GOST 9940 15Х28 Seamless Stainless Steel Pipe
What is GOST 9940 15Х28 Seamless Stainless Steel Pipe
GOST 9940 covers seamless hot-deformed stainless pipe with OD 57–325 mm and wall 3.5–32 mm in two precision classes. Inside that standard, 15Х28 is filed as ferritic high-chromium. Mill brand ЭИ349. Highest chromium ferritic in the 9940 Table 3 set — oxidation first, aqueous second. Buyers working CIS fluid packages should treat 15Х28 as a governed product grade under GOST 9940-81, with GOST 5632 chemistry and Table 3 tensile floors enforced on the same heat. This paragraph is locked to 15Х28 duty: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces.
From pierce through marking and crate protection, SHH STEEL can produce GOST 9940 15Х28 for the sizes and tests on your RFQ. Application sketch: pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists. Size and test clarity on the RFQ lets SHH STEEL lock the correct hot-deformed seamless scope for 15Х28 before production starts. This paragraph is locked to 15Х28 duty: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces.
On the floor people latinise marks; in QA they must not. 15Х28 under GOST 9940 carries specific Table 3 floors that a loose “446” note will not enforce. Caution: high chromium, low toughness if overheated; sulphur control matters for glass sealing heats. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 15Х28 so informal alias language cannot reopen the carbon or molybdenum window after melt. Corrosion framing beside 15Х28: outstanding dry oxidation resistance; aqueous chlorides are not the design case.
Pair standard GOST 9941 uses many of the same marks with colder deformation and different Rm/δ5 pairs — do not mix certificates. Sisters: 15Х25Т, 12Х17, 08Х20Н14С2. Use thread: pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists. Document the medium, design temperature, and weld map beside the 15Х28 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for 15Х28 remains OD ≤219 mm.
Inside this GOST 9940 series, compare GOST 9940 15Х25Т, GOST 9940 12Х17, GOST 9940 08Х20Н14С2. Hub: GOST 9940.
Buyers comparing 15Х28 tubulars with sheet/plate can Stainless Steel Pipes and Tubes covers the tubular parent, Stainless Steel Sheets and Plates covers flats, and ASTM A240 UNS S44600 is the live plate chemistry match — do not merge MTCs. Keep 15Х28 acceptance text on the governing pipe/tube standard.
Chemical Composition of GOST 9940 15Х28
For 15Х28, the melt ticket has to show GOST 5632 compliance — C ≤0.15, Si ≤1.00, Mn ≤0.80, P ≤0.035, S ≤0.025, Cr 27.00–30.00. Optional residual limits still forbid blurring grade identity. Corrosion framing: outstanding dry oxidation resistance; aqueous chlorides are not the design case.
Where Mo, Ti or Nb appear, they are intentional levers for 15Х28, not optional marketing. Confirm them on the MTC line-by-line. Role: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 15Х28 before the order is acknowledged. Application context for 15Х28 stays pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists.
| Grade | C | Si | Mn | P | S | Cr |
|---|---|---|---|---|---|---|
| 15Х28 | ≤0.15 | ≤1.00 | ≤0.80 | ≤0.035 | ≤0.025 | 27.00–30.00 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9940 15Х28
Do not confuse Table 3 hot-deformed floors with GOST 9941 cold-deformed numbers that share the 446 / UNS S44600 (approx) alias. For 15Х28 under 9940 expect Rm min 441 N/mm², elongation δ5 min 17% (yield not normalised in Table 3), verified per heat/lot rules. Note: Yield not normalised.
When comparing 15Х28 to a cold-deformed GOST 9941 sister, expect different Rm/δ5 pairs even at identical GOST 5632 chemistry. Duty: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. Do not substitute GOST 9941 cold-deformed tensile numbers onto a hot-deformed 15Х28 certificate without a written dual-product plan. Keep the 15Х28 caution visible here: high chromium, low toughness if overheated; sulphur control matters for glass sealing heats.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 15Х28 | 441 | — (not normalised) | 17 | 7.6 | ≤219 mm per Table 1 note 1 |
Ambient values from GOST 9940-81 Table 3 for 15Х28. Yield not normalised. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: High-Cr ferritic anneal; glass-to-metal sealing grades need sulphur control.
Seamless Pipe Manufacture of GOST 9940 15Х28
GOST 9940-81 manufactures 15Х28 as seamless hot-deformed stainless pipe only — pierce, roll, or extrude at hot-working temperature, then finish to Table 1 sizes. SHH STEEL confirms the hot-deformed seamless route on the acknowledgement before the billet is pierced; welded pipe and cold-deformed GOST 9941 product are outside this line item.
Precision class (ordinary or high) is an order item for 15Х28; unmarked class means ordinary. Heat treatment: High-Cr ferritic anneal; glass-to-metal sealing grades need sulphur control. Ferritic heats follow softening / anneal practice when HT is ordered — not austenitic solution charts. Grain growth after overheating remains a shop risk.
Hydraulic testing per GOST 3845 and ultrasonic inspection run only when ordered — technology is deemed to ensure pressure capacity, but the certificate lists only tests performed. Manufacture stays seamless hot-deformed. Size: OD ≤219 mm. Hydrostatic pressure or UT class for 15Х28 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Weld-shop note tied to 15Х28: high-Cr ferritic procedure; avoid prolonged 500–800 °C holds that embrittle.
Dimensions and Tolerances for GOST 9940 15Х28
Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 15Х28. Duty: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. Cap: ≤219 mm per Table 1 note 1. Precision class follows the tolerance ordered for 15Х28, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 15Х28 caution visible here: high chromium, low toughness if overheated; sulphur control matters for glass sealing heats.
High precision mainly tightens the plus wall tolerance; the minus side stays punishing — quote class with the size for 15Х28. Fixed lengths and multiple cut lengths for 15Х28 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for 15Х28 remains OD ≤219 mm.
Equivalent Grades for GOST 9940 15Х28
GOST 9940 does not make 446 / UNS S44600 (approx) a drop-in certificate for 15Х28. Use the commercial name in dual-cert talk, then verify every Table limit that matters for this pipe. Sisters in the series are comparison pages, not interchangeable stock codes. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (15Х28).
| System | Designation | Notes |
|---|---|---|
| GOST 9940 | 15Х28 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 446 / UNS S44600 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
We deliberately avoid inventing a false one-to-one for every foreign system on 15Х28. Use GOST 9940 15Х25Т, GOST 9940 12Х17, GOST 9940 08Х20Н14С2 for in-series alternatives, and keep GOST 9940 as the category landing page. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (15Х28).
Heat Treatment and Delivery Condition for GOST 9940 15Х28
Unlike GOST 9941, GOST 9940 does not force heat treatment on every pipe. Confirm for 15Х28. Band note: High-Cr ferritic anneal; glass-to-metal sealing grades need sulphur control. Recorded furnace charts for 15Х28 should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to 15Х28: high-Cr ferritic procedure; avoid prolonged 500–800 °C holds that embrittle.
Party acceptance groups pipes by size, mark, and heat-treatment kind — mixing HT and non-HT lengths in one lot breaks the batch rule for 15Х28. Field heat treatment of 15Х28 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for 15Х28 stays pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists.
Corrosion Resistance of GOST 9940 15Х28
Medium, temperature, crevice geometry and weld condition decide whether 15Х28 is enough. Summary: outstanding dry oxidation resistance; aqueous chlorides are not the design case. Escalate via sisters 15Х25Т, 12Х17, 08Х20Н14С2 when coupons fail. Coupon orientation, weld condition, and surface finish for 15Х28 belong in the corrosion test order so results can be compared to the installed spool honestly. This paragraph is locked to 15Х28 duty: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces.
Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 15Х28. Corrosion framing: outstanding dry oxidation resistance; aqueous chlorides are not the design case. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 15Х28 rather than relying on wall thickness alone. Corrosion framing beside 15Х28: outstanding dry oxidation resistance; aqueous chlorides are not the design case.
Applications of GOST 9940 15Х28 Seamless Pipe
From utility rooms to process racks, 15Х28 shows up wherever CIS fluid specs want ferritic high-chromium hot-deformed seamless behaviour. Use list: pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists. Spool fabricators should copy 15Х28 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside 15Х28: outstanding dry oxidation resistance; aqueous chlorides are not the design case.
If the only reason for 15Х28 is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: high chromium, low toughness if overheated; sulphur control matters for glass sealing heats. Commissioning teams benefit when the as-built dossier repeats 15Х28 beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside 15Х28: outstanding dry oxidation resistance; aqueous chlorides are not the design case.
Weldability of GOST 9940 15Х28
Automatic mill welding is outside GOST 9940; manual and automatic field welds must still respect 15Х28 chemistry. Guidance: high-Cr ferritic procedure; avoid prolonged 500–800 °C holds that embrittle. Procedure qualification for 15Х28 should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. This paragraph is locked to 15Х28 duty: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces.
Ferrite control on high-Ni austenitics and hydrogen management on martensitic 15Х28 are procedure items, not afterthoughts. Guidance: high-Cr ferritic procedure; avoid prolonged 500–800 °C holds that embrittle. Consumable lot control and shielding-gas notes for 15Х28 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Application context for 15Х28 stays pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists.
Surface Finishes for GOST 9940 15Х28
15Х28 under GOST 9940 typically ships annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (15Х28).
| Finish | Typical supply | Order note |
|---|---|---|
| Annealed and pickled | Standard pipe mill finish after anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; inspect before polish on ferritic stock |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
When 15Х28 ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Apps reminder: pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists.
Inspection and Testing for GOST 9940 15Х28
Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GOST 9940 for 15Х28. Sampling plans for 15Х28 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside 15Х28: outstanding dry oxidation resistance; aqueous chlorides are not the design case.
Dimensional inspection against Table 2 tolerances closes the lot. Role: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. Non-conforming 15Х28 lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. This paragraph is locked to 15Х28 duty: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces.
Packaging and Shipping for GOST 9940 15Х28
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 15Х28 stays visible on outer tags. Bundle tickets for 15Х28 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 15Х28 stays pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists.
Container loading plans should keep heavy walls from crushing thin-wall 15Х28 layers. Desiccant and wrap choices for 15Х28 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. This paragraph is locked to 15Х28 duty: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 15Х28. Claims handling for 15Х28 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 15Х28 remains OD ≤219 mm.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats 15Х28 as a governed product grade, not a marketing synonym for 446 / UNS S44600 (approx). Role: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. SHH STEEL can produce and supply 15Х28 against the OD × wall, hot-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Response time stays short because common 15Х28 enquiry sizes and document packs are already exercised on prior GOST-spec orders. Use: pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists. Ask for a written acknowledgement that names 15Х28, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 15Х28 to that written scope.
Supply Capability
Capability framing for 15Х28: GOST-spec seamless hot-deformed pipe, documented heats. Caution remains: high chromium, low toughness if overheated; sulphur control matters for glass sealing heats. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 15Х28 when the mill schedule allows. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 15Х28 when the mill schedule allows. Corrosion framing beside 15Х28: outstanding dry oxidation resistance; aqueous chlorides are not the design case.
| Item | Capability |
|---|---|
| Standard | GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes |
| Grade | 15Х28 (GOST 5632 chemistry; alias 446 / UNS S44600 (approx)) |
| Product form | Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941) |
| Delivery condition | as ordered — heat-treated or without heat treatment |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: ≤219 mm per Table 1 note 1 |
| Precision | Ordinary or high (index “в” when high) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 15Х28 change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. SHH STEEL can supply alternate walls and precision classes for 15Х28 once the design pressure and corrosion allowance are clear.
Repeat orders for 15Х28 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. SHH STEEL can produce trial lengths of 15Х28 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9940 15Х28 seamless stainless steel pipe used for?
- GOST 9940 15Х28 is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — pyrolysis secondary pipe, furnace muffles, and glass-to-metal sealing hardware on CIS equipment lists. Role summary: ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9940 15Х28 seamless only, or does it cover welded pipe?
- Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 15Х28 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 15Х28 under GOST 9940?
- No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: High-Cr ferritic anneal; glass-to-metal sealing grades need sulphur control. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
-
How does 15Х28 compare with sister grades 15Х25Т, 12Х17, 08Х20Н14С2?
- 15Х28 is filed as ferritic high-chromium. Typical sisters on the same RFQ are 15Х25Т, 12Х17, 08Х20Н14С2. Design caution: high chromium, low toughness if overheated; sulphur control matters for glass sealing heats Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 15Х28?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
-
Is 446 / UNS S44600 (approx) the same as ordering 15Х28?
- No. 446 / UNS S44600 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 15Х28 so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9940 15Х28?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 15Х28 within Table 1 practice, respecting the mark’s diameter cap (≤219 mm per Table 1 note 1). Size context: OD ≤219 mm. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
-
How should 15Х28 be welded on site?
- Shop guidance: high-Cr ferritic procedure; avoid prolonged 500–800 °C holds that embrittle. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: high chromium, low toughness if overheated; sulphur control matters for glass sealing heats
-
When should I choose a Mo-bearing or duplex grade instead of 15Х28?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what ferritic high-chromium practice can defend for the temperature and stress state. Caution for this mark: high chromium, low toughness if overheated; sulphur control matters for glass sealing heats Sister pointers: 15Х25Т, 12Х17, 08Х20Н14С2. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9940 15Х28 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 15Х28 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9940 15Х28 differ from GOST 9941 of the same mark?
- GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 15Х28.
Conclusion
GOST 9940 15Х28 is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — ~28% Cr ferritic seamless pipe for high-temperature oxidation and glass-seal interfaces. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 15Х25Т, 12Х17, 08Х20Н14С2. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.