theoretical weight is 7.85 g/cm³.
Q500GJD vs S500Q and GB/T 16270 Q500D: What Building Plate Adds
At 500 MPa the plate itself is not unusual. GB/T 16270 Q500D and EN 10025-6 S500Q are standard QT products. What Q500GJD adds is a building-steel frame around them: a yield ceiling of 640 MPa above 20 mm, a tensile floor of 610 MPa, a CEV cap written into the standard, and Charpy at the GB quality letter.
The trade-off is thickness. GB/T 19879 stops at 50 mm for this grade; EN 10025-6 and GB/T 16270 go much thicker.
| Property | S500Q (EN 10025-6) | Q500D (GB/T 16270) | Q500GJD (GB/T 19879-2023) |
|---|---|---|---|
| Delivery | QT | QT | QT or TMCP |
| Thickness range | to 150 mm | to 150 mm | 12 – 50 mm |
| Yield, ≤ 50 mm | ≥ 500 MPa | ≥ 500 MPa | 500 – 640 MPa above 20 mm |
| Tensile, ≤ 50 mm | 590 – 770 MPa | Per GB/T 16270 | 610 – 770 MPa |
| Yield ratio | No limit | No limit | By agreement (write it on the order) |
| Impact | 0°C / −20°C (Q) | −20°C | −20°C, 47 J |
| Elongation A | 17% | Per GB/T 16270 | 17% |
| CEV ≤ 50 mm | Per EN 10025-6 | Per GB/T 16270 | 0.52% QT / 0.47% TMCP |
If a member is thicker than 50 mm, it cannot be Q500GJD. The designer either splits the plate, or moves to GB/T 16270 Q500D or the EN grade with project-specific yield-cap rules. The TMCP comparison in GB/T 1591 is GB/T 1591 Q500MD.
QT or TMCP? Delivery Condition, CEV and Weldability of Q500GJD
| Route | CEV max (≤ 50 mm) | Pcm max (≤ 50 mm) | Typical use |
|---|---|---|---|
| QT (incl. direct quench) | 0.52% | By agreement | Full strength through 50 mm; highest alloy |
| TMCP, TMCP+T | 0.47% | 0.28% (reference value) | Leaner chemistry; easier welding on thinner plate |
Q500GJ cannot be made as plain hot-rolled or normalized plate; GB/T 19879-2023 lists only QT and TMCP routes for it. The two routes are not equal at the welding bay.
QT Q500GJD carries up to 0.52% CEV, because the mill adds Mn, Ni, Cr, Mo and sometimes B for hardenability. TMCP plate is capped at 0.47%. For welding procedure purposes those are different steels.
The 2023 edition lets TMCP plate ship against Pcm instead of CEV only when buyer and mill agree in the contract. The Pcm figure in the standard for TMCP plate is given for reference.
Q500GJC, Q500GJD or Q500GJE: Which Quality Grade?
| Grade | Impact temperature | Energy, min | C / P / S max (%) | Typical use |
|---|---|---|---|---|
| Q500GJC | 0°C | 55 J | 0.18 / 0.025 / 0.015 | Cold regions, exposed frames |
| Q500GJD | −20°C | 47 J | 0.18 / 0.020 / 0.010 | Severe winters, thick welded nodes |
| Q500GJE | −40°C | 47 J | 0.18 / 0.020 / 0.010 | Arctic and low-temperature sites |
Strength, yield window and CEV do not change from C to E. Only the impact temperature, the C-grade energy (55 J) and the D/E P and S limits move. Choose the letter from the site climate and plate thickness, not from habit.
Q500GJD is the letter for −20°C design temperatures, and the one we suggest when the plate is thick and restrained. For the same letter at another strength level: one level up, Q550GJD; one level down, Q460GJD.
Q500GJDZ15, Q500GJDZ25 and Q500GJDZ35: Through-Thickness Plate
A weld on the face of a thick plate shrinks and pulls the plate apart through its thickness. If the steel holds sulfide stringers, it tears in steps. Z15, Z25 and Z35 prove through-thickness ductility with a short-transverse tensile test.
The designation adds the Z level to the grade, for example Q500GJDZ25. Z tests apply to plate 15–50 mm and follow GB/T 5313-2023.
| Z grade | Heat sulfur, max (%) | Reduction of area, avg / single (%) |
|---|---|---|
| Z15 | 0.010 | 15 / 10 |
| Z25 | 0.007 | 25 / 15 |
| Z35 | 0.005 | 35 / 25 |
The D melt already caps S at 0.010%, the Z15 limit, so Z25 and Z35 are the levels that change the steelmaking.
GB/T 19879-2023 clause 7.6 requires every Z plate to be ultrasonic tested one by one to GB/T 2970, acceptance level III. Z35 costs most: lowest sulfur, more rejects, and a Z test on each plate.
Most projects need Z only on flange and diaphragm plates over about 25–40 mm. Put the Z level on those items alone and keep the rest standard Q500GJD.
Equivalent Material Grades
At 500 MPa every foreign comparison is a QT plate standard, not a building-steel standard. They match strength and toughness temperature. None of them sets a yield ceiling or a yield-ratio rule.
| Designation | Region | Standard | Notes |
|---|---|---|---|
| Q500GJD | China | GB/T 19879-2023 | Grade on this page; 12–50 mm |
| EN 10025-6 S500Q | Europe | EN 10025-6 | QT; closest strength match |
| EN 10025-6 S500QL | Europe | EN 10025-6 | Colder sub-grade |
| GB/T 16270 Q500D | China | GB/T 16270 | QT structural plate; thicker sizes |
| GB/T 1591 Q500MD | China | GB/T 1591-2018 | TMCP route |
| ASTM A709 HPS 70W | USA | ASTM A709 | 485 MPa; one step lower |
See EN 10025-6 and GB/T 16270 for thicker or non-building QT plate.
Weldability
GB/T 19879 makes the mill calculate CEV from the heat analysis and print it, together with the elements used, on every Q500GJD certificate:
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B
| Delivery condition | CEV, max (≤ 50 mm) | Pcm, max (≤ 50 mm) |
|---|---|---|
| QT (quenched + tempered, incl. direct quench) | 0.52 | By agreement |
| TMCP, TMCP+T | 0.47 | 0.28 (for reference) |
Q500GJ plate is high-strength steel and is welded like it: low-hydrogen consumables, measured preheat, interpass limits and a heat-input window that protects the tempered structure.
The impact test on the D letter is at −20°C. Qualify the HAZ Charpy at that temperature, not only the weld metal.
Typical consumables: E62-class low-hydrogen electrodes (GB/T 5118 E6215 types) or matching wire. Shops work to GB 50661 or AWS D1.1. Write the CEV basis (actual heat, not table maximum) into the WPS.
Heat Treatment and Delivery Condition
Q500GJD is delivered QT (quenched and tempered, including in-line direct quenching) or TMCP / TMCP+T. Hot-rolled and normalized delivery are not allowed for this grade.
Most building orders at this level ship QT. TMCP plate is possible on thinner sizes and gives a lower CEV cap, but not every mill can hold the GJ yield ceiling on TMCP plate up to 50 mm.
Tempering temperature and time are mill data. We ask for them on the MTC when the fabricator plans post-weld heat treatment, so that PWHT stays below the tempering temperature. QT references: GB/T 16270 Q500D and EN 10025-6 S500Q.
Test lots follow clause 9.2 of GB/T 19879-2023; retests and judgement follow GB/T 17505.
Dimensions
Typical Q500GJD dimensions on our offers:
- Thickness: 12 mm – 50 mm
- Width: 1500 mm – 3000 mm standard; wider by mill confirmation; QT width depends on the mill’s quench line
- Length: 3000 mm – 12000 mm; longer by enquiry
- Edge: mill edge or cut edge
- Weight: theoretical, on the mean of maximum and minimum thickness, 7.85 g/cm³
Column flanges, diaphragms, stiffeners and gussets are cut to drawing. Rolled sections for the same frame are under steel beam profiles and steel structural profiles.
Tolerances
GB/T 709-2019 governs Q500GJD thickness, width, length and flatness. Under Class B, the default, plate may be up to 0.30 mm thin and the plus side grows with thickness and width. Class C gives zero minus by agreement.
| Nominal thickness (mm) | Width ≤ 1500 mm | Width > 1500 – 2500 mm |
|---|---|---|
| > 8 – 15 | −0.30 / +0.80 | −0.30 / +1.00 |
| > 15 – 25 | −0.30 / +1.00 | −0.30 / +1.20 |
| > 25 – 40 | −0.30 / +1.10 | −0.30 / +1.30 |
| > 40 – 60 | −0.30 / +1.30 | −0.30 / +1.50 |
Flatness and width follow GB/T 709. EN 10029 or ASTM A6 tolerances are possible if written on the order.
Supplementary Requirements
Q500GJD already fixes strength, yield window, CEV and −20°C impact. Anything more goes on the purchase order.
- Edition: GB/T 19879-2023 or -2015. Never write only Q500.
- Product analysis: ask for a second chemistry column checked to GB/T 222.
- Through-thickness: add Z15, Z25 or Z35, e.g. Q500GJDZ25.
- Delivery route: QT or TMCP, and the CEV/Pcm basis.
- Yield ratio: the designer’s limit, since the standard leaves it to agreement.
- Tempering data on the MTC if the fabricator plans post-weld heat treatment.
- Impact: extra test positions (e.g. quarter thickness) or transverse tests, if the owner wants them beyond the D letter.
- Tolerance: Class C for zero minus.
- Inspection: EN 10204 3.2 with SGS, BV, TÜV or a named inspector.
Q500GJD Price Factors and How to Order
There is no single Q500GJD price. Mills price GJ plate as base plus extras, and the order details set the extras.
| Cost driver | Effect on price |
|---|---|
| GJ grade over general Q500 plate | Grade extra for cleaner steel, yield control and CEV |
| Quality letter D | Extra for −20°C testing and the cleaner D melt |
| Delivery route | QT line time is the main cost driver at this level |
| Thickness | 12–20 mm and 40–50 mm carry the most care; 20–40 mm is the core range |
| Z15 / Z25 / Z35 | Desulfurization, plate-by-plate Z test and UT; Z35 costs most |
| Width and length | Over 3000 mm wide or 12 m long needs mill confirmation |
| Quantity per size | Mill rolling minimums per size; small lots come from stock or combined rolling |
| Inspection and cutting | 3.2 witness, profile cutting, blasting and priming are quoted per item |
To get a firm quote in one round, send:
- Grade and edition, e.g. Q500GJDZ25 to GB/T 19879-2023
- Thickness × width × length and pieces or tonnes
- Delivery route, UT standard and class
- Certificate type and inspector
- Destination port and Incoterm
We quote plate price, extras and freight line by line, so you can compare like with like. Need a different letter? See Q500GJE.
Applications
| Sector | Typical Q500GJD components |
|---|---|
| Long-span roofs | Compression chords and diagonals where weight governs |
| Tall buildings | Outrigger and belt truss members, hanger plates |
| Heavy industrial buildings | Crane-runway and support members |
| Special structures | Members where crane capacity or connection size limits plate thickness |
D grade covers severe winters, thick welded nodes and members erected in sub-zero weather.
It is not boiler or pressure-vessel plate (pressure vessel steel plates), and members thicker than 50 mm move to GB/T 16270 or EN 10025-6.
Supply Capability and Global Delivery
SHH STEEL sources Q500GJD from first-line building-steel mills: Wuyang (Wugang), a drafting mill of GB/T 19879, plus Valin Xiangtan and Shougang QT lines.
- Certificates: EN 10204 3.1 standard; 3.2 with third-party witness
- Tests: tensile, −20°C Charpy, bend, Z test to GB/T 5313, UT to GB/T 2970, product analysis
- Processing: CNC plasma and flame cutting, bevelling, drilling, shot blast and primer
- Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
- Marking: steel-stamped and paint-marked with grade, heat, size and mill
Buyers of Q500GJD are usually EPC contractors and fabricators working to Chinese drawings overseas. We ship to the United States, Europe, the Middle East, Southeast Asia, Africa and South America.
QT plate is rolled and heat treated to order: about 45–60 days; 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Singapore and 28–35 days to Rotterdam.
Why Choose SHH STEEL
As a steel manufacturer and exporter and global steel mill sourcing partner, SHH STEEL buys Q500GJD straight from GJ-qualified mills, China origin. No relabelled general plate, no mixed heats.
Before shipment we check four lines on every certificate: yield inside the GJ window, yield ratio inside the agreed limit, CEV inside the thickness band for the delivery route, and −20°C impact at 47 J or more. If one fails, the plate does not ship as GJ.
We also tell buyers when they are over-specifying. If a member is thicker than 50 mm, we tell you before quoting: it cannot be Q500GJD. Browse more structural steel plates and high strength low alloy plates.
FAQ
-
What is Q500GJD steel?
- Q500GJD is high-strength building structure steel plate to GB/T 19879-2023, delivered quenched and tempered or TMCP in 12–50 mm. It has 500 MPa minimum yield, 500–640 MPa yield above 20 mm, 610 – 770 MPa tensile, a CEV cap of 0.52% (QT) and Charpy impact of at least 47 J at −20°C.
-
What is the difference between Q500GJD and S500Q?
- S500Q (EN 10025-6) is QT plate with ≥500 MPa yield up to 50 mm, no yield ceiling and no yield-ratio rule, made to 150 mm. Q500GJD (GB/T 19879-2023) is QT or TMCP building plate, 12–50 mm, with 500–640 MPa yield above 20 mm, 610 – 770 MPa tensile, a CEV cap of 0.52% (QT) and 47 J at −20°C.
-
When should I specify Q500GJD instead of Q500GJC?
- Specify Q500GJD when the lowest service or erection temperature reaches about −20°C, when plate is thick and heavily restrained, or when Z25/Z35 is ordered. D is tested at −20°C (47 J) and its melt is cleaner: C ≤0.18%, P ≤0.020%, S ≤0.010%, against P 0.025% and S 0.015% for C grade.
-
What is the maximum thickness of Q500GJ?
- 50 mm. GB/T 19879-2023 covers Q500GJ from 12 to 50 mm; the 2015 edition stopped at 40 mm. Thicker 500 MPa plate is ordered to GB/T 16270 or EN 10025-6, without the GJ yield ceiling.
-
What does Q500GJDZ35 mean?
- Q500GJDZ35 is Q500GJD plate with Z35 through-thickness properties to GB/T 5313-2023: average reduction of area at least 35%, no single value below 25%, and heat sulfur 0.005% max. It applies to plate 15–50 mm, resists lamellar tearing, and each Z plate is ultrasonic tested.
-
What is the ASTM or EN equivalent of Q500GJD?
- The closest European grade is EN 10025-6 S500Q; the closest Chinese non-building grades are GB/T 16270 Q500D (QT) and GB/T 1591 Q500MD (TMCP). They match strength only: Q500GJD adds a 640 MPa yield ceiling, a CEV cap and a 50 mm thickness limit.
Conclusion
Q500GJD steel plate to GB/T 19879 is building structure plate with 500 MPa minimum yield, a capped yield window, a yield ratio agreed in the contract and 47 J impact at −20°C. It shares its chemistry with Q500GJC but proves toughness at its own letter. It is not general structural plate under GB/T 1591 or GB/T 16270.
With SHH STEEL the Q500GJD certificate is complete: heat chemistry, CEV, yield, tensile, yield ratio and Charpy impact, to EN 10204 3.1 or 3.2. Add product analysis to GB/T 222, a Z15, Z25 or Z35 level, a GB/T 2970 UT class, Class C tolerance or profile cutting as the project needs.
We ship from Shanghai to buyers worldwide. Browse the full GB/T 19879 range or other carbon steel plates.
Tell us the grade edition, sizes, tonnage and any Z, UT or inspection needs. We check the request against the standard first, then confirm mill, route, lead time and price. Contact SHH STEEL today for a mill-direct quotation on Q500GJD building steel plate.