GOST 9940 08Х17Н15М3Т Seamless Stainless Steel Pipe
What is GOST 9940 08Х17Н15М3Т Seamless Stainless Steel Pipe
Russian and CIS piping packages that print GOST 9940 expect hot-deformed seamless stainless pipe, not a welded substitute and not an automatic ASTM A312 certificate. 08Х17Н15М3Т is the Cyrillic mark on Table 3 for this austenitic Mo + Ti (317Ti class) chemistry. Mill brand ЭИ580. The Mo-rich Ti austenitic when 316Ti chemistry is not enough on a GOST pipe BOM.
Mill path for 08Х17Н15М3Т: hot-deformed seamless route, clause 2.1 heat-treatment choice, GOST 5632 chemistry, Table 3 Rm and elongation, optional hydro / UT / IGC when ordered. SHH STEEL can make and supply the grade to that stack. Typical use: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т.
Body text may mention 317Ti / UNS S31726 family (approx) for cross-reference, but the H1 and order line stay on Cyrillic 08Х17Н15М3Т. Silent alias swaps are how wrong carbon ceilings and wrong Table 3 numbers enter the MTC. Keep this caution in view: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard.
Order the standard the drawing and regulatory file actually require. Inside this 9940 series, compare 10Х17Н13М2Т, 08Х18Н10Т, 08Х18Н12Т before stretching surface finish or wall alone. Duty thread: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. Document the medium, design temperature, and weld map beside the 08Х17Н15М3Т line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Weld-shop note tied to 08Х17Н15М3Т: 317L/Mo-bearing fillers; Ti on the heat already; control heat input.
Inside this GOST 9940 series, compare GOST 9940 10Х17Н13М2Т, GOST 9940 08Х18Н10Т, GOST 9940 08Х18Н12Т. Hub: GOST 9940. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP317L, ASTM A312 TP316Ti.
Chemical Composition of GOST 9940 08Х17Н15М3Т
GOST 5632 sets the melt limits for 08Х17Н15М3Т. Highlight band: C ≤0.08, Si ≤0.80, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 14.00–16.00, Cr 16.00–18.00, Mo 3.00–4.00. For pipe intended for welding, GOST 9940 can tighten sulphur to ≤0.020% when the order states that duty. Alias note: 317Ti / UNS S31726 family (approx).
The composition table below is the cast window SHH STEEL quotes against for 08Х17Н15М3Т. Edition framing is GOST 5632 for chemistry and GOST 9940-81 for the pipe product. Use thread: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 08Х17Н15М3Т before the order is acknowledged. This paragraph is locked to 08Х17Н15М3Т duty: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo | Ti |
|---|---|---|---|---|---|---|---|---|---|
| 08Х17Н15М3Т | ≤0.08 | ≤0.80 | ≤2.00 | ≤0.035 | ≤0.020 | 14.00–16.00 | 16.00–18.00 | 3.00–4.00 | 0.30–0.60 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9940 08Х17Н15М3Т
Table 3 mechanical acceptance for 08Х17Н15М3Т: Rm min 510 N/mm², elongation δ5 min 35% (yield not normalised in Table 3). Note: Yield not normalised; thick-wall Rm relief applies. Delivery framing: as ordered — heat-treated or without heat treatment. Density for mass calc: 8.1 g/cm³. Sampling follows GOST 9940 batch rules (party ≤200 pcs).
Elevated-temperature tensile at 623 K (350 °C) and yield determination are purchaser options, not defaults. For 08Х17Н15М3Т, state them on the PO if the stress calculation needs them. Use: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Do not substitute GOST 9941 cold-deformed tensile numbers onto a hot-deformed 08Х17Н15М3Т certificate without a written dual-product plan. Keep the 08Х17Н15М3Т caution visible here: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 08Х17Н15М3Т | 510 | — (not normalised) | 35 | 8.1 | ≤140 mm; exception 159×9 mm allowed |
Ambient values from GOST 9940-81 Table 3 for 08Х17Н15М3Т. Yield not normalised; thick-wall Rm relief applies. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution anneal; Ti stabilisation for welded corrosive duty.
Seamless Pipe Manufacture of GOST 9940 08Х17Н15М3Т
GOST 9940-81 manufactures 08Х17Н15М3Т as seamless hot-deformed stainless pipe only — pierce, roll, or extrude at hot-working temperature, then finish to Table 1 sizes. SHH STEEL confirms the hot-deformed seamless route on the acknowledgement before the billet is pierced; welded pipe and cold-deformed GOST 9941 product are outside this line item.
After hot deformation, 08Х17Н15М3Т receives heat treatment only if the order asks for it — Solution anneal; Ti stabilisation for welded corrosive duty. Austenitic heats usually take solution annealing with rapid cool when HT is ordered; skip inventing a mandatory anneal when the PO says without heat treatment. Use thread: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т.
Marking carries the grade 08Х17Н15М3Т, size, precision cue when high class, manufacturer ID, and GOST 9940 reference. Size hint: ≤140 mm OD (159×9 allowed exception). Weld thread for fabricator joints: 317L/Mo-bearing fillers; Ti on the heat already; control heat input. Hydrostatic pressure or UT class for 08Х17Н15М3Т is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Keep the 08Х17Н15М3Т caution visible here: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard.
Dimensions and Tolerances for GOST 9940 08Х17Н15М3Т
Dimensional order lines for 08Х17Н15М3Т should state OD × wall, length type (random, exact, multiple, or limited), end finish, and precision class. Use: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Max OD for this mark: 140 mm. Precision class follows the tolerance ordered for 08Х17Н15М3Т, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 08Х17Н15М3Т duty: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
Ovality has no separate number — it must not push OD outside the diameter tolerance. Caution: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard. Fixed lengths and multiple cut lengths for 08Х17Н15М3Т are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 08Х17Н15М3Т: 317L/Mo-bearing fillers; Ti on the heat already; control heat input.
Equivalent Grades for GOST 9940 08Х17Н15М3Т
GOST 9940 does not make 317Ti / UNS S31726 family (approx) a drop-in certificate for 08Х17Н15М3Т. Use the commercial name in dual-cert talk, then verify every Table limit that matters for this pipe. Sisters in the series are comparison pages, not interchangeable stock codes. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (08Х17Н15М3Т).
| System | Designation | Notes |
|---|---|---|
| GOST 9940 | 08Х17Н15М3Т | Governing pipe grade for this page |
| Commercial / UNS (body only) | 317Ti / UNS S31726 family (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Inside this series compare GOST 9940 10Х17Н13М2Т, GOST 9940 08Х18Н10Т, GOST 9940 08Х18Н12Т before swapping marks for medium or temperature. Keep this caution visible for 08Х17Н15М3Т: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard. Hub: GOST 9940. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (08Х17Н15М3Т).
On 08Х17Н15М3Т packages that also list flats, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is ASTM A240 UNS S31726. Quote 08Х17Н15М3Т pipe and plate under separate line items.
Heat Treatment and Delivery Condition for GOST 9940 08Х17Н15М3Т
Mill heat treatment for 08Х17Н15М3Т is optional per clause 2.1 — Solution anneal; Ti stabilisation for welded corrosive duty. Bright or descaled finishes are separate order items. Delivery label: as ordered — heat-treated or without heat treatment. Recorded furnace charts for 08Х17Н15М3Т should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Application context for 08Х17Н15М3Т stays urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т.
Certificate wording for 08Х17Н15М3Т should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature — or explicitly “without heat treatment” when that was ordered. Use: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Field heat treatment of 08Х17Н15М3Т after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 08Х17Н15М3Т: Mo ~3–4% plus Ti — above 316Ti for many reducing/chloride mixes.
Corrosion Resistance of GOST 9940 08Х17Н15М3Т
Mo ~3–4% plus Ti — above 316Ti for many reducing/chloride mixes Ordering IGC does not create a blanket corrosion warranty for every medium. Family filing: austenitic Mo + Ti (317Ti class). Coupon orientation, weld condition, and surface finish for 08Х17Н15М3Т belong in the corrosion test order so results can be compared to the installed spool honestly. Size practice for 08Х17Н15М3Т remains ≤140 mm OD (159×9 allowed exception).
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 08Х17Н15М3Т honestly against 10Х17Н13М2Т, 08Х18Н10Т, 08Х18Н12Т. Role: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 08Х17Н15М3Т rather than relying on wall thickness alone. Weld-shop note tied to 08Х17Н15М3Т: 317L/Mo-bearing fillers; Ti on the heat already; control heat input.
Applications of GOST 9940 08Х17Н15М3Т Seamless Pipe
Typical BOM language pairs GOST 9940 08Х17Н15М3Т with OD × wall, precision class, and heat-treatment yes/no. Primary sketch: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Spool fabricators should copy 08Х17Н15М3Т onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 08Х17Н15М3Т caution visible here: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard.
Spell 08Х17Н15М3Т on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 10Х17Н13М2Т, 08Х18Н10Т, 08Х18Н12Т. Commissioning teams benefit when the as-built dossier repeats 08Х17Н15М3Т beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 08Х17Н15М3Т stays urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т.
Weldability of GOST 9940 08Х17Н15М3Т
Weldability of 08Х17Н15М3Т follows austenitic Mo + Ti (317Ti class) practice. Filler/shop note: 317L/Mo-bearing fillers; Ti on the heat already; control heat input. Caution: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard. Procedure qualification for 08Х17Н15М3Т should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Application context for 08Х17Н15М3Т stays urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т.
For corrosive as-welded duty on 08Х17Н15М3Т, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 317L/Mo-bearing fillers; Ti on the heat already; control heat input. Order sulphur ≤0.020% when the pipe is intended for welding. Consumable lot control and shielding-gas notes for 08Х17Н15М3Т stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 08Х17Н15М3Т caution visible here: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard.
Surface Finishes for GOST 9940 08Х17Н15М3Т
On 08Х17Н15М3Т, cosmetics never outrank correct heat treatment. Passivation and polish are sequenced after the anneal that qualifies the pipe. Duty locked here: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. Name which surface carries each finish callout. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (08Х17Н15М3Т).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
For 08Х17Н15М3Т, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this pipe. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 08Х17Н15М3Т.
Inspection and Testing for GOST 9940 08Х17Н15М3Т
SHH STEEL reports the tests actually performed for 08Х17Н15М3Т — no surrogate NDT lines. Hydrostatic versus ultrasonic choice belongs on the PO. Caution: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard. Sampling plans for 08Х17Н15М3Т keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for 08Х17Н15М3Т stays urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т.
Retests use double sample counts from the same party — failures are not silently shipped. Size context: ≤140 mm OD (159×9 allowed exception). Non-conforming 08Х17Н15М3Т lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Size practice for 08Х17Н15М3Т remains ≤140 mm OD (159×9 allowed exception).
Packaging and Shipping for GOST 9940 08Х17Н15М3Т
Export packing for GOST 9940 08Х17Н15М3Т is built around rust prevention and transit abrasion control. Bundle tickets repeat the Cyrillic grade symbol and heat number. Duty: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. Bundle tickets for 08Х17Н15М3Т repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 08Х17Н15М3Т duty: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 08Х17Н15М3Т. Desiccant and wrap choices for 08Х17Н15М3Т follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 08Х17Н15М3Т: Mo ~3–4% plus Ti — above 316Ti for many reducing/chloride mixes.
Photographic packing records are available on request for project QA files on 08Х17Н15М3Т. Claims handling for 08Х17Н15М3Т starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to 08Х17Н15М3Т duty: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids.
Why Choose SHH STEEL
Buyers choose SHH STEEL for 08Х17Н15М3Т because the paperwork matches the stencil: GOST 5632 chemistry, Table 3 tensile, ordered HT, and honest seamless marking. Application fit: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. SHH STEEL can produce and supply 08Х17Н15М3Т against the OD × wall, hot-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 08Х17Н15М3Т cleanly. Ask for a written acknowledgement that names 08Х17Н15М3Т, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х17Н15М3Т to that written scope.
Supply Capability
Supply capability for 08Х17Н15М3Т covers hot-deformed seamless manufacture, ordered heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 08Х17Н15М3Т when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes |
| Grade | 08Х17Н15М3Т (GOST 5632 chemistry; alias 317Ti / UNS S31726 family (approx)) |
| Product form | Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941) |
| Delivery condition | as ordered — heat-treated or without heat treatment |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: ≤140 mm; exception 159×9 mm allowed |
| Precision | Ordinary or high (index “в” when high) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes for 08Х17Н15М3Т: common OD×wall combinations as the project uses. Hot-deformed availability varies by diameter — confirm with the RFQ. Hint: ≤140 mm OD (159×9 allowed exception). SHH STEEL can supply alternate walls and precision classes for 08Х17Н15М3Т once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the 08Х17Н15М3Т supply scope when the PO says so. Use: urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. SHH STEEL can produce trial lengths of 08Х17Н15М3Т for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9940 08Х17Н15М3Т seamless stainless steel pipe used for?
- GOST 9940 08Х17Н15М3Т is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — urea peripheral lines, organic acid condensers, and CIS chemical packages that outgrow 10Х17Н13М2Т. Role summary: high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9940 08Х17Н15М3Т seamless only, or does it cover welded pipe?
- Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 08Х17Н15М3Т when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 08Х17Н15М3Т under GOST 9940?
- No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution anneal; Ti stabilisation for welded corrosive duty. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
-
How does 08Х17Н15М3Т compare with sister grades 10Х17Н13М2Т, 08Х18Н10Т, 08Х18Н12Т?
- 08Х17Н15М3Т is filed as austenitic Mo + Ti (317Ti class). Typical sisters on the same RFQ are 10Х17Н13М2Т, 08Х18Н10Т, 08Х18Н12Т. Design caution: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 08Х17Н15М3Т?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
-
Is 317Ti / UNS S31726 family (approx) the same as ordering 08Х17Н15М3Т?
- No. 317Ti / UNS S31726 family (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 08Х17Н15М3Т so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9940 08Х17Н15М3Т?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х17Н15М3Т within Table 1 practice, respecting the mark’s diameter cap (≤140 mm; exception 159×9 mm allowed). Size context: ≤140 mm OD (159×9 allowed exception). Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
-
How should 08Х17Н15М3Т be welded on site?
- Shop guidance: 317L/Mo-bearing fillers; Ti on the heat already; control heat input. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard
-
When should I choose a Mo-bearing or duplex grade instead of 08Х17Н15М3Т?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic Mo + Ti (317Ti class) practice can defend for the temperature and stress state. Caution for this mark: OD limited (≤140 mm, plus 159×9 exception) — large-bore RFQs may need another standard Sister pointers: 10Х17Н13М2Т, 08Х18Н10Т, 08Х18Н12Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9940 08Х17Н15М3Т with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 08Х17Н15М3Т does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9940 08Х17Н15М3Т differ from GOST 9941 of the same mark?
- GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х17Н15М3Т.
Conclusion
GOST 9940 08Х17Н15М3Т is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — high-Mo Ti-stabilised austenitic seamless pipe for aggressive chloride / organic acids. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 10Х17Н13М2Т, 08Х18Н10Т, 08Х18Н12Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.