GB/T 713 07Cr2AlMoR Cr-Al-Mo pressure vessel steel plate, sulfur-corrosion resistant, normalized and tempered, SHH STEEL

GB/T 713 07Cr2AlMoR Steel Plate | 07Cr2AlMoR Vessel Plate

GB/T 713 07Cr2AlMoR is Chinese Cr-Al-Mo boiler and pressure-vessel plate. Yield is 260 MPa at 6–36 mm. Tensile is 420–580 MPa. SHH STEEL supplies 07Cr2AlMoR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
Keywords
GB/T 713 07Cr2AlMoR, 07Cr2AlMoR, GB/T 713.2 07Cr2AlMoR, 07Cr2AlMoR steel plate, 07Cr2AlMoR vessel plate, 07Cr2AlMoRE
Equivalent Grades:
EN — / ASTM — / JIS — / GB/T 713 (unique, no direct EN/ASTM equivalent) — Material Specification: GB/T 713-2023 — Delivery: Normalized + Tempered (N+T) or Quenched + Tempered (Q+T) as specified
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
Cr-Al-Mo Pressure-Vessel Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 713 07Cr2AlMoR Steel?

GB/T 713 07Cr2AlMoR, also written GB/T 713.2 07Cr2AlMoR, 07Cr2AlMoRE and 07Cr2AlMoR steel plate, is a Chinese low-carbon Cr-Al-Mo boiler and pressure-vessel plate. Current product rules sit in GB/T 713.2-2023. Buyers still search GB/T 713. The name itself is the search term: about 0.07% C, 2% Cr, Al, Mo, and R for vessel. Yield is 260 MPa at 6–36 mm. Tensile is 420–580 MPa. Delivery is normalizing plus tempering. Tempering shall not be lower than 680 °C. Impact is commonly 20 °C, 47 J. Rare earth may be added when the buyer writes it. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade.

A purchase order that only says “CrAlMo vessel plate” is incomplete. Write GB/T 713 07Cr2AlMoR. Do not ship 12Cr2Mo1R against a 07Cr2AlMoR drawing. Do not ship 15CrMoR against a 07Cr2AlMoR drawing. Do not ship Q345R against a 07Cr2AlMoR drawing. Aluminum is required here. Carbon is kept very low. Molybdenum is 0.30–0.50%, not the 0.90–1.10% band used on 12Cr2Mo1R.

07Cr2AlMoR was added in GB/T 713-2014 together with Q420R and 12Cr2Mo1VR. It is used on spherical tanks and petrochemical vessels that want a low-carbon 2% Cr plate with aluminum, not a classic 2.25Cr-1Mo plate.

This page is not carbon Q245R / Q345R. It is not Mn-Mo-Nb 18MnMoNbR. It is not 2.25Cr-1Mo 12Cr2Mo1R. It is not QT alloy under ASME SA543.

Company scope: global steel mill sourcing partner – SHH STEEL.

Material Specification

Specification ElementRequirementSHH STEEL Compliance
GradeGB/T 713 07Cr2AlMoRConfirmed
Product SpecificationGB/T 713.2-2023 (buyers still search GB/T 713)Applied
Service ideaLow-carbon Cr-Al-Mo vesselsConfirmed
Steel typeKilled Cr-Al-Mo vessel plateConfirmed
Usual deliveryN+T, temper ≥680 °CConfirmed
Yield idea260 MPa at 6–36 mmConfirmed
Tensile420–580 MPa at 6–36 mmConfirmed
Impact idea20 °C / 47 JConfirmed
Rare earthOptional, when writtenAs ordered
Supply roleGlobal steel mill sourcing partnerSHH STEEL
MarketsAmericas, Europe, Middle East, Africa, AsiaFOB / CIF as ordered
CertificationEN 10204 3.1 or 3.2 / third-partyAs ordered

This plate sits in pressure vessel steel plates. ASME comparisons belong on ASME SA387, not as automatic substitutes. There is no exact SA-387 twin for the Al addition.

Chemical Composition

GB/T 713 07Cr2AlMoR heat analysis follows GB/T 713.2 Table 1. Product analysis follows the permitted deviations in GB/T 713.1. Write “heat + product analysis” on the order if both are required.

Heat Analysis and Product Analysis — GB/T 713 07Cr2AlMoR

ElementHeat Analysis (%)Product Analysis, when ordered (%)
Carbon (C), max0.090.11
Silicon (Si)0.20 – 0.500.18 – 0.55
Manganese (Mn)0.40 – 0.900.35 – 0.95
Phosphorus (P), max0.0200.025
Sulfur (S), max0.0100.015
Chromium (Cr)2.00 – 2.401.95 – 2.45
Molybdenum (Mo)0.30 – 0.500.28 – 0.53
Acid-soluble aluminum (Alt)0.30 – 0.500.28 – 0.53
Copper (Cu), max0.300.34
Nickel (Ni), max0.300.34
Rare earthOptionalWhen written

Carbon is kept at 0.09% max. Aluminum is required at 0.30–0.50%. That package is the difference versus 12Cr2Mo1R. GB/T 713.2 also allows an appropriate amount of rare earth when the buyer writes it. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.

Mechanical Properties

Yield starts at 260 MPa at 6–36 mm and falls as thickness rises.

Tensile and Yield — GB/T 713 07Cr2AlMoR

Thickness (mm)Yield min (MPa)Tensile (MPa)
6 – 36260420 – 580
36 – 60250410 – 570
Density7.85 g/cm³7.85 g/cm³

Elongation is commonly 21% min. Impact is 20 °C, 47 J. Elevated-temperature proof stress is published for 200–300 °C.

Elevated-temperature yield (typical published minima, MPa, >20–60 mm)

200 °C250 °C300 °C
195185175

Do not quote 260 MPa yield on a 50 mm plate. Do not treat 420–580 MPa tensile as permission to stamp SA387 Gr.22 Cl.2 or SA387 Gr.12 Cl.2. Those books do not use this band.

Material Comparison

radeRouteStrength ideaSwap?
GB/T 713 Q345RC-Mn vessel345 / 510–640No
GB/T 713 15CrMoR1.25Cr-0.5Mo295 / 450–590No
GB/T 713 12Cr2Mo1R2.25Cr-1Mo310 / 520–680No
GB/T 713 07Cr2AlMoRCr-Al-Mo260 / 420–580This page
GB/T 713 12Cr2Mo1VR2.25Cr-1Mo-VDifferent V packageNo
SA387 Gr.22 Cl.22.25Cr-1Mo ASMENo required AlNo

Equivalent Material Grades

These names are project-comparison grades. They are not automatic substitutes. Dual marking is uncommon on 07Cr2AlMoR because the aluminum addition is not a standard SA-387 requirement.

DesignationStandard / regionNotes
GB/T 713 07Cr2AlMoRGB/T 713.2-2023Name on this page
GB/T 713-2014 07Cr2AlMoRPrevious Chinese editionSame commercial name
07Cr2AlMoRECommercial RE-bearing markingRare earth when ordered
12Cr2Mo1RGB/T 713.22.25Cr-1Mo, no required Al
12Cr2Mo1VRGB/T 713.22.25Cr-1Mo-V
15CrMoR / 14Cr1MoRGB/T 713.21.25Cr-0.5Mo
SA387 Gr.22 Cl.2SA-3872.25Cr-1Mo, no Al requirement
SA387 Gr.12 Cl.2SA-3871Cr-0.5Mo
SA387 Gr.11 Cl.2SA-3871.25Cr-0.5Mo
10CrMo9-10EN 10028-22.25Cr-1Mo, no Al requirement
SA516 Gr.70SA-516Carbon vessel
SA662 Gr.CSA-662Low-temp carbon vessel
ASTM A36 steel plateA36Structural, not vessel

ASME SA515 and ASME SA203 are not 07Cr2AlMoR.

Cr-Al-Mo Pressure-Vessel Service

GB/T 713 07Cr2AlMoR is selected for spherical tanks, petrochemical shells and other pressure equipment that name the Chinese low-carbon Cr-Al-Mo vessel book. Aluminum and 2% chromium are the reason this grade exists. It is not a substitute for 12Cr2Mo1R hydrogen-service 2.25Cr-1Mo plate unless the drawing says so.

It is not automatically an ASME Section VIII plate. If the vessel is ASME, the drawing should name an ASME or ASTM grade. Do not assume SA387 Gr.22 Cl.2 covers the Al addition.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia. It is not nickel low-temp plate like SA203 Gr.D. It is not QT Ni-Cr-Mo like SA543 Type B Cl.1. Stainless inquiries belong on ASME SA240 or ASTM A240.

Weldability

07Cr2AlMoR is killed low-carbon Cr-Al-Mo vessel plate. Welding is production welding, and Code welding when the equipment is a vessel.

Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the low-carbon Cr-Al-Mo content, not a 12Cr2Mo1R 2.25Cr-1Mo procedure and not a plain Q345R procedure. Preheat and PWHT follow thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is normalized-and-tempered GB/T 713 07Cr2AlMoR. Tempering shall not be lower than 680 °C. As-rolled shipment is not the default.

If the vessel will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the 650 °C temper route used on 15CrMoR / 14Cr1MoR. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.

The certificate lists GB/T 713 07Cr2AlMoR; heat number; heat analysis; product analysis when ordered; Alt; rare earth when added; tensile results to the correct thickness column; N+T and tempering temperature; impact at 20 °C or the named temperature; elevated-temperature proof stress when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for 07Cr2AlMoR vessel plate:

  • Thickness: commonly 6 mm – 60 mm. Confirm any request above 60 mm against mill capability
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm
  • Cut-to-length plates and nest sizes inside those limits

Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.

Tolerances

Dimensional limits follow GB/T 713.1 and the mill rolling standard named on the order. Do not apply ASTM A36/A36M structural tolerances to a Chinese vessel plate without writing them. UT to GB/T 2970, JB/T 4730, EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.

Supplementary Requirements

Most export GB/T 713 07Cr2AlMoR orders add extras. SHH STEEL does not assume them.

Charpy details. Temperature, energy, location and orientation. GB default is commonly 20 °C / 47 J.

Product analysis. Add this when the destination file wants finished-plate chemistry.

Rare earth. Write it if 07Cr2AlMoRE marking is required.

Elevated-temperature proof stress. 200–300 °C or the design temperature.

Simulated PWHT. When the equipment will be stress-relieved.

NDE. UT per the named method.

Z-direction. Z15 / Z25 / Z35 when the drawing names it.

HIC / NACE / SSC / hydrogen service. Only when written.

Third-party. EN 10204 3.2, with inspectors arranged for US, Mexican, European, Middle East, Japanese or Korean documentation packages.

Applications

IndustryTypical components
Spherical tanksGB/T 713 07Cr2AlMoR shells
Petrochemical vessels07Cr2AlMoR courses
Cr-Al-Mo equipment07Cr2AlMoR plate from SHH STEEL
Fabrication07Cr2AlMoR cut to nest sizes

Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.B, A516 Grade 70, SA533 Type C Cl.1, SA517 Gr.P, SA738 Gr.C.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers outside a single region. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to:

  • North America: USA, Mexico
  • South America: Argentina, Peru and other South American ports
  • Central America: El Salvador
  • Europe: Spain, Netherlands, Germany and surrounding ports
  • Middle East: UAE, Saudi Arabia and nearby Gulf ports
  • Africa: South Africa
  • South / Southeast Asia: India, Thailand, Singapore, Vietnam, Philippines
  • East Asia: Japan, Korea

Typical trade terms: FOB Shanghai, CIF Houston, CIF Rotterdam, CIF Jebel Ali, plus Manzanillo, Callao, Buenos Aires, Barcelona, Durban, Laem Chabang, Ho Chi Minh, Manila, Mumbai, Yokohama and Busan.

Typical lead time for GB/T 713 07Cr2AlMoR:

  • Ex-stock: about 5–7 days
  • Mill rolling, standard N+T: about 45 days
  • Simulated PWHT, 3.2 or extra NDE: about 2 months

Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading. Packing is seaworthy, with edge protection and marking in English as specified on the order.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS / GB steel to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia. On GB/T 713 07Cr2AlMoR that means mill pricing, 07Cr2AlMoR chemistry reported as heat analysis and as product analysis when ordered, recorded N+T with temper ≥680 °C, tensile results to the correct thickness column, 260 MPa yield at 6–36 mm, 3.1 as standard and 3.2 when specified.

We keep the grade on the order. 07Cr2AlMoR is not 12Cr2Mo1R. 07Cr2AlMoR is not 12Cr2Mo1VR. 07Cr2AlMoR is not 15CrMoR. 07Cr2AlMoR is not Q345R. 07Cr2AlMoR is not SA387 Gr.22 Cl.2. If the drawing names 2.25Cr-1Mo without aluminum, we will not ship 07Cr2AlMoR and call it close.

Company scope: global steel mill sourcing partner – SHH STEEL.

FAQ

What is 07Cr2AlMoR steel plate?
07Cr2AlMoR is a GB/T 713 / GB/T 713.2 low-carbon Cr-Al-Mo boiler and pressure-vessel plate. Yield is 260 MPa at 6–36 mm and tensile is 420–580 MPa. Delivery is N+T with temper not lower than 680 °C. SHH STEEL supplies this plate as a global steel mill sourcing partner.
Is 07Cr2AlMoR the same as 07Cr2AlMoRE?
07Cr2AlMoRE is the commercial marking when rare earth is added. GB/T 713.2 allows rare earth on 07Cr2AlMoR when the buyer writes it.
What is the equivalent of 07Cr2AlMoR?
There is no exact ASME twin because of the required aluminum. Related comparisons are 12Cr2Mo1R and SA387 Grade 22, but those grades do not require Al. Dual marking is uncommon.
Does GB/T 713 give product analysis for 07Cr2AlMoR?
Heat analysis is in GB/T 713.2. Product analysis deviations follow GB/T 713.1. SHH STEEL reports both when written on the purchase order.
How is 07Cr2AlMoR different from 12Cr2Mo1R?
12Cr2Mo1R is 2.25Cr-1Mo with higher molybdenum and no required aluminum. 07Cr2AlMoR keeps carbon at 0.09% max and requires Alt 0.30–0.50%. Strength is also lower.
Can SHH STEEL ship 07Cr2AlMoR to Mexico, South America or Southeast Asia?
Yes. SHH STEEL has supplied plates to Mexico, Argentina, El Salvador, Peru, Spain, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea, as well as the USA, Europe and the Middle East.
What is the delivery time for 07Cr2AlMoR?
Ex-stock about 5–7 days. Standard N+T mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.
Can SHH STEEL issue EN 10204 3.2 for 07Cr2AlMoR?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged when written on the order.

Conclusion

GB/T 713 07Cr2AlMoR Steel Plate, also searched as 07Cr2AlMoRE, is Chinese low-carbon Cr-Al-Mo boiler and pressure-vessel plate at the 260 MPa yield step, 420–580 MPa tensile at 6–36 mm, N+T delivery with temper not lower than 680 °C. Whether the inquiry says GB/T 713 07Cr2AlMoR, GB/T 713.2 07Cr2AlMoR or 07Cr2AlMoR Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 07Cr2AlMoR chemistry, heat and product analysis when ordered, recorded N+T, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies GB/T 713 07Cr2AlMoR Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.

Contact SHH STEEL for mill rolling, stock inquiry, N+T, rare-earth addition, 3.2 inspection or a quotation.

GB/T 713 07Cr2AlMoR Steel Plate, GB/T 713.2 07Cr2AlMoR, 07Cr2AlMoRE, 07Cr2AlMoR vessel plate, 07Cr2AlMoR supplier, global steel mill sourcing partner SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X