GOST 9940 08Х18Н10 Seamless Stainless Steel Pipe
What is GOST 9940 08Х18Н10 Seamless Stainless Steel Pipe
GOST 9940 covers seamless hot-deformed stainless pipe with OD 57–325 mm and wall 3.5–32 mm in two precision classes. Inside that standard, 08Х18Н10 is filed as austenitic 18-8. The everyday 18-8 hot-deformed seamless mark — not a silent ASTM A312 certificate. Buyers working CIS fluid packages should treat 08Х18Н10 as a governed product grade under GOST 9940-81, with GOST 5632 chemistry and Table 3 tensile floors enforced on the same heat. Weld-shop note tied to 08Х18Н10: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty.
From pierce through marking and crate protection, SHH STEEL can produce GOST 9940 08Х18Н10 for the sizes and tests on your RFQ. Application sketch: water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9940. Size and test clarity on the RFQ lets SHH STEEL lock the correct hot-deformed seamless scope for 08Х18Н10 before production starts. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.
On the floor people latinise marks; in QA they must not. 08Х18Н10 under GOST 9940 carries specific Table 3 floors that a loose “304” note will not enforce. Caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 08Х18Н10 so informal alias language cannot reopen the carbon or molybdenum window after melt. Weld-shop note tied to 08Х18Н10: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty.
Pair standard GOST 9941 uses many of the same marks with colder deformation and different Rm/δ5 pairs — do not mix certificates. Sisters: 04Х18Н10, 08Х18Н10Т, 12Х18Н9. Use thread: water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9940. Document the medium, design temperature, and weld map beside the 08Х18Н10 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the 08Х18Н10 caution visible here: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.
Inside this GOST 9940 series, compare GOST 9940 04Х18Н10, GOST 9940 08Х18Н10Т, GOST 9940 12Х18Н9. Hub: GOST 9940. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP304.
For 08Х18Н10, vertical navigation stays form-specific — keep tubular RFQs under Stainless Steel Pipes and Tubes, flat RFQs under Stainless Steel Sheets and Plates, and pin the plate twin with ASTM A240 Type 304. Keep 08Х18Н10 acceptance text on the governing pipe/tube standard.
Chemical Composition of GOST 9940 08Х18Н10
For 08Х18Н10, the melt ticket has to show GOST 5632 compliance — C ≤0.08, Si ≤0.80, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 9.00–11.00, Cr 17.00–19.00. Optional residual limits still forbid blurring grade identity. Corrosion framing: classic chromium-nickel passive film; chlorides and reducing acids limit outdoor life.
Where Mo, Ti or Nb appear, they are intentional levers for 08Х18Н10, not optional marketing. Confirm them on the MTC line-by-line. Role: standard 18-8 austenitic seamless pipe for general CIS fluid service. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 08Х18Н10 before the order is acknowledged. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 08Х18Н10 | ≤0.08 | ≤0.80 | ≤2.00 | ≤0.035 | ≤0.020 | 9.00–11.00 | 17.00–19.00 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9940 08Х18Н10
Do not confuse Table 3 hot-deformed floors with GOST 9941 cold-deformed numbers that share the 304 / UNS S30400 (approx) alias. For 08Х18Н10 under 9940 expect Rm min 510 N/mm², elongation δ5 min 40% (yield not normalised in Table 3), verified per heat/lot rules. Note: Yield not normalised; thick-wall Rm relief applies.
When comparing 08Х18Н10 to a cold-deformed GOST 9941 sister, expect different Rm/δ5 pairs even at identical GOST 5632 chemistry. Duty: standard 18-8 austenitic seamless pipe for general CIS fluid service. Do not substitute GOST 9941 cold-deformed tensile numbers onto a hot-deformed 08Х18Н10 certificate without a written dual-product plan. Size practice for 08Х18Н10 remains full OD to 325 mm.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 08Х18Н10 | 510 | — (not normalised) | 40 | 7.9 | full Table 1 range |
Ambient values from GOST 9940-81 Table 3 for 08Х18Н10. Yield not normalised; thick-wall Rm relief applies. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution anneal when ordered.
Seamless Pipe Manufacture of GOST 9940 08Х18Н10
Seamless is not optional wording for 08Х18Н10: GOST 9940 covers hot-deformed seamless corrosion-resistant pipe. Cold- and warm-deformed sisters live under GOST 9941-81 with different tensile floors. SHH STEEL will not quietly substitute a welded or cold-drawn route under a 9940 PO. Seamless hot-deformed manufacture remains the only valid order path for 08Х18Н10 under GOST 9940; the acknowledgement repeats that route so production cannot silently change after the PO is firm. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.
Precision class (ordinary or high) is an order item for 08Х18Н10; unmarked class means ordinary. Heat treatment: Solution anneal when ordered. Austenitic heats usually take solution annealing with rapid cool when HT is ordered; skip inventing a mandatory anneal when the PO says without heat treatment. Pickling or descaling decisions for 08Х18Н10 stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.
Hydraulic testing per GOST 3845 and ultrasonic inspection run only when ordered — technology is deemed to ensure pressure capacity, but the certificate lists only tests performed. Manufacture stays seamless hot-deformed. Size: full OD to 325 mm. Hydrostatic pressure or UT class for 08Х18Н10 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Application context for 08Х18Н10 stays water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9940.
Dimensions and Tolerances for GOST 9940 08Х18Н10
Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 08Х18Н10. Duty: standard 18-8 austenitic seamless pipe for general CIS fluid service. Cap: full Table 1 range. Precision class follows the tolerance ordered for 08Х18Н10, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for 08Х18Н10 remains full OD to 325 mm.
High precision mainly tightens the plus wall tolerance; the minus side stays punishing — quote class with the size for 08Х18Н10. Fixed lengths and multiple cut lengths for 08Х18Н10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for 08Х18Н10 remains full OD to 325 mm.
Equivalent Grades for GOST 9940 08Х18Н10
08Х18Н10 is the GOST 9940 designation for this seamless stainless steel pipe (hot-deformed). Alias 304 / UNS S30400 (approx) appears only as a cross-walk. When a dual-cert path is required, list both GOST 9940 08Х18Н10 and the foreign mark with separate scopes instead of assuming one chemistry line clears both files.
| System | Designation | Notes |
|---|---|---|
| GOST 9940 | 08Х18Н10 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 304 / UNS S30400 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 304 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | EN 1.4301 | Starting point for comparison only; no automatic dual-cert |
Read the notes column literally for 08Х18Н10: related chemistry is not automatic dual-cert. Cross-check GOST 9940 04Х18Н10, GOST 9940 08Х18Н10Т, GOST 9940 12Х18Н9 when Mo, stabilisation, or carbon ceilings change the selection. Hub: GOST 9940. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (08Х18Н10). Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (08Х18Н10).
Heat Treatment and Delivery Condition for GOST 9940 08Х18Н10
Unlike GOST 9941, GOST 9940 does not force heat treatment on every pipe. Confirm for 08Х18Н10. Band note: Solution anneal when ordered. Recorded furnace charts for 08Х18Н10 should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Application context for 08Х18Н10 stays water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9940.
Party acceptance groups pipes by size, mark, and heat-treatment kind — mixing HT and non-HT lengths in one lot breaks the batch rule for 08Х18Н10. Field heat treatment of 08Х18Н10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 08Х18Н10 caution visible here: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.
Corrosion Resistance of GOST 9940 08Х18Н10
Medium, temperature, crevice geometry and weld condition decide whether 08Х18Н10 is enough. Summary: classic chromium-nickel passive film; chlorides and reducing acids limit outdoor life. Escalate via sisters 04Х18Н10, 08Х18Н10Т, 12Х18Н9 when coupons fail. Coupon orientation, weld condition, and surface finish for 08Х18Н10 belong in the corrosion test order so results can be compared to the installed spool honestly. Keep the 08Х18Н10 caution visible here: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.
Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 08Х18Н10. Corrosion framing: classic chromium-nickel passive film; chlorides and reducing acids limit outdoor life. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 08Х18Н10 rather than relying on wall thickness alone. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.
Applications of GOST 9940 08Х18Н10 Seamless Pipe
From utility rooms to process racks, 08Х18Н10 shows up wherever CIS fluid specs want austenitic 18-8 hot-deformed seamless behaviour. Use list: water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9940. Spool fabricators should copy 08Х18Н10 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.
If the only reason for 08Х18Н10 is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed. Commissioning teams benefit when the as-built dossier repeats 08Х18Н10 beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.
Weldability of GOST 9940 08Х18Н10
Automatic mill welding is outside GOST 9940; manual and automatic field welds must still respect 08Х18Н10 chemistry. Guidance: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty. Procedure qualification for 08Х18Н10 should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Keep the 08Х18Н10 caution visible here: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed.
Ferrite control on high-Ni austenitics and hydrogen management on martensitic 08Х18Н10 are procedure items, not afterthoughts. Guidance: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty. Consumable lot control and shielding-gas notes for 08Х18Н10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.
Surface Finishes for GOST 9940 08Х18Н10
On 08Х18Н10, cosmetics never outrank correct heat treatment. Passivation and polish are sequenced after the anneal that qualifies the pipe. Duty locked here: standard 18-8 austenitic seamless pipe for general CIS fluid service. Name which surface carries each finish callout. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for 08Х18Н10.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Bright or polished callouts for 08Х18Н10 never waive heat-treatment proof. After finishing, keep iron-free handling through storage and shipment so GOST 9940 pipe does not leave the yard with free-iron blooms. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (08Х18Н10).
Inspection and Testing for GOST 9940 08Х18Н10
Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GOST 9940 for 08Х18Н10. Sampling plans for 08Х18Н10 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Size practice for 08Х18Н10 remains full OD to 325 mm.
Dimensional inspection against Table 2 tolerances closes the lot. Role: standard 18-8 austenitic seamless pipe for general CIS fluid service. Non-conforming 08Х18Н10 lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. This paragraph is locked to 08Х18Н10 duty: standard 18-8 austenitic seamless pipe for general CIS fluid service.
Packaging and Shipping for GOST 9940 08Х18Н10
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 08Х18Н10 stays visible on outer tags. Bundle tickets for 08Х18Н10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 08Х18Н10: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty.
Container loading plans should keep heavy walls from crushing thin-wall 08Х18Н10 layers. Desiccant and wrap choices for 08Х18Н10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 08Х18Н10: classic chromium-nickel passive film; chlorides and reducing acids limit outdoor life.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 08Х18Н10. Claims handling for 08Х18Н10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 08Х18Н10 stays water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9940.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats 08Х18Н10 as a governed product grade, not a marketing synonym for 304 / UNS S30400 (approx). Role: standard 18-8 austenitic seamless pipe for general CIS fluid service. SHH STEEL can produce and supply 08Х18Н10 against the OD × wall, hot-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Response time stays short because common 08Х18Н10 enquiry sizes and document packs are already exercised on prior GOST-spec orders. Use: water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9940. Ask for a written acknowledgement that names 08Х18Н10, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х18Н10 to that written scope.
Supply Capability
Capability framing for 08Х18Н10: GOST-spec seamless hot-deformed pipe, documented heats. Caution remains: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 08Х18Н10 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes |
| Grade | 08Х18Н10 (GOST 5632 chemistry; alias 304 / UNS S30400 (approx)) |
| Product form | Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941) |
| Delivery condition | as ordered — heat-treated or without heat treatment |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: full Table 1 range |
| Precision | Ordinary or high (index “в” when high) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 08Х18Н10 change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: standard 18-8 austenitic seamless pipe for general CIS fluid service. SHH STEEL can supply alternate walls and precision classes for 08Х18Н10 once the design pressure and corrosion allowance are clear.
Repeat orders for 08Х18Н10 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: standard 18-8 austenitic seamless pipe for general CIS fluid service. SHH STEEL can produce trial lengths of 08Х18Н10 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9940 08Х18Н10 seamless stainless steel pipe used for?
- GOST 9940 08Х18Н10 is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — water, steam condensate, food-adjacent transfer, and general process pipe written to GOST 9940. Role summary: standard 18-8 austenitic seamless pipe for general CIS fluid service. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9940 08Х18Н10 seamless only, or does it cover welded pipe?
- Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 08Х18Н10 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 08Х18Н10 under GOST 9940?
- No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution anneal when ordered. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
-
How does 08Х18Н10 compare with sister grades 04Х18Н10, 08Х18Н10Т, 12Х18Н9?
- 08Х18Н10 is filed as austenitic 18-8. Typical sisters on the same RFQ are 04Х18Н10, 08Х18Н10Т, 12Х18Н9. Design caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 08Х18Н10?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
-
Is 304 / UNS S30400 (approx) the same as ordering 08Х18Н10?
- No. 304 / UNS S30400 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 08Х18Н10 so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9940 08Х18Н10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х18Н10 within Table 1 practice, respecting the mark’s diameter cap (full Table 1 range). Size context: full OD to 325 mm. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
-
How should 08Х18Н10 be welded on site?
- Shop guidance: 308/308L fillers; consider low-C or Ti sister for corrosive as-welded duty. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed
-
When should I choose a Mo-bearing or duplex grade instead of 08Х18Н10?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic 18-8 practice can defend for the temperature and stress state. Caution for this mark: C ≤0.08% is not automatic IGC immunity after heavy welding — specify 04Х18Н10 or Ti grades when needed Sister pointers: 04Х18Н10, 08Х18Н10Т, 12Х18Н9. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9940 08Х18Н10 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 08Х18Н10 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9940 08Х18Н10 differ from GOST 9941 of the same mark?
- GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х18Н10.
Conclusion
GOST 9940 08Х18Н10 is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — standard 18-8 austenitic seamless pipe for general CIS fluid service. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 04Х18Н10, 08Х18Н10Т, 12Х18Н9. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.