Stacked Q550GJE building steel plates GB/T 19879 ready for dispatch at SHH STEEL

GB/T 19879 Q550GJE Building Steel Plate Supplier

GB/T 19879 Q550GJE is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 550 – 690 MPa yield above 20 mm, 670 – 830 MPa tensile, CEV ≤0.54% and 47 J at −40°C. SHH STEEL supplies Q550GJE mill-direct with Z15–Z35 options and full heat and product analysis.
Keywords
Q550GJE, Q550GJE steel plate, GB/T 19879 Q550GJE, Q550GJ-E, Q550GJEZ15, Q550GJEZ25, Q550GJEZ35, Q550GJ, building structure steel plate, Q550GJE supplier, Q550GJE QT plate
Equivalent Grades
GB/T 19879 Q550GJE / EN 10025-6 S550QL (QT, strength only) / GB/T 16270 Q550E (QT) / GB/T 1591 Q550ME (TMCP) — Material Specification: GB/T 19879-2023 (supersedes GB/T 19879-2015) — Delivery: QT, TMCP or TMCP+T; −40°C impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q550GJE vs S550QL
QT or TMCP?
Material Comparison
Z15 / Z25 / Z35
Equivalent Material Grades
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 19879 Q550GJE Building Steel Plate?

Q550GJE, also written Q550GJ-E or Q550 GJE, is high-strength plate for building structures under GB/T 19879-2023. Q means yield, 550 is the minimum yield in MPa, GJ (gao jian) marks high-performance building steel, and E is the quality grade: Charpy V-notch at −40°C, at least 47 J.

The GJ rules still apply at this strength. Q550GJE has a yield ceiling of 690 MPa above 20 mm, a CEV cap of 0.54% for QT plate and low P and S. Unlike Q235GJ–Q460GJ, it is made only by quenching and tempering or TMCP, only from 12 to 50 mm, and its yield ratio is agreed in the contract.

Q550GJE pairs 550 MPa with 47 J at −40°C. It is a small-tonnage, project-specific grade; we plan it with the mill’s quench line schedule, not from stock.

GB/T 19879-2023 replaced GB/T 19879-2015 on 1 April 2024. Q550GJ entered GB/T 19879 in the 2015 edition; the 2005 edition stopped at Q460GJ. In 2015 the grade covered 12–40 mm and reported ReL. The 2023 edition keeps the same chemistry, extends the range to 50 mm, reports ReH, and sets 55 J at 0°C for C and 47 J at −20°C / −40°C for D and E. Sister grades are listed under GB/T 19879, including Q550GJC.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q550GJE cut to size with an EN 10204 3.1 or 3.2 certificate.

Material Specification

Specification element Requirement SHH STEEL compliance
Plate standard GB/T 19879-2023 Q550GJE (GB/T 19879-2015 when the drawing names it) Confirmed
Thickness for Q550GJ 12 mm – 50 mm Confirmed
Yield strength 550 MPa min; 550 – 690 MPa above 20 mm Confirmed
Tensile strength 670 – 830 MPa Confirmed
Yield ratio By agreement; we print it on the MTC Printed on MTC
Quality grade E, Charpy V at −40°C, KV2 ≥ 47 J, longitudinal Confirmed
Delivery condition QT, TMCP or TMCP+T As ordered
Through-thickness Z15, Z25 or Z35 to GB/T 5313 As ordered
Dimensions GB/T 709-2019, thickness tolerance Class B Confirmed
Chemistry report Heat analysis + CEV; product analysis on request Confirmed
Certificate EN 10204 3.1 or 3.2 As ordered

Grades often confused with it are GB/T 16270 Q550E and GB/T 1591 Q550ME. None of them carries the GJ yield cap.

Chemical Composition: Heat Analysis and Product Analysis

GB/T 19879 controls chemistry twice. The heat (ladle) analysis is taken from the melt and must meet Table 1 of the standard. The product analysis is taken from the finished plate and may sit slightly outside Table 1, by the permitted deviations of GB/T 222 (clause 7.1.4). Both are valid acceptance checks, but they are not the same number.

Table 1 below is the heat analysis for Q550GJE. The columns on the right show the quality-grade groups at Q550GJ.

Table 1. Heat (ladle) analysis, GB/T 19879-2023 Table 1, %

Element Q550GJE heat analysis (%) Q550GJ C Q550GJ D / E
C, max 0.18 0.18 0.18
Si, max 0.60 0.60 0.60
Mn, max 2.00 2.00 2.00
P, max 0.020 0.025 0.020
S, max 0.010 0.015 0.010
V, max 0.120 0.120 0.120
Nb, max 0.110 0.110 0.110
Ti, max 0.030 0.030 0.030
Als, min 0.015 0.015 0.015
Cr, max 1.20 1.20 1.20
Cu, max 0.50 0.50 0.50
Ni, max 2.00 2.00 2.00
Mo, max 0.60 0.60 0.60
B, max (if added) 0.003 0.003 0.003

Notes to Table 1. Total aluminium (Alt ≥ 0.020%) may replace acid-soluble aluminium. If Al, V, Nb or Ti is added alone or together at 0.015% or more, the minimum aluminium does not apply. When boron is added, and for any QT plate, B ≤ 0.003%. These limits are the same in the 2015 and 2023 editions.

The C and D/E columns differ only in P and S: the D and E letters tighten P to 0.020% and S to 0.010%. Carbon stays at 0.18% for every quality letter at this level.

Table 2. Product analysis limits for Q550GJE, GB/T 19879 clause 7.1.4 with GB/T 222-2025, %

Element Heat limit (%) Permitted deviation, GB/T 222-2025 Table 2 (alloy steel) Q550GJE product analysis limit (%)
C ≤ 0.18 +0.01 ≤ 0.19
Si ≤ 0.60 +0.04 ≤ 0.64
Mn ≤ 2.00 +0.04 ≤ 2.04
P ≤ 0.020 +0.005 ≤ 0.025
S ≤ 0.010 +0.005 ≤ 0.015
V ≤ 0.120 +0.03 ≤ 0.150
Nb ≤ 0.110 Agree in contract Agree in contract
Ti ≤ 0.030 +0.02 ≤ 0.050
Als ≥ 0.015 ±0.005 band (Al ≤ 0.10%) Agree in contract
Cr ≤ 1.20 +0.05 ≤ 1.25
Cu ≤ 0.50 +0.03 ≤ 0.53
Ni ≤ 2.00 +0.05 ≤ 2.05
Mo ≤ 0.60 +0.02 ≤ 0.62
B (if added) ≤ 0.003 Agree in contract Agree in contract

How to read Table 2. Q500GJ–Q690GJ heats carry Ni, Cr, Mo and often B for hardenability, which normally classes them as alloy steel, so the alloy-steel table of GB/T 222 applies. For Q550GJE, Mn ≤2.00% sits in the 1.00–2.00% band (±0.04), and Ni ≤2.00% in the 1.00–2.00% band (±0.05). GB/T 222 clause 5.4 says one steel uses one table only, so the certificate should state which table was applied.

GB/T 222-2025 replaced GB/T 222-2006 on 1 December 2025. One more rule from it matters to buyers: if no reliable heat analysis exists, the product analysis must meet the heat limits with no deviation at all (clause 5.6).

Z-grade plate is cleaner still. GB/T 5313-2023 limits sulfur by heat analysis:

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

CEV and Pcm are always worked out from the heat analysis, not the product analysis. SHH STEEL prints the heat values used and adds a product-analysis column on request. This is building steel, not boiler chemistry such as GB/T 713 Q345R in GB/T 713.

Mechanical Properties

Values below follow Table 4 and Table 5 of GB/T 19879-2023 for Q550GJ. Tensile specimens are transverse; Charpy specimens are longitudinal.

Thickness Upper yield ReH (MPa) Tensile Rm (MPa) Yield ratio, max Elongation A, min
12 – 20 mm ≥ 550 670 – 830 By agreement 17%
> 20 – 50 mm 550 – 690 670 – 830 By agreement 17%

Below 20 mm only the 550 MPa minimum applies; from 20 to 50 mm the 550 – 690 MPa window applies. Write the yield-ratio limit into the contract; GB/T 19879-2023 leaves it to agreement for this grade.

Test Q550GJE requirement
Charpy V-notch, longitudinal −40°C, KV2 ≥ 47 J, average of 3
Single value One value may fall below the average requirement, not below 70% of it (GB/T 17505)
Sub-size specimens 7.5 mm or 5 mm wide when plate is too thin: 75% or 50% of the required energy
180° bend Per Table 6 to GB/T 232; may be omitted when the mill guarantees it (7.4.3.2)
Through-thickness (≥ 15 mm) Z15, Z25 or Z35 to GB/T 5313, when ordered

Density for theoretical weight is 7.85 g/cm³.

Q550GJE vs S550QL and GB/T 16270 Q550E: What Building Plate Adds

At 550 MPa the plate itself is not unusual. GB/T 16270 Q550E and EN 10025-6 S550QL are standard QT products. What Q550GJE adds is a building-steel frame around them: a yield ceiling of 690 MPa above 20 mm, a tensile floor of 670 MPa, a CEV cap written into the standard, and Charpy at the GB quality letter.

The trade-off is thickness. GB/T 19879 stops at 50 mm for this grade; EN 10025-6 and GB/T 16270 go much thicker.

Property S550QL (EN 10025-6) Q550E (GB/T 16270) Q550GJE (GB/T 19879-2023)
Delivery QT QT QT or TMCP
Thickness range to 150 mm to 150 mm 12 – 50 mm
Yield, ≤ 50 mm ≥ 550 MPa ≥ 550 MPa 550 – 690 MPa above 20 mm
Tensile, ≤ 50 mm 640 – 820 MPa Per GB/T 16270 670 – 830 MPa
Yield ratio No limit No limit By agreement (write it on the order)
Impact −20°C / −40°C (QL) −40°C −40°C, 47 J
Elongation A 16% Per GB/T 16270 17%
CEV ≤ 50 mm Per EN 10025-6 Per GB/T 16270 0.54% QT / 0.47% TMCP

If a member is thicker than 50 mm, it cannot be Q550GJE. The designer either splits the plate, or moves to GB/T 16270 Q550E or the EN grade with project-specific yield-cap rules. The TMCP comparison in GB/T 1591 is GB/T 1591 Q550ME.

QT or TMCP? Delivery Condition, CEV and Weldability of Q550GJE

Route CEV max (≤ 50 mm) Pcm max (≤ 50 mm) Typical use
QT (incl. direct quench) 0.54% By agreement Full strength through 50 mm; highest alloy
TMCP, TMCP+T 0.47% 0.29% (reference value) Leaner chemistry; easier welding on thinner plate

Q550GJ cannot be made as plain hot-rolled or normalized plate; GB/T 19879-2023 lists only QT and TMCP routes for it. The two routes are not equal at the welding bay.

QT Q550GJE carries up to 0.54% CEV, because the mill adds Mn, Ni, Cr, Mo and sometimes B for hardenability. TMCP plate is capped at 0.47%. For welding procedure purposes those are different steels.

The 2023 edition lets TMCP plate ship against Pcm instead of CEV only when buyer and mill agree in the contract. The Pcm figure in the standard for TMCP plate is given for reference.

Q550GJC, Q550GJD or Q550GJE: Which Quality Grade?

Grade Impact temperature Energy, min C / P / S max (%) Typical use
Q550GJC 0°C 55 J 0.18 / 0.025 / 0.015 Cold regions, exposed frames
Q550GJD −20°C 47 J 0.18 / 0.020 / 0.010 Severe winters, thick welded nodes
Q550GJE −40°C 47 J 0.18 / 0.020 / 0.010 Arctic and low-temperature sites

Strength, yield window and CEV do not change from C to E. Only the impact temperature, the C-grade energy (55 J) and the D/E P and S limits move. Pick the letter from the lowest service or erection temperature.

Q550GJE is the coldest letter in GB/T 19879; there is no F grade in this standard. For the same letter at another strength level: one level up, Q620GJE; one level down, Q500GJE.

Q550GJEZ15, Q550GJEZ25 and Q550GJEZ35: Through-Thickness Plate

Thick plate loaded across its thickness can tear in layers under weld shrinkage. Column flanges at beam-flange welds, diaphragm plates in box columns and base plates under heavy tension are the usual places. A Z grade guarantees ductility in that direction.

The designation adds the Z level to the grade, for example Q550GJEZ25. Z tests apply to plate 15–50 mm and follow GB/T 5313-2023.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

The E melt already caps S at 0.010%, the Z15 limit, so Z25 and Z35 are the levels that change the steelmaking.

GB/T 19879-2023 clause 7.6 requires every Z plate to be ultrasonic tested one by one to GB/T 2970, acceptance level III. Z35 costs most: lowest sulfur, more rejects, and a Z test on each plate.

Ask for Z only where the joint needs it. Over-specifying Z35 across a whole order adds cost and lead time without helping the frame.

Equivalent Material Grades

At 550 MPa every foreign comparison is a QT plate standard, not a building-steel standard. They match strength and toughness temperature. None of them sets a yield ceiling or a yield-ratio rule.

Designation Region Standard Notes
Q550GJE China GB/T 19879-2023 Grade on this page; 12–50 mm
EN 10025-6 S550QL Europe EN 10025-6 QT; closest strength match
EN 10025-6 S550QL1 Europe EN 10025-6 Colder sub-grade
GB/T 16270 Q550E China GB/T 16270 QT structural plate; thicker sizes
GB/T 1591 Q550ME China GB/T 1591-2018 TMCP route

See EN 10025-6 and GB/T 16270 for thicker or non-building QT plate.

Weldability

GB/T 19879 makes the mill calculate CEV from the heat analysis and print it, together with the elements used, on every Q550GJE certificate:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Delivery condition CEV, max (≤ 50 mm) Pcm, max (≤ 50 mm)
QT (quenched + tempered, incl. direct quench) 0.54 By agreement
TMCP, TMCP+T 0.47 0.29 (for reference)

Q550GJ shares the Q500GJ welding logic but with up to 2.00% Mn and Ni. Hydrogen control and heat input are the two numbers the WPS has to pin down.

The impact test on the E letter is at −40°C. Qualify the HAZ Charpy at that temperature, not only the weld metal.

Typical consumables: E62- or E69-class low-hydrogen consumables, matched to the 670 MPa tensile floor. Shops work to GB 50661 or AWS D1.1. Write the CEV basis (actual heat, not table maximum) into the WPS.

Heat Treatment and Delivery Condition

Q550GJE is delivered QT (quenched and tempered, including in-line direct quenching) or TMCP / TMCP+T. Hot-rolled and normalized delivery are not allowed for this grade.

Most building orders at this level ship QT. TMCP plate is possible on thinner sizes and gives a lower CEV cap, but not every mill can hold the GJ yield ceiling on TMCP plate up to 50 mm.

Tempering temperature and time are mill data. We ask for them on the MTC when the fabricator plans post-weld heat treatment, so that PWHT stays below the tempering temperature. QT references: GB/T 16270 Q550E and EN 10025-6 S550QL.

Test lots follow clause 9.2 of GB/T 19879-2023; retests and judgement follow GB/T 17505.

Dimensions

Usual Q550GJE supply range from SHH STEEL:

  • Thickness: 12 mm – 50 mm
  • Width: 1500 mm – 3000 mm standard; wider by mill confirmation; QT width depends on the mill’s quench line
  • Length: 3000 mm – 12000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, on the mean of maximum and minimum thickness, 7.85 g/cm³

Column flanges, diaphragms, stiffeners and gussets are cut to drawing. Rolled sections for the same frame are under steel beam profiles and steel structural profiles.

Tolerances

GB/T 19879-2023 sends dimensions and shape to GB/T 709-2019. Thickness tolerance is Class B by default: fixed minus 0.30 mm, plus by thickness and width. Class C (zero minus) is available by agreement.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50

Flatness and width follow GB/T 709. EN 10029 or ASTM A6 tolerances are possible if written on the order.

Supplementary Requirements

Q550GJE already fixes strength, yield window, CEV and −40°C impact. Anything more goes on the purchase order.

  • Edition: GB/T 19879-2023 or -2015. Never write only Q550.
  • Product analysis: ask for a second chemistry column checked to GB/T 222.
  • Through-thickness: add Z15, Z25 or Z35, e.g. Q550GJEZ25.
  • Delivery route: QT or TMCP, and the CEV/Pcm basis.
  • Yield ratio: the designer’s limit, since the standard leaves it to agreement.
  • Tempering data on the MTC if the fabricator plans post-weld heat treatment.
  • Impact: extra test positions (e.g. quarter thickness) or transverse tests, if the owner wants them beyond the E letter.
  • Tolerance: Class C for zero minus.
  • Inspection: EN 10204 3.2 with SGS, BV, TÜV or a named inspector.

Q550GJE Price Factors and How to Order

A Q550GJE price per ton is a base price plus extras. The extras explain most gaps between quotes.

Cost driver Effect on price
GJ grade over general Q550 plate Grade extra for cleaner steel, yield control and CEV
Quality letter E Highest letter extra: −40°C testing, cleaner melt, more retest risk
Delivery route QT line time is the main cost driver at this level
Thickness 12–20 mm and 40–50 mm carry the most care; 20–40 mm is the core range
Z15 / Z25 / Z35 Desulfurization, plate-by-plate Z test and UT; Z35 costs most
Width and length Over 3000 mm wide or 12 m long needs mill confirmation
Quantity per size Mill rolling minimums per size; small lots come from stock or combined rolling
Inspection and cutting 3.2 witness, profile cutting, blasting and priming are quoted per item

To get a firm quote in one round, send:

  • Grade and edition, e.g. Q550GJEZ25 to GB/T 19879-2023
  • Thickness × width × length and pieces or tonnes
  • Delivery route, UT standard and class
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line, so you can compare like with like. Need a different letter? See Q550GJD.

Applications

Sector Typical Q550GJE components
Long-span roofs Compression chords and diagonals where weight governs
Tall buildings Outrigger and belt truss members, hanger plates
Heavy industrial buildings Crane-runway and support members
Special structures Members where crane capacity or connection size limits plate thickness

E grade is for the coldest sites and for owners who specify −40°C for every primary member.

It is not boiler or pressure-vessel plate (pressure vessel steel plates), and members thicker than 50 mm move to GB/T 16270 or EN 10025-6.

Supply Capability and Global Delivery

SHH STEEL sources Q550GJE from first-line building-steel mills: Wuyang (Wugang), a drafting mill of GB/T 19879, plus Valin Xiangtan and Shougang QT lines.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness
  • Tests: tensile, −40°C Charpy, bend, Z test to GB/T 5313, UT to GB/T 2970, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blast and primer
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill

We ship GB, ASTM, ASME, EN, DIN and JIS plate to the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Q550GJE mostly goes to EPC contractors building Chinese-code projects abroad.

QT plate is rolled and heat treated to order: about 45–60 days; 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Singapore and 28–35 days to Rotterdam.

Why Choose SHH STEEL

SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. For Q550GJE that means real GJ plate at mill price, not relabelled general structural plate.

Before shipment we check four lines on every certificate: yield inside the GJ window, yield ratio inside the agreed limit, CEV inside the thickness band for the delivery route, and −40°C impact at 47 J or more. If one fails, the plate does not ship as GJ.

We also tell buyers when they are over-specifying. If a member is thicker than 50 mm, we tell you before quoting: it cannot be Q550GJE. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q550GJE steel?
Q550GJE is high-strength building structure steel plate to GB/T 19879-2023, delivered quenched and tempered or TMCP in 12–50 mm. It has 550 MPa minimum yield, 550–690 MPa yield above 20 mm, 670 – 830 MPa tensile, a CEV cap of 0.54% (QT) and Charpy impact of at least 47 J at −40°C.
What is the difference between Q550GJE and S550QL?
S550QL (EN 10025-6) is QT plate with ≥550 MPa yield up to 50 mm, no yield ceiling and no yield-ratio rule, made to 150 mm. Q550GJE (GB/T 19879-2023) is QT or TMCP building plate, 12–50 mm, with 550–690 MPa yield above 20 mm, 670 – 830 MPa tensile, a CEV cap of 0.54% (QT) and 47 J at −40°C.
Is Q550GJE suitable for −40°C service?
Yes. Q550GJE is Charpy tested at −40°C and must average at least 47 J on longitudinal specimens. GB/T 19879 has no colder letter, so for design temperatures below −40°C look at GB/T 16270 Q550F or EN 10025-6 S550QL1 (−60°C) and check the yield-cap rules separately.
What CEV does Q550GJ have?
CEV is capped at 0.54% for QT plate and 0.47% for TMCP plate up to 50 mm. For TMCP plate a Pcm of 0.29% is listed for reference, and Pcm may replace CEV only if agreed in the contract.
Is GB/T 19879-2015 still valid?
No. GB/T 19879-2023 replaced GB/T 19879-2015 from 1 April 2024. Drawings may still name the 2015 edition, so state the edition on the order; the mill then tests to the matching tables.
What is the ASTM or EN equivalent of Q550GJE?
The closest European grade is EN 10025-6 S550QL; the closest Chinese non-building grades are GB/T 16270 Q550E (QT) and GB/T 1591 Q550ME (TMCP). They match strength only: Q550GJE adds a 690 MPa yield ceiling, a CEV cap and a 50 mm thickness limit.

Conclusion

Q550GJE steel plate to GB/T 19879 is building structure plate with 550 MPa minimum yield, a capped yield window, a yield ratio agreed in the contract and 47 J impact at −40°C. It shares its chemistry with Q550GJC but proves toughness at its own letter. It is not general structural plate under GB/T 1591 or GB/T 16270.

SHH STEEL supplies Q550GJE with heat analysis, CEV, yield ratio and impact on an EN 10204 3.1 or 3.2 certificate, and adds a product analysis checked to GB/T 222 when you need it. Z15, Z25 or Z35, UT to GB/T 2970, Class B or C tolerance, cutting and blasting are available.

We ship from Shanghai to buyers worldwide. Browse the full GB/T 19879 range or other carbon steel plates.

Send the edition, quality letter, Z level and size list; we confirm mill, delivery route, lead time and price in one reply. Contact SHH STEEL for a mill-direct quotation on Q550GJE building steel plate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X