GOST 9940 10Х17Н13М2Т Seamless Stainless Steel Pipe

GOST 9940 10Х17Н13М2Т seamless stainless steel pipe (316Ti / UNS S31635 (approx)), austenitic Mo + Ti (316Ti class), GOST 5632 cast analysis, Rm min 529 N/mm² / δ5 min 35%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
Grade
10Х17Н13М2Т (GOST 5632 / 316Ti / UNS S31635 (approx) — body alias)
Standard
GOST 9940-81
Product form
Seamless stainless steel pipe (hot-deformed), delivery as ordered — heat-treated or without heat treatment
Size
OD × wall per Table 1; mark cap ≤219 mm per Table 1 note 1; random length typically 1.5–10 m
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GOST 9940 10Х17Н13М2Т Seamless Stainless Steel Pipe

Russian and CIS piping packages that print GOST 9940 expect hot-deformed seamless stainless pipe, not a welded substitute and not an automatic ASTM A312 certificate. 10Х17Н13М2Т is the Cyrillic mark on Table 3 for this austenitic Mo + Ti (316Ti class) chemistry. Mill brand ЭИ448. Russian 316Ti-class seamless pipe under hot-deformed GOST 9940.

Mill path for 10Х17Н13М2Т: hot-deformed seamless route, clause 2.1 heat-treatment choice, GOST 5632 chemistry, Table 3 Rm and elongation, optional hydro / UT / IGC when ordered. SHH STEEL can make and supply the grade to that stack. Typical use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.

Body text may mention 316Ti / UNS S31635 (approx) for cross-reference, but the H1 and order line stay on Cyrillic 10Х17Н13М2Т. Silent alias swaps are how wrong carbon ceilings and wrong Table 3 numbers enter the MTC. Keep this caution in view: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo.

Order the standard the drawing and regulatory file actually require. Inside this 9940 series, compare 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т before stretching surface finish or wall alone. Duty thread: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. Document the medium, design temperature, and weld map beside the 10Х17Н13М2Т line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Application context for 10Х17Н13М2Т stays chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.

Inside this GOST 9940 series, compare GOST 9940 08Х17Н15М3Т, GOST 9940 08Х18Н10Т, GOST 9940 12Х18Н10Т. Hub: GOST 9940. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP316Ti.

On 10Х17Н13М2Т packages that also list flats, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is ASTM A240 UNS S31635. Keep 10Х17Н13М2Т acceptance text on the governing pipe/tube standard.

Chemical Composition of GOST 9940 10Х17Н13М2Т

GOST 5632 sets the melt limits for 10Х17Н13М2Т. Highlight band: C ≤0.10, Si ≤0.80, Mn ≤2.00, P ≤0.035, S ≤0.020, Ni 12.00–14.00, Cr 16.00–18.00, Mo 2.00–3.00. For pipe intended for welding, GOST 9940 can tighten sulphur to ≤0.020% when the order states that duty. Alias note: 316Ti / UNS S31635 (approx).

The composition table below is the cast window SHH STEEL quotes against for 10Х17Н13М2Т. Edition framing is GOST 5632 for chemistry and GOST 9940-81 for the pipe product. Use thread: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 10Х17Н13М2Т before the order is acknowledged. This paragraph is locked to 10Х17Н13М2Т duty: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty.

Grade C Si Mn P S Ni Cr Mo Ti
10Х17Н13М2Т ≤0.10 ≤0.80 ≤2.00 ≤0.035 ≤0.020 12.00–14.00 16.00–18.00 2.00–3.00 5×C–0.70

Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.

Mechanical Properties of GOST 9940 10Х17Н13М2Т

Table 3 mechanical acceptance for 10Х17Н13М2Т: Rm min 529 N/mm², elongation δ5 min 35% (yield not normalised in Table 3). Note: Yield not normalised; thick-wall Rm relief applies. Delivery framing: as ordered — heat-treated or without heat treatment. Density for mass calc: 8.0 g/cm³. Sampling follows GOST 9940 batch rules (party ≤200 pcs).

Elevated-temperature tensile at 623 K (350 °C) and yield determination are purchaser options, not defaults. For 10Х17Н13М2Т, state them on the PO if the stress calculation needs them. Use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Do not substitute GOST 9941 cold-deformed tensile numbers onto a hot-deformed 10Х17Н13М2Т certificate without a written dual-product plan. Corrosion framing beside 10Х17Н13М2Т: Mo raises PREN versus 18-8; Ti covers as-welded IGC.

Grade Rm min (N/mm²) Rp0.2 min (N/mm²) δ5 min (%) Density (g/cm³) Max OD note
10Х17Н13М2Т 529 — (not normalised) 35 8.0 ≤219 mm per Table 1 note 1

Ambient values from GOST 9940-81 Table 3 for 10Х17Н13М2Т. Yield not normalised; thick-wall Rm relief applies. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution anneal; Ti for as-welded chloride/organic duty.

Seamless Pipe Manufacture of GOST 9940 10Х17Н13М2Т

For 10Х17Н13М2Т, the mill path is hot pierce / elongate / size — never ERW under GOST 9940. Heat treatment is ordered or omitted per clause 2.1; silence means the mill may ship without HT unless the purchase order freezes a schedule. Order ordinary or high precision class with the size. Seamless hot-deformed routes are the only valid order paths for 10Х17Н13М2Т under GOST 9940.

After hot deformation, 10Х17Н13М2Т receives heat treatment only if the order asks for it — Solution anneal; Ti for as-welded chloride/organic duty. Austenitic heats usually take solution annealing with rapid cool when HT is ordered; skip inventing a mandatory anneal when the PO says without heat treatment. Use thread: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.

Marking carries the grade 10Х17Н13М2Т, size, precision cue when high class, manufacturer ID, and GOST 9940 reference. Size hint: OD not above 219 mm. Weld thread for fabricator joints: 316L/316Ti-class fillers; keep Mo in the weld metal. Hydrostatic pressure or UT class for 10Х17Н13М2Т is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Keep the 10Х17Н13М2Т caution visible here: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo.

Dimensions and Tolerances for GOST 9940 10Х17Н13М2Т

Dimensional order lines for 10Х17Н13М2Т should state OD × wall, length type (random, exact, multiple, or limited), end finish, and precision class. Use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Max OD for this mark: 219 mm. Precision class follows the tolerance ordered for 10Х17Н13М2Т, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 10Х17Н13М2Т caution visible here: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo.

Ovality has no separate number — it must not push OD outside the diameter tolerance. Caution: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo. Fixed lengths and multiple cut lengths for 10Х17Н13М2Т are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the 10Х17Н13М2Т caution visible here: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo.

Equivalent Grades for GOST 9940 10Х17Н13М2Т

Under GOST 9940, 10Х17Н13М2Т is the governing seamless stainless steel pipe (hot-deformed) designation on this page. Commercial shorthand such as 316Ti / UNS S31635 (approx) helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the GOST 9940 10Х17Н13М2Т line. ASTM A312 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.

System Designation Notes
GOST 9940 10Х17Н13М2Т Governing pipe grade for this page
Commercial / UNS (body only) 316Ti / UNS S31635 (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other EN 1.4571 Starting point for comparison only; no automatic dual-cert

Read the notes column literally for 10Х17Н13М2Т: related chemistry is not automatic dual-cert. Cross-check GOST 9940 08Х17Н15М3Т, GOST 9940 08Х18Н10Т, GOST 9940 12Х18Н10Т when Mo, stabilisation, or carbon ceilings change the selection. Hub: GOST 9940. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (10Х17Н13М2Т). Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (10Х17Н13М2Т).

Heat Treatment and Delivery Condition for GOST 9940 10Х17Н13М2Т

Mill heat treatment for 10Х17Н13М2Т is optional per clause 2.1 — Solution anneal; Ti for as-welded chloride/organic duty. Bright or descaled finishes are separate order items. Delivery label: as ordered — heat-treated or without heat treatment. Recorded furnace charts for 10Х17Н13М2Т should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 10Х17Н13М2Т duty: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty.

Certificate wording for 10Х17Н13М2Т should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature — or explicitly “without heat treatment” when that was ordered. Use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Field heat treatment of 10Х17Н13М2Т after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 10Х17Н13М2Т remains OD not above 219 mm.

Corrosion Resistance of GOST 9940 10Х17Н13М2Т

Mo raises PREN versus 18-8; Ti covers as-welded IGC Ordering IGC does not create a blanket corrosion warranty for every medium. Family filing: austenitic Mo + Ti (316Ti class). Coupon orientation, weld condition, and surface finish for 10Х17Н13М2Т belong in the corrosion test order so results can be compared to the installed spool honestly. Size practice for 10Х17Н13М2Т remains OD not above 219 mm.

Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 10Х17Н13М2Т honestly against 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. Role: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 10Х17Н13М2Т rather than relying on wall thickness alone. This paragraph is locked to 10Х17Н13М2Т duty: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty.

Applications of GOST 9940 10Х17Н13М2Т Seamless Pipe

Typical BOM language pairs GOST 9940 10Х17Н13М2Т with OD × wall, precision class, and heat-treatment yes/no. Primary sketch: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Spool fabricators should copy 10Х17Н13М2Т onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 10Х17Н13М2Т caution visible here: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo.

Spell 10Х17Н13М2Т on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. Commissioning teams benefit when the as-built dossier repeats 10Х17Н13М2Т beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to 10Х17Н13М2Т: 316L/316Ti-class fillers; keep Mo in the weld metal.

Weldability of GOST 9940 10Х17Н13М2Т

Weldability of 10Х17Н13М2Т follows austenitic Mo + Ti (316Ti class) practice. Filler/shop note: 316L/316Ti-class fillers; keep Mo in the weld metal. Caution: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo. Procedure qualification for 10Х17Н13М2Т should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Keep the 10Х17Н13М2Т caution visible here: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo.

For corrosive as-welded duty on 10Х17Н13М2Т, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 316L/316Ti-class fillers; keep Mo in the weld metal. Order sulphur ≤0.020% when the pipe is intended for welding. Consumable lot control and shielding-gas notes for 10Х17Н13М2Т stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 10Х17Н13М2Т caution visible here: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo.

Surface Finishes for GOST 9940 10Х17Н13М2Т

10Х17Н13М2Т under GOST 9940 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (10Х17Н13М2Т).

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

SHH STEEL sequences pickle, optional passivation, and any agreed polish for 10Х17Н13М2Т after the heat-treatment evidence is on the certificate. Free-iron control and packing discipline matter as much as Ra numbers for long pipe life in the field. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (10Х17Н13М2Т).

Inspection and Testing for GOST 9940 10Х17Н13М2Т

SHH STEEL reports the tests actually performed for 10Х17Н13М2Т — no surrogate NDT lines. Hydrostatic versus ultrasonic choice belongs on the PO. Caution: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo. Sampling plans for 10Х17Н13М2Т keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside 10Х17Н13М2Т: Mo raises PREN versus 18-8; Ti covers as-welded IGC.

Retests use double sample counts from the same party — failures are not silently shipped. Size context: OD not above 219 mm. Non-conforming 10Х17Н13М2Т lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Application context for 10Х17Н13М2Т stays chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т.

Packaging and Shipping for GOST 9940 10Х17Н13М2Т

Export packing for GOST 9940 10Х17Н13М2Т is built around rust prevention and transit abrasion control. Bundle tickets repeat the Cyrillic grade symbol and heat number. Duty: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. Bundle tickets for 10Х17Н13М2Т repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 10Х17Н13М2Т: Mo raises PREN versus 18-8; Ti covers as-welded IGC.

Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 10Х17Н13М2Т. Desiccant and wrap choices for 10Х17Н13М2Т follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 10Х17Н13М2Т remains OD not above 219 mm.

Photographic packing records are available on request for project QA files on 10Х17Н13М2Т. Claims handling for 10Х17Н13М2Т starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for 10Х17Н13М2Т remains OD not above 219 mm.

Why Choose SHH STEEL

Buyers choose SHH STEEL for 10Х17Н13М2Т because the paperwork matches the stencil: GOST 5632 chemistry, Table 3 tensile, ordered HT, and honest seamless marking. Application fit: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. SHH STEEL can produce and supply 10Х17Н13М2Т against the OD × wall, hot-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 10Х17Н13М2Т cleanly. Ask for a written acknowledgement that names 10Х17Н13М2Т, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 10Х17Н13М2Т to that written scope.

Supply Capability

Supply capability for 10Х17Н13М2Т covers hot-deformed seamless manufacture, ordered heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 10Х17Н13М2Т when the mill schedule allows. Size practice for 10Х17Н13М2Т remains OD not above 219 mm.

Item Capability
Standard GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes
Grade 10Х17Н13М2Т (GOST 5632 chemistry; alias 316Ti / UNS S31635 (approx))
Product form Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941)
Delivery condition as ordered — heat-treated or without heat treatment
Documents Quality document per GOST 10692 / EN 10204 3.1 style as ordered
Typical size practice OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: ≤219 mm per Table 1 note 1
Precision Ordinary or high (index “в” when high)
Tests Tensile per party; hydro / UT / flatten / IGC / yield when ordered

Stock / Available sizes

Stock / Available sizes for 10Х17Н13М2Т: common OD×wall combinations as the project uses. Hot-deformed availability varies by diameter — confirm with the RFQ. Hint: OD not above 219 mm. SHH STEEL can supply alternate walls and precision classes for 10Х17Н13М2Т once the design pressure and corrosion allowance are clear.

Mill certificates, packing photos, and third-party witness can be bundled into the 10Х17Н13М2Т supply scope when the PO says so. Use: chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. SHH STEEL can produce trial lengths of 10Х17Н13М2Т for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GOST 9940 10Х17Н13М2Т seamless stainless steel pipe used for?
GOST 9940 10Х17Н13М2Т is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — chemical plant chloride-bearing lines, pulp liquor stubs, and CIS packages migrating from 08Х18Н10Т. Role summary: Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
Is GOST 9940 10Х17Н13М2Т seamless only, or does it cover welded pipe?
Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 10Х17Н13М2Т when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
Is heat treatment mandatory for 10Х17Н13М2Т under GOST 9940?
No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution anneal; Ti for as-welded chloride/organic duty. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
How does 10Х17Н13М2Т compare with sister grades 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т?
10Х17Н13М2Т is filed as austenitic Mo + Ti (316Ti class). Typical sisters on the same RFQ are 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. Design caution: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 10Х17Н13М2Т?
Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
Is 316Ti / UNS S31635 (approx) the same as ordering 10Х17Н13М2Т?
No. 316Ti / UNS S31635 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 10Х17Н13М2Т so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GOST 9940 10Х17Н13М2Т?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 10Х17Н13М2Т within Table 1 practice, respecting the mark’s diameter cap (≤219 mm per Table 1 note 1). Size context: OD not above 219 mm. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
How should 10Х17Н13М2Т be welded on site?
Shop guidance: 316L/316Ti-class fillers; keep Mo in the weld metal. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo
When should I choose a Mo-bearing or duplex grade instead of 10Х17Н13М2Т?
Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic Mo + Ti (316Ti class) practice can defend for the temperature and stress state. Caution for this mark: OD ≤219 mm; Mo 2–3% is not superaustenitic — severe seawater may need lean duplex or higher Mo Sister pointers: 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GOST 9940 10Х17Н13М2Т with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 10Х17Н13М2Т does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
How does GOST 9940 10Х17Н13М2Т differ from GOST 9941 of the same mark?
GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 10Х17Н13М2Т.

Conclusion

GOST 9940 10Х17Н13М2Т is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — Mo + Ti austenitic seamless pipe — the GOST 316Ti analogue for chloride / organic duty. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х17Н15М3Т, 08Х18Н10Т, 12Х18Н10Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X