EN 10028-3 P355NL1 Steel Plate | P355NL1 -40°C Vessel Plate supplier
What is EN 10028-3 P355NL1 Steel?
P355NL1 is the −40 °C quality in the P355 family of EN 10028-3. Buyers search EN 10028-3 P355NL1, P355NL1 steel plate, 1.0566, P355NL1 -40°C vessel plate and P355NL1 supplier. NL1 is the low-temperature letter set. This page is not P355N. N is room-temperature quality. This page is not P355NH. NH is elevated-temperature quality. This page is not P355NL2. NL2 is −50 °C. This page is not EN 10028-2 P355GH. This page is not S355NL. S355NL is EN 10025-3 structural steel.
Yield is 355 MPa at ≤16 mm. Tensile is 490–630 MPa. Steel number is 1.0566. Delivery is normalized (+N). Charpy is specified at −40 °C when the order follows NL1. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-3, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.
If a drawing says P355N, we will not ship P355NL1 and call 355 enough. If a drawing says P355NL2, we will not ship P355NL1 and call minus forty close to minus fifty. Dual marking with 16MnDR steel plate is possible only when both books are fully met.
Company scope: global exporter SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | EN 10028-3 P355NL1 | Confirmed |
| Steel number | 1.0566 | Confirmed |
| Product specification | EN 10028-3 + EN 10028-1 | Applied |
| Steel type | Weldable fine-grain, normalized, −40 °C | Confirmed |
| Usual delivery | +N normalized | Confirmed |
| Yield idea | 355 MPa at ≤16 mm | Confirmed |
| Tensile | 490–630 MPa at ≤16 mm | Confirmed |
| Impact idea | −40 °C | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates and carbon steel plates. Chinese −40 °C comparisons belong on GB/T 713.3. EN 10028-2 high-temperature sisters belong on EN 10028-2.
Chemical Composition
EN 10028-3 P355NL1 Steel Plate | P355NL1 -40°C Vessel Plate supplier
Brief Description
EN 10028-3 P355NL1 is European normalized fine-grain low-temperature vessel plate, steel number 1.0566. Yield is 355 MPa at ≤16 mm. Impact is −40 °C. SHH STEEL supplies P355NL1 worldwide as a global steel mill sourcing partner.
SEO Title
EN 10028-3 P355NL1 Steel Plate | P355NL1 -40°C Vessel Plate supplier – SHH STEEL
SEO Keywords
EN 10028-3 P355NL1, P355NL1, P355NL1 steel plate, 1.0566, P355NL1 -40°C vessel plate, P355NL1 equivalent, P355NL1 supplier
SEO Description
SHH STEEL supplies EN 10028-3 P355NL1 -40°C fine grain vessel plate worldwide, 355 MPa yield, 490–630 MPa tensile, steel number 1.0566. EN 10204 3.1/3.2 mill-direct supply. Contact now.
General Description
P355NL1 is the −40 °C quality in the P355 family of EN 10028-3. Buyers search EN 10028-3 P355NL1, P355NL1 steel plate, 1.0566, P355NL1 -40°C vessel plate and P355NL1 supplier. NL1 is the low-temperature letter set. This page is not P355N. N is room-temperature quality. This page is not P355NH. NH is elevated-temperature quality. This page is not P355NL2. NL2 is −50 °C. This page is not EN 10028-2 P355GH. This page is not S355NL. S355NL is EN 10025-3 structural steel.
Yield is 355 MPa at ≤16 mm. Tensile is 490–630 MPa. Steel number is 1.0566. Delivery is normalized (+N). Charpy is specified at −40 °C when the order follows NL1. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-3, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.
If a drawing says P355N, we will not ship P355NL1 and call 355 enough. If a drawing says P355NL2, we will not ship P355NL1 and call minus forty close to minus fifty. Dual marking with 16MnDR steel plate is possible only when both books are fully met.
Company scope: global exporter SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | EN 10028-3 P355NL1 | Confirmed |
| Steel number | 1.0566 | Confirmed |
| Product specification | EN 10028-3 + EN 10028-1 | Applied |
| Steel type | Weldable fine-grain, normalized, −40 °C | Confirmed |
| Usual delivery | +N normalized | Confirmed |
| Yield idea | 355 MPa at ≤16 mm | Confirmed |
| Tensile | 490–630 MPa at ≤16 mm | Confirmed |
| Impact idea | −40 °C | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates and carbon steel plates. Chinese −40 °C comparisons belong on GB/T 713.3. EN 10028-2 high-temperature sisters belong on EN 10028-2.
Chemical Composition
Cast analysis follows EN 10028-3. Product analysis follows EN 10028-1 when ordered.
Cast Analysis and Product Analysis — EN 10028-3 P355NL1 (1.0566)
| Element | Cast Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), max | 0.18 | 0.20 |
| Silicon (Si), max | 0.50 | 0.55 |
| Manganese (Mn) | 1.10 – 1.70 | 1.05 – 1.80 |
| Phosphorus (P), max | 0.025 | 0.030 |
| Sulfur (S), max | 0.010 | 0.013 |
| Aluminum total (Al), min | 0.020 | 0.015 |
| Nitrogen (N), max | 0.012 | 0.014 |
| Chromium (Cr), max | 0.30 | 0.35 |
| Copper (Cu), max | 0.30 | 0.35 |
| Molybdenum (Mo), max | 0.08 | 0.10 |
| Nickel (Ni), max | 0.50 | 0.55 |
| Niobium (Nb), max | 0.05 | 0.06 |
| Titanium (Ti), max | 0.03 | 0.04 |
| Vanadium (V), max | 0.10 | 0.12 |
Nickel may sit toward the top of the residual band because NL1 is a toughness quality. Sulfur and phosphorus stay tight. This is still C-Mn fine-grain plate, not 3.5Ni. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.
Mechanical Properties
Buyers search P355NL1 mechanical properties, P355NL1 impact and P355NL1 -40°C. Yield still falls with thickness. Impact is the NL1 item.
Tensile and Yield — EN 10028-3 P355NL1
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) |
|---|---|---|
| ≤ 16 | 355 | 490 – 630 |
| 16 – 40 | 345 | 490 – 630 |
| 40 – 60 | 335 | 490 – 630 |
| 60 – 100 | 315 | 470 – 630 |
| 100 – 150 | 295 | 460 – 630 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Elongation is typically 22% min on thinner plate. Charpy for NL1 is −40 °C. Energy is commonly 27 J average when the order follows the book. Location and orientation must be written. Do not assume NL2 −50 °C on this page.
Do not quote 355 MPa yield on an 80 mm plate. Do not treat −40 °C as permission to stamp 16MnDR steel plate or SA516 Grade 70 without checking both books.
Material Comparison
| Grade | Book | What buyers search | Swap? |
|---|---|---|---|
| EN 10028-3 P355N | EN 10028-3 | P355N steel plate | No |
| EN 10028-3 P355NH | EN 10028-3 | P355NH steel plate | No |
| EN 10028-3 P355NL1 | EN 10028-3 | P355NL1 steel plate | This page |
| EN 10028-3 P355NL2 | EN 10028-3 | P355NL2 | No |
| EN 10028-3 P275NL1 | EN 10028-3 | P275NL1 | No |
| 16MnDR steel plate | GB/T 713.3 | 16MnDR | No auto swap |
| SA662 Grade B | SA-662 | SA662 Gr.B | No auto swap |
| SA516 Grade 70 | SA-516 | SA516 Gr.70 | No |
| Q345R steel plate | GB/T 713.2 | Q345R | No |
| TStE355 steel plate | DIN 17102 | TStE355 | No |
Equivalent Material Grades
| Designation | Standard / region | Notes |
|---|---|---|
| EN 10028-3 P355NL1 / 1.0566 | EN 10028-3 | Name on this page |
| P355N / 1.0562 | EN 10028-3 | Room-temp sister |
| P355NH / 1.0565 | EN 10028-3 | Elevated-temp sister |
| P355NL2 / 1.1106 | EN 10028-3 | −50 °C sister |
| 16MnDR steel plate | GB/T 713.3 | Chinese −40 °C |
| SA662 Grade B | SA-662 | ASME low-temp carbon |
| SA516 Grade 70 | SA-516 | ASME carbon, impact extra |
| SA203 Grade A | SA-203 | 2.25Ni, different family |
| SPV355 steel plate | JIS G3115 | Japanese vessel |
| EStE355 steel plate | DIN 17102 | Fine-grain low-temp talk |
-40°C Fine-Grain Pressure-Vessel Service
Buyers pick P355NL1 when a PED file wants 355 MPa fine-grain plate and Charpy at −40 °C. Search phrases such as P355NL1 -40°C, P355NL1 boiler plate and 1.0566 steel plate all point here.
It is not a substitute for 09MnNiDR steel plate. That grade is −70 °C. It is not a substitute for 08Ni3DR steel plate. That grade is 3.5Ni. An ASME file should name SA-662 or SA-516 with a written −40 °C extra. Dual marking is possible only when both books are met.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.
Weldability
P355NL1 is killed fine-grain C-Mn vessel plate. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.
Qualify to the applicable code. Consumables must keep toughness at −40 °C. A procedure written for SA516 Grade 70 without an impact extra is not automatically valid. A nickel procedure written for SA203 Grade D is the wrong family. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized EN 10028-3 P355NL1 (+N).
If the vessel will see PWHT, say so. Impact after simulated PWHT is worth naming on a −40 °C file. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists EN 10028-3 P355NL1; 1.0566; heat number; cast analysis; product analysis when ordered; tensile to the correct thickness column; +N; Charpy at −40 °C when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for P355NL1 -40°C vessel plate:
- Thickness: commonly 6 mm – 150 mm, thicker by mill agreement
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
Structural fine-grain plate belongs on EN 10025-3. Ship plate belongs on shipbuilding steel plates.
Tolerances
Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another table. Class A is the usual default. If the calculation used minimum thickness after corrosion, write the allowed minus. Do not apply ASTM A36 structural tolerances to a PED −40 °C plate without writing them. When dual-named against SA516 Grade 70, write whether EN 10029 or SA-20 governs thickness extra.
Supplementary Requirements
Charpy details. Write −40 °C, joules, location and orientation. Do not write “impact as per EN 10028-3” and expect NL2.
Impact after simulated PWHT. When the vessel will be stress-relieved.
Product analysis. Especially P, S, Al and N.
Through-thickness / Z-test. When the plate is a thick nozzle or pad.
NDE. EN 10160 or ASTM A435 / A578 as named.
Third-party. EN 10204 3.2 when written.
Applications
| Industry | Typical components |
|---|---|
| PED low-temp vessels | EN 10028-3 P355NL1 shells at −40 °C |
| Storage tanks and drums | P355NL1 courses |
| Heat-exchanger shells | P355NL1 channels from SHH STEEL |
| Dual-certified export | P355NL1 / 16MnDR steel plate when both books fit |
| ASME comparison jobs | P355NL1 next to SA662 Grade B |
P355NL1 is the plate for a 355 MPa PED file at −40 °C that is not yet in the 3.5Ni book. It is the wrong plate for LNG inner tanks. That work belongs on 06Ni9DR steel plate. It is the wrong plate for −50 °C. That work is P355NL2.
Supply Capability
SHH STEEL sources EN 10028-3 P355NL1 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or normalizing route requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, thicker by mill agreement.
Processing: CNC or flame cutting, bevel, flattening, UT to EN 10160 or the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days; standard +N about 45 days; simulated PWHT / 3.2 about 2 months.
Company scope: worldwide delivery SHH STEEL.
Why Choose SHH STEEL
Experience on this grade is simple: keep the letters after P355. N, NH, NL1 and NL2 are four different purchase orders. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices P355NL1 from first-line mills, reports 1.0566 chemistry, records +N, prints Charpy at −40 °C when ordered, and issues 3.1 as standard or 3.2 when specified.
We keep the grade on the order. P355NL1 is not P355N. P355NL1 is not P355NH. P355NL1 is not P355NL2. P355NL1 is not Q345R steel plate. If the drawing says −50 °C, we will not ship NL1 and call minus forty close.
Company scope: global exporter SHH STEEL.
FAQ
-
What is P355NL1 steel plate?
- P355NL1 is an EN 10028-3 normalized fine-grain pressure-vessel plate, steel number 1.0566. Yield is 355 MPa at ≤16 mm and tensile is 490–630 MPa. NL1 means Charpy at −40 °C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
What is the equivalent of P355NL1?
- Related comparisons are 16MnDR and SA-662 Grade B. Dual marking is possible only when both books are fully met.
-
How is P355NL1 different from P355N and P355NH?
- N is room-temperature quality. NH is elevated-temperature quality. NL1 is −40 °C quality.
-
How is P355NL1 different from P355NL2?
- NL2 is −50 °C. Do not ship NL1 against an NL2 drawing.
-
How is P355NL1 different from 16MnDR?
- 16MnDR is GB/T 713.3. P355NL1 is EN 10028-3. Both are −40 °C talk grades, not automatic substitutes.
-
s P355NL1 the same as S355NL?
- No. S355NL is EN 10025-3 structural steel. P355NL1 is EN 10028-3 pressure-vessel plate.
Conclusion
EN 10028-3 P355NL1 Steel Plate is European normalized fine-grain −40 °C pressure-vessel plate, steel number 1.0566, at the 355 MPa yield step and 490–630 MPa tensile at ≤16 mm, usually +N. Whether the inquiry says EN 10028-3 P355NL1, 1.0566, P355NL1 -40°C Vessel Plate or P355NL1 supplier, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with P355NL1 chemistry, recorded +N, Charpy at −40 °C when ordered, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies EN 10028-3 P355NL1 -40°C Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.
Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.
EN 10028-3 P355NL1 Steel Plate, P355NL1 -40°C vessel plate, 1.0566, P355NL1 supplier, global exporter SHH STEEL