GOST 9940 10Х23Н18 Seamless Stainless Steel Pipe
What is GOST 9940 10Х23Н18 Seamless Stainless Steel Pipe
Russian and CIS piping packages that print GOST 9940 expect hot-deformed seamless stainless pipe, not a welded substitute and not an automatic ASTM A312 certificate. 10Х23Н18 is the Cyrillic mark on Table 3 for this austenitic heat-resisting 25-20 class chemistry. Russian 25Cr-20Ni heat-resisting seamless pipe under the hot-deformed standard.
Mill path for 10Х23Н18: hot-deformed seamless route, clause 2.1 heat-treatment choice, GOST 5632 chemistry, Table 3 Rm and elongation, optional hydro / UT / IGC when ordered. SHH STEEL can make and supply the grade to that stack. Typical use: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys.
Body text may mention 310 / UNS S31000 family (approx) for cross-reference, but the H1 and order line stay on Cyrillic 10Х23Н18. Silent alias swaps are how wrong carbon ceilings and wrong Table 3 numbers enter the MTC. Keep this caution in view: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note.
Order the standard the drawing and regulatory file actually require. Inside this 9940 series, compare 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9 before stretching surface finish or wall alone. Duty thread: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. Document the medium, design temperature, and weld map beside the 10Х23Н18 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for 10Х23Н18 remains OD capped at 168 mm for this mark.
Inside this GOST 9940 series, compare GOST 9940 08Х20Н14С2, GOST 9940 12Х18Н12Т, GOST 9940 17Х18Н9. Hub: GOST 9940. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP310S.
10Х23Н18 sourcing notes should keep forms separate: open Stainless Steel Pipes and Tubes for pipes/tubes and Stainless Steel Sheets and Plates for sheets/plates, then use ASTM A240 Type 310S only when the flat form is required. Keep 10Х23Н18 acceptance text on the governing pipe/tube standard.
Chemical Composition of GOST 9940 10Х23Н18
GOST 5632 sets the melt limits for 10Х23Н18. Highlight band: C ≤0.10, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 17.00–20.00, Cr 22.00–25.00. For pipe intended for welding, GOST 9940 can tighten sulphur to ≤0.020% when the order states that duty. Alias note: 310 / UNS S31000 family (approx).
The composition table below is the cast window SHH STEEL quotes against for 10Х23Н18. Edition framing is GOST 5632 for chemistry and GOST 9940-81 for the pipe product. Use thread: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 10Х23Н18 before the order is acknowledged. Corrosion framing beside 10Х23Н18: oxidation and carburisation resistance dominate; aqueous chlorides are secondary.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 10Х23Н18 | ≤0.10 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.020 | 17.00–20.00 | 22.00–25.00 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9940 10Х23Н18
Table 3 mechanical acceptance for 10Х23Н18: Rm min 491 N/mm², elongation δ5 min 37% (yield not normalised in Table 3). Note: Yield not normalised; thick-wall Rm relief 19.6 N/mm² applies. Delivery framing: as ordered — heat-treated or without heat treatment. Density for mass calc: 7.95 g/cm³. Sampling follows GOST 9940 batch rules (party ≤200 pcs).
Elevated-temperature tensile at 623 K (350 °C) and yield determination are purchaser options, not defaults. For 10Х23Н18, state them on the PO if the stress calculation needs them. Use: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Do not substitute GOST 9941 cold-deformed tensile numbers onto a hot-deformed 10Х23Н18 certificate without a written dual-product plan. Size practice for 10Х23Н18 remains OD capped at 168 mm for this mark.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 10Х23Н18 | 491 | — (not normalised) | 37 | 7.95 | ≤168 mm per Table 1 note 1 |
Ambient values from GOST 9940-81 Table 3 for 10Х23Н18. Yield not normalised; thick-wall Rm relief 19.6 N/mm² applies. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution anneal for corrosion duty; furnace oxidation service may specify as-hot-finished.
Seamless Pipe Manufacture of GOST 9940 10Х23Н18
SHH STEEL can produce 10Х23Н18 as hot-deformed seamless pipe to GOST 9940-81, then apply ordered heat treatment, scale removal, and end finish. Plain square-cut ends are default; weld bevels on walls over 5 mm only when the purchaser asks. Seamless hot-deformed manufacture remains the only valid order path for 10Х23Н18 under GOST 9940; the acknowledgement repeats that route so production cannot silently change after the PO is firm. Keep the 10Х23Н18 caution visible here: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note.
After hot deformation, 10Х23Н18 receives heat treatment only if the order asks for it — Solution anneal for corrosion duty; furnace oxidation service may specify as-hot-finished. Austenitic heats usually take solution annealing with rapid cool when HT is ordered; skip inventing a mandatory anneal when the PO says without heat treatment. Use thread: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys.
Marking carries the grade 10Х23Н18, size, precision cue when high class, manufacturer ID, and GOST 9940 reference. Size hint: OD capped at 168 mm for this mark. Weld thread for fabricator joints: 310-class fillers; control ferrite and hot cracking on thick wall. Hydrostatic pressure or UT class for 10Х23Н18 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Size practice for 10Х23Н18 remains OD capped at 168 mm for this mark.
Dimensions and Tolerances for GOST 9940 10Х23Н18
Dimensional order lines for 10Х23Н18 should state OD × wall, length type (random, exact, multiple, or limited), end finish, and precision class. Use: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Max OD for this mark: 168 mm. Precision class follows the tolerance ordered for 10Х23Н18, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 10Х23Н18 duty: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
Ovality has no separate number — it must not push OD outside the diameter tolerance. Caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note. Fixed lengths and multiple cut lengths for 10Х23Н18 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 10Х23Н18: 310-class fillers; control ferrite and hot cracking on thick wall.
Equivalent Grades for GOST 9940 10Х23Н18
Do not treat 310 / UNS S31000 family (approx) as interchangeable paperwork for GOST 9940 10Х23Н18. Chemistry kinship is not acceptance kinship under this product standard. Hydrostatic, NDT, and heat-treatment text diverge across systems even when the cast analysis looks familiar. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (10Х23Н18).
| System | Designation | Notes |
|---|---|---|
| GOST 9940 | 10Х23Н18 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 310 / UNS S31000 family (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 310 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | EN 1.4845 | Starting point for comparison only; no automatic dual-cert |
Read the notes column literally for 10Х23Н18: related chemistry is not automatic dual-cert. Cross-check GOST 9940 08Х20Н14С2, GOST 9940 12Х18Н12Т, GOST 9940 17Х18Н9 when Mo, stabilisation, or carbon ceilings change the selection. Hub: GOST 9940. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (10Х23Н18).
Heat Treatment and Delivery Condition for GOST 9940 10Х23Н18
Mill heat treatment for 10Х23Н18 is optional per clause 2.1 — Solution anneal for corrosion duty; furnace oxidation service may specify as-hot-finished. Bright or descaled finishes are separate order items. Delivery label: as ordered — heat-treated or without heat treatment. Recorded furnace charts for 10Х23Н18 should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Corrosion framing beside 10Х23Н18: oxidation and carburisation resistance dominate; aqueous chlorides are secondary.
Certificate wording for 10Х23Н18 should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature — or explicitly “without heat treatment” when that was ordered. Use: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Field heat treatment of 10Х23Н18 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 10Х23Н18: oxidation and carburisation resistance dominate; aqueous chlorides are secondary.
Corrosion Resistance of GOST 9940 10Х23Н18
oxidation and carburisation resistance dominate; aqueous chlorides are secondary Ordering IGC does not create a blanket corrosion warranty for every medium. Family filing: austenitic heat-resisting 25-20 class. Coupon orientation, weld condition, and surface finish for 10Х23Н18 belong in the corrosion test order so results can be compared to the installed spool honestly. Size practice for 10Х23Н18 remains OD capped at 168 mm for this mark.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 10Х23Н18 honestly against 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. Role: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 10Х23Н18 rather than relying on wall thickness alone. Keep the 10Х23Н18 caution visible here: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note.
Applications of GOST 9940 10Х23Н18 Seamless Pipe
Typical BOM language pairs GOST 9940 10Х23Н18 with OD × wall, precision class, and heat-treatment yes/no. Primary sketch: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Spool fabricators should copy 10Х23Н18 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 10Х23Н18 remains OD capped at 168 mm for this mark.
Spell 10Х23Н18 on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. Commissioning teams benefit when the as-built dossier repeats 10Х23Н18 beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 10Х23Н18 stays reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys.
Weldability of GOST 9940 10Х23Н18
Weldability of 10Х23Н18 follows austenitic heat-resisting 25-20 class practice. Filler/shop note: 310-class fillers; control ferrite and hot cracking on thick wall. Caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note. Procedure qualification for 10Х23Н18 should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Keep the 10Х23Н18 caution visible here: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note.
For corrosive as-welded duty on 10Х23Н18, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 310-class fillers; control ferrite and hot cracking on thick wall. Order sulphur ≤0.020% when the pipe is intended for welding. Consumable lot control and shielding-gas notes for 10Х23Н18 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 10Х23Н18: oxidation and carburisation resistance dominate; aqueous chlorides are secondary.
Surface Finishes for GOST 9940 10Х23Н18
Finish options for 10Х23Н18 follow the ordered heat-treatment route under GOST 9940. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: as ordered — heat-treated or without heat treatment. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 10Х23Н18.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Bright or polished callouts for 10Х23Н18 never waive heat-treatment proof. After finishing, keep iron-free handling through storage and shipment so GOST 9940 pipe does not leave the yard with free-iron blooms. Caution retained: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (10Х23Н18).
Inspection and Testing for GOST 9940 10Х23Н18
SHH STEEL reports the tests actually performed for 10Х23Н18 — no surrogate NDT lines. Hydrostatic versus ultrasonic choice belongs on the PO. Caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note. Sampling plans for 10Х23Н18 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Size practice for 10Х23Н18 remains OD capped at 168 mm for this mark.
Retests use double sample counts from the same party — failures are not silently shipped. Size context: OD capped at 168 mm for this mark. Non-conforming 10Х23Н18 lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Application context for 10Х23Н18 stays reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys.
Packaging and Shipping for GOST 9940 10Х23Н18
Export packing for GOST 9940 10Х23Н18 is built around rust prevention and transit abrasion control. Bundle tickets repeat the Cyrillic grade symbol and heat number. Duty: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. Bundle tickets for 10Х23Н18 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 10Х23Н18 duty: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 10Х23Н18. Desiccant and wrap choices for 10Х23Н18 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 10Х23Н18 caution visible here: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note.
Photographic packing records are available on request for project QA files on 10Х23Н18. Claims handling for 10Х23Н18 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 10Х23Н18: oxidation and carburisation resistance dominate; aqueous chlorides are secondary.
Why Choose SHH STEEL
Buyers choose SHH STEEL for 10Х23Н18 because the paperwork matches the stencil: GOST 5632 chemistry, Table 3 tensile, ordered HT, and honest seamless marking. Application fit: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. SHH STEEL can produce and supply 10Х23Н18 against the OD × wall, hot-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 10Х23Н18 cleanly. Ask for a written acknowledgement that names 10Х23Н18, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 10Х23Н18 to that written scope.
Supply Capability
Supply capability for 10Х23Н18 covers hot-deformed seamless manufacture, ordered heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 10Х23Н18 when the mill schedule allows. This paragraph is locked to 10Х23Н18 duty: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines.
| Item | Capability |
|---|---|
| Standard | GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes |
| Grade | 10Х23Н18 (GOST 5632 chemistry; alias 310 / UNS S31000 family (approx)) |
| Product form | Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941) |
| Delivery condition | as ordered — heat-treated or without heat treatment |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: ≤168 mm per Table 1 note 1 |
| Precision | Ordinary or high (index “в” when high) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes for 10Х23Н18: common OD×wall combinations as the project uses. Hot-deformed availability varies by diameter — confirm with the RFQ. Hint: OD capped at 168 mm for this mark. SHH STEEL can supply alternate walls and precision classes for 10Х23Н18 once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the 10Х23Н18 supply scope when the PO says so. Use: reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. SHH STEEL can produce trial lengths of 10Х23Н18 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9940 10Х23Н18 seamless stainless steel pipe used for?
- GOST 9940 10Х23Н18 is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — reformer outlets, furnace coils, and high-temperature CIS process pipe short of true nickel alloys. Role summary: 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9940 10Х23Н18 seamless only, or does it cover welded pipe?
- Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 10Х23Н18 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 10Х23Н18 under GOST 9940?
- No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution anneal for corrosion duty; furnace oxidation service may specify as-hot-finished. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
-
How does 10Х23Н18 compare with sister grades 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9?
- 10Х23Н18 is filed as austenitic heat-resisting 25-20 class. Typical sisters on the same RFQ are 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. Design caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 10Х23Н18?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
-
Is 310 / UNS S31000 family (approx) the same as ordering 10Х23Н18?
- No. 310 / UNS S31000 family (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 10Х23Н18 so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9940 10Х23Н18?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 10Х23Н18 within Table 1 practice, respecting the mark’s diameter cap (≤168 mm per Table 1 note 1). Size context: OD capped at 168 mm for this mark. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
-
How should 10Х23Н18 be welded on site?
- Shop guidance: 310-class fillers; control ferrite and hot cracking on thick wall. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note
-
When should I choose a Mo-bearing or duplex grade instead of 10Х23Н18?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic heat-resisting 25-20 class practice can defend for the temperature and stress state. Caution for this mark: sulphur-bearing atmospheres attack chromium films — check the gas analysis before copying a 310S note Sister pointers: 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9940 10Х23Н18 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 10Х23Н18 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9940 10Х23Н18 differ from GOST 9941 of the same mark?
- GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 10Х23Н18.
Conclusion
GOST 9940 10Х23Н18 is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — 25-20 class heat-resisting austenitic seamless pipe for furnace and hot-gas lines. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х20Н14С2, 12Х18Н12Т, 17Х18Н9. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.