GOST 9940 08Х13 Seamless Stainless Steel Pipe
What is GOST 9940 08Х13 Seamless Stainless Steel Pipe
GOST 9940 covers seamless hot-deformed stainless pipe with OD 57–325 mm and wall 3.5–32 mm in two precision classes. Inside that standard, 08Х13 is filed as ferritic-martensitic chromium. Mill brand ЭИ496. It is the soft chromium mark under GOST 9940 Table 3, not a drop-in for 18-8 austenitic pipe.
From pierce through marking and crate protection, SHH STEEL can produce GOST 9940 08Х13 for the sizes and tests on your RFQ. Application sketch: turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs. Size and test clarity on the RFQ lets SHH STEEL lock the correct hot-deformed seamless scope for 08Х13 before production starts. Corrosion framing beside 08Х13: chromium passive film for mild water and wet steam; chlorides and reducing acids are outside the usual window.
On the floor people latinise marks; in QA they must not. 08Х13 under GOST 9940 carries specific Table 3 floors that a loose “410S” note will not enforce. Caution: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 08Х13 so informal alias language cannot reopen the carbon or molybdenum window after melt. Corrosion framing beside 08Х13: chromium passive film for mild water and wet steam; chlorides and reducing acids are outside the usual window.
Pair standard GOST 9941 uses many of the same marks with colder deformation and different Rm/δ5 pairs — do not mix certificates. Sisters: 12Х13, 08Х17Т, 12Х17. Use thread: turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs. Document the medium, design temperature, and weld map beside the 08Х13 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the 08Х13 caution visible here: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up.
Inside this GOST 9940 series, compare GOST 9940 12Х13, GOST 9940 08Х17Т, GOST 9940 12Х17. Hub: GOST 9940.
Beside this 08Х13 page, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is ASTM A240 Type 410. Keep 08Х13 acceptance text on the governing pipe/tube standard.
Chemical Composition of GOST 9940 08Х13
For 08Х13, the melt ticket has to show GOST 5632 compliance — C ≤0.08, Si ≤0.80, Mn ≤0.80, P ≤0.030, S ≤0.025, Cr 12.00–14.00. Optional residual limits still forbid blurring grade identity. Corrosion framing: chromium passive film for mild water and wet steam; chlorides and reducing acids are outside the usual window.
Where Mo, Ti or Nb appear, they are intentional levers for 08Х13, not optional marketing. Confirm them on the MTC line-by-line. Role: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 08Х13 before the order is acknowledged. Corrosion framing beside 08Х13: chromium passive film for mild water and wet steam; chlorides and reducing acids are outside the usual window.
| Grade | C | Si | Mn | P | S | Cr |
|---|---|---|---|---|---|---|
| 08Х13 | ≤0.08 | ≤0.80 | ≤0.80 | ≤0.030 | ≤0.025 | 12.00–14.00 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9940 08Х13
Do not confuse Table 3 hot-deformed floors with GOST 9941 cold-deformed numbers that share the 410S / UNS S41008 (approx) alias. For 08Х13 under 9940 expect Rm min 372 N/mm², elongation δ5 min 22% (yield not normalised in Table 3), verified per heat/lot rules. Note: Yield not normalised in GOST 9940 Table 3.
When comparing 08Х13 to a cold-deformed GOST 9941 sister, expect different Rm/δ5 pairs even at identical GOST 5632 chemistry. Duty: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted. Do not substitute GOST 9941 cold-deformed tensile numbers onto a hot-deformed 08Х13 certificate without a written dual-product plan. Keep the 08Х13 caution visible here: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 08Х13 | 372 | — (not normalised) | 22 | 7.7 | full Table 1 range |
Ambient values from GOST 9940-81 Table 3 for 08Х13. Yield not normalised in GOST 9940 Table 3. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Annealing / softening when heat treatment is ordered; GOST 9940 does not mandate HT.
Seamless Pipe Manufacture of GOST 9940 08Х13
GOST 9940-81 manufactures 08Х13 as seamless hot-deformed stainless pipe only — pierce, roll, or extrude at hot-working temperature, then finish to Table 1 sizes. SHH STEEL confirms the hot-deformed seamless route on the acknowledgement before the billet is pierced; welded pipe and cold-deformed GOST 9941 product are outside this line item.
Precision class (ordinary or high) is an order item for 08Х13; unmarked class means ordinary. Heat treatment: Annealing / softening when heat treatment is ordered; GOST 9940 does not mandate HT. Ferritic heats follow softening / anneal practice when HT is ordered — not austenitic solution charts. Grain growth after overheating remains a shop risk.
Hydraulic testing per GOST 3845 and ultrasonic inspection run only when ordered — technology is deemed to ensure pressure capacity, but the certificate lists only tests performed. Manufacture stays seamless hot-deformed. Size: full hot-deformed OD band to 325 mm when mill capacity allows; wall from 3.5 mm up. Hydrostatic pressure or UT class for 08Х13 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Application context for 08Х13 stays turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs.
Dimensions and Tolerances for GOST 9940 08Х13
Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 08Х13. Duty: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted. Cap: full Table 1 range. Precision class follows the tolerance ordered for 08Х13, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for 08Х13 remains full hot-deformed OD band to 325 mm when mill capacity allows; wall from 3.5 mm up.
High precision mainly tightens the plus wall tolerance; the minus side stays punishing — quote class with the size for 08Х13. Fixed lengths and multiple cut lengths for 08Х13 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to 08Х13: preheat/control HAZ hardness; 410/soft-martensitic fillers or matching practice — do not treat like 08Х18Н10Т.
Equivalent Grades for GOST 9940 08Х13
Do not treat 410S / UNS S41008 (approx) as interchangeable paperwork for GOST 9940 08Х13. Chemistry kinship is not acceptance kinship under this product standard. Hydrostatic, NDT, and heat-treatment text diverge across systems even when the cast analysis looks familiar. Dual marking is a purchase-order option that still requires every limit that matters for 08Х13 to be verified on the heat.
| System | Designation | Notes |
|---|---|---|
| GOST 9940 | 08Х13 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 410S / UNS S41008 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | EN 1.4000 | Starting point for comparison only; no automatic dual-cert |
When the service outgrows 08Х13, move to a sister rather than stretching the alias: GOST 9940 12Х13, GOST 9940 08Х17Т, GOST 9940 12Х17. Apps context: turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs. Full list under GOST 9940. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (08Х13).
Heat Treatment and Delivery Condition for GOST 9940 08Х13
Unlike GOST 9941, GOST 9940 does not force heat treatment on every pipe. Confirm for 08Х13. Band note: Annealing / softening when heat treatment is ordered; GOST 9940 does not mandate HT. Recorded furnace charts for 08Х13 should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Application context for 08Х13 stays turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs.
Party acceptance groups pipes by size, mark, and heat-treatment kind — mixing HT and non-HT lengths in one lot breaks the batch rule for 08Х13. Field heat treatment of 08Х13 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 08Х13 remains full hot-deformed OD band to 325 mm when mill capacity allows; wall from 3.5 mm up.
Corrosion Resistance of GOST 9940 08Х13
Medium, temperature, crevice geometry and weld condition decide whether 08Х13 is enough. Summary: chromium passive film for mild water and wet steam; chlorides and reducing acids are outside the usual window. Escalate via sisters 12Х13, 08Х17Т, 12Х17 when coupons fail. Coupon orientation, weld condition, and surface finish for 08Х13 belong in the corrosion test order so results can be compared to the installed spool honestly. This paragraph is locked to 08Х13 duty: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted.
Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 08Х13. Corrosion framing: chromium passive film for mild water and wet steam; chlorides and reducing acids are outside the usual window. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 08Х13 rather than relying on wall thickness alone. Size practice for 08Х13 remains full hot-deformed OD band to 325 mm when mill capacity allows; wall from 3.5 mm up.
Applications of GOST 9940 08Х13 Seamless Pipe
From utility rooms to process racks, 08Х13 shows up wherever CIS fluid specs want ferritic-martensitic chromium hot-deformed seamless behaviour. Use list: turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs. Spool fabricators should copy 08Х13 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 08Х13 caution visible here: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up.
If the only reason for 08Х13 is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up. Commissioning teams benefit when the as-built dossier repeats 08Х13 beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to 08Х13 duty: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted.
Weldability of GOST 9940 08Х13
Automatic mill welding is outside GOST 9940; manual and automatic field welds must still respect 08Х13 chemistry. Guidance: preheat/control HAZ hardness; 410/soft-martensitic fillers or matching practice — do not treat like 08Х18Н10Т. Procedure qualification for 08Х13 should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Keep the 08Х13 caution visible here: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up.
Ferrite control on high-Ni austenitics and hydrogen management on martensitic 08Х13 are procedure items, not afterthoughts. Guidance: preheat/control HAZ hardness; 410/soft-martensitic fillers or matching practice — do not treat like 08Х18Н10Т. Consumable lot control and shielding-gas notes for 08Х13 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 08Х13 remains full hot-deformed OD band to 325 mm when mill capacity allows; wall from 3.5 mm up.
Surface Finishes for GOST 9940 08Х13
Surface supply for 08Х13 should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless pipe, so finish is part of performance, not only appearance. Application framing: turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs. Ambiguous “bright pipe” language is clarified before finishing slots are booked.
| Finish | Typical supply | Order note |
|---|---|---|
| Annealed and pickled | Standard pipe mill finish after anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; inspect before polish on ferritic stock |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
For 08Х13, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this pipe. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (08Х13).
Inspection and Testing for GOST 9940 08Х13
Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GOST 9940 for 08Х13. Sampling plans for 08Х13 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to 08Х13: preheat/control HAZ hardness; 410/soft-martensitic fillers or matching practice — do not treat like 08Х18Н10Т.
Dimensional inspection against Table 2 tolerances closes the lot. Role: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted. Non-conforming 08Х13 lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Keep the 08Х13 caution visible here: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up.
Packaging and Shipping for GOST 9940 08Х13
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 08Х13 stays visible on outer tags. Bundle tickets for 08Х13 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 08Х13 stays turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs.
Container loading plans should keep heavy walls from crushing thin-wall 08Х13 layers. Desiccant and wrap choices for 08Х13 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for 08Х13 stays turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 08Х13. Claims handling for 08Х13 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the 08Х13 caution visible here: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats 08Х13 as a governed product grade, not a marketing synonym for 410S / UNS S41008 (approx). Role: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted. SHH STEEL can produce and supply 08Х13 against the OD × wall, hot-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Response time stays short because common 08Х13 enquiry sizes and document packs are already exercised on prior GOST-spec orders. Use: turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs. Ask for a written acknowledgement that names 08Х13, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х13 to that written scope.
Supply Capability
Capability framing for 08Х13: GOST-spec seamless hot-deformed pipe, documented heats. Caution remains: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 08Х13 when the mill schedule allows. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 08Х13 when the mill schedule allows. Corrosion framing beside 08Х13: chromium passive film for mild water and wet steam; chlorides and reducing acids are outside the usual window.
| Item | Capability |
|---|---|
| Standard | GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes |
| Grade | 08Х13 (GOST 5632 chemistry; alias 410S / UNS S41008 (approx)) |
| Product form | Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941) |
| Delivery condition | as ordered — heat-treated or without heat treatment |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: full Table 1 range |
| Precision | Ordinary or high (index “в” when high) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 08Х13 change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted. SHH STEEL can supply alternate walls and precision classes for 08Х13 once design pressure and corrosion allowance are clear. Application context for 08Х13 stays turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs.
Repeat orders for 08Х13 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted. SHH STEEL can produce trial lengths of 08Х13 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9940 08Х13 seamless stainless steel pipe used for?
- GOST 9940 08Х13 is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — turbine gland cooling, low-pressure condensate, pump columns, and general chromium stainless utility lines on CIS project specs. Role summary: soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9940 08Х13 seamless only, or does it cover welded pipe?
- Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 08Х13 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 08Х13 under GOST 9940?
- No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Annealing / softening when heat treatment is ordered; GOST 9940 does not mandate HT. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
-
How does 08Х13 compare with sister grades 12Х13, 08Х17Т, 12Х17?
- 08Х13 is filed as ferritic-martensitic chromium. Typical sisters on the same RFQ are 12Х13, 08Х17Т, 12Х17. Design caution: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 08Х13?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
-
Is 410S / UNS S41008 (approx) the same as ordering 08Х13?
- No. 410S / UNS S41008 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 08Х13 so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9940 08Х13?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х13 within Table 1 practice, respecting the mark’s diameter cap (full Table 1 range). Size context: full hot-deformed OD band to 325 mm when mill capacity allows; wall from 3.5 mm up. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
-
How should 08Х13 be welded on site?
- Shop guidance: preheat/control HAZ hardness; 410/soft-martensitic fillers or matching practice — do not treat like 08Х18Н10Т. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up
-
When should I choose a Mo-bearing or duplex grade instead of 08Х13?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what ferritic-martensitic chromium practice can defend for the temperature and stress state. Caution for this mark: not austenitic — magnetic, limited chloride tolerance, and weld HAZ can harden if carbon drifts up Sister pointers: 12Х13, 08Х17Т, 12Х17. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9940 08Х13 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 08Х13 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9940 08Х13 differ from GOST 9941 of the same mark?
- GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х13.
Conclusion
GOST 9940 08Х13 is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — soft 13% Cr seamless pipe for mildly corrosive aqueous and steam-side spools where a hardenable 410 is unwanted. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 12Х13, 08Х17Т, 12Х17. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.