GOST 9940 08Х18Н10Т Seamless Stainless Steel Pipe
What is GOST 9940 08Х18Н10Т Seamless Stainless Steel Pipe
GOST 9940-81 is the Soviet / CIS product standard for seamless hot-deformed corrosion-resistant steel pipes — geometry, tensile floors, and acceptance in one document. Grade 08Х18Н10Т sits in the austenitic Ti-stabilised 18-8 set under Table 3. Mill brand ЭИ914. Titanium-stabilised 18-8 under GOST 9940 — the CIS cousin of 321 pipe.
SHH STEEL can produce and supply GOST 9940 08Х18Н10Т as hot-deformed seamless pipe across the enquiry OD×wall band (within the mark’s diameter cap), heat-treated or without HT as ordered, descaled or bright-finished, and documented on mill certificates tied to GOST 5632 cast analysis and Table 3 tensile results. Duty focus: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines.
Shop language may still say “321 pipe,” yet that commercial alias does not select GOST 5632 cast limits, hot-deformed tensile floors, or GOST 9940 marking. The purchase order has to name GOST 9940 and 08Х18Н10Т so the mill applies the correct analysis, optional heat treatment, mechanical floors, and stencil. Design caution: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker.
Scope discipline: 08Х18Н10Т is hot-deformed seamless pipe under GOST 9940, not cold-deformed GOST 9941 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 12Х18Н10Т, 08Х18Н12Т, 08Х18Н12Б. Role reminder: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines. Diameter note: full Table 1 range.
Inside this GOST 9940 series, compare GOST 9940 12Х18Н10Т, GOST 9940 08Х18Н12Т, GOST 9940 08Х18Н12Б. Hub: GOST 9940. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP321.
Beside this 08Х18Н10Т page, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is ASTM A240 Type 321. Quote 08Х18Н10Т pipe and plate under separate line items.
Chemical Composition of GOST 9940 08Х18Н10Т
Cast analysis for GOST 9940 08Х18Н10Т is not printed inside 9940 itself — clause 2.1 points to GOST 5632. Key windows on a typical certificate include C ≤0.08, Si ≤0.80, Mn ≤2.00, P ≤0.040, S ≤0.020, Ni 9.00–11.00, Cr 17.00–19.00, Ti 5×C–0.70. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 321 / UNS S32100 (approx). Mill brand ЭИ914. Corrosion thread: as-welded IGC resistance is the point versus plain 08Х18Н10; chlorides still prefer Mo grades.
Chemical limits for 08Х18Н10Т appear in the table underneath (GOST 5632-2014 extract). Source priority is the paid GOST 5632 table if your client cites a different edition footnote — send it before the heat is melted. Duty thread: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines.
| Grade | C | Si | Mn | P | S | Ni | Cr | Ti |
|---|---|---|---|---|---|---|---|---|
| 08Х18Н10Т | ≤0.08 | ≤0.80 | ≤2.00 | ≤0.040 | ≤0.020 | 9.00–11.00 | 17.00–19.00 | 5×C–0.70 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9940 08Х18Н10Т
Ambient tensile floors for 08Х18Н10Т come from GOST 9940-81 Table 3: Rm min 510 N/mm², elongation δ5 min 40% (yield not normalised in Table 3). Note: Yield not normalised; thick-wall Rm relief applies. These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic Ti-stabilised 18-8. Caution: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker.
Yield strength is numerically normalised in GOST 9940 only for 12Х18Н10Т (≥216 N/mm²) when the purchaser orders it — for 08Х18Н10Т, treat Rp0.2 as an ordered extra unless that mark exception applies. Thick-wall pipes with D/s ≤8 on thirteen named marks may reduce Rm by 19.6 N/mm² per Table 3 note 1. Density 7.9 g/cm³. Role: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 08Х18Н10Т | 510 | — (not normalised) | 40 | 7.9 | full Table 1 range |
Ambient values from GOST 9940-81 Table 3 for 08Х18Н10Т. Yield not normalised; thick-wall Rm relief applies. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution anneal; Ti for IGC resistance after welding.
Seamless Pipe Manufacture of GOST 9940 08Х18Н10Т
For 08Х18Н10Т, the mill path is hot pierce / elongate / size — never ERW under GOST 9940. Heat treatment is ordered or omitted per clause 2.1; silence means the mill may ship without HT unless the purchase order freezes a schedule. Order ordinary or high precision class with the size. Seamless hot-deformed manufacture remains the only valid order path for 08Х18Н10Т under GOST 9940; the acknowledgement repeats that route so production cannot silently change after the PO is firm. Weld-shop note tied to 08Х18Н10Т: 347/321-class or matching Ti-bearing fillers; avoid losing Ti in the weld pool.
Austenitic heats usually take solution annealing with rapid cool when HT is ordered; skip inventing a mandatory anneal when the PO says without heat treatment. Heat-treatment note for 08Х18Н10Т: Solution anneal; Ti for IGC resistance after welding. Scale removal follows when ordered; clause defaults do not automatically pickle every pipe. Duty thread: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines.
When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 08Х18Н10Т: full OD to 325 mm — one of the most quoted 9940 marks. Diameter cap: full Table 1 range.
Dimensions and Tolerances for GOST 9940 08Х18Н10Т
SHH STEEL aligns nominal OD, wall, length type, and precision class (ordinary / high) for 08Х18Н10Т before the mill slot is locked. Table 1 lists OD from 57 to 325 mm and wall from 3.5 to 32 mm, with measured length limits per size cell. Size hint: full OD to 325 mm — one of the most quoted 9940 marks. Mark cap: full Table 1 range.
OD tolerance is ±1.5% (ordinary) or ±1.0% (high). Wall minus tolerance reaches 15% on many gauges — design min wall with that minus in view. Curvature limits: 1.5 / 2 / 4 mm per metre by wall band. Duty thread: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines.
Equivalent Grades for GOST 9940 08Х18Н10Т
08Х18Н10Т is the GOST 9940 designation for this seamless stainless steel pipe (hot-deformed). Alias 321 / UNS S32100 (approx) appears only as a cross-walk. When a dual-cert path is required, list both GOST 9940 08Х18Н10Т and the foreign mark with separate scopes instead of assuming one chemistry line clears both files.
| System | Designation | Notes |
|---|---|---|
| GOST 9940 | 08Х18Н10Т | Governing pipe grade for this page |
| Commercial / UNS (body only) | 321 / UNS S32100 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 321 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | EN 1.4541 | Starting point for comparison only; no automatic dual-cert |
Read the notes column literally for 08Х18Н10Т: related chemistry is not automatic dual-cert. Cross-check GOST 9940 12Х18Н10Т, GOST 9940 08Х18Н12Т, GOST 9940 08Х18Н12Б when Mo, stabilisation, or carbon ceilings change the selection. Hub: GOST 9940. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (08Х18Н10Т). Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (08Х18Н10Т).
Heat Treatment and Delivery Condition for GOST 9940 08Х18Н10Т
08Х18Н10Т is delivered as ordered — heat-treated or without heat treatment under GOST 9940. Guidance: Solution anneal; Ti for IGC resistance after welding. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 347/321-class or matching Ti-bearing fillers; avoid losing Ti in the weld pool.
Cooling type matters — austenitics need rapid cool after solution treatment when HT is ordered; ferritic/martensitic anneal practice follows air or slow-cool notes. Duty thread: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines. Density 7.9 g/cm³ for weight calcs. Field heat treatment of 08Х18Н10Т after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for 08Х18Н10Т stays chemical plant welded headers, heat-exchanger connecting pipe, and GOST packages that print 08Х18Н10Т instead of 321.
Corrosion Resistance of GOST 9940 08Х18Н10Т
Corrosion behaviour of GOST 9940 08Х18Н10Т tracks its austenitic Ti-stabilised 18-8 balance: as-welded IGC resistance is the point versus plain 08Х18Н10; chlorides still prefer Mo grades. Intergranular corrosion testing is a purchaser option under GOST 9940, not an automatic coupon on every lot. Design caution: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 08Х18Н10Т is filed as austenitic Ti-stabilised 18-8. Caution: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker.
Applications of GOST 9940 08Х18Н10Т Seamless Pipe
Applications of GOST 9940 08Х18Н10Т seamless pipe centre on chemical plant welded headers, heat-exchanger connecting pipe, and GOST packages that print 08Х18Н10Т instead of 321. Role summary: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same Cyrillic grade symbol on cut lists so informal latinised substitutions do not creep in. Primary application sketch: chemical plant welded headers, heat-exchanger connecting pipe, and GOST packages that print 08Х18Н10Т instead of 321. Duty thread: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines.
Weldability of GOST 9940 08Х18Н10Т
08Х18Н10Т ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: 347/321-class or matching Ti-bearing fillers; avoid losing Ti in the weld pool. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 08Х18Н10Т should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Size practice for 08Х18Н10Т remains full OD to 325 mm — one of the most quoted 9940 marks.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic Ti-stabilised 18-8 — not a single shop habit. Caution: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker. Consumable lot control and shielding-gas notes for 08Х18Н10Т stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 08Х18Н10Т: as-welded IGC resistance is the point versus plain 08Х18Н10; chlorides still prefer Mo grades.
Surface Finishes for GOST 9940 08Х18Н10Т
On 08Х18Н10Т, cosmetics never outrank correct heat treatment. Passivation and polish are sequenced after the anneal that qualifies the pipe. Duty locked here: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines. Name which surface carries each finish callout. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (08Х18Н10Т).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Bright or polished callouts for 08Х18Н10Т never waive heat-treatment proof. After finishing, keep iron-free handling through storage and shipment so GOST 9940 pipe does not leave the yard with free-iron blooms. Caution retained: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker.
Inspection and Testing for GOST 9940 08Х18Н10Т
Inspection for GOST 9940 08Х18Н10Т covers dimensions and appearance on every pipe; tensile on two pipes per party; flattening or expanding on one when ordered; IGC on two when ordered. Hydrostatic and ultrasonic tests run when the purchaser asks. Documents follow GOST 10692 with chemistry taken from the billet certificate.
Marking includes 08Х18Н10Т, manufacturer, size, and GOST 9940. Traceability from stencil to MTC is part of supply, not an upgrade. Use: chemical plant welded headers, heat-exchanger connecting pipe, and GOST packages that print 08Х18Н10Т instead of 321. Non-conforming 08Х18Н10Т lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Corrosion framing beside 08Х18Н10Т: as-welded IGC resistance is the point versus plain 08Х18Н10; chlorides still prefer Mo grades.
Packaging and Shipping for GOST 9940 08Х18Н10Т
Packaging for 08Х18Н10Т uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect descaled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 08Х18Н10Т repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 08Х18Н10Т: as-welded IGC resistance is the point versus plain 08Х18Н10; chlorides still prefer Mo grades.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker. Desiccant and wrap choices for 08Х18Н10Т follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 08Х18Н10Т: 347/321-class or matching Ti-bearing fillers; avoid losing Ti in the weld pool.
Shipping documents list GOST 9940, 08Х18Н10Т, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines. Claims handling for 08Х18Н10Т starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 08Х18Н10Т remains full OD to 325 mm — one of the most quoted 9940 marks.
Why Choose SHH STEEL
SHH STEEL can produce and supply GOST 9940 08Х18Н10Т with the hot-deformed seamless route, heat-treatment choice, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless hot capacity covering this mark’s OD band. Duty focus: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines.
Technical sales can map 08Х18Н10Т against sisters 12Х18Н10Т, 08Х18Н12Т, 08Х18Н12Б and live ASTM A312 pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 08Х18Н10Т, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х18Н10Т to that written scope.
Supply Capability
SHH STEEL can produce and supply GOST 9940 08Х18Н10Т across enquiry-oriented OD × wall bands (within full Table 1 range), in the hot-deformed seamless route, with certificates and optional tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue.
| Item | Capability |
|---|---|
| Standard | GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes |
| Grade | 08Х18Н10Т (GOST 5632 chemistry; alias 321 / UNS S32100 (approx)) |
| Product form | Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941) |
| Delivery condition | as ordered — heat-treated or without heat treatment |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: full Table 1 range |
| Precision | Ordinary or high (index “в” when high) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
SHH STEEL can produce and supply GOST 9940 08Х18Н10Т. Stock / Available sizes: enquiry band typically aligns with GOST 9940 Table 1 OD×wall practice, with ordinary or high precision as ordered. For 08Х18Н10Т, practical fast-track sizes often sit inside the mark’s diameter cap — send the OD × wall list for a firm acknowledgement. Context: full OD to 325 mm — one of the most quoted 9940 marks. Cap: full Table 1 range.
Cut lengths, bevels, special NDT, IGC, and HT extras add lead time — call them early. Sisters often quoted alongside: 12Х18Н10Т, 08Х18Н12Т, 08Х18Н12Б. Email the size list to start. SHH STEEL can produce trial lengths of 08Х18Н10Т for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9940 08Х18Н10Т seamless stainless steel pipe used for?
- GOST 9940 08Х18Н10Т is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — chemical plant welded headers, heat-exchanger connecting pipe, and GOST packages that print 08Х18Н10Т instead of 321. Role summary: Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9940 08Х18Н10Т seamless only, or does it cover welded pipe?
- Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 08Х18Н10Т when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 08Х18Н10Т under GOST 9940?
- No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution anneal; Ti for IGC resistance after welding. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
-
How does 08Х18Н10Т compare with sister grades 12Х18Н10Т, 08Х18Н12Т, 08Х18Н12Б?
- 08Х18Н10Т is filed as austenitic Ti-stabilised 18-8. Typical sisters on the same RFQ are 12Х18Н10Т, 08Х18Н12Т, 08Х18Н12Б. Design caution: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 08Х18Н10Т?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
-
Is 321 / UNS S32100 (approx) the same as ordering 08Х18Н10Т?
- No. 321 / UNS S32100 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 08Х18Н10Т so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9940 08Х18Н10Т?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х18Н10Т within Table 1 practice, respecting the mark’s diameter cap (full Table 1 range). Size context: full OD to 325 mm — one of the most quoted 9940 marks. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
-
How should 08Х18Н10Т be welded on site?
- Shop guidance: 347/321-class or matching Ti-bearing fillers; avoid losing Ti in the weld pool. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker
-
When should I choose a Mo-bearing or duplex grade instead of 08Х18Н10Т?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic Ti-stabilised 18-8 practice can defend for the temperature and stress state. Caution for this mark: Ti must meet 5×C floor — under-stabilised heats fail IGC even with a 321 sticker Sister pointers: 12Х18Н10Т, 08Х18Н12Т, 08Х18Н12Б. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9940 08Х18Н10Т with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 08Х18Н10Т does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9940 08Х18Н10Т differ from GOST 9941 of the same mark?
- GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х18Н10Т.
Conclusion
GOST 9940 08Х18Н10Т is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — Ti-stabilised 18-8 austenitic seamless pipe for welded corrosive and moderate-temperature CIS lines. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 12Х18Н10Т, 08Х18Н12Т, 08Х18Н12Б. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.