GOST 9940 08Х22Н6Т Seamless Stainless Steel Pipe

GOST 9940 08Х22Н6Т seamless stainless steel pipe (lean duplex / 22Cr-6Ni Ti (approx)), austenitic-ferritic (duplex-lean) Ti-stabilised, GOST 5632 cast analysis, Rm min 588 N/mm² / δ5 min 24%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
Grade
08Х22Н6Т (GOST 5632 / lean duplex / 22Cr-6Ni Ti (approx) — body alias)
Standard
GOST 9940-81
Product form
Seamless stainless steel pipe (hot-deformed), delivery as ordered — heat-treated or without heat treatment
Size
OD × wall per Table 1; mark cap ≤108 mm per Table 1 note 1; random length typically 1.5–10 m
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GOST 9940 08Х22Н6Т Seamless Stainless Steel Pipe

When the approved vendor list and isometric say GOST 9940, the grade mark has to be the GOST 5632 designation. 08Х22Н6Т is the full product grade for this austenitic-ferritic (duplex-lean) Ti-stabilised seamless pipe. Mill brand ЭП53. The duplex-lean Russian mark that tops Table 3 tensile strength under GOST 9940.

SHH STEEL can supply 08Х22Н6Т seamless pipe in the hot-deformed route, with plain or bevelled ends, random or cut lengths, and GOST 10692 / EN 10204 3.1 style inspection documents when specified. Role on the line: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3.

Equivalence talk to lean duplex / 22Cr-6Ni Ti (approx) belongs in engineering notes, not as a substitute for the GOST mark. Lock GOST 9940 08Х22Н6Т, OD × wall, precision class, and HT yes/no before melt. Watch-out: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 08Х22Н6Т so informal alias language cannot reopen the carbon or molybdenum window after melt. Application context for 08Х22Н6Т stays chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8.

Related ASTM A312 pipe pages share chemistry families but not GOST acceptance text — confirm before dual-cert claims. Sisters on this hub: 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2. Use thread: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Document the medium, design temperature, and weld map beside the 08Х22Н6Т line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside 08Х22Н6Т: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr.

Inside this GOST 9940 series, compare GOST 9940 08Х18Н10Т, GOST 9940 10Х17Н13М2Т, GOST 9940 08Х20Н14С2. Hub: GOST 9940.

Chemical Composition of GOST 9940 08Х22Н6Т

Chemistry control on 08Х22Н6Т starts at the ladle under GOST 5632. Expect C ≤0.08, Si ≤0.80, Mn ≤0.80, P ≤0.035, S ≤0.025, Ni 5.30–6.30, Cr 21.00–23.00, Ti 5×C–0.65 within the mark’s windows, reported on the inspection document against the heat. Body alias lean duplex / 22Cr-6Ni Ti (approx) does not widen those windows.

Read the table with the family in mind — austenitic-ferritic (duplex-lean) Ti-stabilised — and with caution OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ. Numbers without the matching Table 3 tensile row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 08Х22Н6Т before the order is acknowledged. Corrosion framing beside 08Х22Н6Т: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr.

Grade C Si Mn P S Ni Cr Ti
08Х22Н6Т ≤0.08 ≤0.80 ≤0.80 ≤0.035 ≤0.025 5.30–6.30 21.00–23.00 5×C–0.65

Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.

Mechanical Properties of GOST 9940 08Х22Н6Т

Tensile minima for 08Х22Н6Т sit at Rm min 588 N/mm², elongation δ5 min 24% (yield not normalised in Table 3). Note: Highest Rm in Table 3; yield not normalised; thick-wall Rm relief applies. Flattening or drift expanding backs ductility when ordered. Watch-out: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ.

Elongation δ5 floors and Rm floors travel together on the MTC for 08Х22Н6Т. Do not accept a certificate that quotes only hardness. Caution: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ. Do not substitute GOST 9941 cold-deformed tensile numbers onto a hot-deformed 08Х22Н6Т certificate without a written dual-product plan. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3.

Grade Rm min (N/mm²) Rp0.2 min (N/mm²) δ5 min (%) Density (g/cm³) Max OD note
08Х22Н6Т 588 — (not normalised) 24 7.6 ≤108 mm per Table 1 note 1

Ambient values from GOST 9940-81 Table 3 for 08Х22Н6Т. Highest Rm in Table 3; yield not normalised; thick-wall Rm relief applies. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution / duplex anneal when ordered; do not copy pure-austenitic furnace charts.

Seamless Pipe Manufacture of GOST 9940 08Х22Н6Т

SHH STEEL can produce 08Х22Н6Т as hot-deformed seamless pipe to GOST 9940-81, then apply ordered heat treatment, scale removal, and end finish. Plain square-cut ends are default; weld bevels on walls over 5 mm only when the purchaser asks. Seamless hot-deformed manufacture remains the only valid order path for 08Х22Н6Т under GOST 9940; the acknowledgement repeats that route so production cannot silently change after the PO is firm. Size practice for 08Х22Н6Т remains OD not above 108 mm.

Process control for 08Х22Н6Т ends with verified dimensions, surface, and any ordered HT (Solution / duplex anneal when ordered; do not copy pure-austenitic furnace charts). Duplex-lean heats need phase-balance-aware anneal when HT is ordered; austenitic-only quench charts are the wrong default. Pickling or descaling decisions for 08Х22Н6Т stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. Size practice for 08Х22Н6Т remains OD not above 108 mm.

Bevel geometry on walls over 5 mm is by agreement when ordered without a drawing. Size practice: OD not above 108 mm. Density for theoretical weight of 08Х22Н6Т: 7.6 g/cm³. Hydrostatic pressure or UT class for 08Х22Н6Т is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Corrosion framing beside 08Х22Н6Т: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr.

Dimensions and Tolerances for GOST 9940 08Х22Н6Т

Random length is typically 1.5–10 m (longer by agreement); exact lengths take +15 mm; multiple lengths add 5 mm per cut. For 08Х22Н6Т, confirm whether your project hits the mark-specific OD ceiling. Context: OD not above 108 mm. Precision class follows the tolerance ordered for 08Х22Н6Т, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 08Х22Н6Т caution visible here: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ.

Mass of 1 m uses M = π/1000 · (D − s) · s · ρ with ρ = 7.6 g/cm³ for 08Х22Н6Т. Size reminder: OD not above 108 mm. Fixed lengths and multiple cut lengths for 08Х22Н6Т are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 08Х22Н6Т caution visible here: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ.

Equivalent Grades for GOST 9940 08Х22Н6Т

Lock 08Х22Н6Т on the PO when the datasheet owner wants GOST 9940 seamless stainless steel pipe (hot-deformed). Commercial talk as lean duplex / 22Cr-6Ni Ti (approx) is fine in emails; mill paperwork must still show GOST 9940 08Х22Н6Т. Application framing: duplex WPS — control heat input and ferrite; Ti present on cast.

System Designation Notes
GOST 9940 08Х22Н6Т Governing pipe grade for this page
Commercial / UNS (body only) lean duplex / 22Cr-6Ni Ti (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

When the service outgrows 08Х22Н6Т, move to a sister rather than stretching the alias: GOST 9940 08Х18Н10Т, GOST 9940 10Х17Н13М2Т, GOST 9940 08Х20Н14С2. Apps context: duplex WPS — control heat input and ferrite; Ti present on cast. Full list under GOST 9940. Dual marking is a purchase-order option that still requires every limit that matters for 08Х22Н6Т to be verified on the heat.

08Х22Н6Т sourcing notes should keep forms separate: start from Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; add a plate product link later once the slug returns 200. Do not stretch a 08Х22Н6Т pipe certificate onto plate.

Heat Treatment and Delivery Condition for GOST 9940 08Х22Н6Т

Other heat-treatment schedules are allowed only by written agreement — silence does not invent a mandatory anneal. For 08Х22Н6Т: Solution / duplex anneal when ordered; do not copy pure-austenitic furnace charts. Recorded furnace charts for 08Х22Н6Т should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

After local hot work in the field, restore ordered HT practice when the corrosion file demands it. Caution: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ. Field heat treatment of 08Х22Н6Т after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 08Х22Н6Т: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr.

Corrosion Resistance of GOST 9940 08Х22Н6Т

Pick tests that match how 08Х22Н6Т is filed — austenitic-ferritic (duplex-lean) Ti-stabilised. Corrosion thread: higher strength and often better chloride resistance than 08Х18Н10Т at similar Cr. Caution: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ. Coupon orientation, weld condition, and surface finish for 08Х22Н6Т belong in the corrosion test order so results can be compared to the installed spool honestly. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

Sulphur atmospheres, carburising gases, and chlorides are different failure modes — match the mark to the gas or liquid analysis. Use thread: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 08Х22Н6Т rather than relying on wall thickness alone. Keep the 08Х22Н6Т caution visible here: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ.

Applications of GOST 9940 08Х22Н6Т Seamless Pipe

Project types that repeatedly call 08Х22Н6Т: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3. Caution still applies: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ.

Furnace, chemical, and aqueous lines all appear in 9940 RFQs — alloy choice still follows the medium. For this mark: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3. Commissioning teams benefit when the as-built dossier repeats 08Х22Н6Т beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3.

Weldability of GOST 9940 08Х22Н6Т

Even hot-deformed seamless pipe of 08Х22Н6Т will see field welds. Use: duplex WPS — control heat input and ferrite; Ti present on cast. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for 08Х22Н6Т should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

Dissimilar welds to carbon steel need buttering and dilution control — especially on Mo and high-Ni grades. Role context: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3. Consumable lot control and shielding-gas notes for 08Х22Н6Т stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 08Х22Н6Т remains OD not above 108 mm.

Surface Finishes for GOST 9940 08Х22Н6Т

08Х22Н6Т under GOST 9940 typically ships annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (08Х22Н6Т).

Finish Typical supply Order note
Annealed and pickled Standard pipe mill finish after anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; inspect before polish on ferritic stock
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

When 08Х22Н6Т ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Apps reminder: duplex WPS — control heat input and ferrite; Ti present on cast. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (08Х22Н6Т).

Inspection and Testing for GOST 9940 08Х22Н6Т

Batching rules limit a party to 200 pieces of one size, one mark, and one heat-treatment kind (and one heat when ordered). For 08Х22Н6Т, keep the heat identity unbroken from melt to bundle tag. Duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3.

Intergranular corrosion, elevated tensile, and yield checks are extras — see the mechanical note for 08Х22Н6Т. Order them under the PO when the stress or corrosion file needs them. Non-conforming 08Х22Н6Т lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3.

Packaging and Shipping for GOST 9940 08Х22Н6Т

Small-OD 08Х22Н6Т often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Bundle tickets for 08Х22Н6Т repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3.

Bevelled ends get protectors so landing edges survive trucking. Size hint: OD not above 108 mm. Desiccant and wrap choices for 08Х22Н6Т follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Claims handling for 08Х22Н6Т starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

Why Choose SHH STEEL

Project teams working to CIS pipe specs need a supplier that reads Cyrillic grade names correctly. SHH STEEL can make 08Х22Н6Т to that discipline. Caution we keep visible: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ. SHH STEEL can produce and supply 08Х22Н6Т against the OD × wall, hot-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

Dual-cert discussions (GOST + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2. Ask for a written acknowledgement that names 08Х22Н6Т, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х22Н6Т to that written scope.

Supply Capability

Whether you need prototype spools or project tonnage of 08Х22Н6Т, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 08Х22Н6Т when the mill schedule allows.

Item Capability
Standard GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes
Grade 08Х22Н6Т (GOST 5632 chemistry; alias lean duplex / 22Cr-6Ni Ti (approx))
Product form Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941)
Delivery condition as ordered — heat-treated or without heat treatment
Documents Quality document per GOST 10692 / EN 10204 3.1 style as ordered
Typical size practice OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: ≤108 mm per Table 1 note 1
Precision Ordinary or high (index “в” when high)
Tests Tensile per party; hydro / UT / flatten / IGC / yield when ordered

Stock / Available sizes

Stock / Available sizes: SHH STEEL quotes piercing slots for 08Х22Н6Т rather than promising anonymous warehouse tons. Typical conversation starts around OD not above 108 mm. SHH STEEL can supply alternate walls and precision classes for 08Х22Н6Т once the design pressure and corrosion allowance are clear. SHH STEEL can supply alternate walls and precision classes for 08Х22Н6Т once design pressure and corrosion allowance are clear. Weld-shop note tied to 08Х22Н6Т: duplex WPS — control heat input and ferrite; Ti present on cast.

If the project needs dual GOST 9940 + ASTM documentation, say so before melt. Caution: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ. SHH STEEL can produce trial lengths of 08Х22Н6Т for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of 08Х22Н6Т for procedure qualification before bulk release when the project calendar needs it. This paragraph is locked to 08Х22Н6Т duty: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3.

FAQ

What is GOST 9940 08Х22Н6Т seamless stainless steel pipe used for?
GOST 9940 08Х22Н6Т is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — chloride-bearing aqueous lines where CIS specs allow substituting duplex-lean for 18-8. Role summary: lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
Is GOST 9940 08Х22Н6Т seamless only, or does it cover welded pipe?
Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 08Х22Н6Т when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
Is heat treatment mandatory for 08Х22Н6Т under GOST 9940?
No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution / duplex anneal when ordered; do not copy pure-austenitic furnace charts. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
How does 08Х22Н6Т compare with sister grades 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2?
08Х22Н6Т is filed as austenitic-ferritic (duplex-lean) Ti-stabilised. Typical sisters on the same RFQ are 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2. Design caution: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 08Х22Н6Т?
Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
Is lean duplex / 22Cr-6Ni Ti (approx) the same as ordering 08Х22Н6Т?
No. lean duplex / 22Cr-6Ni Ti (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 08Х22Н6Т so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GOST 9940 08Х22Н6Т?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х22Н6Т within Table 1 practice, respecting the mark’s diameter cap (≤108 mm per Table 1 note 1). Size context: OD not above 108 mm. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
How should 08Х22Н6Т be welded on site?
Shop guidance: duplex WPS — control heat input and ferrite; Ti present on cast. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ
When should I choose a Mo-bearing or duplex grade instead of 08Х22Н6Т?
Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic-ferritic (duplex-lean) Ti-stabilised practice can defend for the temperature and stress state. Caution for this mark: OD ≤108 mm; not ASTM A790 S31803 — phase balance and PREN differ Sister pointers: 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GOST 9940 08Х22Н6Т with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 08Х22Н6Т does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
How does GOST 9940 08Х22Н6Т differ from GOST 9941 of the same mark?
GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х22Н6Т.

Conclusion

GOST 9940 08Х22Н6Т is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — lean duplex (austenitic-ferritic) Ti-stabilised seamless pipe — highest Rm in GOST 9940 Table 3. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х18Н10Т, 10Х17Н13М2Т, 08Х20Н14С2. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X