GB/T 713 13MnNiMoR Steel Plate | 13MnNiMoR Vessel Plate
What is GB/T 713 13MnNiMoR Steel?
GB/T 713 13MnNiMoR, also written GB/T 713.2 13MnNiMoR and 13MnNiMoR steel plate, is a Chinese Mn-Ni-Mo boiler and pressure-vessel plate. Current product rules sit in GB/T 713.2-2023. Buyers still search GB/T 713. The name itself is the search term: about 0.13% C, Mn, Ni, Mo, and R for vessel. Yield is 390 MPa at 30–100 mm. Tensile is 570–720 MPa. Delivery is normalizing plus tempering. Tempering shall not be lower than 620 °C. Impact is commonly 0 °C, 47 J. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade.
A purchase order that only says “MnNiMo vessel plate” is incomplete. Write GB/T 713 13MnNiMoR. Do not ship Q345R or Q370R against a 13MnNiMoR drawing. Do not ship 18MnMoNbR against a 13MnNiMoR drawing. Do not ship SA302 Gr.C and stamp 13MnNiMoR because both contain nickel and molybdenum.
This page is not Q245R / Q345R carbon vessel plate. It is not Cr-Mo 15CrMoR. It is not QT alloy under ASME SA387. It is not low-temperature 16MnDR under GB/T 713.3.
Company scope: global steel mill sourcing partner – SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | GB/T 713 13MnNiMoR | Confirmed |
| Product Specification | GB/T 713.2-2023 (buyers still search GB/T 713) | Applied |
| Service idea | Mn-Ni-Mo boiler and pressure vessels | Confirmed |
| Steel type | Killed Mn-Ni-Mo vessel plate | Confirmed |
| Usual delivery | N+T, temper ≥620 °C | Confirmed |
| Yield idea | 390 MPa at 30–100 mm | Confirmed |
| Tensile | 570–720 MPa | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | Americas, Europe, Middle East, Africa, Asia | FOB / CIF as ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates. ASME comparisons belong on ASME SA302 and ASME SA533, not as automatic substitutes.
Chemical Composition
GB/T 713 13MnNiMoR heat analysis follows GB/T 713.2 Table 1. Product analysis follows the permitted deviations in GB/T 713.1. Write “heat + product analysis” on the order if both are required.
Heat Analysis and Product Analysis — GB/T 713 13MnNiMoR
| Element | Heat Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), max | 0.15 | 0.17 |
| Silicon (Si) | 0.15 – 0.50 | 0.13 – 0.55 |
| Manganese (Mn) | 1.20 – 1.60 | 1.15 – 1.70 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.010 | 0.015 |
| Nickel (Ni) | 0.60 – 1.00 | 0.55 – 1.05 |
| Chromium (Cr) | 0.20 – 0.40 | 0.18 – 0.43 |
| Molybdenum (Mo) | 0.20 – 0.40 | 0.18 – 0.43 |
| Niobium (Nb) | 0.005 – 0.020 | 0.004 – 0.025 |
| Copper (Cu), max | 0.30 | 0.34 |
Nickel, chromium and molybdenum are required. That is the difference versus 18MnMoNbR, which uses niobium instead of nickel. Do not treat 18MnMoNbR chemistry as 13MnNiMoR. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.
Mechanical Properties
Yield starts at 390 MPa at 30–100 mm and falls as thickness rises.
Tensile and Yield — GB/T 713 13MnNiMoR
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) |
|---|---|---|
| 30 – 100 | 390 | 570 – 720 |
| 100 – 150 | 380 | 570 – 720 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Elongation is commonly 18% min. Impact is 0 °C, 47 J. Elevated-temperature proof stress is published for this grade. Write the design temperature on the order if the vessel file needs those values.
Typical published elevated-temperature yield minima at 30–100 mm: about 355 MPa at 200 °C, 350 MPa at 250 °C, 345 MPa at 300 °C, 335 MPa at 350 °C, 305 MPa at 400 °C. Confirm the exact GB/T 713.2 Table 3 column for the ordered thickness.
Do not treat 570–720 MPa tensile as permission to stamp SA302 Gr.C, SA302 Gr.D or SA533 Type B Cl.1 without checking yield, impact and PWHT.
Material Comparison
| Grade | Route | Strength idea | Swap? |
|---|---|---|---|
| GB/T 713 Q345R | C-Mn vessel | 345 / 510–640 | No |
| GB/T 713 18MnMoNbR | Mn-Mo-Nb vessel | 400 / 570–720 | No |
| GB/T 713 13MnNiMoR | Mn-Ni-Mo vessel | 390 / 570–720 | This page |
| SA302 Gr.C | Mn-Mo-Ni vessel | Related idea | Comparison only |
| SA533 Type B Cl.1 | Mn-Mo-Ni QT vessel | Different heat treatment | No |
| 15CrMoR | Cr-Mo vessel | Different alloy | No |
Equivalent Material Grades
These names are project-comparison grades. They are not automatic substitutes.
| Designation | Standard / region | Notes |
|---|---|---|
| GB/T 713 13MnNiMoR | GB/T 713.2-2023 | Name on this page |
| GB/T 713-2014 13MnNiMoR | Previous Chinese edition | Same commercial name |
| SA302 Gr.C | SA-302 | Mn-Mo-Ni vessel comparison |
| SA302 Gr.D | SA-302 | Higher Ni Mn-Mo-Ni |
| SA302 Gr.B | SA-302 | Mn-Mo, little or no Ni |
| SA533 Type A Cl.1 | SA-533 | Mn-Mo-Ni QT vessel |
| SA533 Type B Cl.1 | SA-533 | Higher Ni QT vessel |
| SA533 Type C Cl.1 | SA-533 | Higher Ni QT vessel |
| ASTM A302 | A302 family | ASTM twin of SA302 |
| ASTM A533 | A533 family | ASTM twin of SA533 |
| 18MnMoNbR | GB/T 713.2 | Nb sister, no required Ni |
| Q345R / Q370R / Q420R | GB/T 713.2 | Carbon / fine-grain sisters |
| 15CrMoR / 14Cr1MoR | GB/T 713.2 | Cr-Mo, not Mn-Ni-Mo |
| SA387 Gr.12 Cl.2 | SA-387 | Cr-Mo, different alloy |
| SA516 Gr.70 | SA-516 | Carbon vessel, no Ni-Mo |
| JIS G3119 SBV2 | JIS G3119 | Mn-Mo-Ni vessel comparison |
| ASTM A36 steel plate | A36 | Structural, not vessel |
ASME SA515, ASME SA387 Grade 22 and ASME SA203 are not 13MnNiMoR.
Mn-Ni-Mo Pressure-Vessel Service
GB/T 713 13MnNiMoR is selected for boilers, drums, thick shells and other pressure equipment that name the Chinese Mn-Ni-Mo vessel book. Nickel supports toughness. Molybdenum supports elevated-temperature strength. It is not automatically an ASME Section VIII plate. If the vessel is ASME, the drawing should name an ASME or ASTM grade such as SA302 Gr.C, SA302 Gr.D or SA533 Type B Cl.1.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia. It is not nickel low-temp plate like SA203 Gr.D. It is not QT Ni-Cr-Mo like SA543 Type B Cl.1. It is not Cr-Mo like SA387 Gr.22 Cl.2. Stainless inquiries belong on ASME SA240 or ASTM A240.
Weldability
13MnNiMoR is killed Mn-Ni-Mo vessel plate. Welding is production welding, and Code welding when the equipment is a vessel.
Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the 570–720 MPa tensile band and the Ni-Mo content, not a plain Q345R procedure and not a SA387 Gr.22 Cl.2 Cr-Mo procedure. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized-and-tempered GB/T 713 13MnNiMoR. Tempering shall not be lower than 620 °C. As-rolled shipment is not the default.
If the vessel will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the carbon normalize route used on Q345R and not the Cr-Mo N+T route used on 15CrMoR. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.
The certificate lists GB/T 713 13MnNiMoR; heat number; heat analysis; product analysis when ordered; tensile results to the correct thickness column; N+T and tempering temperature; impact at 0 °C or the named temperature; elevated-temperature proof stress when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for 13MnNiMoR vessel plate:
- Thickness: commonly 30 mm – 150 mm. Confirm any request outside that band against mill capability
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
- Cut-to-length plates and nest sizes inside those limits
Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.
Tolerances
Dimensional limits follow GB/T 713.1 and the mill rolling standard named on the order. Do not apply ASTM A36/A36M structural tolerances to a Chinese vessel plate without writing them. UT to GB/T 2970, JB/T 4730, EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.
Supplementary Requirements
Most export GB/T 713 13MnNiMoR orders add extras. SHH STEEL does not assume them.
Charpy details. Temperature, energy, location and orientation. GB default is commonly 0 °C / 47 J.
Product analysis. Add this when the destination file wants finished-plate chemistry.
Elevated-temperature proof stress. Design temperature as written.
Simulated PWHT. When the equipment will be stress-relieved.
NDE. UT per the named method.
Z-direction. Z15 / Z25 / Z35 when the drawing names it.
HIC / NACE / SSC. Only when written.
Third-party. EN 10204 3.2, with inspectors arranged for US, Mexican, European, Middle East, Japanese or Korean documentation packages.
Applications
| Industry | Typical components |
|---|---|
| Mn-Ni-Mo vessels | GB/T 713 13MnNiMoR shells |
| Boilers and thick drums | 13MnNiMoR courses |
| Elevated-temperature equipment | 13MnNiMoR plate from SHH STEEL |
| Fabrication | 13MnNiMoR cut to nest sizes |
Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.A, A516 Grade 70, SA533 Type C Cl.2, SA517 Gr.P, SA738 Gr.C.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers outside a single region. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to:
- North America: USA, Mexico
- South America: Argentina, Peru and other South American ports
- Central America: El Salvador
- Europe: Spain, Netherlands, Germany and surrounding ports
- Middle East: UAE, Saudi Arabia and nearby Gulf ports
- Africa: South Africa
- South / Southeast Asia: India, Thailand, Singapore, Vietnam, Philippines
- East Asia: Japan, Korea
Typical trade terms: FOB Shanghai, CIF Houston, CIF Rotterdam, CIF Jebel Ali, plus Manzanillo, Callao, Buenos Aires, Barcelona, Durban, Laem Chabang, Ho Chi Minh, Manila, Mumbai, Yokohama and Busan.
Typical lead time for GB/T 713 13MnNiMoR:
- Ex-stock: about 5–7 days
- Mill rolling, standard N+T: about 45 days
- Simulated PWHT, 3.2 or extra NDE: about 2 months
Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading. Packing is seaworthy, with edge protection and marking in English as specified on the order.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS / GB steel to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia. On GB/T 713 13MnNiMoR that means mill pricing, 13MnNiMoR chemistry reported as heat analysis and as product analysis when ordered, recorded N+T with temper ≥620 °C, tensile results to the correct thickness column, 390 MPa yield at 30–100 mm, 3.1 as standard and 3.2 when specified.
We keep the grade on the order. 13MnNiMoR is not Q345R. 13MnNiMoR is not 18MnMoNbR. 13MnNiMoR is not 15CrMoR. 13MnNiMoR is not SA302 Gr.C unless both books are met. 13MnNiMoR is not SA387 Gr.22 Cl.2.
Company scope: global steel mill sourcing partner – SHH STEEL.
FAQ
-
What is 13MnNiMoR steel plate?
- 13MnNiMoR is a GB/T 713 / GB/T 713.2 Mn-Ni-Mo boiler and pressure-vessel plate. Yield is 390 MPa at 30–100 mm and tensile is 570–720 MPa. Delivery is N+T with temper not lower than 620 °C. SHH STEEL supplies this plate as a global steel mill sourcing partner.
-
What is the equivalent of 13MnNiMoR?
- The usual ASME comparison is SA302 Grade C. Other comparisons are SA302 Grade D and SA533 Type B Class 1. Dual marking is possible only when both books are fully met.
-
Does GB/T 713 give product analysis for 13MnNiMoR?
- Heat analysis is in GB/T 713.2. Product analysis deviations follow GB/T 713.1. SHH STEEL reports both when written on the purchase order.
-
How is 13MnNiMoR different from 18MnMoNbR?
- 13MnNiMoR requires nickel, chromium and molybdenum. 18MnMoNbR requires molybdenum and niobium and does not require nickel
-
How is 13MnNiMoR different from Q345R?
- Q345R is C-Mn vessel plate without required Ni-Mo. 13MnNiMoR requires nickel and molybdenum and ships N+T.
-
Can SHH STEEL ship 13MnNiMoR to Mexico, South America or Southeast Asia?
- Yes. SHH STEEL has supplied plates to Mexico, Argentina, El Salvador, Peru, Spain, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea, as well as the USA, Europe and the Middle East.
-
What is the delivery time for 13MnNiMoR?
- Ex-stock about 5–7 days. Standard N+T mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.
-
Can SHH STEEL issue EN 10204 3.2 for 13MnNiMoR?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged when written on the order.
Conclusion
GB/T 713 13MnNiMoR Steel Plate is Chinese Mn-Ni-Mo boiler and pressure-vessel plate at the 390 MPa yield step, 570–720 MPa tensile, N+T delivery with temper not lower than 620 °C. Whether the inquiry says GB/T 713 13MnNiMoR, GB/T 713.2 13MnNiMoR or 13MnNiMoR Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 13MnNiMoR chemistry, heat and product analysis when ordered, recorded N+T, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies GB/T 713 13MnNiMoR Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.
Contact SHH STEEL for mill rolling, stock inquiry, N+T, elevated-temperature testing, 3.2 inspection or a quotation.