Q235GJB Building Steel Plate GB/T 19879 Supplier
What is Q235GJB Building Steel Plate GB/T 19879?
Q235GJB, also written GB/T 19879 Q235GJB, Q235GJ-B or Q235 GJB, is a hot-rolled steel plate for building structures. Q stands for yield, 235 is the minimum lower yield strength in MPa, GJ (gao jian) marks high-performance building steel, and B is the quality grade with Charpy V-notch impact at +20°C.
The GJ letters are the whole point. Ordinary Q235B only sets a minimum yield. Q235GJB also sets a maximum yield, limits the yield ratio to 0.80, caps carbon equivalent by thickness and tightens phosphorus and sulfur. Those rules give a frame room to yield and redistribute load in an earthquake before it fractures. That is why Chinese structural designers name GB/T 19879 on columns, transfer girders and node plates in tall and long-span buildings.
The standard covers Q235GJ plate from 6 mm to 150 mm. GB/T 19879-2015 was replaced by GB/T 19879-2023 from 1 April 2024. The 2023 edition keeps the Q235GJ yield ratio and CEV limits, but it revises some thickness bands and delivery codes, so the certificate must print the edition the drawing names. Higher-strength sister grades are Q345GJ (Q355GJ in the 2023 edition), Q390GJ, Q420GJ and Q460GJ. All grades of this family, from Q235GJ to Q690GJ, are grouped under GB/T 19879. When the drawing asks for general structural plate without the GJ rules, the right family is GB/T 1591 or structural steel plates.
SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We roll and ship Q235GJB plate from first-line building-steel mills, print heat analysis, CEV and yield ratio on the certificate, and cut to size before export. Related pages include carbon steel plates and the structural steel plates range.
Material Specification
| Specification element | Requirement | SHH STEEL compliance |
|---|---|---|
| Plate standard | GB/T 19879-2015 Q235GJB (or GB/T 19879-2023 when named) | Confirmed |
| Other search names | Q235GJ-B, Q235GJ B, Q235 GJB, building structure steel plate | Covered |
| Thickness range in the standard | 6 mm – 150 mm | Confirmed |
| Lower yield strength ReL | 235 MPa min; upper limit applies above 16 mm | Confirmed |
| Yield ratio ReL/Rm | ≤ 0.80 | Printed on MTC |
| Quality grade | B, Charpy impact at +20°C, KV2 ≥ 47 J | Confirmed |
| Steelmaking | BOF or EAF with secondary (ladle) refining | Confirmed |
| Delivery condition | Hot rolled, controlled rolled or normalized | As ordered |
| Through-thickness option | Z15, Z25 or Z35 to GB/T 5313 | As ordered |
| Dimensional standard | GB/T 709, thickness tolerance Class B | Confirmed |
| Certification | EN 10204 3.1 or 3.2 | As ordered |
| Not this page | GB/T 700 Q235B, GB/T 1591 Q355B | Different books |
Buyers who compare grade names often land on GB/T 1591 Q355B, EN 10025-2 S235JR or ASTM A36. None of them carries the GJ yield cap or yield-ratio rule, so none is a direct swap.
Chemical Composition: Heat Analysis and Product Analysis
GB/T 19879 checks chemistry twice. The heat (ladle) analysis is taken from the melt and must meet Table 1 of the standard. The product analysis is taken from the finished plate and may sit slightly outside Table 1, by the permitted deviations of GB/T 222. Both are acceptance checks, but they are not the same number.
Q235GJB and Q235GJC share one chemistry column. D and E grades tighten carbon, phosphorus and sulfur for −20°C and −40°C testing.
Table 1. Heat (ladle) analysis, GB/T 19879-2015 / -2023 Table 1, %
| Element | Q235GJB heat analysis (%) | Q235GJB / Q235GJC | Q235GJD / Q235GJE |
|---|---|---|---|
| C, max | 0.20 | 0.20 | 0.18 |
| Si, max | 0.35 | 0.35 | 0.35 |
| Mn | 0.60 – 1.50 | 0.60 – 1.50 | 0.60 – 1.50 |
| P, max | 0.025 | 0.025 | 0.020 |
| S, max | 0.015 | 0.015 | 0.010 |
| Als, min | 0.015 | 0.015 | 0.015 |
| Cr, max | 0.30 | 0.30 | 0.30 |
| Cu, max | 0.30 | 0.30 | 0.30 |
| Ni, max | 0.30 | 0.30 | 0.30 |
| Mo, max | 0.08 | 0.08 | 0.08 |
| V + Nb + Ti, max (if combined) | 0.15 | 0.15 | 0.15 |
Total aluminium (Alt ≥ 0.020%) may replace acid-soluble aluminium. If Al, V, Nb or Ti is added alone or together at 0.015% or more, the minimum aluminium does not apply. The limits are identical in the 2015 and 2023 editions.
Table 2. Product analysis limits for Q235GJB, GB/T 19879 with GB/T 222-2025 Table 1, %
| Element | Heat limit (%) | Permitted deviation, GB/T 222 | Q235GJB product analysis limit (%) |
|---|---|---|---|
| C | ≤ 0.20 | +0.02 | ≤ 0.22 |
| Si | ≤ 0.35 | +0.03 | ≤ 0.38 |
| Mn | 0.60 – 1.50 | ±0.06 | 0.54 – 1.56 |
| P | ≤ 0.025 | +0.005 | ≤ 0.030 |
| S | ≤ 0.015 | +0.005 | ≤ 0.020 |
| Als | ≥ 0.015 | −0.003 | ≥ 0.012 |
| Cr | ≤ 0.30 | +0.05 | ≤ 0.35 |
| Cu | ≤ 0.30 | +0.05 | ≤ 0.35 |
| Ni | ≤ 0.30 | +0.05 | ≤ 0.35 |
| Mo | ≤ 0.08 | Not listed in Table 1 | Agree in contract (see note) |
| V, Ti (each, if added) | — | +0.02 / −0.01 | Heat value + 0.02 |
| Nb (if added) | — | ±0.005 | Heat value ± 0.005 |
The deviation band is picked by the upper limit in Table 1, so Mn takes ±0.06% at both ends. For one heat, an element may deviate in one direction only. Mo has no entry in GB/T 222 Table 1, so any product limit is agreed in the contract. V+Nb+Ti is a heat-analysis sum; deviations apply per element.
GB/T 222-2025 replaced GB/T 222-2006 on 1 December 2025. The C, Si, Mn, P, Cu, Cr and Ni deviations did not change; sulfur now has sub-classes, and Al, N and Ca rows were added.
Z-grade plate adds a heat sulfur limit from GB/T 5313: Z15 ≤ 0.010%, Z25 ≤ 0.007%, Z35 ≤ 0.005%. CEV and Pcm are always calculated from the heat analysis. SHH STEEL prints the heat values and adds a product-analysis column on request.
Mechanical Properties
Buyers search Q235GJB mechanical properties, Q235GJB yield strength and Q235GJB yield ratio. The values below are Table 4 of GB/T 19879-2015 for Q235GJ. Tensile tests are transverse; Charpy specimens are longitudinal.
| Thickness | Lower yield ReL (MPa) | Tensile Rm (MPa) | Yield ratio, max | Elongation A, min |
|---|---|---|---|---|
| 6 – 16 mm | ≥ 235 | 400 – 510 | 0.80 | 23% |
| > 16 – 50 mm | 235 – 345 | 400 – 510 | 0.80 | 23% |
| > 50 – 100 mm | 225 – 335 | 400 – 510 | 0.80 | 23% |
| > 100 – 150 mm | 215 – 325 | 380 – 510 | 0.80 | 23% |
| Test | Q235GJB requirement |
|---|---|
| Charpy V-notch, longitudinal | +20°C, KV2 ≥ 47 J (average of 3) |
| Single value | May fall below 47 J but not below 70% of it |
| Sub-size, >8 – <12 mm plate | 7.5 × 10 mm specimen, ≥ 75% of required value |
| Sub-size, 6 – 8 mm plate | 5 × 10 mm specimen, ≥ 50% of required value |
| 180° bend | D = 2a up to 16 mm; D = 3a above 16 mm |
Grade B is the +20°C letter. If the project needs 0°C, order Q235GJC; for −20°C order Q235GJD; for −40°C order Q235GJE. The energy stays 47 J in each case.
Through-thickness ductility is optional and applies to plate 15 mm and thicker. It is tested to GB/T 5313 and reported as reduction of area Z:
| Z grade | Average of 3 specimens, min | Single specimen, min |
|---|---|---|
| Z15 | 15% | 10% |
| Z25 | 25% | 15% |
| Z35 | 35% | 25% |
A Z-grade plate is marked by adding the level after the quality letter, for example Q235GJBZ25. Density for theoretical weight is 7.85 g/cm³.
Under GB/T 19879-2023 yield is reported as upper yield ReH, and the Q235GJ bands become: ≥235 MPa to 16 mm, 235–345 MPa for >16–100 mm, and 215–325 MPa for >100–150 mm, with Rm 400–510 MPa to 100 mm. Write the edition on the order.
Q235GJB vs Q235B: Why Buildings Specify GJ Steel
Q235B and Q235GJB share a 235 MPa yield on paper, and Q235B is cheaper. Seismic design cares about what happens after yield. Ordinary Q235B can leave the mill well above 300 MPa with a high yield ratio, which moves plastic hinges into welds and columns. GJ steel keeps the yield inside a 110 MPa window and the ratio at 0.80 or lower.
| Grade | Standard | Yield, thin plate | Upper yield limit | Yield ratio limit | Impact |
|---|---|---|---|---|---|
| Q235GJB | GB/T 19879 | 235 MPa | Yes, above 16 mm | ≤ 0.80 | +20°C, 47 J |
| Q235GJC | GB/T 19879 | 235 MPa | Yes | ≤ 0.80 | 0°C, 47 J |
| Q235B | GB/T 700 | 235 MPa | No | No | +20°C, 27 J |
| GB/T 1591 Q355B | GB/T 1591 | 355 MPa | No | No | +20°C, 34 J |
| EN 10025-2 S235JR | EN 10025-2 | 235 MPa | No | No | +20°C, 27 J |
| JIS G3106 SM400B | JIS G3106 | 245 MPa | No | No | 0°C, 27 J |
| ASTM A36 | ASTM A36 | 250 MPa | No | No | Not required |
The main difference between Q235GJB and Q235B is control. Q235B under GB/T 700 allows up to 0.045% phosphorus and sulfur, has no yield cap and no yield-ratio rule. Q235GJB holds P ≤ 0.025% and S ≤ 0.015%, keeps yield inside a 110 MPa window above 16 mm, and doubles the impact energy floor to 47 J.
Moving up in strength, Q345GJ is the next GJ grade. If the drawing only needs 355 MPa without the GJ rules, GB/T 1591 Q355C, GB/T 1591 Q355NB or GB/T 1591 Q355MB are the general structural choices. EN 10025-2 S275J0 and EN 10025-2 S355J2 are the usual European comparisons in that range.
Equivalent Material Grades
No foreign grade copies every GB/T 19879 rule. The closest counterpart is JIS G3136 SN400B, a Japanese building-structure plate that also limits the yield range and yield ratio. Other grades below match strength level only.
| Designation | Region | Standard | Notes |
|---|---|---|---|
| Q235GJB | China | GB/T 19879 | Grade on this page |
| SN400B | Japan | JIS G3136 | Closest building-steel counterpart; check impact temperature |
| JIS G3106 SM400B | Japan | JIS G3106 | Welded structural plate; no yield-ratio rule |
| EN 10025-2 S235JR | Europe | EN 10025-2 | Strength comparison, +20°C, 27 J |
| EN 10025-2 S235J0 | Europe | EN 10025-2 | 0°C comparison, nearer Q235GJC |
| EN 10025-2 S235J2 | Europe | EN 10025-2 | −20°C comparison, nearer Q235GJD |
| ASTM A36 | USA | ASTM A36 | About 250 MPa yield, no ratio limit |
| ASTM A709 Grade 36 | USA | ASTM A709 | Bridge grade, strength comparison |
| DIN 17100 St37-3 | Germany | DIN 17100 (withdrawn) | Legacy name on old drawings |
| ASTM A283 Grade C | USA | ASTM A283 | Lower yield, not a substitute |
Through-thickness grades map loosely to EN 10164 Z15/Z25/Z35, which are added to EN 10025-2 plate in Europe. SHH STEEL does not dual-mark ASTM A36/A36M or JIS G3106 on a Q235GJB certificate unless the purchase order names both books and both tables are met.
Building Structure Service
Q235GJB is chosen when a building frame needs ductility more than strength. The capped yield keeps the real plate close to design yield, so plastic hinges form where the engineer put them. The 0.80 yield ratio leaves a reserve between yield and fracture. Low CEV keeps heavy welded joints manageable on site.
Typical drawings that call it out are box and H columns in high-rise towers, transfer girders, long-span roof trusses, stadium and terminal space frames, and the thick node plates where beams meet columns. Where those plates carry tension across their thickness, the designer adds Z15, Z25 or Z35 to resist lamellar tearing.
It is the wrong plate when the drawing needs 345 MPa or higher. That work is Q345GJ or, for non-seismic members, GB/T 1591. It is the wrong plate for a pressure vessel, which belongs on pressure vessel steel plates. It is the wrong plate for exposed bare steel; that is weathering steel plates. For rolled sections in the same frame, see steel beam profiles.
Weldability
Q235GJB is readily weldable. GB/T 19879 requires the carbon equivalent to be calculated from the heat analysis and printed on the certificate:
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
By agreement written in the contract, the weld-cracking parameter Pcm can be used instead:
Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B
| Thickness | CEV, max (%) | Pcm, max (%) |
|---|---|---|
| ≤ 50 mm | 0.34 | 0.24 |
| > 50 – 100 mm | 0.36 | 0.26 |
| > 100 – 150 mm | 0.38 | 0.27 |
Limits apply to hot-rolled, controlled-rolled and normalized Q235GJ. Thin plate usually welds without preheat. Thick column plate, high restraint or cold sites still need preheat set by the qualified WPS, not by the grade name.
Common consumables are E43-class (about 420 MPa weld metal) low-hydrogen electrodes and wires, or E70xx-type equivalents. Fabricators work to GB 50661 in China or AWS D1.1 abroad. A procedure qualified on ASTM A36 or ASME SA36 can be a starting point, but it should be re-checked against the actual CEV and thickness. We share mill heat data for that review.
Heat Treatment and Delivery Condition
GB/T 19879-2015 lists three delivery conditions for Q235GJ: hot rolled (WAR), controlled rolled (WCR) and normalized (N). The 2023 edition writes them as AR, CR, NR and N. The condition is agreed and written in the contract.
Most Q235GJB plate up to about 50 mm ships as hot rolled or controlled rolled. Thick plate, Z25/Z35 plate and orders with tight UT classes are often normalized, which evens out grain size through the section. Steel is made in BOF or EAF and ladle refined.
Q235GJB is not quenched and tempered. QT building and machinery plate sits under GB/T 16270, for example GB/T 16270 Q460C. For a European normalized comparison see EN 10025-3 S275N in EN 10025-3; for a TMCP comparison see EN 10025-4 S275M in EN 10025-4.
Plates are tested in batches of the same heat, thickness and delivery condition, no more than 60 t per batch. Batches by rolled plate are possible by agreement. The certificate shows grade, heat number, delivery condition, chemistry, CEV or Pcm, tensile, yield ratio, impact and any Z test.
Dimensions
Usual Q235GJB supply range from SHH STEEL:
- Thickness: 6 mm – 150 mm as allowed by GB/T 19879; most orders 8 mm – 100 mm
- Width: 1500 mm – 3000 mm standard; wider plate by mill confirmation
- Length: 3000 mm – 12000 mm; longer plate by enquiry
- Edge: mill edge or sheared/cut edge
- Weight: theoretical, calculated on the average of maximum and minimum allowed thickness at 7.85 g/cm³
Cut-to-size column flanges, stiffeners, base plates and gussets are available. More sizes are listed under structural steel plates.
Tolerances
GB/T 19879-2015 sends dimensions and shape to GB/T 709-2006 (now revised as GB/T 709-2019). Thickness tolerance is Class B by default: a fixed minus of 0.30 mm with a plus value by thickness and width. Class C (zero minus) is available when agreed.
| Nominal thickness (mm) | Width ≤ 1500 mm | Width > 1500 – 2500 mm |
|---|---|---|
| > 8 – 15 | −0.30 / +0.80 | −0.30 / +1.00 |
| > 15 – 25 | −0.30 / +1.00 | −0.30 / +1.20 |
| > 25 – 40 | −0.30 / +1.10 | −0.30 / +1.30 |
| > 40 – 60 | −0.30 / +1.30 | −0.30 / +1.50 |
| > 60 – 100 | −0.30 / +1.50 | −0.30 / +1.80 |
| > 100 – 150 | −0.30 / +2.10 | −0.30 / +2.50 |
Width, length, flatness and squareness follow GB/T 709. Wider plates take the larger plus values of the same table. When a buyer abroad wants EN 10029 class B or ASTM A6 instead, write it on the order and SHH STEEL will confirm it with the mill before rolling.
Supplementary Requirements
Q235GJB already fixes strength, yield ratio, CEV and +20°C impact. Anything beyond that must be written on the purchase order.
- Standard edition. Write GB/T 19879-2015 or GB/T 19879-2023. Do not write only Q235.
- Quality letter. B is +20°C. Write Q235GJC, D or E for 0°C, −20°C or −40°C.
- Through-thickness. Add Z15, Z25 or Z35, for example Q235GJBZ25. Z plates are UT tested plate by plate.
- Ultrasonic testing. Name GB/T 2970 and the acceptance class, or EN 10160 / ASTM A578 if the owner requires.
- Delivery condition. Write normalized if hot rolled is not acceptable.
- Weld index. Write Pcm if it should replace CEV.
- Tolerance. Write Class C if zero minus thickness is required.
- Product analysis. Write it if a second chemistry column is needed.
- Surface. Shot blasting and shop primer, if needed before shipment.
- Inspection. EN 10204 3.2 with SGS, BV, TÜV, Lloyd’s or the named inspector.
Z15, Z25 and Z35 Through-Thickness Plate Explained
Welded T, cruciform and corner joints pull a plate through its thickness. Sulfide inclusions in ordinary plate can split into steps under that load. This is lamellar tearing, and it often shows up only after welding.
Z grades prove the plate can take that load. A tensile specimen is cut through the thickness and its reduction of area is measured to GB/T 5313-2023.
| Z grade | Heat sulfur, max | Reduction of area, avg of 3 | Single, min | Typical use |
|---|---|---|---|---|
| Z15 | 0.010% | 15% | 10% | Moderate restraint, thinner nodes |
| Z25 | 0.007% | 25% | 15% | Column flanges, beam-to-column plates |
| Z35 | 0.005% | 35% | 25% | Thick, highly restrained nodes |
Z grades apply to plate 15 mm and thicker. Z25 and Z35 plate is tested plate by plate, and UT to GB/T 2970 is part of the requirement. The grade is written after the quality letter, for example Q235GJBZ25.
Specify the level the joint needs, not the highest one. Z35 costs more and limits mill choice. All Z options are available across the GB/T 19879 range.
Applications
| Sector | Typical Q235GJB components |
|---|---|
| High-rise buildings | Box column plates, H-column flanges, transfer girders |
| Long-span structures | Roof trusses, space-frame nodes, stadium and airport roofs |
| Seismic frames | Beam-to-column connection plates, link and brace gussets |
| Industrial buildings | Crane girders, mezzanine framing, base plates |
| Public works | Exhibition halls, railway stations, convention centres |
Q235GJB suits members sized by stiffness or ductility, not strength. When 345 MPa is needed, move to Q345GJ. When the job is a bridge in North America, the normal books are ASTM A709 or ASTM A572 Gr.50 under ASTM A572.
Supply Capability
SHH STEEL supplies Q235GJB from first-line Chinese building-steel mills. Partner mills include Wuyang (Wugang), one of the drafting mills of GB/T 19879, plus Hanye, Xinyu, Shougang, Angang and other qualified mills when size requires.
- Certificates: EN 10204 3.1 as standard; EN 10204 3.2 with third-party witness.
- Testing: tensile, Charpy, bend, Z-direction to GB/T 5313, UT to GB/T 2970.
- Processing: CNC plasma and flame cutting, bevelling, drilling, flattening, shot blast and primer.
- Terms: FOB Shanghai main, CFR and CIF available. Payment by TT, LC, or TT + LC.
- Packing: bundled or loose, steel-stamped and paint-marked with grade, heat, size and mill.
Global Delivery and Markets
SHH STEEL supplies GB, ASTM, ASME, EN, DIN and JIS plate to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Q235GJB usually goes to contractors and fabricators building projects designed to Chinese codes abroad, for example EPC towers, terminals and industrial parks.
Typical lead time: stock sizes about 5–7 days; mill rolling about 30–45 days; 3.2 inspection or Z35 plate adds about 1–2 weeks. Ocean time from Shanghai: Singapore 7–12 days, Jebel Ali 18–25 days, Rotterdam 28–35 days, US Gulf 28–35 days.
Why Choose SHH STEEL
SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. For Q235GJB that means mill price on building-grade plate, not a stockist mark-up on relabelled Q235B.
We check three lines on every certificate before shipment: the yield sits inside the GJ window, the yield ratio is ≤ 0.80, and CEV is inside the thickness band. If one fails, the plate does not ship as GJ.
We will not upgrade DIN 17100 St37-2 or plain Q235B paper to Q235GJB, and we will not drop Z25 to save a UT pass. If the drawing really needs 355 MPa, we will say so and quote Q345GJ or GB/T 1591 Q355B instead.
FAQ
-
What is Q235GJB steel?
- Q235GJB is high-performance building structure steel plate to GB/T 19879. It has 235 MPa minimum yield, a yield cap above 16 mm, a yield ratio of 0.80 or less, CEV limits and Charpy impact of at least 47 J at +20°C. GJ stands for gao jian, high-performance building steel.
-
What is the difference between Q235GJB and Q235B?
- Q235B (GB/T 700) only sets a minimum yield and 27 J at +20°C. Q235GJB (GB/T 19879) adds a maximum yield, a 0.80 yield ratio limit, CEV limits, lower P and S, and 47 J impact. Q235GJB can replace Q235B; Q235B cannot replace Q235GJB.
-
Should I specify Q235GJB or Q235GJC?
- Choose by the lowest service temperature. Q235GJB is impact tested at +20°C and Q235GJC at 0°C, both at 47 J minimum. Chemistry, strength, yield ratio and CEV are the same. Use Q235GJD (−20°C) or Q235GJE (−40°C) for colder sites.
-
What is the equivalent of Q235GJB?
- There is no exact equivalent. The closest is JIS G3136 SN400B, which also limits yield range and yield ratio. EN 10025-2 S235JR and ASTM A36 match strength only; they have no yield cap or ratio limit, so they are not direct substitutes.
-
What is the difference between heat analysis and product analysis?
- Heat (ladle) analysis is taken from the molten steel and must meet the standard's table. Product analysis is taken from the finished plate and may exceed the table by the deviations in GB/T 222, for example +0.02% carbon or +0.005% phosphorus. CEV is always calculated from the heat analysis.
-
Is GB/T 19879-2015 still valid?
- No. GB/T 19879-2023 replaced GB/T 19879-2015 from 1 April 2024. Q235GJ chemistry, CEV, yield ratio and 47 J impact are unchanged, but the 2023 edition uses upper yield ReH, new thickness bands and AR/CR/NR/N delivery codes. State the edition on the order.
Conclusion
Q235GJB steel plate to GB/T 19879 is building structure plate with 235 MPa yield, a capped yield range, a 0.80 yield ratio limit and 47 J impact at +20°C. It is not ordinary GB/T 700 Q235B, and it is not GB/T 1591 Q355B under GB/T 1591. The nearest foreign counterpart is JIS G3136 SN400B; EN 10025-2 S235JR, ASTM A36 and JIS G3106 SM400C match strength only.
Whether the inquiry says Q235GJB, Q235GJ-B or Q235GJBZ25, SHH STEEL supplies plate with full GJ chemistry, CEV or Pcm, yield ratio and impact on an EN 10204 3.1 or 3.2 certificate. We add Z15, Z25 or Z35, UT to GB/T 2970, GB/T 709 Class B or C tolerances, cutting and shot blast to the order.
We ship from Shanghai to the United States, Europe, the Middle East, Africa, Asia and South America. Browse the full GB/T 19879 range, or other high strength low alloy plates.
Contact SHH STEEL for mill rolling, Z-direction testing, UT, third-party inspection or a worldwide quotation for Q235GJB building steel plate.