GOST 9940 04Х18Н10 Seamless Stainless Steel Pipe
What is GOST 9940 04Х18Н10 Seamless Stainless Steel Pipe
GOST 9940-81 is the Soviet / CIS product standard for seamless hot-deformed corrosion-resistant steel pipes — geometry, tensile floors, and acceptance in one document. Grade 04Х18Н10 sits in the austenitic low-carbon 18-8 set under Table 3. Mill brand ЭИ842 / ЭП550. The low-carbon 18-8 mark when the Russian PO wants welded corrosion duty without titanium.
SHH STEEL can produce and supply GOST 9940 04Х18Н10 as hot-deformed seamless pipe across the enquiry OD×wall band (within the mark’s diameter cap), heat-treated or without HT as ordered, descaled or bright-finished, and documented on mill certificates tied to GOST 5632 cast analysis and Table 3 tensile results. Duty focus: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
Shop language may still say “304L pipe,” yet that commercial alias does not select GOST 5632 cast limits, hot-deformed tensile floors, or GOST 9940 marking. The purchase order has to name GOST 9940 and 04Х18Н10 so the mill applies the correct analysis, optional heat treatment, mechanical floors, and stencil. Design caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
Scope discipline: 04Х18Н10 is hot-deformed seamless pipe under GOST 9940, not cold-deformed GOST 9941 and not an ASTM A312 order by default. Sister marks often compared on the same RFQ include 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. Role reminder: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940. Diameter note: full Table 1 range.
Inside this GOST 9940 series, compare GOST 9940 08Х18Н10, GOST 9940 08Х18Н10Т, GOST 9940 12Х18Н10Т. Hub: GOST 9940. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP304L.
On 04Х18Н10 packages that also list flats, keep tubular RFQs under Stainless Steel Pipes and Tubes, flat RFQs under Stainless Steel Sheets and Plates, and pin the plate twin with ASTM A240 Type 304L. Quote 04Х18Н10 pipe and plate under separate line items.
Chemical Composition of GOST 9940 04Х18Н10
Cast analysis for GOST 9940 04Х18Н10 is not printed inside 9940 itself — clause 2.1 points to GOST 5632. Key windows on a typical certificate include C ≤0.04, Si ≤0.80, Mn ≤2.00, P ≤0.030, S ≤0.020, Ni 9.00–11.00, Cr 17.00–19.00. SHH STEEL ties the heat number on the pipe marking to the same cast line on the MTC. Commercial alias 304L / UNS S30403 (approx). Mill brand ЭИ842 / ЭП550. Corrosion thread: 304L-class aqueous resistance; Mo-bearing sisters when chlorides climb.
Chemical limits for 04Х18Н10 appear in the table underneath (GOST 5632-2014 extract). Source priority is the paid GOST 5632 table if your client cites a different edition footnote — send it before the heat is melted. Duty thread: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 04Х18Н10 | ≤0.04 | ≤0.80 | ≤2.00 | ≤0.030 | ≤0.020 | 9.00–11.00 | 17.00–19.00 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9940 04Х18Н10
Ambient tensile floors for 04Х18Н10 come from GOST 9940-81 Table 3: Rm min 441 N/mm², elongation δ5 min 40% (yield not normalised in Table 3). Note: Yield not normalised; thick-wall D/s≤8 may drop Rm by 19.6 N/mm². These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic low-carbon 18-8. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
Yield strength is numerically normalised in GOST 9940 only for 12Х18Н10Т (≥216 N/mm²) when the purchaser orders it — for 04Х18Н10, treat Rp0.2 as an ordered extra unless that mark exception applies. Thick-wall pipes with D/s ≤8 on thirteen named marks may reduce Rm by 19.6 N/mm² per Table 3 note 1. Density 7.9 g/cm³. Role: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 04Х18Н10 | 441 | — (not normalised) | 40 | 7.9 | full Table 1 range |
Ambient values from GOST 9940-81 Table 3 for 04Х18Н10. Yield not normalised; thick-wall D/s≤8 may drop Rm by 19.6 N/mm². Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Solution anneal when heat treatment is ordered (typical 1000–1100 °C, rapid cool).
Seamless Pipe Manufacture of GOST 9940 04Х18Н10
For 04Х18Н10, the mill path is hot pierce / elongate / size — never ERW under GOST 9940. Heat treatment is ordered or omitted per clause 2.1; silence means the mill may ship without HT unless the purchase order freezes a schedule. Order ordinary or high precision class with the size. Seamless hot-deformed manufacture remains the only valid order path for 04Х18Н10 under GOST 9940; the acknowledgement repeats that route so production cannot silently change after the PO is firm. Weld-shop note tied to 04Х18Н10: 308L-class fillers; low-C cast already helps as-welded IGC.
Austenitic heats usually take solution annealing with rapid cool when HT is ordered; skip inventing a mandatory anneal when the PO says without heat treatment. Heat-treatment note for 04Х18Н10: Solution anneal when heat treatment is ordered (typical 1000–1100 °C, rapid cool). Scale removal follows when ordered; clause defaults do not automatically pickle every pipe. Duty thread: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
When dual documentation against ASTM A312 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for 04Х18Н10: full hot-deformed band to 325 mm. Diameter cap: full Table 1 range.
Dimensions and Tolerances for GOST 9940 04Х18Н10
SHH STEEL aligns nominal OD, wall, length type, and precision class (ordinary / high) for 04Х18Н10 before the mill slot is locked. Table 1 lists OD from 57 to 325 mm and wall from 3.5 to 32 mm, with measured length limits per size cell. Size hint: full hot-deformed band to 325 mm. Mark cap: full Table 1 range.
OD tolerance is ±1.5% (ordinary) or ±1.0% (high). Wall minus tolerance reaches 15% on many gauges — design min wall with that minus in view. Curvature limits: 1.5 / 2 / 4 mm per metre by wall band. Duty thread: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
Equivalent Grades for GOST 9940 04Х18Н10
Identity first: GOST 9940 04Х18Н10 is the HX/pipe grade for this page. 304L / UNS S30403 (approx) helps buyers who think in AISI/UNS labels. Role: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940. Foreign product standards remain separate documents. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (04Х18Н10).
| System | Designation | Notes |
|---|---|---|
| GOST 9940 | 04Х18Н10 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 304L / UNS S30403 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 304L chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Inside this series compare GOST 9940 08Х18Н10, GOST 9940 08Х18Н10Т, GOST 9940 12Х18Н10Т before swapping marks for medium or temperature. Keep this caution visible for 04Х18Н10: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades. Hub: GOST 9940. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (04Х18Н10).
Heat Treatment and Delivery Condition for GOST 9940 04Х18Н10
04Х18Н10 is delivered as ordered — heat-treated or without heat treatment under GOST 9940. Guidance: Solution anneal when heat treatment is ordered (typical 1000–1100 °C, rapid cool). Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 308L-class fillers; low-C cast already helps as-welded IGC.
Cooling type matters — austenitics need rapid cool after solution treatment when HT is ordered; ferritic/martensitic anneal practice follows air or slow-cool notes. Duty thread: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940. Density 7.9 g/cm³ for weight calcs. Field heat treatment of 04Х18Н10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 04Х18Н10 caution visible here: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
Corrosion Resistance of GOST 9940 04Х18Н10
Corrosion behaviour of GOST 9940 04Х18Н10 tracks its austenitic low-carbon 18-8 balance: 304L-class aqueous resistance; Mo-bearing sisters when chlorides climb. Intergranular corrosion testing is a purchaser option under GOST 9940, not an automatic coupon on every lot. Design caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. 04Х18Н10 is filed as austenitic low-carbon 18-8. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades.
Applications of GOST 9940 04Х18Н10 Seamless Pipe
Applications of GOST 9940 04Х18Н10 seamless pipe centre on chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. Role summary: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940. When a related chemistry is required under ASTM A312, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same Cyrillic grade symbol on cut lists so informal latinised substitutions do not creep in. Primary application sketch: chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. Duty thread: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
Weldability of GOST 9940 04Х18Н10
04Х18Н10 ships as seamless mill product, but fabricator joints on spools still need a qualified WPS. Shop guidance: 308L-class fillers; low-C cast already helps as-welded IGC. Mill heat treatment of the pipe does not replace qualified welding procedures on site joints. Procedure qualification for 04Х18Н10 should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. This paragraph is locked to 04Х18Н10 duty: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic low-carbon 18-8 — not a single shop habit. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades. Consumable lot control and shielding-gas notes for 04Х18Н10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Application context for 04Х18Н10 stays chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9.
Surface Finishes for GOST 9940 04Х18Н10
04Х18Н10 under GOST 9940 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (04Х18Н10).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Passivation restores the chromium-rich film after pickling or light fabrication on 04Х18Н10; it does not replace the heat treatment that sets mechanical properties under GOST 9940. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.
Inspection and Testing for GOST 9940 04Х18Н10
Inspection for GOST 9940 04Х18Н10 covers dimensions and appearance on every pipe; tensile on two pipes per party; flattening or expanding on one when ordered; IGC on two when ordered. Hydrostatic and ultrasonic tests run when the purchaser asks. Documents follow GOST 10692 with chemistry taken from the billet certificate.
Marking includes 04Х18Н10, manufacturer, size, and GOST 9940. Traceability from stencil to MTC is part of supply, not an upgrade. Use: chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. Non-conforming 04Х18Н10 lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Corrosion framing beside 04Х18Н10: 304L-class aqueous resistance; Mo-bearing sisters when chlorides climb.
Packaging and Shipping for GOST 9940 04Х18Н10
Packaging for 04Х18Н10 uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect descaled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for 04Х18Н10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to 04Х18Н10 duty: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades. Desiccant and wrap choices for 04Х18Н10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 04Х18Н10 remains full hot-deformed band to 325 mm.
Shipping documents list GOST 9940, 04Х18Н10, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940. Claims handling for 04Х18Н10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to 04Х18Н10 duty: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
Why Choose SHH STEEL
SHH STEEL can produce and supply GOST 9940 04Х18Н10 with the hot-deformed seamless route, heat-treatment choice, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless seamless hot capacity covering this mark’s OD band. Duty focus: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940.
Technical sales can map 04Х18Н10 against sisters 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т and live ASTM A312 pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names 04Х18Н10, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 04Х18Н10 to that written scope.
Supply Capability
SHH STEEL can produce and supply GOST 9940 04Х18Н10 across enquiry-oriented OD × wall bands (within full Table 1 range), in the hot-deformed seamless route, with certificates and optional tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue.
| Item | Capability |
|---|---|
| Standard | GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes |
| Grade | 04Х18Н10 (GOST 5632 chemistry; alias 304L / UNS S30403 (approx)) |
| Product form | Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941) |
| Delivery condition | as ordered — heat-treated or without heat treatment |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: full Table 1 range |
| Precision | Ordinary or high (index “в” when high) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
SHH STEEL can produce and supply GOST 9940 04Х18Н10. Stock / Available sizes: enquiry band typically aligns with GOST 9940 Table 1 OD×wall practice, with ordinary or high precision as ordered. For 04Х18Н10, practical fast-track sizes often sit inside the mark’s diameter cap — send the OD × wall list for a firm acknowledgement. Context: full hot-deformed band to 325 mm. Cap: full Table 1 range.
Cut lengths, bevels, special NDT, IGC, and HT extras add lead time — call them early. Sisters often quoted alongside: 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. Email the size list to start. SHH STEEL can produce trial lengths of 04Х18Н10 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9940 04Х18Н10 seamless stainless steel pipe used for?
- GOST 9940 04Х18Н10 is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — chemical plant transfer lines, food/pharma-adjacent CIS packages, and welded manifolds that refuse higher-carbon 12Х18Н9. Role summary: low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9940 04Х18Н10 seamless only, or does it cover welded pipe?
- Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 04Х18Н10 when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 04Х18Н10 under GOST 9940?
- No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Solution anneal when heat treatment is ordered (typical 1000–1100 °C, rapid cool). Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
-
How does 04Х18Н10 compare with sister grades 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т?
- 04Х18Н10 is filed as austenitic low-carbon 18-8. Typical sisters on the same RFQ are 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. Design caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 04Х18Н10?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
-
Is 304L / UNS S30403 (approx) the same as ordering 04Х18Н10?
- No. 304L / UNS S30403 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 04Х18Н10 so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9940 04Х18Н10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 04Х18Н10 within Table 1 practice, respecting the mark’s diameter cap (full Table 1 range). Size context: full hot-deformed band to 325 mm. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
-
How should 04Х18Н10 be welded on site?
- Shop guidance: 308L-class fillers; low-C cast already helps as-welded IGC. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades
-
When should I choose a Mo-bearing or duplex grade instead of 04Х18Н10?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what austenitic low-carbon 18-8 practice can defend for the temperature and stress state. Caution for this mark: low C helps IGC but PREN is still plain 18-8 — chlorides push you to Mo grades Sister pointers: 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9940 04Х18Н10 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 04Х18Н10 does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9940 04Х18Н10 differ from GOST 9941 of the same mark?
- GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 04Х18Н10.
Conclusion
GOST 9940 04Х18Н10 is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — low-carbon 18-8 austenitic seamless pipe for welded corrosive aqueous service on GOST 9940. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 08Х18Н10, 08Х18Н10Т, 12Х18Н10Т. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.