GOST 9940 12Х18Н9 Seamless Stainless Steel Pipe

GOST 9940 12Х18Н9 seamless stainless steel pipe (302 / UNS S30200 (approx)), austenitic 18-9 (higher C), GOST 5632 cast analysis, Rm min 529 N/mm² / δ5 min 40%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
Grade
12Х18Н9 (GOST 5632 / 302 / UNS S30200 (approx) — body alias)
Standard
GOST 9940-81
Product form
Seamless stainless steel pipe (hot-deformed), delivery as ordered — heat-treated or without heat treatment
Size
OD × wall per Table 1; mark cap full Table 1 range; random length typically 1.5–10 m
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GOST 9940 12Х18Н9 Seamless Stainless Steel Pipe

GOST 9940 covers seamless hot-deformed stainless pipe with OD 57–325 mm and wall 3.5–32 mm in two precision classes. Inside that standard, 12Х18Н9 is filed as austenitic 18-9 (higher C). The older higher-carbon 18-8 mark — still on many Russian isometrics. Buyers working CIS fluid packages should treat 12Х18Н9 as a governed product grade under GOST 9940-81, with GOST 5632 chemistry and Table 3 tensile floors enforced on the same heat. This paragraph is locked to 12Х18Н9 duty: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs.

From pierce through marking and crate protection, SHH STEEL can produce GOST 9940 12Х18Н9 for the sizes and tests on your RFQ. Application sketch: general process transfer, utility steam, and retrofit spools that have not moved to 08Х18Н10. Size and test clarity on the RFQ lets SHH STEEL lock the correct hot-deformed seamless scope for 12Х18Н9 before production starts. Weld-shop note tied to 12Х18Н9: 308/308L; treat upper-carbon heats as sensitisation-sensitive.

On the floor people latinise marks; in QA they must not. 12Х18Н9 under GOST 9940 carries specific Table 3 floors that a loose “302” note will not enforce. Caution: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds.

Pair standard GOST 9941 uses many of the same marks with colder deformation and different Rm/δ5 pairs — do not mix certificates. Sisters: 08Х18Н10, 12Х18Н10Т, 17Х18Н9. Use thread: general process transfer, utility steam, and retrofit spools that have not moved to 08Х18Н10. Document the medium, design temperature, and weld map beside the 12Х18Н9 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for 12Х18Н9 remains full OD to 325 mm.

Inside this GOST 9940 series, compare GOST 9940 08Х18Н10, GOST 9940 12Х18Н10Т, GOST 9940 17Х18Н9. Hub: GOST 9940. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP304, ASTM A312 TP304H.

Project teams specifying 12Х18Н9 should Stainless Steel Pipes and Tubes covers the tubular parent, Stainless Steel Sheets and Plates covers flats, and ASTM A240 UNS S30200 is the live plate chemistry match — do not merge MTCs. Confirm 12Х18Н9 OD × wall and plate thickness on separate drawings.

Chemical Composition of GOST 9940 12Х18Н9

For 12Х18Н9, the melt ticket has to show GOST 5632 compliance — C ≤0.12, Si ≤0.80, Mn ≤2.00, P ≤0.040, S ≤0.020, Ni 8.00–10.00, Cr 17.00–19.00. Optional residual limits still forbid blurring grade identity. Corrosion framing: 18-8 passive film; carbon is the weldability differentiator versus 08Х18Н10.

Where Mo, Ti or Nb appear, they are intentional levers for 12Х18Н9, not optional marketing. Confirm them on the MTC line-by-line. Role: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 12Х18Н9 before the order is acknowledged. This paragraph is locked to 12Х18Н9 duty: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs.

Grade C Si Mn P S Ni Cr
12Х18Н9 ≤0.12 ≤0.80 ≤2.00 ≤0.040 ≤0.020 8.00–10.00 17.00–19.00

Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.

Mechanical Properties of GOST 9940 12Х18Н9

Do not confuse Table 3 hot-deformed floors with GOST 9941 cold-deformed numbers that share the 302 / UNS S30200 (approx) alias. For 12Х18Н9 under 9940 expect Rm min 529 N/mm², elongation δ5 min 40% (yield not normalised in Table 3), verified per heat/lot rules. Note: Yield not normalised; thick-wall Rm relief applies.

When comparing 12Х18Н9 to a cold-deformed GOST 9941 sister, expect different Rm/δ5 pairs even at identical GOST 5632 chemistry. Duty: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. Do not substitute GOST 9941 cold-deformed tensile numbers onto a hot-deformed 12Х18Н9 certificate without a written dual-product plan. Application context for 12Х18Н9 stays general process transfer, utility steam, and retrofit spools that have not moved to 08Х18Н10.

Grade Rm min (N/mm²) Rp0.2 min (N/mm²) δ5 min (%) Density (g/cm³) Max OD note
12Х18Н9 529 — (not normalised) 40 7.9 full Table 1 range

Ambient values from GOST 9940-81 Table 3 for 12Х18Н9. Yield not normalised; thick-wall Rm relief applies. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution anneal; watch as-welded IGC versus low-C sisters.

Seamless Pipe Manufacture of GOST 9940 12Х18Н9

SHH STEEL can produce 12Х18Н9 as hot-deformed seamless pipe to GOST 9940-81, then apply ordered heat treatment, scale removal, and end finish. Plain square-cut ends are default; weld bevels on walls over 5 mm only when the purchaser asks. Seamless hot-deformed manufacture remains the only valid order path for 12Х18Н9 under GOST 9940; the acknowledgement repeats that route so production cannot silently change after the PO is firm. Size practice for 12Х18Н9 remains full OD to 325 mm.

Precision class (ordinary or high) is an order item for 12Х18Н9; unmarked class means ordinary. Heat treatment: Solution anneal; watch as-welded IGC versus low-C sisters. Austenitic heats usually take solution annealing with rapid cool when HT is ordered; skip inventing a mandatory anneal when the PO says without heat treatment.

Hydraulic testing per GOST 3845 and ultrasonic inspection run only when ordered — technology is deemed to ensure pressure capacity, but the certificate lists only tests performed. Manufacture stays seamless hot-deformed. Size: full OD to 325 mm. Hydrostatic pressure or UT class for 12Х18Н9 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. This paragraph is locked to 12Х18Н9 duty: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs.

Dimensions and Tolerances for GOST 9940 12Х18Н9

Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 12Х18Н9. Duty: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. Cap: full Table 1 range. Precision class follows the tolerance ordered for 12Х18Н9, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for 12Х18Н9 stays general process transfer, utility steam, and retrofit spools that have not moved to 08Х18Н10.

High precision mainly tightens the plus wall tolerance; the minus side stays punishing — quote class with the size for 12Х18Н9. Fixed lengths and multiple cut lengths for 12Х18Н9 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for 12Х18Н9 remains full OD to 325 mm.

Equivalent Grades for GOST 9940 12Х18Н9

Cross-references help sourcing 12Х18Н9, but they do not replace the GOST 9940 grade line on the enquiry. Family framing here is austenitic 18-9 (higher C); delivery practice from the crib is “as ordered — heat-treated or without heat treatment”. Related ASTM or EN numbers are starting points for engineering comparison, not automatic substitutes.

System Designation Notes
GOST 9940 12Х18Н9 Governing pipe grade for this page
Commercial / UNS (body only) 302 / UNS S30200 (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other EN 1.4310 Starting point for comparison only; no automatic dual-cert

Sister pages worth reading beside 12Х18Н9: GOST 9940 08Х18Н10, GOST 9940 12Х18Н10Т, GOST 9940 17Х18Н9. Duty locked here: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. Any EN or ASTM designation above is a starting point for comparison, not a substitute grade on the GOST 9940 certificate. Series hub: GOST 9940.

Heat Treatment and Delivery Condition for GOST 9940 12Х18Н9

Unlike GOST 9941, GOST 9940 does not force heat treatment on every pipe. Confirm for 12Х18Н9. Band note: Solution anneal; watch as-welded IGC versus low-C sisters. Recorded furnace charts for 12Х18Н9 should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Keep the 12Х18Н9 caution visible here: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds.

Party acceptance groups pipes by size, mark, and heat-treatment kind — mixing HT and non-HT lengths in one lot breaks the batch rule for 12Х18Н9. Field heat treatment of 12Х18Н9 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 12Х18Н9 duty: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs.

Corrosion Resistance of GOST 9940 12Х18Н9

Medium, temperature, crevice geometry and weld condition decide whether 12Х18Н9 is enough. Summary: 18-8 passive film; carbon is the weldability differentiator versus 08Х18Н10. Escalate via sisters 08Х18Н10, 12Х18Н10Т, 17Х18Н9 when coupons fail. Coupon orientation, weld condition, and surface finish for 12Х18Н9 belong in the corrosion test order so results can be compared to the installed spool honestly. Size practice for 12Х18Н9 remains full OD to 325 mm.

Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 12Х18Н9. Corrosion framing: 18-8 passive film; carbon is the weldability differentiator versus 08Х18Н10. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 12Х18Н9 rather than relying on wall thickness alone. Weld-shop note tied to 12Х18Н9: 308/308L; treat upper-carbon heats as sensitisation-sensitive.

Applications of GOST 9940 12Х18Н9 Seamless Pipe

From utility rooms to process racks, 12Х18Н9 shows up wherever CIS fluid specs want austenitic 18-9 (higher C) hot-deformed seamless behaviour. Use list: general process transfer, utility steam, and retrofit spools that have not moved to 08Х18Н10. Spool fabricators should copy 12Х18Н9 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside 12Х18Н9: 18-8 passive film; carbon is the weldability differentiator versus 08Х18Н10.

If the only reason for 12Х18Н9 is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds. Commissioning teams benefit when the as-built dossier repeats 12Х18Н9 beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to 12Х18Н9 duty: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs.

Weldability of GOST 9940 12Х18Н9

Automatic mill welding is outside GOST 9940; manual and automatic field welds must still respect 12Х18Н9 chemistry. Guidance: 308/308L; treat upper-carbon heats as sensitisation-sensitive. Procedure qualification for 12Х18Н9 should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Weld-shop note tied to 12Х18Н9: 308/308L; treat upper-carbon heats as sensitisation-sensitive.

Ferrite control on high-Ni austenitics and hydrogen management on martensitic 12Х18Н9 are procedure items, not afterthoughts. Guidance: 308/308L; treat upper-carbon heats as sensitisation-sensitive. Consumable lot control and shielding-gas notes for 12Х18Н9 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 12Х18Н9 remains full OD to 325 mm.

Surface Finishes for GOST 9940 12Х18Н9

12Х18Н9 under GOST 9940 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (12Х18Н9).

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Passivation restores the chromium-rich film after pickling or light fabrication on 12Х18Н9; it does not replace the heat treatment that sets mechanical properties under GOST 9940. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.

Inspection and Testing for GOST 9940 12Х18Н9

Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GOST 9940 for 12Х18Н9. Sampling plans for 12Х18Н9 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 12Х18Н9 caution visible here: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds.

Dimensional inspection against Table 2 tolerances closes the lot. Role: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. Non-conforming 12Х18Н9 lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Size practice for 12Х18Н9 remains full OD to 325 mm.

Packaging and Shipping for GOST 9940 12Х18Н9

Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 12Х18Н9 stays visible on outer tags. Bundle tickets for 12Х18Н9 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 12Х18Н9 caution visible here: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds.

Container loading plans should keep heavy walls from crushing thin-wall 12Х18Н9 layers. Desiccant and wrap choices for 12Х18Н9 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 12Х18Н9 remains full OD to 325 mm.

Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 12Х18Н9. Claims handling for 12Х18Н9 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the 12Х18Н9 caution visible here: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds.

Why Choose SHH STEEL

From RFQ clarification through MTC release, SHH STEEL treats 12Х18Н9 as a governed product grade, not a marketing synonym for 302 / UNS S30200 (approx). Role: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. SHH STEEL can produce and supply 12Х18Н9 against the OD × wall, hot-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

Response time stays short because common 12Х18Н9 enquiry sizes and document packs are already exercised on prior GOST-spec orders. Use: general process transfer, utility steam, and retrofit spools that have not moved to 08Х18Н10. Ask for a written acknowledgement that names 12Х18Н9, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 12Х18Н9 to that written scope.

Supply Capability

Capability framing for 12Х18Н9: GOST-spec seamless hot-deformed pipe, documented heats. Caution remains: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 12Х18Н9 when the mill schedule allows.

Item Capability
Standard GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes
Grade 12Х18Н9 (GOST 5632 chemistry; alias 302 / UNS S30200 (approx))
Product form Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941)
Delivery condition as ordered — heat-treated or without heat treatment
Documents Quality document per GOST 10692 / EN 10204 3.1 style as ordered
Typical size practice OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: full Table 1 range
Precision Ordinary or high (index “в” when high)
Tests Tensile per party; hydro / UT / flatten / IGC / yield when ordered

Stock / Available sizes

Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 12Х18Н9 change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. SHH STEEL can supply alternate walls and precision classes for 12Х18Н9 once the design pressure and corrosion allowance are clear.

Repeat orders for 12Х18Н9 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. SHH STEEL can produce trial lengths of 12Х18Н9 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GOST 9940 12Х18Н9 seamless stainless steel pipe used for?
GOST 9940 12Х18Н9 is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — general process transfer, utility steam, and retrofit spools that have not moved to 08Х18Н10. Role summary: higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
Is GOST 9940 12Х18Н9 seamless only, or does it cover welded pipe?
Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 12Х18Н9 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
Is heat treatment mandatory for 12Х18Н9 under GOST 9940?
No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution anneal; watch as-welded IGC versus low-C sisters. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
How does 12Х18Н9 compare with sister grades 08Х18Н10, 12Х18Н10Т, 17Х18Н9?
12Х18Н9 is filed as austenitic 18-9 (higher C). Typical sisters on the same RFQ are 08Х18Н10, 12Х18Н10Т, 17Х18Н9. Design caution: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 12Х18Н9?
Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
Is 302 / UNS S30200 (approx) the same as ordering 12Х18Н9?
No. 302 / UNS S30200 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 12Х18Н9 so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GOST 9940 12Х18Н9?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 12Х18Н9 within Table 1 practice, respecting the mark’s diameter cap (full Table 1 range). Size context: full OD to 325 mm. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
How should 12Х18Н9 be welded on site?
Shop guidance: 308/308L; treat upper-carbon heats as sensitisation-sensitive. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds
When should I choose a Mo-bearing or duplex grade instead of 12Х18Н9?
Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic 18-9 (higher C) practice can defend for the temperature and stress state. Caution for this mark: C up to 0.12% raises as-welded IGC risk — prefer 04Х18Н10 or Ti grades for corrosive field welds Sister pointers: 08Х18Н10, 12Х18Н10Т, 17Х18Н9. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GOST 9940 12Х18Н9 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 12Х18Н9 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
How does GOST 9940 12Х18Н9 differ from GOST 9941 of the same mark?
GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 12Х18Н9.

Conclusion

GOST 9940 12Х18Н9 is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — higher-carbon 18-9 austenitic seamless pipe still written on older CIS fluid BOMs. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х18Н10, 12Х18Н10Т, 17Х18Н9. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X