GOST 9940 08Х17Т Seamless Stainless Steel Pipe
What is GOST 9940 08Х17Т Seamless Stainless Steel Pipe
When the approved vendor list and isometric say GOST 9940, the grade mark has to be the GOST 5632 designation. 08Х17Т is the full product grade for this ferritic chromium (Ti-stabilised) seamless pipe. Mill brand ЭИ645. Titanium in the melt is why this ferritic survives welded assemblies better than plain 12Х17.
SHH STEEL can supply 08Х17Т seamless pipe in the hot-deformed route, with plain or bevelled ends, random or cut lengths, and GOST 10692 / EN 10204 3.1 style inspection documents when specified. Role on the line: Ti-stabilised 17% Cr ferritic seamless pipe for heat-transfer and mildly oxidising aqueous duty.
Equivalence talk to 430Ti / UNS S43036 (approx) belongs in engineering notes, not as a substitute for the GOST mark. Lock GOST 9940 08Х17Т, OD × wall, precision class, and HT yes/no before melt. Watch-out: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility.
Related ASTM A312 pipe pages share chemistry families but not GOST acceptance text — confirm before dual-cert claims. Sisters on this hub: 12Х17, 15Х25Т, 08Х13. Use thread: heat-exchanger shells on CIS BOMs, nitric-adjacent equipment notes, and ferritic replacements where nickel must stay low. Document the medium, design temperature, and weld map beside the 08Х17Т line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Weld-shop note tied to 08Х17Т: matching ferritic or 430Ti-class fillers; low heat input; Ti already on the cast analysis.
Inside this GOST 9940 series, compare GOST 9940 12Х17, GOST 9940 15Х25Т, GOST 9940 08Х13. Hub: GOST 9940.
08Х17Т sourcing notes should keep forms separate: start from Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; add a plate product link later once the slug returns 200. Confirm 08Х17Т OD × wall and plate thickness on separate drawings.
Chemical Composition of GOST 9940 08Х17Т
Chemistry control on 08Х17Т starts at the ladle under GOST 5632. Expect C ≤0.08, Si ≤0.80, Mn ≤0.80, P ≤0.035, S ≤0.025, Cr 16.00–18.00, Ti 5×C–0.80 within the mark’s windows, reported on the inspection document against the heat. Body alias 430Ti / UNS S43036 (approx) does not widen those windows.
Read the table with the family in mind — ferritic chromium (Ti-stabilised) — and with caution ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility. Numbers without the matching Table 3 tensile row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond GOST 5632, SHH STEEL will confirm melt feasibility for 08Х17Т before the order is acknowledged. Application context for 08Х17Т stays heat-exchanger shells on CIS BOMs, nitric-adjacent equipment notes, and ferritic replacements where nickel must stay low.
| Grade | C | Si | Mn | P | S | Cr | Ti |
|---|---|---|---|---|---|---|---|
| 08Х17Т | ≤0.08 | ≤0.80 | ≤0.80 | ≤0.035 | ≤0.025 | 16.00–18.00 | 5×C–0.80 |
Cast analysis windows from GOST 5632 (chemistry is not tabulated inside GOST 9940-81). Sulphur may be tightened to ≤0.020% when the order states the pipe is intended for welding.
Mechanical Properties of GOST 9940 08Х17Т
Tensile minima for 08Х17Т sit at Rm min 372 N/mm², elongation δ5 min 17% (yield not normalised in Table 3). Note: Yield not normalised. Flattening or drift expanding backs ductility when ordered. Watch-out: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility.
Elongation δ5 floors and Rm floors travel together on the MTC for 08Х17Т. Do not accept a certificate that quotes only hardness. Caution: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility. Do not substitute GOST 9941 cold-deformed tensile numbers onto a hot-deformed 08Х17Т certificate without a written dual-product plan. Keep the 08Х17Т caution visible here: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility.
| Grade | Rm min (N/mm²) | Rp0.2 min (N/mm²) | δ5 min (%) | Density (g/cm³) | Max OD note |
|---|---|---|---|---|---|
| 08Х17Т | 372 | — (not normalised) | 17 | 7.7 | ≤219 mm per Table 1 note 1 |
Ambient values from GOST 9940-81 Table 3 for 08Х17Т. Yield not normalised. Delivery: as ordered — heat-treated or without heat treatment. Heat-treatment guidance: Ferritic anneal when ordered; Ti binds carbon for weldability.
Seamless Pipe Manufacture of GOST 9940 08Х17Т
Seamless is not optional wording for 08Х17Т: GOST 9940 covers hot-deformed seamless corrosion-resistant pipe. Cold- and warm-deformed sisters live under GOST 9941-81 with different tensile floors. SHH STEEL will not quietly substitute a welded or cold-drawn route under a 9940 PO. Seamless hot-deformed manufacture remains the only valid order path for 08Х17Т under GOST 9940; the acknowledgement repeats that route so production cannot silently change after the PO is firm. This paragraph is locked to 08Х17Т duty: Ti-stabilised 17% Cr ferritic seamless pipe for heat-transfer and mildly oxidising aqueous duty.
Process control for 08Х17Т ends with verified dimensions, surface, and any ordered HT (Ferritic anneal when ordered; Ti binds carbon for weldability). Ferritic heats follow softening / anneal practice when HT is ordered — not austenitic solution charts. Grain growth after overheating remains a shop risk. Pickling or descaling decisions for 08Х17Т stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. Corrosion framing beside 08Х17Т: good in many oxidising aqueous media; chlorides and crevices remain the outdoor limiter.
Bevel geometry on walls over 5 mm is by agreement when ordered without a drawing. Size practice: OD capped at 219 mm for this mark under Table 1 note 1. Density for theoretical weight of 08Х17Т: 7.7 g/cm³. Hydrostatic pressure or UT class for 08Х17Т is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Corrosion framing beside 08Х17Т: good in many oxidising aqueous media; chlorides and crevices remain the outdoor limiter.
Dimensions and Tolerances for GOST 9940 08Х17Т
Random length is typically 1.5–10 m (longer by agreement); exact lengths take +15 mm; multiple lengths add 5 mm per cut. For 08Х17Т, confirm whether your project hits the mark-specific OD ceiling. Context: OD capped at 219 mm for this mark under Table 1 note 1. Precision class follows the tolerance ordered for 08Х17Т, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 08Х17Т caution visible here: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility.
Mass of 1 m uses M = π/1000 · (D − s) · s · ρ with ρ = 7.7 g/cm³ for 08Х17Т. Size reminder: OD capped at 219 mm for this mark under Table 1 note 1. Fixed lengths and multiple cut lengths for 08Х17Т are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside 08Х17Т: good in many oxidising aqueous media; chlorides and crevices remain the outdoor limiter.
Equivalent Grades for GOST 9940 08Х17Т
The table below maps GOST 9940 08Х17Т to commercial aliases and related systems without inventing false one-to-one substitutes. Alias 430Ti / UNS S43036 (approx) stays body-only. Pack caution: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (08Х17Т).
| System | Designation | Notes |
|---|---|---|
| GOST 9940 | 08Х17Т | Governing pipe grade for this page |
| Commercial / UNS (body only) | 430Ti / UNS S43036 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Read the notes column literally for 08Х17Т: related chemistry is not automatic dual-cert. Cross-check GOST 9940 12Х17, GOST 9940 15Х25Т, GOST 9940 08Х13 when Mo, stabilisation, or carbon ceilings change the selection. Hub: GOST 9940. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (08Х17Т).
Heat Treatment and Delivery Condition for GOST 9940 08Х17Т
Other heat-treatment schedules are allowed only by written agreement — silence does not invent a mandatory anneal. For 08Х17Т: Ferritic anneal when ordered; Ti binds carbon for weldability. Recorded furnace charts for 08Х17Т should support the heat-treatment claim on the certificate when HT was ordered, including quench or cool method where the family requires rapid cooling. Size practice for 08Х17Т remains OD capped at 219 mm for this mark under Table 1 note 1.
After local hot work in the field, restore ordered HT practice when the corrosion file demands it. Caution: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility. Field heat treatment of 08Х17Т after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 08Х17Т duty: Ti-stabilised 17% Cr ferritic seamless pipe for heat-transfer and mildly oxidising aqueous duty.
Corrosion Resistance of GOST 9940 08Х17Т
Pick tests that match how 08Х17Т is filed — ferritic chromium (Ti-stabilised). Corrosion thread: good in many oxidising aqueous media; chlorides and crevices remain the outdoor limiter. Caution: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility. Coupon orientation, weld condition, and surface finish for 08Х17Т belong in the corrosion test order so results can be compared to the installed spool honestly. Application context for 08Х17Т stays heat-exchanger shells on CIS BOMs, nitric-adjacent equipment notes, and ferritic replacements where nickel must stay low.
Sulphur atmospheres, carburising gases, and chlorides are different failure modes — match the mark to the gas or liquid analysis. Use thread: heat-exchanger shells on CIS BOMs, nitric-adjacent equipment notes, and ferritic replacements where nickel must stay low. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 08Х17Т rather than relying on wall thickness alone. Weld-shop note tied to 08Х17Т: matching ferritic or 430Ti-class fillers; low heat input; Ti already on the cast analysis.
Applications of GOST 9940 08Х17Т Seamless Pipe
Project types that repeatedly call 08Х17Т: heat-exchanger shells on CIS BOMs, nitric-adjacent equipment notes, and ferritic replacements where nickel must stay low. Duty: Ti-stabilised 17% Cr ferritic seamless pipe for heat-transfer and mildly oxidising aqueous duty. Caution still applies: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility.
Furnace, chemical, and aqueous lines all appear in 9940 RFQs — alloy choice still follows the medium. For this mark: Ti-stabilised 17% Cr ferritic seamless pipe for heat-transfer and mildly oxidising aqueous duty. Commissioning teams benefit when the as-built dossier repeats 08Х17Т beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 08Х17Т remains OD capped at 219 mm for this mark under Table 1 note 1.
Weldability of GOST 9940 08Х17Т
Even hot-deformed seamless pipe of 08Х17Т will see field welds. Use: matching ferritic or 430Ti-class fillers; low heat input; Ti already on the cast analysis. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for 08Х17Т should use the same product form and wall class as production, including the hot-deformed seamless finish that will ship. Corrosion framing beside 08Х17Т: good in many oxidising aqueous media; chlorides and crevices remain the outdoor limiter.
Dissimilar welds to carbon steel need buttering and dilution control — especially on Mo and high-Ni grades. Role context: Ti-stabilised 17% Cr ferritic seamless pipe for heat-transfer and mildly oxidising aqueous duty. Consumable lot control and shielding-gas notes for 08Х17Т stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside 08Х17Т: good in many oxidising aqueous media; chlorides and crevices remain the outdoor limiter.
Surface Finishes for GOST 9940 08Х17Т
Pickled mill finish covers most RFQs for 08Х17Т. Bright anneal, grind, or polish only when the enquiry writes a measurable target and names OD, ID, or both. Pack caution carried into finish control: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility.
| Finish | Typical supply | Order note |
|---|---|---|
| Annealed and pickled | Standard pipe mill finish after anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; inspect before polish on ferritic stock |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Do not polish over unresolved defects on 08Х17Т; inspection comes before cosmetics. Passivation after pickle or shop welding is good practice in chloride-lean service, but GOST 9940 acceptance still rests on correct heat treatment. Pack away from carbon-steel contact. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 08Х17Т.
Inspection and Testing for GOST 9940 08Х17Т
Batching rules limit a party to 200 pieces of one size, one mark, and one heat-treatment kind (and one heat when ordered). For 08Х17Т, keep the heat identity unbroken from melt to bundle tag. Duty: Ti-stabilised 17% Cr ferritic seamless pipe for heat-transfer and mildly oxidising aqueous duty.
Intergranular corrosion, elevated tensile, and yield checks are extras — see the mechanical note for 08Х17Т. Order them under the PO when the stress or corrosion file needs them. Non-conforming 08Х17Т lengths are segregated and retested or rejected under GOST 9940 rather than reworked into unmarked stock. Weld-shop note tied to 08Х17Т: matching ferritic or 430Ti-class fillers; low heat input; Ti already on the cast analysis.
Packaging and Shipping for GOST 9940 08Х17Т
Small-OD 08Х17Т often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: heat-exchanger shells on CIS BOMs, nitric-adjacent equipment notes, and ferritic replacements where nickel must stay low. Bundle tickets for 08Х17Т repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the 08Х17Т caution visible here: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility.
Bevelled ends get protectors so landing edges survive trucking. Size hint: OD capped at 219 mm for this mark under Table 1 note 1. Desiccant and wrap choices for 08Х17Т follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 08Х17Т remains OD capped at 219 mm for this mark under Table 1 note 1.
Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: heat-exchanger shells on CIS BOMs, nitric-adjacent equipment notes, and ferritic replacements where nickel must stay low. Claims handling for 08Х17Т starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 08Х17Т: good in many oxidising aqueous media; chlorides and crevices remain the outdoor limiter.
Why Choose SHH STEEL
Project teams working to CIS pipe specs need a supplier that reads Cyrillic grade names correctly. SHH STEEL can make 08Х17Т to that discipline. Caution we keep visible: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility. SHH STEEL can produce and supply 08Х17Т against the OD × wall, hot-deformed seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Dual-cert discussions (GOST + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: 12Х17, 15Х25Т, 08Х13. Ask for a written acknowledgement that names 08Х17Т, precision class, and heat-treatment yes or no before melt. SHH STEEL can make 08Х17Т to that written scope.
Supply Capability
Whether you need prototype spools or project tonnage of 08Х17Т, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: heat-exchanger shells on CIS BOMs, nitric-adjacent equipment notes, and ferritic replacements where nickel must stay low. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for 08Х17Т when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GOST 9940-81 seamless hot-deformed corrosion-resistant steel pipes |
| Grade | 08Х17Т (GOST 5632 chemistry; alias 430Ti / UNS S43036 (approx)) |
| Product form | Seamless pipe only — hot-deformed (cold/warm deformed = GOST 9941) |
| Delivery condition | as ordered — heat-treated or without heat treatment |
| Documents | Quality document per GOST 10692 / EN 10204 3.1 style as ordered |
| Typical size practice | OD 57–325 mm × wall 3.5–32 mm per Table 1; mark cap: ≤219 mm per Table 1 note 1 |
| Precision | Ordinary or high (index “в” when high) |
| Tests | Tensile per party; hydro / UT / flatten / IGC / yield when ordered |
Stock / Available sizes
Stock / Available sizes: SHH STEEL quotes piercing slots for 08Х17Т rather than promising anonymous warehouse tons. Typical conversation starts around OD capped at 219 mm for this mark under Table 1 note 1. SHH STEEL can supply alternate walls and precision classes for 08Х17Т once the design pressure and corrosion allowance are clear.
If the project needs dual GOST 9940 + ASTM documentation, say so before melt. Caution: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility. SHH STEEL can produce trial lengths of 08Х17Т for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GOST 9940 08Х17Т seamless stainless steel pipe used for?
- GOST 9940 08Х17Т is hot-deformed seamless stainless pipe for corrosion-resistant and heat-resistant CIS fluid service — heat-exchanger shells on CIS BOMs, nitric-adjacent equipment notes, and ferritic replacements where nickel must stay low. Role summary: Ti-stabilised 17% Cr ferritic seamless pipe for heat-transfer and mildly oxidising aqueous duty. It is a GOST product standard grade (chemistry from GOST 5632), not an automatic ASTM A312 certificate.
-
Is GOST 9940 08Х17Т seamless only, or does it cover welded pipe?
- Seamless only — and specifically hot-deformed. Cold- and warm-deformed pipe of related marks belongs under GOST 9941-81. SHH STEEL can produce and supply the hot-deformed seamless route for 08Х17Т when the mill can meet the ordered size and tests. Welded pipe is outside both 9940 and 9941.
-
Is heat treatment mandatory for 08Х17Т under GOST 9940?
- No. Clause 2.1 lets pipes ship heat-treated or without heat treatment as the order states. Guidance for this mark: Ferritic anneal when ordered; Ti binds carbon for weldability. Certificate wording should match the treatment actually performed — or explicitly state without heat treatment. Delivery: as ordered — heat-treated or without heat treatment.
-
How does 08Х17Т compare with sister grades 12Х17, 15Х25Т, 08Х13?
- 08Х17Т is filed as ferritic chromium (Ti-stabilised). Typical sisters on the same RFQ are 12Х17, 15Х25Т, 08Х13. Design caution: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility Pick the sister when the medium or diameter cap outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 08Х17Т?
- Expect GOST 5632 cast analysis (from the billet document), room-temperature tensile results (Table 3 Rm and δ5), dimensions, and every optional hydro, UT, flattening, IGC, or yield test actually ordered. Documents follow GOST 10692 or EN 10204 3.1 style when specified. Party size max 200 pieces.
-
Is 430Ti / UNS S43036 (approx) the same as ordering 08Х17Т?
- No. 430Ti / UNS S43036 (approx) is a commercial cross-walk for body text. The purchase order should lock GOST 9940 and Cyrillic 08Х17Т so cast limits, hot-deformed tensile floors, and optional HT are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GOST 9940 08Х17Т?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 08Х17Т within Table 1 practice, respecting the mark’s diameter cap (≤219 mm per Table 1 note 1). Size context: OD capped at 219 mm for this mark under Table 1 note 1. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue. Random length typically 1.5–10 m.
-
How should 08Х17Т be welded on site?
- Shop guidance: matching ferritic or 430Ti-class fillers; low heat input; Ti already on the cast analysis. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, sulphur ≤0.020%, or anneal practice as applicable. Caution: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility
-
When should I choose a Mo-bearing or duplex grade instead of 08Х17Т?
- Move when chloride pitting, crevice attack, reducing-acid risk, or strength demand exceeds what ferritic chromium (Ti-stabilised) practice can defend for the temperature and stress state. Caution for this mark: ferritic toughness and grain growth after high heat input — Ti helps welds but does not create austenitic ductility Sister pointers: 12Х17, 15Х25Т, 08Х13. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GOST 9940 08Х17Т with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GOST 9940 08Х17Т does not clear ASTM A312 acceptance by default. State both standards, sizes, and test scopes before melt.
-
How does GOST 9940 08Х17Т differ from GOST 9941 of the same mark?
- GOST 9940 is hot-deformed (OD 57–325 mm, wall 3.5–32 mm, HT optional); GOST 9941 is cold/warm deformed (smaller OD, thinner wall, HT mandatory by default) with different Rm/δ5 pairs for most marks. SHH STEEL can produce and supply either standard when the PO names it clearly — do not mix certificates for 08Х17Т.
Conclusion
GOST 9940 08Х17Т is hot-deformed seamless stainless steel pipe for CIS corrosion-resistant service — Ti-stabilised 17% Cr ferritic seamless pipe for heat-transfer and mildly oxidising aqueous duty. SHH STEEL can produce and supply it in the hot-deformed seamless route with the heat-treatment choice, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 12Х17, 15Х25Т, 08Х13. Related ASTM A312 pages share chemistry families but not GOST acceptance text. Email admin@steelspecs.com with OD × wall, precision class, HT yes/no, and medium notes to start the quote.