GB/T 713 14Cr1MoR Steel Plate | 14Cr1MoR Cr-Mo Vessel Plate
What is GB/T 713 14Cr1MoR Steel?
GB/T 713 14Cr1MoR, also written GB/T 713.2 14Cr1MoR and 14Cr1MoR steel plate, is a Chinese 1.25Cr-0.5Mo boiler and pressure-vessel plate. Current product rules sit in GB/T 713.2-2023. Buyers still search GB/T 713. The name itself is the search term: about 0.14% C, 1% Cr, Mo, and R for vessel. Yield is 310 MPa at 6–100 mm. Tensile is 520–680 MPa. Delivery is normalizing plus tempering. Tempering shall not be lower than 650 °C. Impact is commonly 20 °C, 47 J. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade. Plate is produced to GB/T 713 / GB/T 713.2 and shipped to buyers in the USA, Mexico, South America, Europe, Middle East, Africa and Asia.
A purchase order that only says “CrMo vessel plate” is incomplete. Write GB/T 713 14Cr1MoR. Do not ship 15CrMoR against a 14Cr1MoR drawing. Do not ship 12Cr1MoVR against a 14Cr1MoR drawing. Do not ship 12Cr2Mo1R against a 14Cr1MoR drawing. Do not ship SA387 Gr.11 Cl.2 and stamp 14Cr1MoR because tensile looks close. Dual marking is possible only when chemistry, tensile, Class, impact and PWHT fit both named editions.
14Cr1MoR sits one step above 15CrMoR in the Chinese Cr-Mo vessel family. Chromium is higher. Tensile is higher. Yield is higher. That is why a drawing that names 14Cr1MoR will reject 15CrMoR even when both plates look “Cr-Mo enough” in a warehouse list.
This page is not carbon Q245R / Q345R. It is not Mn-Mo-Nb 18MnMoNbR. It is not Mn-Ni-Mo 13MnNiMoR. It is not 2.25Cr-1Mo 12Cr2Mo1R. It is not QT alloy under ASME SA543.
Company scope: global steel mill sourcing partner – SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | GB/T 713 14Cr1MoR | Confirmed |
| Product Specification | GB/T 713.2-2023 (buyers still search GB/T 713) | Applied |
| Service idea | 1.25Cr-0.5Mo boiler and pressure vessels | Confirmed |
| Steel type | Killed Cr-Mo vessel plate | Confirmed |
| Usual delivery | N+T, temper ≥650 °C | Confirmed |
| Yield idea | 310 MPa at 6–100 mm | Confirmed |
| Tensile | 520–680 MPa at 6–100 mm | Confirmed |
| Impact idea | 20 °C / 47 J | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | Americas, Europe, Middle East, Africa, Asia | FOB / CIF as ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates and ASME SA387 comparison work. ASME comparisons belong on ASME SA387 Grade 11, not as automatic substitutes.
Chemical Composition
GB/T 713 14Cr1MoR Steel Plate | 14Cr1MoR Cr-Mo Vessel Plate
Brief Description
GB/T 713 14Cr1MoR is Chinese 1.25Cr-0.5Mo boiler and pressure-vessel plate. Yield is 310 MPa at 6–100 mm. Tensile is 520–680 MPa. SHH STEEL supplies 14Cr1MoR worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
SEO Title
GB/T 713 14Cr1MoR Steel Plate | 14Cr1MoR Cr-Mo Vessel Plate – SHH STEEL
SEO Keywords
GB/T 713 14Cr1MoR, 14Cr1MoR, GB/T 713.2 14Cr1MoR, 14Cr1MoR steel plate, 14Cr1MoR Cr-Mo vessel plate, 14Cr1MoR supplier
SEO Description
SHH STEEL supplies GB/T 713 14Cr1MoR 1.25Cr-0.5Mo vessel plate worldwide, 310 MPa yield, 520–680 MPa tensile. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali. EN 10204 3.1/3.2. Contact now.
General Description
GB/T 713 14Cr1MoR, also written GB/T 713.2 14Cr1MoR and 14Cr1MoR steel plate, is a Chinese 1.25Cr-0.5Mo boiler and pressure-vessel plate. Current product rules sit in GB/T 713.2-2023. Buyers still search GB/T 713. The name itself is the search term: about 0.14% C, 1% Cr, Mo, and R for vessel. Yield is 310 MPa at 6–100 mm. Tensile is 520–680 MPa. Delivery is normalizing plus tempering. Tempering shall not be lower than 650 °C. Impact is commonly 20 °C, 47 J. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade. Plate is produced to GB/T 713 / GB/T 713.2 and shipped to buyers in the USA, Mexico, South America, Europe, Middle East, Africa and Asia.
A purchase order that only says “CrMo vessel plate” is incomplete. Write GB/T 713 14Cr1MoR. Do not ship 15CrMoR against a 14Cr1MoR drawing. Do not ship 12Cr1MoVR against a 14Cr1MoR drawing. Do not ship 12Cr2Mo1R against a 14Cr1MoR drawing. Do not ship SA387 Gr.11 Cl.2 and stamp 14Cr1MoR because tensile looks close. Dual marking is possible only when chemistry, tensile, Class, impact and PWHT fit both named editions.
14Cr1MoR sits one step above 15CrMoR in the Chinese Cr-Mo vessel family. Chromium is higher. Tensile is higher. Yield is higher. That is why a drawing that names 14Cr1MoR will reject 15CrMoR even when both plates look “Cr-Mo enough” in a warehouse list.
This page is not carbon Q245R / Q345R. It is not Mn-Mo-Nb 18MnMoNbR. It is not Mn-Ni-Mo 13MnNiMoR. It is not 2.25Cr-1Mo 12Cr2Mo1R. It is not QT alloy under ASME SA543.
Company scope: global steel mill sourcing partner – SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | GB/T 713 14Cr1MoR | Confirmed |
| Product Specification | GB/T 713.2-2023 (buyers still search GB/T 713) | Applied |
| Service idea | 1.25Cr-0.5Mo boiler and pressure vessels | Confirmed |
| Steel type | Killed Cr-Mo vessel plate | Confirmed |
| Usual delivery | N+T, temper ≥650 °C | Confirmed |
| Yield idea | 310 MPa at 6–100 mm | Confirmed |
| Tensile | 520–680 MPa at 6–100 mm | Confirmed |
| Impact idea | 20 °C / 47 J | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | Americas, Europe, Middle East, Africa, Asia | FOB / CIF as ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates and ASME SA387 comparison work. ASME comparisons belong on ASME SA387 Grade 11, not as automatic substitutes.
Chemical Composition
GB/T 713 14Cr1MoR heat analysis follows GB/T 713.2 Table 1. Product analysis follows the permitted deviations in GB/T 713.1. Write “heat + product analysis” on the order if both are required.
Heat Analysis and Product Analysis — GB/T 713 14Cr1MoR
| Element | Heat Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), max | 0.17 | 0.19 |
| Silicon (Si) | 0.15 – 0.40 | 0.13 – 0.45 |
| Manganese (Mn) | 0.40 – 0.80 | 0.35 – 0.85 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.010 | 0.015 |
| Chromium (Cr) | 1.15 – 1.50 | 1.10 – 1.55 |
| Molybdenum (Mo) | 0.45 – 0.65 | 0.43 – 0.68 |
| Copper (Cu), max | 0.30 | 0.34 |
| Nickel (Ni), max | 0.30 | 0.34 |
Chromium and molybdenum are required. Chromium is higher than on 15CrMoR. That is the main chemistry difference. Do not treat 15CrMoR chemistry as 14Cr1MoR. Do not treat 12Cr1MoVR chemistry as 14Cr1MoR. Vanadium is not the defining addition on 14Cr1MoR. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.
Mechanical Properties
Yield starts at 310 MPa at 6–100 mm and falls as thickness rises.
Tensile and Yield — GB/T 713 14Cr1MoR
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) |
|---|---|---|
| 6 – 100 | 310 | 520 – 680 |
| 100 – 150 | 300 | 510 – 670 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Elongation is commonly 19% min. Impact is 20 °C, 47 J. Elevated-temperature proof stress is published for this grade. Write the design temperature on the order if the vessel file needs those values.
Do not quote 310 MPa yield on a 120 mm plate. Do not treat 520–680 MPa tensile as permission to stamp SA387 Gr.11 Cl.1 or SA387 Gr.11 Cl.2 without checking Class, yield, impact and PWHT. Class 1 and Class 2 are not the same ASME delivery.
Material Comparison
| Grade | Route | Strength idea | Swap? |
|---|---|---|---|
| GB/T 713 15CrMoR | 1.25Cr-0.5Mo lower | 295 / 450–590 | No |
| GB/T 713 14Cr1MoR | 1.25Cr-0.5Mo | 310 / 520–680 | This page |
| GB/T 713 12Cr1MoVR | V-bearing Cr-Mo | Different chemistry | No |
| GB/T 713 12Cr2Mo1R | 2.25Cr-1Mo | Different alloy | No |
| SA387 Gr.11 Cl.2 | 1.25Cr-0.5Mo ASME | Related idea | Comparison only |
| SA387 Gr.12 Cl.2 | 1Cr-0.5Mo ASME | Closer to 15CrMoR | No |
Equivalent Material Grades
These names are project-comparison grades. They are not automatic substitutes. Dual marking is possible only when chemistry, tensile, Class, impact, delivery condition and all extras fit both named editions.
| Designation | Standard / region | Notes |
|---|---|---|
| GB/T 713 14Cr1MoR | GB/T 713.2-2023 | Name on this page |
| GB/T 713-2014 14Cr1MoR | Previous Chinese edition | Same commercial name |
| SA387 Gr.11 Cl.2 | SA-387 | Closest ASME 1.25Cr-0.5Mo Class 2 |
| SA387 Gr.11 Cl.1 | SA-387 | Lower Class |
| ASTM A387 Grade 11 | ASTM A387 | ASTM twin of SA387 Gr.11 |
| 13CrMo4-5 / 1.7335 | EN 10028-2 | Related EN Cr-Mo |
| 13CrMoSi5-5 | EN 10028-2 | Related EN Cr-Mo |
| 15CrMoR | GB/T 713.2 | Lower Chinese Cr-Mo step |
| 12Cr1MoVR | GB/T 713.2 | V-bearing Chinese Cr-Mo |
| 12Cr2Mo1R | GB/T 713.2 | 2.25Cr-1Mo |
| 12Cr2Mo1VR | GB/T 713.2 | V-bearing 2.25Cr-1Mo |
| SA387 Gr.12 Cl.2 | SA-387 | Closer to 15CrMoR |
| SA387 Gr.22 Cl.2 | SA-387 | 2.25Cr-1Mo, not 14Cr1MoR |
| SA387 Gr.21 Cl.2 | SA-387 | 3Cr-1Mo family |
| SA302 Gr.B | SA-302 | Mn-Mo, no Cr |
| SA516 Gr.70 | SA-516 | Carbon vessel, no Cr-Mo |
| JIS G4109 SCMV3 | JIS G4109 | Japanese Cr-Mo vessel comparison |
| ASTM A36 steel plate | A36 | Structural, not vessel |
ASME SA515 and ASME SA203 are not 14Cr1MoR.
Cr-Mo Pressure-Vessel Service
GB/T 713 14Cr1MoR is selected for boilers, heat exchangers, hydrogen service shells and other pressure equipment that name the Chinese 1.25Cr-0.5Mo vessel book at the 310 MPa step. Chromium and molybdenum support elevated-temperature strength and oxidation resistance. The extra chromium versus 15CrMoR is why this grade is named separately.
It is not automatically an ASME Section VIII plate. If the vessel is ASME, the drawing should name SA387 Gr.11 Cl.2 or SA387 Gr.11 Cl.1. If the vessel is 2.25Cr-1Mo, the drawing should name 12Cr2Mo1R or SA387 Gr.22 Cl.2, not 14Cr1MoR.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia. It is not nickel low-temp plate like SA203 Gr.D. It is not QT Ni-Cr-Mo like SA543 Type B Cl.1. Stainless inquiries belong on ASME SA240 or ASTM A240.
Weldability
14Cr1MoR is killed 1.25Cr-0.5Mo vessel plate. Welding is production welding, and Code welding when the equipment is a vessel.
Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the Cr-Mo content, typically 1.25Cr-0.5Mo filler, not a plain Q345R procedure and not a SA387 Gr.22 Cl.2 2.25Cr-1Mo procedure. Preheat and PWHT follow thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Hydrogen service, HIC and NACE extras are not automatic. Write them if the equipment file needs them.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized-and-tempered GB/T 713 14Cr1MoR. Tempering shall not be lower than 650 °C. As-rolled shipment is not the default.
If the vessel will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the carbon normalize route used on Q345R and not the Mn-Mo-Nb N+T route used on 18MnMoNbR. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.
The certificate lists GB/T 713 14Cr1MoR; heat number; heat analysis; product analysis when ordered; tensile results to the correct thickness column; N+T and tempering temperature; impact at 20 °C or the named temperature; elevated-temperature proof stress when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to SA387 Gr.11 Cl.2 is available only when both books are met.
Dimensions
Usual supply range from SHH STEEL for 14Cr1MoR Cr-Mo vessel plate:
- Thickness: commonly 6 mm – 150 mm. Confirm any request above 150 mm against mill capability
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
- Cut-to-length plates and nest sizes inside those limits
Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.
Tolerances
Dimensional limits follow GB/T 713.1 and the mill rolling standard named on the order. Do not apply ASTM A36/A36M structural tolerances to a Chinese vessel plate without writing them. UT to GB/T 2970, JB/T 4730, EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.
Thickness tolerance, flatness and camber must be written if the destination file is tighter than the GB default. Edge condition, mill edge or cut edge, also belongs on the order.
Supplementary Requirements
Most export GB/T 713 14Cr1MoR orders add extras. SHH STEEL does not assume them.
Charpy details. Temperature, energy, location and orientation. GB default is commonly 20 °C / 47 J.
Product analysis. Add this when the destination file wants finished-plate chemistry.
Elevated-temperature proof stress. Design temperature as written.
Simulated PWHT. When the equipment will be stress-relieved.
NDE. UT per the named method.
Z-direction. Z15 / Z25 / Z35 when the drawing names it.
HIC / NACE / SSC / hydrogen service. Only when written.
Third-party. EN 10204 3.2, with inspectors arranged for US, Mexican, European, Middle East, Japanese or Korean documentation packages.
Applications
| Industry | Typical components |
|---|---|
| Cr-Mo vessels | GB/T 713 14Cr1MoR shells |
| Heat exchangers and boilers | 14Cr1MoR courses |
| Elevated-temperature equipment | 14Cr1MoR plate from SHH STEEL |
| Dual-certified export | 14Cr1MoR / SA387 Gr.11 Cl.2 when chemistry fits |
Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.B, A516 Grade 70, SA533 Type C Cl.1, SA517 Gr.P, SA738 Gr.C.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers outside a single region. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to:
- North America: USA, Mexico
- South America: Argentina, Peru and other South American ports
- Central America: El Salvador
- Europe: Spain, Netherlands, Germany and surrounding ports
- Middle East: UAE, Saudi Arabia and nearby Gulf ports
- Africa: South Africa
- South / Southeast Asia: India, Thailand, Singapore, Vietnam, Philippines
- East Asia: Japan, Korea
Typical trade terms: FOB Shanghai, CIF Houston, CIF Rotterdam, CIF Jebel Ali, plus Manzanillo, Callao, Buenos Aires, Barcelona, Durban, Laem Chabang, Ho Chi Minh, Manila, Mumbai, Yokohama and Busan.
Typical lead time for GB/T 713 14Cr1MoR:
- Ex-stock: about 5–7 days
- Mill rolling, standard N+T: about 45 days
- Simulated PWHT, 3.2 or extra NDE: about 2 months
Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading. Packing is seaworthy, with edge protection and marking in English as specified on the order.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS / GB steel to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia. On GB/T 713 14Cr1MoR that means mill pricing, 14Cr1MoR chemistry reported as heat analysis and as product analysis when ordered, recorded N+T with temper ≥650 °C, tensile results to the correct thickness column, 310 MPa yield at 6–100 mm, 3.1 as standard and 3.2 when specified.
We keep the grade on the order. 14Cr1MoR is not 15CrMoR. 14Cr1MoR is not 12Cr1MoVR. 14Cr1MoR is not 12Cr2Mo1R. 14Cr1MoR is not Q345R. 14Cr1MoR is not SA387 Gr.11 Cl.2 unless both books are met. 14Cr1MoR is not SA387 Gr.22 Cl.2. If the drawing names 15CrMoR, we will not ship 14Cr1MoR and call it close.
Company scope: global steel mill sourcing partner – SHH STEEL.
FAQ
-
What is 14Cr1MoR steel plate?
- 14Cr1MoR is a GB/T 713 / GB/T 713.2 1.25Cr-0.5Mo boiler and pressure-vessel plate. Yield is 310 MPa at 6–100 mm and tensile is 520–680 MPa. Delivery is N+T with temper not lower than 650 °C. SHH STEEL supplies this plate as a global steel mill sourcing partner.
-
What is the equivalent of 14Cr1MoR?
- The usual ASME comparison is SA387 Grade 11 Class 2. Related comparisons are SA387 Grade 11 Class 1 and 13CrMo4-5. Dual marking is possible only when both books are fully met.
-
Does GB/T 713 give product analysis for 14Cr1MoR?
- Heat analysis is in GB/T 713.2. Product analysis deviations follow GB/T 713.1. SHH STEEL reports both when written on the purchase order.
-
How is 14Cr1MoR different from 15CrMoR?
- 15CrMoR yield is 295 MPa and tensile is 450–590 MPa. 14Cr1MoR yield is 310 MPa and tensile is 520–680 MPa. Chromium is also higher on 14Cr1MoR.
-
How is 14Cr1MoR different from SA387 Grade 11?
- Chemistry is close. Class, yield, impact and PWHT still have to match both books before dual marking.
-
How is 14Cr1MoR different from 12Cr2Mo1R?
- 12Cr2Mo1R is 2.25Cr-1Mo. 14Cr1MoR is 1.25Cr-0.5Mo. They are not interchangeable.
-
Can SHH STEEL ship 14Cr1MoR to Mexico, South America or Southeast Asia?
- Yes. SHH STEEL has supplied plates to Mexico, Argentina, El Salvador, Peru, Spain, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea, as well as the USA, Europe and the Middle East.
-
What is the delivery time for 14Cr1MoR?
- Ex-stock about 5–7 days. Standard N+T mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.
-
Can SHH STEEL issue EN 10204 3.2 for 14Cr1MoR?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged when written on the order.
-
What is the density of 14Cr1MoR?
- .85 g/cm³.
Conclusion
GB/T 713 14Cr1MoR Steel Plate is Chinese 1.25Cr-0.5Mo boiler and pressure-vessel plate at the 310 MPa yield step, 520–680 MPa tensile at 6–100 mm, N+T delivery with temper not lower than 650 °C. Whether the inquiry says GB/T 713 14Cr1MoR, GB/T 713.2 14Cr1MoR or 14Cr1MoR Cr-Mo Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 14Cr1MoR chemistry, heat and product analysis when ordered, recorded N+T, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies GB/T 713 14Cr1MoR Cr-Mo Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.
Contact SHH STEEL for mill rolling, stock inquiry, N+T, dual SA387 Gr.11 marking when eligible, 3.2 inspection or a quotation.
GB/T 713 14Cr1MoR Steel Plate, GB/T 713.2 14Cr1MoR, 14Cr1MoR Cr-Mo vessel plate, 14Cr1MoR supplier, global steel mill sourcing partner SHH STEEL