GOST 9940 08Х18Н12Б Seamless Stainless Steel Pipe
What is GOST 9940 08Х18Н12Б Seamless Stainless Steel Pipe
GOST 9940-81 is the Soviet / CIS product standard for seamless hot-deformed corrosion-resistant steel pipes — geometry, tensile floors, and acceptance in one document. Grade 08Х18Н12Б sits in the austenitic Nb-stabilised 18-12 set under Table 3. Mill brand ЭИ402. Niobium-stabilised sister of the Ti 18-8 marks — smaller OD envelope.
SHH STEEL can produce and supply GOST 9940 08Х18Н12Б as hot-deformed seamless pipe across the enquiry OD×wall band (within the mark’s diameter cap), heat-treated or without HT as ordered, descaled or bright-finished, and documented on mill certificates tied to GOST 5632 cast analysis and Table 3 tensile results. Duty focus: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
Shop language may still say “347 pipe,” yet that commercial alias does not select GOST 5632 cast limits, hot-deformed tensile floors, or GOST 9940 marking. The purchase order has to name GOST 9940 and 08Х18Н12Б so the mill applies the correct analysis, optional heat treatment, mechanical floors, and stencil. Design caution: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore.
Scope discipline: 08Х18Н12Б is hot-deformed seamless pipe under GOST 9940, not cold-deformed GOST 9941 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т. Role reminder: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. Diameter note: ≤108 mm per Table 1 note 1.
Inside this GOST 9940 series, compare GOST 9940 08Х18Н12Т, GOST 9940 08Х18Н10Т, GOST 9940 12Х18Н10Т. Hub: GOST 9940. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP347.
Chemical Composition of GOST 9940 08Х18Н12Б
Cast analysis for GOST 9940 08Х18Н12Б is not printed inside 9940 itself — clause 2.1 points to GOST 5632. Key windows on a typical certificate include C ≤0.08, Si ≤0.80, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 11.00–13.00, Cr 17.00–19.00, Nb 10×C–1.10. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 347 / UNS S34700 (approx). Mill brand ЭИ402. Corrosion thread: Nb stabilisation for IGC after welding; hot strength similar to 347 practice.
Chemical limits for 08Х18Н12Б appear in the table underneath (GOST 5632-2014 extract). Source priority is the paid GOST 5632 table if your client cites a different edition footnote — send it before the heat is melted. Duty thread: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
| Grade | C | Si | Mn | P | S | Ni | Cr | Nb |
|---|---|---|---|---|---|---|---|---|
| 08Х18Н12Б | ≤0.08 | ≤0.80 | ≤2.00 | ≤0.035 | ≤0.020 | 11.00–13.00 | 17.00–19.00 | 10×C–1.10 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9940 08Х18Н12Б
Ambient tensile floors for 08Х18Н12Б come from GOST 9940-81 Table 3: Rm min 510 N/mm², elongation δ5 min 38% (yield not normalised in Table 3). Note: Yield not normalised. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic Nb-stabilised 18-12. Caution: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore.
Yield strength is numerically normalised in GOST 9940 only for 12Х18Н10Т (≥216 N/mm²) when the purchaser orders it — for 08Х18Н12Б, treat Rp0.2 as an ordered extra unless that mark exception applies. Thick-wall pipes with D/s ≤8 on thirteen named marks may reduce Rm by 19.6 N/mm² per Table 3 note 1. Density 7.9 g/cm³. Role: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 08Х18Н12Б | 510 | — (not normalised) | 38 | 7.9 | ≤108 mm per Table 1 note 1 |
Ambient values from GOST 9940-81 Table 3 for 08Х18Н12Б. Yield not normalised. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution anneal; Nb for welded high-temp corrosive service.
Seamless Pipe Manufacture of GOST 9940 08Х18Н12Б
SHH STEEL can produce 08Х18Н12Б as hot-deformed seamless pipe to GOST 9940-81, then apply ordered heat treatment, scale removal, and end finish. Plain square-cut ends are default; weld bevels on walls over 5 mm only when the purchaser asks. Seamless hot-deformed manufacture remains the only valid order path for 08Х18Н12Б under GOST 9940; the acknowledgement repeats that route so production cannot silently change after the PO is firm. Application context for 08Х18Н12Б stays furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium.
Austenitic heats usually take solution annealing with rapid cool when HT is ordered; skip inventing a mandatory anneal when the PO says without heat treatment. Heat-treatment note for 08Х18Н12Б: Solution anneal; Nb for welded high-temp corrosive service. Scale removal follows when ordered; clause defaults do not automatically pickle every pipe. Duty thread: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 08Х18Н12Б: OD not above 108 mm. Diameter cap: ≤108 mm per Table 1 note 1.
Dimensions and Tolerances for GOST 9940 08Х18Н12Б
SHH STEEL aligns nominal OD, wall, length type, and precision class (ordinary / high) for 08Х18Н12Б before the mill slot is locked. Table 1 lists OD from 57 to 325 mm and wall from 3.5 to 32 mm, with measured length limits per size cell. Size hint: OD not above 108 mm. Mark cap: ≤108 mm per Table 1 note 1.
OD tolerance is ±1.5% (ordinary) or ±1.0% (high). Wall minus tolerance reaches 15% on many gauges — design min wall with that minus in view. Curvature limits: 1.5 / 2 / 4 mm per metre by wall band. Duty thread: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
Equivalent Grades for GOST 9940 08Х18Н12Б
The table below maps GOST 9940 08Х18Н12Б to commercial aliases and related systems without inventing false one-to-one substitutes. Alias 347 / UNS S34700 (approx) stays body-only. Pack caution: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (08Х18Н12Б).
| System | Designation | Notes |
|---|---|---|
| GOST 9940 | 08Х18Н12Б | Governing pipe grade for this page |
| Commercial / UNS (body only) | 347 / UNS S34700 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 347 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | EN 1.4550 | Starting point for comparison only; no automatic dual-cert |
Order discipline for 08Х18Н12Б still points at GOST 9940, not the brochure alias. Neighbours GOST 9940 08Х18Н12Т, GOST 9940 08Х18Н10Т, GOST 9940 12Х18Н10Т each carry their own mechanical table. Category hub: GOST 9940. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (08Х18Н12Б).
Project teams specifying 08Х18Н12Б should link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and ASTM A240 Type 347 so purchasing does not treat one product form as the other. Confirm 08Х18Н12Б OD × wall and plate thickness on separate drawings.
Heat Treatment and Delivery Condition for GOST 9940 08Х18Н12Б
08Х18Н12Б is delivered as ordered — heat-treated or without heat treatment under GOST 9940. Guidance: Solution anneal; Nb for welded high-temp corrosive service. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: Nb-bearing 347-class fillers; match Nb:C intent on the WPS.
Cooling type matters — austenitics need rapid cool after solution treatment when HT is ordered; ferritic/martensitic anneal practice follows air or slow-cool notes. Duty thread: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. Density 7.9 g/cm³ for weight calcs. Field heat treatment of 08Х18Н12Б after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 08Х18Н12Б duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
Corrosion Resistance of GOST 9940 08Х18Н12Б
Corrosion behaviour of GOST 9940 08Х18Н12Б tracks its austenitic Nb-stabilised 18-12 balance: Nb stabilisation for IGC after welding; hot strength similar to 347 practice. Intergranular corrosion testing is a purchaser option under GOST 9940, not an automatic coupon on every lot. Design caution: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 08Х18Н12Б is filed as austenitic Nb-stabilised 18-12. Caution: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore.
Applications of GOST 9940 08Х18Н12Б Seamless Pipe
Applications of GOST 9940 08Х18Н12Б seamless pipe centre on furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium. Role summary: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same Cyrillic grade symbol on cut lists so informal latinised substitutions do not creep in. Primary application sketch: furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium. Duty thread: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
Weldability of GOST 9940 08Х18Н12Б
08Х18Н12Б ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: Nb-bearing 347-class fillers; match Nb:C intent on the WPS. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 08Х18Н12Б should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Keep the 08Х18Н12Б caution visible here: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic Nb-stabilised 18-12 — not a single shop habit. Caution: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore. Consumable lot control and shielding-gas notes for 08Х18Н12Б stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 08Х18Н12Б duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
Surface Finishes for GOST 9940 08Х18Н12Б
For GOST 9940 08Х18Н12Б, pickled finish after heat treatment is the usual mill supply for seamless stainless steel pipe (hot-deformed): matte, scale-free, and ready for fabrication. Bright anneal or a ground/polished callout is available by agreement, but the order must name whether OD, ID, or both surfaces are in scope. Duty: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
When 08Х18Н12Б ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for solution anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Apps reminder: furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium.
Inspection and Testing for GOST 9940 08Х18Н12Б
Inspection for GOST 9940 08Х18Н12Б covers dimensions and appearance on every pipe; tensile on two pipes per party; flattening or expanding on one when ordered; IGC on two when ordered. Hydrostatic and ultrasonic tests run when the purchaser asks. Documents follow GOST 10692 with chemistry taken from the billet certificate.
Marking includes 08Х18Н12Б, manufacturer, size, and GOST 9940. Traceability from stencil to MTC is part of supply, not an upgrade. Use: furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium. Non-conforming 08Х18Н12Б lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Keep the 08Х18Н12Б caution visible here: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore.
Packaging and Shipping for GOST 9940 08Х18Н12Б
Packaging for 08Х18Н12Б uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect descaled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 08Х18Н12Б repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 08Х18Н12Б: Nb-bearing 347-class fillers; match Nb:C intent on the WPS.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore. Desiccant and wrap choices for 08Х18Н12Б follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 08Х18Н12Б: Nb-bearing 347-class fillers; match Nb:C intent on the WPS.
Shipping documents list GOST 9940, 08Х18Н12Б, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. Claims handling for 08Х18Н12Б starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 08Х18Н12Б remains OD not above 108 mm.
Why Choose SHH STEEL
SHH STEEL can produce and supply GOST 9940 08Х18Н12Б with the hot-deformed seamless route, heat-treatment choice, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless hot capacity covering this mark’s OD band. Duty focus: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service.
Technical sales can map 08Х18Н12Б against sisters 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т and live ASTM A312 pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 08Х18Н12Б, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х18Н12Б to that written scope.
Supply Capability
SHH STEEL can produce and supply GOST 9940 08Х18Н12Б across enquiry-oriented OD × wall bands (within ≤108 mm per Table 1 note 1), in the hot-deformed seamless route, with certificates and optional tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue.
| Item | Capability |
|---|---|
| Standard | GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes |
| Grade | 08Х18Н12Б (GOST 5632 chemistry; alias 347 / UNS S34700 (approx)) |
| Product form | Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941) |
| Delivery condition | as ordered — heat-treated or without heat treatment |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: ≤108 mm per Table 1 note 1 |
| Precision | Ordinary or high (index “в” when high) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
SHH STEEL can produce and supply GOST 9940 08Х18Н12Б. Stock / Available sizes: enquiry band typically aligns with GOST 9940 Table 1 OD×wall practice, with ordinary or high precision as ordered. For 08Х18Н12Б, practical fast-track sizes often sit inside the mark’s diameter cap — send the OD × wall list for a firm acknowledgement. Context: OD not above 108 mm. Cap: ≤108 mm per Table 1 note 1.
Cut lengths, bevels, special NDT, IGC, and HT extras add lead time — call them early. Sisters often quoted alongside: 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т. Email the size list to start. SHH STEEL can produce trial lengths of 08Х18Н12Б for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9940 08Х18Н12Б seamless stainless steel pipe used for?
- GOST 9940 08Х18Н12Б is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — furnace connecting pipe, chemical plant hot legs, and CIS BOMs that prefer niobium over titanium. Role summary: Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9940 08Х18Н12Б seamless only, or does it cover welded pipe?
- Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 08Х18Н12Б when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 08Х18Н12Б under GOST 9940?
- No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution anneal; Nb for welded high-temp corrosive service. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
-
How does 08Х18Н12Б compare with sister grades 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т?
- 08Х18Н12Б is filed as austenitic Nb-stabilised 18-12. Typical sisters on the same RFQ are 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т. Design caution: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 08Х18Н12Б?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
-
Is 347 / UNS S34700 (approx) the same as ordering 08Х18Н12Б?
- No. 347 / UNS S34700 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 08Х18Н12Б so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9940 08Х18Н12Б?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х18Н12Б within Table 1 practice, respecting the mark’s diameter cap (≤108 mm per Table 1 note 1). Size context: OD not above 108 mm. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
-
How should 08Х18Н12Б be welded on site?
- Shop guidance: Nb-bearing 347-class fillers; match Nb:C intent on the WPS. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore
-
When should I choose a Mo-bearing or duplex grade instead of 08Х18Н12Б?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic Nb-stabilised 18-12 practice can defend for the temperature and stress state. Caution for this mark: OD ≤108 mm for this mark — check Table 1 note 1 before quoting large bore Sister pointers: 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9940 08Х18Н12Б with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 08Х18Н12Б does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9940 08Х18Н12Б differ from GOST 9941 of the same mark?
- GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х18Н12Б.
Conclusion
GOST 9940 08Х18Н12Б is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — Nb-stabilised 18-12 austenitic seamless pipe for welded high-temperature corrosive service. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х18Н12Т, 08Х18Н10Т, 12Х18Н10Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.