GOST 9940 Stainless Steel Products
SHH STEEL offers GOST 9940-compliant 304/316 stainless steel tubes. GOST 9940 specifies seamless corrosion-resistant and heat-resistant stainless steel tubes for high-temperature and high-pressure environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GOST 9940 10Х23Н18 Seamless Stainless Steel Pipe
GOST 9940 10Х23Н18 seamless stainless steel pipe (310 / UNS S31000 family (approx)), austenitic heat-resisting 25-20 class, GOST 5632 cast analysis, Rm min 491 N/mm² / δ5 min 37%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.View More -
GOST 9940 04Х18Н10 Seamless Stainless Steel Pipe
GOST 9940 04Х18Н10 seamless stainless steel pipe (304L / UNS S30403 (approx)), austenitic low-carbon 18-8, GOST 5632 cast analysis, Rm min 441 N/mm² / δ5 min 40%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.View More -
GOST 9940 15Х25Т Seamless Stainless Steel Pipe
GOST 9940 15Х25Т seamless stainless steel pipe (446Ti / UNS S44600 family (approx)), ferritic high-chromium (Ti-stabilised), GOST 5632 cast analysis, Rm min 441 N/mm² / δ5 min 17%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.View More -
GOST 9940 15Х28 Seamless Stainless Steel Pipe
GOST 9940 15Х28 seamless stainless steel pipe (446 / UNS S44600 (approx)), ferritic high-chromium, GOST 5632 cast analysis, Rm min 441 N/mm² / δ5 min 17%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.View More -
GOST 9940 12Х17 Seamless Stainless Steel Pipe
GOST 9940 12Х17 seamless stainless steel pipe (430 / UNS S43000 (approx)), ferritic chromium, GOST 5632 cast analysis, Rm min 441 N/mm² / δ5 min 17%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.View More -
GOST 9940 12Х13 Seamless Stainless Steel Pipe
GOST 9940 12Х13 seamless stainless steel pipe (410 / UNS S41000 (approx)), martensitic chromium, GOST 5632 cast analysis, Rm min 392 N/mm² / δ5 min 21%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.View More -
GOST 9940 08Х17Т Seamless Stainless Steel Pipe
GOST 9940 08Х17Т seamless stainless steel pipe (430Ti / UNS S43036 (approx)), ferritic chromium (Ti-stabilised), GOST 5632 cast analysis, Rm min 372 N/mm² / δ5 min 17%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.View More -
GOST 9940 08Х13 Seamless Stainless Steel Pipe
GOST 9940 08Х13 seamless stainless steel pipe (410S / UNS S41008 (approx)), ferritic-martensitic chromium, GOST 5632 cast analysis, Rm min 372 N/mm² / δ5 min 22%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.View More
GOST 9940 Stainless Steel Products
Stainless Steel Pipes and Tubes
SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.