GOST 9940 08Х20Н14С2 Seamless Stainless Steel Pipe

GOST 9940 08Х20Н14С2 seamless stainless steel pipe (309Si / heat-resisting Si grade (approx)), austenitic heat-resisting Si-bearing, GOST 5632 cast analysis, Rm min 510 N/mm² / δ5 min 35%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
Grade
08Х20Н14С2 (GOST 5632 / 309Si / heat-resisting Si grade (approx) — body alias)
Standard
GOST 9940-81
Product form
Seamless stainless steel pipe (hot-deformed), delivery as ordered — heat-treated or without heat treatment
Size
OD × wall per Table 1; mark cap ≤108 mm per Table 1 note 1; random length typically 1.5–10 m
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GOST 9940 08Х20Н14С2 Seamless Stainless Steel Pipe

GOST 9940-81 is the Soviet / CIS product standard for seamless hot-deformed corrosion-resistant steel pipes — geometry, tensile floors, and acceptance in one document. Grade 08Х20Н14С2 sits in the austenitic heat-resisting Si-bearing set under Table 3. Mill brand ЭИ732. Silicon is intentional — this mark fights carburising gases, not seawater.

SHH STEEL can produce and supply GOST 9940 08Х20Н14С2 as hot-deformed seamless pipe across the enquiry OD×wall band (within the mark’s diameter cap), heat-treated or without HT as ordered, descaled or bright-finished, and documented on mill certificates tied to GOST 5632 cast analysis and Table 3 tensile results. Duty focus: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.

Shop language may still say “309Si pipe,” yet that commercial alias does not select GOST 5632 cast limits, hot-deformed tensile floors, or GOST 9940 marking. The purchase order has to name GOST 9940 and 08Х20Н14С2 so the mill applies the correct analysis, optional heat treatment, mechanical floors, and stencil. Design caution: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8.

Scope discipline: 08Х20Н14С2 is hot-deformed seamless pipe under GOST 9940, not cold-deformed GOST 9941 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 10Х23Н18, 15Х28, 08Х22Н6Т. Role reminder: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. Diameter note: ≤108 mm per Table 1 note 1.

Inside this GOST 9940 series, compare GOST 9940 10Х23Н18, GOST 9940 15Х28, GOST 9940 08Х22Н6Т. Hub: GOST 9940. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP309S.

Project teams specifying 08Х20Н14С2 should form hubs stay Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates — no verified plate product page is attached for this chemistry yet. Do not stretch a 08Х20Н14С2 pipe certificate onto plate.

Chemical Composition of GOST 9940 08Х20Н14С2

Cast analysis for GOST 9940 08Х20Н14С2 is not printed inside 9940 itself — clause 2.1 points to GOST 5632. Key windows on a typical certificate include C ≤0.08, Si 2.00–3.00, Mn ≤1.50, P ≤0.035, S ≤0.025, Ni 12.00–15.00, Cr 19.00–22.00. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 309Si / heat-resisting Si grade (approx). Mill brand ЭИ732. Corrosion thread: designed for carburisation / oxidation — not a chloride aqueous champion.

Chemical limits for 08Х20Н14С2 appear in the table underneath (GOST 5632-2014 extract). Source priority is the paid GOST 5632 table if your client cites a different edition footnote — send it before the heat is melted. Duty thread: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.

Grade C Si Mn P S Ni Cr
08Х20Н14С2 ≤0.08 2.00–3.00 ≤1.50 ≤0.035 ≤0.025 12.00–15.00 19.00–22.00

Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.

Mechanical Properties of GOST 9940 08Х20Н14С2

Ambient tensile floors for 08Х20Н14С2 come from GOST 9940-81 Table 3: Rm min 510 N/mm², elongation δ5 min 35% (yield not normalised in Table 3). Note: Yield not normalised; thick-wall Rm relief applies. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic heat-resisting Si-bearing. Caution: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8.

Yield strength is numerically normalised in GOST 9940 only for 12Х18Н10Т (≥216 N/mm²) when the purchaser orders it — for 08Х20Н14С2, treat Rp0.2 as an ordered extra unless that mark exception applies. Thick-wall pipes with D/s ≤8 on thirteen named marks may reduce Rm by 19.6 N/mm² per Table 3 note 1. Density 7.7 g/cm³. Role: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.

Grade Rm min (N/mm²) Rp0.2 min (N/mm²) δ5 min (%) Density (g/cm³) Max OD note
08Х20Н14С2 510 — (not normalised) 35 7.7 ≤108 mm per Table 1 note 1

Ambient values from GOST 9940-81 Table 3 for 08Х20Н14С2. Yield not normalised; thick-wall Rm relief applies. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution or process anneal per order; oxidation/carburisation duty common.

Seamless Pipe Manufacture of GOST 9940 08Х20Н14С2

Seamless is not optional wording for 08Х20Н14С2: GOST 9940 covers hot-deformed seamless corrosion-resistant pipe. Cold- and warm-deformed sisters live under GOST 9941-81 with different tensile floors. SHH STEEL will not quietly substitute a welded or cold-drawn route under a 9940 PO. Seamless hot-deformed manufacture remains the only valid order path for 08Х20Н14С2 under GOST 9940; the acknowledgement repeats that route so production cannot silently change after the PO is firm. Keep the 08Х20Н14С2 caution visible here: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8.

Austenitic heats usually take solution annealing with rapid cool when HT is ordered; skip inventing a mandatory anneal when the PO says without heat treatment. Heat-treatment note for 08Х20Н14С2: Solution or process anneal per order; oxidation/carburisation duty common. Scale removal follows when ordered; clause defaults do not automatically pickle every pipe. Duty thread: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.

When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 08Х20Н14С2: OD capped at 108 mm. Diameter cap: ≤108 mm per Table 1 note 1.

Dimensions and Tolerances for GOST 9940 08Х20Н14С2

SHH STEEL aligns nominal OD, wall, length type, and precision class (ordinary / high) for 08Х20Н14С2 before the mill slot is locked. Table 1 lists OD from 57 to 325 mm and wall from 3.5 to 32 mm, with measured length limits per size cell. Size hint: OD capped at 108 mm. Mark cap: ≤108 mm per Table 1 note 1.

OD tolerance is ±1.5% (ordinary) or ±1.0% (high). Wall minus tolerance reaches 15% on many gauges — design min wall with that minus in view. Curvature limits: 1.5 / 2 / 4 mm per metre by wall band. Duty thread: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. Fixed lengths and multiple cut lengths for 08Х20Н14С2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 08Х20Н14С2 duty: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.

Equivalent Grades for GOST 9940 08Х20Н14С2

The table below maps GOST 9940 08Х20Н14С2 to commercial aliases and related systems without inventing false one-to-one substitutes. Alias 309Si / heat-resisting Si grade (approx) stays body-only. Pack caution: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (08Х20Н14С2).

System Designation Notes
GOST 9940 08Х20Н14С2 Governing pipe grade for this page
Commercial / UNS (body only) 309Si / heat-resisting Si grade (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

When the service outgrows 08Х20Н14С2, move to a sister rather than stretching the alias: GOST 9940 10Х23Н18, GOST 9940 15Х28, GOST 9940 08Х22Н6Т. Apps context: carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Full list under GOST 9940. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (08Х20Н14С2).

Heat Treatment and Delivery Condition for GOST 9940 08Х20Н14С2

08Х20Н14С2 is delivered as ordered — heat-treated or without heat treatment under GOST 9940. Guidance: Solution or process anneal per order; oxidation/carburisation duty common. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: heat-resisting austenitic fillers; control hot cracking on Si-rich weld metal.

Cooling type matters — austenitics need rapid cool after solution treatment when HT is ordered; ferritic/martensitic anneal practice follows air or slow-cool notes. Duty thread: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. Density 7.7 g/cm³ for weight calcs. Field heat treatment of 08Х20Н14С2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 08Х20Н14С2 caution visible here: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8.

Corrosion Resistance of GOST 9940 08Х20Н14С2

Corrosion behaviour of GOST 9940 08Х20Н14С2 tracks its austenitic heat-resisting Si-bearing balance: designed for carburisation / oxidation — not a chloride aqueous champion. Intergranular corrosion testing is a purchaser option under GOST 9940, not an automatic coupon on every lot. Design caution: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 08Х20Н14С2 is filed as austenitic heat-resisting Si-bearing. Caution: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8.

Applications of GOST 9940 08Х20Н14С2 Seamless Pipe

Applications of GOST 9940 08Х20Н14С2 seamless pipe centre on carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Role summary: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same Cyrillic grade symbol on cut lists so informal latinised substitutions do not creep in. Primary application sketch: carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Duty thread: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. Commissioning teams benefit when the as-built dossier repeats 08Х20Н14С2 beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 08Х20Н14С2 stays carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732.

Weldability of GOST 9940 08Х20Н14С2

08Х20Н14С2 ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: heat-resisting austenitic fillers; control hot cracking on Si-rich weld metal. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 08Х20Н14С2 should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Corrosion framing beside 08Х20Н14С2: designed for carburisation / oxidation — not a chloride aqueous champion.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic heat-resisting Si-bearing — not a single shop habit. Caution: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8. Consumable lot control and shielding-gas notes for 08Х20Н14С2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 08Х20Н14С2 duty: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.

Surface Finishes for GOST 9940 08Х20Н14С2

Finish options for 08Х20Н14С2 follow the ordered heat-treatment route under GOST 9940. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: as ordered — heat-treated or without heat treatment. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (08Х20Н14С2).

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Reject grinding burns, embedded free iron, and unrepaired undercut on 08Х20Н14С2 before bundles close. Passivation analogues (A967-style) are optional extras — the governing step remains correct heat treatment under GOST 9940 for this austenitic heat-resisting Si-bearing mark. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (08Х20Н14С2).

Inspection and Testing for GOST 9940 08Х20Н14С2

Inspection for GOST 9940 08Х20Н14С2 covers dimensions and appearance on every pipe; tensile on two pipes per party; flattening or expanding on one when ordered; IGC on two when ordered. Hydrostatic and ultrasonic tests run when the purchaser asks. Documents follow GOST 10692 with chemistry taken from the billet certificate.

Marking includes 08Х20Н14С2, manufacturer, size, and GOST 9940. Traceability from stencil to MTC is part of supply, not an upgrade. Use: carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Non-conforming 08Х20Н14С2 lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Size practice for 08Х20Н14С2 remains OD capped at 108 mm.

Packaging and Shipping for GOST 9940 08Х20Н14С2

Packaging for 08Х20Н14С2 uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect descaled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 08Х20Н14С2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 08Х20Н14С2 stays carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8. Desiccant and wrap choices for 08Х20Н14С2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside 08Х20Н14С2: designed for carburisation / oxidation — not a chloride aqueous champion.

Shipping documents list GOST 9940, 08Х20Н14С2, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. Claims handling for 08Х20Н14С2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 08Х20Н14С2: heat-resisting austenitic fillers; control hot cracking on Si-rich weld metal.

Why Choose SHH STEEL

SHH STEEL can produce and supply GOST 9940 08Х20Н14С2 with the hot-deformed seamless route, heat-treatment choice, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless hot capacity covering this mark’s OD band. Duty focus: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres.

Technical sales can map 08Х20Н14С2 against sisters 10Х23Н18, 15Х28, 08Х22Н6Т and live ASTM A312 pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 08Х20Н14С2, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х20Н14С2 to that written scope.

Supply Capability

SHH STEEL can produce and supply GOST 9940 08Х20Н14С2 across enquiry-oriented OD × wall bands (within ≤108 mm per Table 1 note 1), in the hot-deformed seamless route, with certificates and optional tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue.

Item Capability
Standard GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes
Grade 08Х20Н14С2 (GOST 5632 chemistry; alias 309Si / heat-resisting Si grade (approx))
Product form Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941)
Delivery condition as ordered — heat-treated or without heat treatment
Documents Quality document per GOST 10692 / EN 10204 3.1 style as ordered
Typical size practice OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: ≤108 mm per Table 1 note 1
Precision Ordinary or high (index “в” when high)
Tests Tensile per party; hydro / UT / flatten / IGC / yield when ordered

Stock / Available sizes

SHH STEEL can produce and supply GOST 9940 08Х20Н14С2. Stock / Available sizes: enquiry band typically aligns with GOST 9940 Table 1 OD×wall practice, with ordinary or high precision as ordered. For 08Х20Н14С2, practical fast-track sizes often sit inside the mark’s diameter cap — send the OD × wall list for a firm acknowledgement. Context: OD capped at 108 mm. Cap: ≤108 mm per Table 1 note 1.

Cut lengths, bevels, special NDT, IGC, and HT extras add lead time — call them early. Sisters often quoted alongside: 10Х23Н18, 15Х28, 08Х22Н6Т. Email the size list to start. SHH STEEL can produce trial lengths of 08Х20Н14С2 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GOST 9940 08Х20Н14С2 seamless stainless steel pipe used for?
GOST 9940 08Х20Н14С2 is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — carburising furnace tubes, radiant coils, and CIS heat-treat shop pipe that names ЭИ732. Role summary: Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
Is GOST 9940 08Х20Н14С2 seamless only, or does it cover welded pipe?
Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 08Х20Н14С2 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
Is heat treatment mandatory for 08Х20Н14С2 under GOST 9940?
No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution or process anneal per order; oxidation/carburisation duty common. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
How does 08Х20Н14С2 compare with sister grades 10Х23Н18, 15Х28, 08Х22Н6Т?
08Х20Н14С2 is filed as austenitic heat-resisting Si-bearing. Typical sisters on the same RFQ are 10Х23Н18, 15Х28, 08Х22Н6Т. Design caution: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8 Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 08Х20Н14С2?
Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
Is 309Si / heat-resisting Si grade (approx) the same as ordering 08Х20Н14С2?
No. 309Si / heat-resisting Si grade (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 08Х20Н14С2 so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GOST 9940 08Х20Н14С2?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х20Н14С2 within Table 1 practice, respecting the mark’s diameter cap (≤108 mm per Table 1 note 1). Size context: OD capped at 108 mm. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
How should 08Х20Н14С2 be welded on site?
Shop guidance: heat-resisting austenitic fillers; control hot cracking on Si-rich weld metal. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8
When should I choose a Mo-bearing or duplex grade instead of 08Х20Н14С2?
Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic heat-resisting Si-bearing practice can defend for the temperature and stress state. Caution for this mark: OD ≤108 mm; Si 2–3% changes weld pool fluidity versus plain 18-8 Sister pointers: 10Х23Н18, 15Х28, 08Х22Н6Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GOST 9940 08Х20Н14С2 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 08Х20Н14С2 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
How does GOST 9940 08Х20Н14С2 differ from GOST 9941 of the same mark?
GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х20Н14С2.

Conclusion

GOST 9940 08Х20Н14С2 is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — Si-bearing heat-resisting austenitic seamless pipe for carburising furnace atmospheres. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 10Х23Н18, 15Х28, 08Х22Н6Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X