EN 10028-3 P355NH normalized elevated-temperature fine-grain pressure vessel steel plate, 1.0565, SHH STEEL

EN 10028-3 P355NH Steel Plate | P355NH Fine Grain Vessel Plate supplier

EN 10028-3 P355NH is European normalized fine-grain vessel plate with elevated-temperature properties, steel number 1.0565. Yield is 355 MPa at ≤16 mm. Tensile is 490–630 MPa. SHH STEEL supplies P355NH worldwide as a global steel mill sourcing partner.
Keywords
EN 10028-3 P355NH, P355NH, P355NH steel plate, 1.0565, P355NH fine grain vessel plate, P355NH equivalent, P355NH supplier
Equivalent Grades:
N P355NH / ASTM A516 Gr 70 (high-temp ref) / JIS G3115 SPV355 / GB Q345R — Material Specification: EN 10028-3 — Delivery: Normalized (N); high-temp yield
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Elevated-Temperature Fine-Grain Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10028-3 P355NH Steel?

P355NH is the elevated-temperature quality in the P355 family of EN 10028-3. Buyers search EN 10028-3 P355NH, P355NH steel plate, 1.0565, P355NH fine grain vessel plate and P355NH supplier. The letters NH mean normalized fine-grain plate with specified elevated-temperature properties. This page is not P355N. N is room-temperature quality. This page is not P355NL1 or P355NL2. Those grades carry −40 °C or −50 °C impact. This page is not EN 10028-2 P355GH. GH is a different part of EN 10028. This page is not S355N. S355N is EN 10025-3 structural steel.

Yield is 355 MPa at ≤16 mm. Tensile is 490–630 MPa. Steel number is 1.0565. Delivery is normalized (+N). Elevated-temperature proof strength is the reason the H is in the name. Ask for that table when the vessel calculation uses design temperature. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-3, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.

If a drawing says P355N, we will not ship P355NH and call H extra without the buyer writing it. If a drawing says P355NL1, we will not ship P355NH and call 355 MPa enough. Dual marking is possible only when chemistry, tensile, impact, elevated-temperature values and delivery all fit both books.

Company scope: global exporter SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade EN 10028-3 P355NH Confirmed
Steel number 1.0565 Confirmed
Product specification EN 10028-3 + EN 10028-1 Applied
Steel type Weldable fine-grain, normalized, elevated temperature Confirmed
Usual delivery +N normalized Confirmed
Yield idea 355 MPa at ≤16 mm Confirmed
Tensile 490–630 MPa at ≤16 mm Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates and carbon steel plates. EN 10028-2 high-temperature sisters belong on EN 10028-2. Chinese vessel comparisons belong on GB/T 713.

Chemical Composition

Cast analysis follows EN 10028-3. Product analysis follows EN 10028-1 when ordered. Thickness can tighten carbon. Always read the certificate against the ordered thickness.

Cast Analysis and Product Analysis — EN 10028-3 P355NH (1.0565)

Element Cast Analysis (%) Product Analysis, when ordered (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.50 0.55
Manganese (Mn) 1.10 – 1.70 1.05 – 1.80
Phosphorus (P), max 0.025 0.030
Sulfur (S), max 0.010 0.013
Aluminum total (Al), min 0.020 0.015
Nitrogen (N), max 0.012 0.014
Chromium (Cr), max 0.30 0.35
Copper (Cu), max 0.30 0.35
Molybdenum (Mo), max 0.08 0.10
Nickel (Ni), max 0.50 0.55
Niobium (Nb), max 0.05 0.06
Titanium (Ti), max 0.03 0.04
Vanadium (V), max 0.10 0.12

Aluminum minimum is there to kill the steel and help grain size. This is C-Mn fine-grain plate, not 0.3Mo and not 1.25Cr-0.5Mo. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search P355NH mechanical properties, P355NH yield strength and P355NH elevated temperature. Yield falls as thickness rises.

Tensile and Yield — EN 10028-3 P355NH

Thickness (mm) Yield min (MPa) Tensile (MPa)
≤ 16 355 490 – 630
16 – 40 345 490 – 630
40 – 60 335 490 – 630
60 – 100 315 470 – 630
100 – 150 295 460 – 630
150 – 250 280 450 – 630
Density 7.85 g/cm³ 7.85 g/cm³

Elongation is typically 22% min on thinner plate. Impact for NH is commonly specified at 0 °C, 27 J, when the order names it. That is not −40 °C. Elevated-temperature proof strength is the NH item. Ask for the EN 10028-3 high-temperature table when the vessel calculation uses design temperature. SHH STEEL will not print those values on a P355N certificate and call it NH.

Do not treat 490–630 MPa tensile as permission to stamp Q345R steel plate or SA516 Grade 70 without checking both books.

Material Comparison

Grade Book What buyers search Swap?
EN 10028-3 P355N EN 10028-3 P355N steel plate No
EN 10028-3 P355NH EN 10028-3 P355NH steel plate This page
EN 10028-3 P355NL1 EN 10028-3 P355NL1 No
EN 10028-3 P355NL2 EN 10028-3 P355NL2 No
EN 10028-2 P355GH EN 10028-2 P355GH No
EN 10028-2 P265GH EN 10028-2 P265GH No
Q345R steel plate GB/T 713.2 Q345R No auto swap
SA516 Grade 70 SA-516 SA516 Gr.70 No auto swap
SA515 Grade 70 SA-515 SA515 Gr.70 No
StE355 steel plate DIN 17102 StE355 No

Equivalent Material Grades

Designation Standard / region Notes
EN 10028-3 P355NH / 1.0565 EN 10028-3 Name on this page
P355N / 1.0562 EN 10028-3 Room-temp sister
P355NL1 / 1.0566 EN 10028-3 −40 °C sister
EN 10028-2 P355GH EN 10028-2 High-temp carbon, different part
Q345R steel plate GB/T 713.2 Closest Chinese carbon
Q370R steel plate GB/T 713.2 Stronger Chinese vessel
SA516 Grade 70 SA-516 ASME carbon
A516 Grade 70 A516 ASTM twin
SA515 Grade 70 SA-515 High-temp carbon
SPV355 steel plate JIS G3115 Japanese vessel
WStE355 steel plate DIN 17102 Fine-grain comparison

Elevated-Temperature Fine-Grain Service

P355NH is used on PED drums, shells and heat-exchanger courses that need 355 MPa fine-grain plate and elevated-temperature proof strength. That is the H. A designer who only wants room-temperature quality is asking for P355N. A designer who wants −40 °C Charpy is asking for P355NL1.

It is not a substitute for EN 10028-2 16Mo3. That grade is 0.3Mo. It is not a substitute for EN 10028-2 13CrMo4-5. That grade is 1.25Cr-0.5Mo. An ASME file should name SA-516 or SA-515 and then write extras. Dual marking is possible only when both books are met.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

P355NH is killed fine-grain C-Mn vessel plate in the 490–630 MPa tensile band. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.

Qualify to the applicable code. Consumables must match the P355NH tensile band. A procedure written for SA516 Grade 60 may be light. A Cr-Mo procedure written for SA387 Grade 12 Class 1 is the wrong family. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is normalized EN 10028-3 P355NH (+N).

If the vessel will see PWHT, say so. Test coupons then follow a simulated cycle. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists EN 10028-3 P355NH; 1.0565; heat number; cast analysis; product analysis when ordered; tensile to the correct thickness column; +N; impact when ordered; elevated-temperature values when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for P355NH fine grain vessel plate:

  • Thickness: commonly 6 mm – 150 mm, thicker by mill agreement
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Ship plate inquiries belong on shipbuilding steel plates. Structural fine-grain plate belongs on EN 10025-3.

Tolerances

Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another table. Class A is the usual default. If the calculation used minimum thickness after corrosion, write the allowed minus. Do not apply ASTM A36 structural tolerances to a PED fine-grain vessel plate without writing them. When dual-named against SA516 Grade 70, write whether EN 10029 or SA-20 governs thickness extra.

Supplementary Requirements

Charpy details. NH commonly uses 0 °C. Do not assume −40 °C.

Elevated-temperature proof strength. This is the NH item. Write the design temperatures needed on the certificate.

Product analysis. Add this when the destination file wants finished-plate chemistry.

Simulated PWHT. When the equipment will be stress-relieved.

NDE. EN 10160 or the named UT class.

Third-party. EN 10204 3.2 when written.

Applications

Industry Typical components
PED boilers and drums EN 10028-3 P355NH shells
Fine-grain heat-exchanger shells P355NH courses
Elevated-temp fine-grain vessels P355NH plate from SHH STEEL
Dual-certified export P355NH / SA516 Grade 70 when both books fit

P355NH is the plate for a file that wants 355 MPa fine-grain normalized steel and elevated-temperature values. It is the wrong plate for a winter tank at −40 °C. That work is P355NL1. It is the wrong plate for a file that only wants room-temperature quality. That work is P355N.

SHH STEEL Supply Capability

SHH STEEL sources EN 10028-3 P355NH from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or normalizing route requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, thicker by mill agreement.

Processing: CNC or flame cutting, bevel, flattening, UT to EN 10160 or the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard +N about 45 days; simulated PWHT / 3.2 about 2 months.

Company scope: worldwide delivery SHH STEEL.

Why Choose SHH STEEL

Experience on this grade is simple: keep the letters after P355. N, NH, NL1 and NL2 are four different purchase orders. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices P355NH from first-line mills, reports 1.0565 chemistry as cast analysis and as product analysis when ordered, records +N, prints elevated-temperature values when ordered, and issues 3.1 as standard or 3.2 when specified.

We keep the grade on the order. P355NH is not P355N. P355NH is not P355NL1. P355NH is not EN 10028-2 P355GH. P355NH is not Q345R steel plate. If the drawing says P355N, we will not ship NH and call H free.

Company scope: global exporter SHH STEEL.

FAQ

What is P355NH steel plate?
P355NH is an EN 10028-3 normalized fine-grain pressure-vessel plate, steel number 1.0565. Yield is 355 MPa at ≤16 mm and tensile is 490–630 MPa. NH means elevated-temperature properties on a fine-grain route. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
What is the equivalent of P355NH?
Related comparisons are Q345R, SA-516 Grade 70 and P355GH. Dual marking is possible only when both books are fully met.
How is P355NH different from P355N?
N is room-temperature quality. NH adds specified elevated-temperature properties.
How is P355NH different from P355NL1?
NL1 is −40 °C impact quality. NH is elevated-temperature quality.
How is P355NH different from P355GH?
P355GH is EN 10028-2. P355NH is EN 10028-3 fine-grain plate. They are not the same part of the standard.
What is the delivery time for P355NH?
Ex-stock about 5–7 days when plate is in yard. Standard +N mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.

Conclusion

EN 10028-3 P355NH Steel Plate is European normalized fine-grain pressure-vessel plate with elevated-temperature properties, steel number 1.0565, at the 355 MPa yield step and 490–630 MPa tensile at ≤16 mm, usually +N. Whether the inquiry says EN 10028-3 P355NH, 1.0565, P355NH Fine Grain Vessel Plate or P355NH supplier, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with P355NH chemistry, heat and product analysis when ordered, recorded +N, elevated-temperature values when ordered, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies EN 10028-3 P355NH Fine Grain Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.

Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.

EN 10028-3 P355NH Steel Plate, P355NH fine grain vessel plate, 1.0565, P355NH supplier, global exporter SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X