What is GB/T 713 12Cr2Mo1VR Steel ?
GB/T 713 12Cr2Mo1VR, also written GB/T 713.2 12Cr2Mo1VR and 12Cr2Mo1VR steel plate, is a Chinese 2.25Cr-1Mo-V boiler and pressure-vessel plate. Current product rules sit in GB/T 713.2-2023. Buyers still search GB/T 713. The name itself is the search term: about 0.12% C, 2% Cr, 1% Mo, V, and R for vessel. Yield is 310 MPa in the usual thickness band. Tensile is 520–680 MPa. Delivery is normalizing plus tempering. Tempering shall not be lower than 680 °C. Impact is commonly 20 °C, 47 J. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade. Plate is produced to GB/T 713 / GB/T 713.2 and shipped to buyers in the USA, Mexico, South America, Europe, Middle East, Africa and Asia.
A purchase order that only says “2.25Cr-1Mo-V vessel plate” is incomplete. Write GB/T 713 12Cr2Mo1VR. Do not ship 12Cr2Mo1R against a 12Cr2Mo1VR drawing. Do not ship 12Cr1MoVR against a 12Cr2Mo1VR drawing. Do not ship 15CrMoR or 14Cr1MoR against a 12Cr2Mo1VR drawing. Vanadium is required here. Chromium is near 2.25%, not 1%.
12Cr2Mo1VR is the vanadium-bearing sister of 12Cr2Mo1R. It is the plate named when the Chinese vessel book still applies and the alloy is 2.25Cr-1Mo-V, not plain 2.25Cr-1Mo.
This page is not carbon Q245R / Q345R. It is not Mn-Mo-Nb 18MnMoNbR. It is not 1Cr-0.3Mo-V 12Cr1MoVR. It is not QT alloy under ASME SA543.
Company scope: global steel mill sourcing partner – SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | GB/T 713 12Cr2Mo1VR | Confirmed |
| Product Specification | GB/T 713.2-2023 (buyers still search GB/T 713) | Applied |
| Service idea | 2.25Cr-1Mo-V boiler and pressure vessels | Confirmed |
| Steel type | Killed Cr-Mo-V vessel plate | Confirmed |
| Usual delivery | N+T, temper ≥680 °C | Confirmed |
| Yield idea | 310 MPa in the usual band | Confirmed |
| Tensile | 520–680 MPa | Confirmed |
| Impact idea | 20 °C / 47 J | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | Americas, Europe, Middle East, Africa, Asia | FOB / CIF as ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates and ASME SA387 comparison work. ASME comparisons belong on ASME SA387 Grade 22 and ASME SA542, not as automatic substitutes.
Chemical Composition
GB/T 713 12Cr2Mo1VR heat analysis follows GB/T 713.2 Table 1. Product analysis follows the permitted deviations in GB/T 713.1. Write “heat + product analysis” on the order if both are required.
Heat Analysis and Product Analysis — GB/T 713 12Cr2Mo1VR
| Element | Heat Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C) | 0.11 – 0.15 | 0.09 – 0.17 |
| Silicon (Si), max | 0.10 | 0.15 |
| Manganese (Mn) | 0.30 – 0.60 | 0.25 – 0.65 |
| Phosphorus (P), max | 0.010 | 0.015 |
| Sulfur (S), max | 0.010 | 0.015 |
| Chromium (Cr) | 2.00 – 2.50 | 1.95 – 2.55 |
| Molybdenum (Mo) | 0.90 – 1.10 | 0.87 – 1.13 |
| Vanadium (V) | 0.25 – 0.35 | 0.23 – 0.38 |
| Copper (Cu), max | 0.20 | 0.24 |
| Nickel (Ni), max | 0.25 | 0.29 |
Vanadium is required. Chromium near 2.25% and molybdenum near 1.00% are required. Silicon is kept low on many mill tables for this grade. That package is the difference versus 12Cr2Mo1R, which does not use V as the defining addition, and versus 12Cr1MoVR, which is 1Cr-0.3Mo-V. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.
Mechanical Properties
Yield starts at 310 MPa in the usual thickness band.
Tensile and Yield — GB/T 713 12Cr2Mo1VR
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) |
|---|---|---|
| 6 – 200, usual published band | 310 | 520 – 680 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Elongation is commonly 19% min. Impact is 20 °C, 47 J. Elevated-temperature proof stress is published for this grade. Write the design temperature on the order if the vessel file needs those values.
Do not treat 520–680 MPa tensile as permission to stamp SA387 Gr.22 Cl.2 or SA542 Type C Cl.4 without checking vanadium, Class, yield, impact and PWHT. SA-387 Grade 22 does not automatically include vanadium. SA-542 Type C is a different book and a different heat-treatment route.
Material Comparison
| Grade | Route | Strength idea | Swap? |
|---|---|---|---|
| GB/T 713 12Cr2Mo1R | 2.25Cr-1Mo | 310 / 520–680 | No |
| GB/T 713 12Cr2Mo1VR | 2.25Cr-1Mo-V | 310 / 520–680 | This page |
| GB/T 713 12Cr1MoVR | 1Cr-0.3Mo-V | 245 / 440–590 | No |
| GB/T 713 15CrMoR | 1.25Cr-0.5Mo | 295 / 450–590 | No |
| SA387 Gr.22 Cl.2 | 2.25Cr-1Mo ASME | Related, V not required | Comparison only |
| SA542 Type C Cl.4 | QT Cr-Mo-V | Different book | No |
Equivalent Material Grades
These names are project-comparison grades. They are not automatic substitutes. Dual marking is possible only when chemistry, tensile, Class, impact, delivery condition and all extras fit both named editions.
| Designation | Standard / region | Notes |
|---|---|---|
| GB/T 713 12Cr2Mo1VR | GB/T 713.2-2023 | Name on this page |
| GB/T 713-2014 12Cr2Mo1VR | Previous Chinese edition | Same commercial name |
| 12Cr2Mo1R | GB/T 713.2 | Sister without required V |
| SA387 Gr.22 Cl.2 | SA-387 | 2.25Cr-1Mo, V not required |
| SA387 Gr.22 Cl.1 | SA-387 | Lower Class |
| ASTM A387 Grade 22 | ASTM A387 | ASTM twin of SA387 Gr.22 |
| SA542 Type C Cl.4 | SA-542 | QT Cr-Mo-V comparison |
| SA542 Type C Cl.4a | SA-542 | Related QT Class |
| SA832 22V | SA-832 | Cr-Mo-V vessel comparison |
| 10CrMo9-10 / 1.7380 | EN 10028-2 | 2.25Cr-1Mo, V not required |
| 12CrMoV9-10 | EN 10028-2 | Closer EN Cr-Mo-V idea |
| 12Cr1MoVR | GB/T 713.2 | 1Cr-0.3Mo-V sister |
| 15CrMoR / 14Cr1MoR | GB/T 713.2 | 1.25Cr-0.5Mo sisters |
| SA387 Gr.12 Cl.2 | SA-387 | 1Cr-0.5Mo |
| SA387 Gr.21 Cl.2 | SA-387 | 3Cr-1Mo family |
| SA516 Gr.70 | SA-516 | Carbon vessel, no Cr-Mo-V |
| JIS G4109 SCMV4 | JIS G4109 | Japanese 2.25Cr-1Mo vessel |
| ASTM A36 steel plate | A36 | Structural, not vessel |
ASME SA515 and ASME SA203 are not 12Cr2Mo1VR.
2.25Cr-1Mo-V Pressure-Vessel Service
GB/T 713 12Cr2Mo1VR is selected for boilers, hydrotreaters, heat exchangers and other pressure equipment that name the Chinese 2.25Cr-1Mo-V vessel book. Vanadium supports elevated-temperature strength and temper resistance after N+T. Chromium near 2.25% and molybdenum near 1% keep the alloy in the same family as 12Cr2Mo1R, with V as the extra addition.
It is not automatically an ASME Section VIII plate. If the vessel is ASME, the drawing should name SA387 Gr.22 Cl.2 only when vanadium is accepted, or a Cr-Mo-V book such as SA542 Type C Cl.4 or SA832 22V.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia. It is not nickel low-temp plate like SA203 Gr.D. It is not QT Ni-Cr-Mo like SA543 Type B Cl.1. It is not 1.25Cr-0.5Mo like SA387 Gr.12 Cl.2. Stainless inquiries belong on ASME SA240 or ASTM A240.
Weldability
12Cr2Mo1VR is killed 2.25Cr-1Mo-V vessel plate. Welding is production welding, and Code welding when the equipment is a vessel.
Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the 2.25Cr-1Mo-V content, not a 12Cr2Mo1R-only procedure, not a 12Cr1MoVR procedure, and not a plain Q345R procedure. Preheat and PWHT follow thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Hydrogen service, HIC and NACE extras are not automatic. Write them if the equipment file needs them.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized-and-tempered GB/T 713 12Cr2Mo1VR. Tempering shall not be lower than 680 °C. As-rolled shipment is not the default.
If the vessel will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the 650 °C temper route used on 15CrMoR / 14Cr1MoR and not the QT route used on SA542 Type C Cl.4. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.
The certificate lists GB/T 713 12Cr2Mo1VR; heat number; heat analysis; product analysis when ordered; tensile results to the correct thickness column; N+T and tempering temperature; impact at 20 °C or the named temperature; elevated-temperature proof stress when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to SA387 Gr.22 Cl.2 is available only when both books are met and vanadium is accepted.
Dimensions
Usual supply range from SHH STEEL for 12Cr2Mo1VR Cr-Mo-V vessel plate:
- Thickness: commonly 6 mm – 200 mm. Confirm any request above 150 mm against mill capability
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
- Cut-to-length plates and nest sizes inside those limits
Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.
Tolerances
Dimensional limits follow GB/T 713.1 and the mill rolling standard named on the order. Do not apply ASTM A36/A36M structural tolerances to a Chinese vessel plate without writing them. UT to GB/T 2970, JB/T 4730, EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.
Thickness tolerance, flatness and camber must be written if the destination file is tighter than the GB default. Edge condition, mill edge or cut edge, also belongs on the order.
Supplementary Requirements
Most export GB/T 713 12Cr2Mo1VR orders add extras. SHH STEEL does not assume them.
Charpy details. Temperature, energy, location and orientation. GB default is commonly 20 °C / 47 J.
Product analysis. Add this when the destination file wants finished-plate chemistry.
Elevated-temperature proof stress. Design temperature as written.
Simulated PWHT. When the equipment will be stress-relieved.
NDE. UT per the named method.
Z-direction. Z15 / Z25 / Z35 when the drawing names it.
HIC / NACE / SSC / hydrogen service. Only when written.
Third-party. EN 10204 3.2, with inspectors arranged for US, Mexican, European, Middle East, Japanese or Korean documentation packages.
Applications
| Industry | Typical components |
|---|---|
| 2.25Cr-1Mo-V vessels | GB/T 713 12Cr2Mo1VR shells |
| Hydrotreaters and boilers | 12Cr2Mo1VR courses |
| Elevated-temperature equipment | 12Cr2Mo1VR plate from SHH STEEL |
| Dual-certified export | 12Cr2Mo1VR / SA387 Gr.22 when V is accepted |
Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.B, A516 Grade 70, SA533 Type C Cl.1, SA517 Gr.P, SA738 Gr.C.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers outside a single region. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to:
- North America: USA, Mexico
- South America: Argentina, Peru and other South American ports
- Central America: El Salvador
- Europe: Spain, Netherlands, Germany and surrounding ports
- Middle East: UAE, Saudi Arabia and nearby Gulf ports
- Africa: South Africa
- South / Southeast Asia: India, Thailand, Singapore, Vietnam, Philippines
- East Asia: Japan, Korea
Typical trade terms: FOB Shanghai, CIF Houston, CIF Rotterdam, CIF Jebel Ali, plus Manzanillo, Callao, Buenos Aires, Barcelona, Durban, Laem Chabang, Ho Chi Minh, Manila, Mumbai, Yokohama and Busan.
Typical lead time for GB/T 713 12Cr2Mo1VR:
- Ex-stock: about 5–7 days
- Mill rolling, standard N+T: about 45 days
- Simulated PWHT, 3.2 or extra NDE: about 2 months
Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading. Packing is seaworthy, with edge protection and marking in English as specified on the order.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS / GB steel to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia. On GB/T 713 12Cr2Mo1VR that means mill pricing, 12Cr2Mo1VR chemistry reported as heat analysis and as product analysis when ordered, recorded N+T with temper ≥680 °C, tensile results to the correct thickness column, 310 MPa yield in the usual band, 3.1 as standard and 3.2 when specified.
We keep the grade on the order. 12Cr2Mo1VR is not 12Cr2Mo1R. 12Cr2Mo1VR is not 12Cr1MoVR. 12Cr2Mo1VR is not 15CrMoR. 12Cr2Mo1VR is not 14Cr1MoR. 12Cr2Mo1VR is not SA387 Gr.22 Cl.2 unless both books are met and vanadium is accepted. If the drawing names plain 2.25Cr-1Mo without V, we will not ship 12Cr2Mo1VR and call it close.
Company scope: global steel mill sourcing partner – SHH STEEL.
FAQ
-
What is 12Cr2Mo1VR steel plate?
- 12Cr2Mo1VR is a GB/T 713 / GB/T 713.2 2.25Cr-1Mo-V boiler and pressure-vessel plate. Yield is 310 MPa in the usual band and tensile is 520–680 MPa. Delivery is N+T with temper not lower than 680 °C. SHH STEEL supplies this plate as a global steel mill sourcing partner.
-
What is the equivalent of 12Cr2Mo1VR?
- Related ASME comparisons are SA387 Grade 22 Class 2 when vanadium is accepted, SA542 Type C and SA832 22V. Related EN comparison is 12CrMoV9-10. Dual marking is possible only when both books are fully met.
-
Does GB/T 713 give product analysis for 12Cr2Mo1VR?
- Heat analysis is in GB/T 713.2. Product analysis deviations follow GB/T 713.1. SHH STEEL reports both when written on the purchase order.
-
How is 12Cr2Mo1VR different from 12Cr2Mo1R?
- 12Cr2Mo1R is 2.25Cr-1Mo without required vanadium. 12Cr2Mo1VR requires vanadium.
-
How is 12Cr2Mo1VR different from 12Cr1MoVR?
- 12Cr1MoVR is 1Cr-0.3Mo-V. 12Cr2Mo1VR is 2.25Cr-1Mo-V. They are not interchangeable.
-
How is 12Cr2Mo1VR different from SA387 Grade 22?
- Chemistry is close on Cr and Mo. Vanadium, Class, yield, impact and PWHT still have to match both books before dual marking.
-
Can SHH STEEL ship 12Cr2Mo1VR to Mexico, South America or Southeast Asia?
- es. SHH STEEL has supplied plates to Mexico, Argentina, El Salvador, Peru, Spain, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea, as well as the USA, Europe and the Middle East.
-
What is the delivery time for 12Cr2Mo1VR?
- Ex-stock about 5–7 days. Standard N+T mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.
Conclusion
GB/T 713 12Cr2Mo1VR Steel Plate is Chinese 2.25Cr-1Mo-V boiler and pressure-vessel plate at the 310 MPa yield step, 520–680 MPa tensile, N+T delivery with temper not lower than 680 °C. Whether the inquiry says GB/T 713 12Cr2Mo1VR, GB/T 713.2 12Cr2Mo1VR or 12Cr2Mo1VR Cr-Mo-V Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 12Cr2Mo1VR chemistry, heat and product analysis when ordered, recorded N+T, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies GB/T 713 12Cr2Mo1VR Cr-Mo-V Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.
Contact SHH STEEL for mill rolling, stock inquiry, N+T, dual SA387 Gr.22 marking when V is accepted, 3.2 inspection or a quotation.