P275NH is the 275 MPa normalized fine-grain grade in EN 10028-3. Buyers search EN 10028-3 P275NH, P275NH steel plate, 1.0486, P275NH fine grain vessel plate and P275NH supplier. NH means the plate carries specified elevated-temperature properties on a normalized fine-grain route. This page is not EN 10028-2 P265GH. P265GH is non-alloy high-temperature plate without the EN 10028-3 fine-grain quality system. This page is not P275NL1 and not P275NL2. Those sisters are low-temperature qualities.
Yield is 275 MPa at ≤16 mm. Tensile is 390–510 MPa. Steel number is 1.0486. Delivery is normalized (+N). Grain refining (Al, and Nb/Ti/V when used) is part of the book. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplying this grade to the USA, Europe, Middle East, Southeast Asia, Africa and South America.
Do not ship EN 10028-2 P265GH against a P275NH drawing and call 265 close to 275. Do not ship EN 10028-2 P355GH and call carbon the same as fine-grain NH. Do not ship Q245R steel plate unless both books are written. Dual marking is possible only when chemistry, tensile, impact, grain and delivery all fit.
Company scope: global exporter SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | EN 10028-3 P275NH | Confirmed |
| Steel number | 1.0486 | Confirmed |
| Product specification | EN 10028-3 + EN 10028-1 | Applied |
| Steel type | Weldable fine-grain, normalized, elevated temperature | Confirmed |
| Usual delivery | +N normalized | Confirmed |
| Yield idea | 275 MPa at ≤16 mm | Confirmed |
| Tensile | 390–510 MPa at ≤16 mm | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | USA, Europe, Middle East, SE Asia, Africa, South America | As ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates and carbon steel plates. EN 10028-2 high-temperature sisters belong on EN 10028-2. Chinese low-temperature sisters belong on GB/T 713.3. Fine-grain structural steel is a different book: EN 10025-3.
Chemical Composition
Cast analysis follows EN 10028-3. Product analysis follows EN 10028-1 when ordered. People who search P275NH chemical composition and 1.0486 chemistry want a fine-grain killed analysis, not a P355GH table copied across.
Cast Analysis and Product Analysis — EN 10028-3 P275NH (1.0486)
| Element | Cast Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), max | 0.16 | 0.18 |
| Silicon (Si), max | 0.40 | 0.45 |
| Manganese (Mn) | 0.80 – 1.50 | 0.75 – 1.60 |
| Phosphorus (P), max | 0.025 | 0.030 |
| Sulfur (S), max | 0.010 | 0.013 |
| Aluminum total (Al), min | 0.020 | 0.015 |
| Nitrogen (N), max | 0.012 | 0.014 |
| Chromium (Cr), max | 0.30 | 0.35 |
| Copper (Cu), max | 0.30 | 0.35 |
| Molybdenum (Mo), max | 0.08 | 0.10 |
| Nickel (Ni), max | 0.30 | 0.35 |
| Niobium (Nb), max | 0.05 | 0.06 |
| Titanium (Ti), max | 0.03 | 0.04 |
| Vanadium (V), max | 0.05 | 0.06 |
Aluminum minimum is there to kill the steel and help grain size. Niobium, titanium and vanadium stay limited. This is still a C-Mn fine-grain plate, not 0.3Mo and not 1.25Cr-0.5Mo. SHH STEEL reports cast analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.
Mechanical Properties
Buyers search P275NH mechanical properties, P275NH yield strength and P275NH tensile strength. Yield falls as thickness rises. Use the thickness column on the mill certificate.
Tensile and Yield — EN 10028-3 P275NH
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) |
|---|---|---|
| ≤ 16 | 275 | 390 – 510 |
| 16 – 40 | 265 | 390 – 510 |
| 40 – 60 | 255 | 390 – 510 |
| 60 – 100 | 235 | 370 – 510 |
| 100 – 150 | 225 | 360 – 500 |
| 150 – 250 | 215 | 350 – 500 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Elongation is typically 24% min on thinner plate. Impact for NH quality is commonly specified at 0 °C, 27 J, when the order names it. Elevated-temperature proof strength is the NH reason for existing. Ask for that table when the vessel calculation uses design temperature.
Do not quote 275 MPa yield on an 80 mm plate. Do not treat 390–510 MPa tensile as permission to stamp SA516 Grade 60 or Q245R steel plate without checking both books.
Material Comparison
| Grade | Book | What buyers search | Swap? |
|---|---|---|---|
| EN 10028-2 P235GH | EN 10028-2 | P235GH steel plate | No |
| EN 10028-2 P265GH | EN 10028-2 | P265GH steel plate | No |
| EN 10028-3 P275NH | EN 10028-3 | P275NH steel plate | This page |
| EN 10028-3 P275NL1 | EN 10028-3 | P275NL1 | No |
| EN 10028-3 P275NL2 | EN 10028-3 | P275NL2 | No |
| EN 10028-3 P355NH | EN 10028-3 | P355NH | No |
| Q245R steel plate | GB/T 713.2 | Q245R | No auto swap |
| SA516 Grade 60 | SA-516 | SA516 Gr.60 | No auto swap |
| SA662 Grade A | SA-662 | SA662 Gr.A | No |
| SPV235 steel plate | JIS G3115 | SPV235 | No |
| StE255 steel plate | DIN 17102 | StE255 | No |
Equivalent Material Grades
Search habits mix P275NH equivalent, 1.0486 equivalent and P275NH vs P265GH. Those names help a buyer find the right page. They do not authorize substitution.
| Designation | Standard / region | Notes |
|---|---|---|
| EN 10028-3 P275NH / 1.0486 | EN 10028-3 | Name on this page |
| P275NL1 | EN 10028-3 | Low-temperature sister |
| P275NL2 | EN 10028-3 | Lower-temperature sister |
| EN 10028-2 P265GH | EN 10028-2 | High-temp carbon, different part |
| Q245R steel plate | GB/T 713.2 | Chinese carbon |
| SA516 Grade 60 | SA-516 | ASME carbon |
| A516 Grade 60 | A516 | ASTM twin |
| SA662 Grade A | SA-662 | Low-temp carbon |
| 16MnDR steel plate | GB/T 713.3 | −40 °C Chinese |
| SPV315 steel plate | JIS G3115 | Japanese vessel |
| WStE255 steel plate | DIN 17102 | Fine-grain comparison |
Fine-Grain Pressure-Vessel Service
Buyers pick P275NH when a PED file wants normalized fine-grain plate at the 275 MPa step with elevated-temperature values, and does not need P355NH strength or NL1 / NL2 impact. Search phrases such as P275NH boiler plate, P275NH pressure vessel plate and 1.0486 steel plate all point here.
It is not a substitute for 16MnDR steel plate. That grade is GB/T 713.3 −40 °C plate. It is not a substitute for 09MnNiDR steel plate. That grade is −70 °C nickel plate. It is not 0.3Mo plate like EN 10028-2 16Mo3.
An ASME file should name SA-516 or SA-662 and then write extras. Dual marking is possible only when both books are met. SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.
Weldability
P275NH is killed fine-grain C-Mn vessel plate in the 390–510 MPa tensile band. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.
Qualify to the applicable code. Consumables must match the P275NH tensile band. A procedure written for SA516 Grade 70 is stronger metal and is not automatically valid. A Cr-Mo procedure written for SA387 Grade 12 Class 1 is the wrong family. Fine-grain plate usually welds cleanly if heat input and hydrogen are controlled. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized EN 10028-3 P275NH (+N). As-rolled is not the default for this book. Buyers who search P275NH normalized or P275NH +N are asking for this route.
If the vessel will see PWHT, say so. Test coupons then follow a simulated cycle. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists EN 10028-3 P275NH; 1.0486; heat number; cast analysis; product analysis when ordered; tensile to the correct thickness column; +N; impact when ordered; elevated-temperature values when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for P275NH fine grain vessel plate:
- Thickness: commonly 6 mm – 150 mm, thicker by mill agreement
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
Ship plate inquiries belong on shipbuilding steel plates. Structural fine-grain plate belongs on EN 10025-3, not on this vessel page.
Tolerances
Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another table. Class A is the usual default. If the calculation used minimum thickness after corrosion, write the allowed minus. Do not apply ASTM A36 structural tolerances to a PED fine-grain vessel plate without writing them.
Supplementary Requirements
Charpy details. Temperature, energy, location and orientation. NH is not NL1. Do not assume −40 °C.
Product analysis. Add this when the destination file wants finished-plate chemistry.
Elevated-temperature proof strength. This is the NH item. Write it when the calculation uses design temperature.
Simulated PWHT. When the equipment will be stress-relieved.
NDE. EN 10160 or the named UT class.
Third-party. EN 10204 3.2 when written.
Applications
| Industry | Typical components |
|---|---|
| PED boilers and drums | EN 10028-3 P275NH shells |
| Fine-grain heat-exchanger shells | P275NH courses |
| Elevated-temp carbon vessels | P275NH plate from SHH STEEL |
| Dual-certified export | P275NH / SA516 Grade 60 when both books fit |
Supply Capability
SHH STEEL sources EN 10028-3 P275NH from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or normalizing route requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual stock and rolling thickness for this family: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, with thicker plate by mill agreement.
Processing available with the plate: CNC or flame cutting to drawing, bevel preparation, flattening, and ultrasonic testing to EN 10160 or the named class.
Trade terms: FOB Shanghai is the usual main term. CIF to the buyer’s destination port can be quoted. Payment is TT, LC, or TT + LC, as agreed on the contract.
Destination ports and typical ocean time from Shanghai, subject to sailing and customs:
- US West Coast (Los Angeles / Long Beach / Oakland): about 14–18 days
- US Gulf (Houston / New Orleans): about 28–35 days
- Rotterdam / Antwerp: about 28–35 days
- Jebel Ali: about 18–25 days
- Singapore: about 7–12 days
- Other major ports in Mexico, South America, the Mediterranean, India, Africa, Japan and Korea: quoted case by case
Third-party inspection can be SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector the buyer names.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin. The commercial offer is not limited to one region.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time:
- Ex-stock: about 5–7 days when P275NH is in yard
- Mill rolling, standard +N: about 45 days
- Simulated PWHT, 3.2 or extra NDE: about 2 months
Company scope: worldwide delivery SHH STEEL.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). On EN 10028-3 P275NH that means mill pricing from Wuyang, Angang, Baosteel and other first-line mills, 1.0486 chemistry reported as cast analysis and as product analysis when ordered, recorded +N, tensile to the correct thickness column, 3.1 as standard and 3.2 when specified.
We keep the grade on the order. P275NH is not P275NL1. P275NH is not EN 10028-2 P265GH. P275NH is not Q345R steel plate. If the drawing says P355NH, we will not ship P275NH and call fine grain close.
Company scope: global exporter SHH STEEL.
FAQ
-
What is P275NH steel plate?
- P275NH is an EN 10028-3 normalized fine-grain pressure-vessel plate, steel number 1.0486. Yield is 275 MPa at ≤16 mm and tensile is 390–510 MPa. NH means elevated-temperature properties on a fine-grain route. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
What is the equivalent of P275NH?
- Related comparisons are P265GH, SA-516 Grade 60 and Q245R. Dual marking is possible only when both books are fully met.
-
How is P275NH different from P265GH?
- P265GH is EN 10028-2 high-temperature carbon plate. P275NH is EN 10028-3 fine-grain plate with a 275 MPa yield step and NH elevated-temperature values.
-
How is P275NH different from P275NL1 and P275NL2?
- NL1 and NL2 are low-temperature qualities. NH is the elevated-temperature quality. Do not assume −40 °C impact on P275NH.
-
Is P275NH the same as S275N?
- No. S275N is EN 10025-3 structural fine-grain steel. P275NH is EN 10028-3 pressure-vessel plate.
-
Can SHH STEEL ship P275NH to the USA, Europe or the Middle East?
- Yes. SHH STEEL quotes FOB Shanghai and CIF to US West, US Gulf, Rotterdam, Jebel Ali, Singapore and other major ports.
-
What is the delivery time for P275NH?
- Ex-stock about 5–7 days when plate is in yard. Standard +N mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.
Conclusion
EN 10028-3 P275NH Steel Plate is European normalized fine-grain pressure-vessel plate, steel number 1.0486, at the 275 MPa yield step and 390–510 MPa tensile at ≤16 mm, usually +N. Whether the inquiry says EN 10028-3 P275NH, 1.0486, P275NH Fine Grain Vessel Plate or P275NH supplier, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with P275NH chemistry, heat and product analysis when ordered, recorded +N, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies EN 10028-3 P275NH Fine Grain Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.
Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.
EN 10028-3 P275NH Steel Plate, P275NH fine grain vessel plate, 1.0486, P275NH supplier, global exporter SHH STEEL