Product Showcase
GB/T 4237 Stainless Steel Products
SHH STEEL offers GB/T 4237-compliant 304/316 stainless steel plates. GB/T 4237 specifies hot-rolled stainless steel plates, sheets, and strips for general applications. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GB/T 4237 022Cr21Mn3Ni3Mo2N S22193 Stainless Steel Plate Supplier
GB/T 4237 022Cr21Mn3Ni3Mo2N (S22193) is an austenitic-ferritic (lean duplex) stainless steel plate equivalent to S81921, with 450 MPa minimum proof strength and 620 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 60 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr21Mn5Ni2N S22152 Stainless Steel Plate Supplier
GB/T 4237 022Cr21Mn5Ni2N (S22152) is an austenitic-ferritic (lean duplex) stainless steel plate equivalent to S32001 / 19D-type, with 450 MPa minimum proof strength and 620 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 60 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr21Ni3Mo2N S22153 Stainless Steel Plate Supplier
GB/T 4237 022Cr21Ni3Mo2N (S22153) is an austenitic-ferritic (lean duplex) stainless steel plate equivalent to 2003, with 450 MPa minimum proof strength and 655 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 60 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 03Cr25Ni6Mo3Cu2N S25554 Stainless Steel Plate Supplier
GB/T 4237 03Cr25Ni6Mo3Cu2N (S25554) is an austenitic-ferritic (super duplex) stainless steel plate equivalent to 255 / Ferralium-type, with 550 MPa minimum proof strength and 760 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 60 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr25Ni7Mo4WCuN S27603 Stainless Steel Plate Supplier
GB/T 4237 022Cr25Ni7Mo4WCuN (S27603) is an austenitic-ferritic (super duplex) stainless steel plate equivalent to S32760 / Zeron 100-type, with 550 MPa minimum proof strength and 750 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 60 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr25Ni6Mo2N S22553 Stainless Steel Plate Supplier
GB/T 4237 022Cr25Ni6Mo2N (S22553) is an austenitic-ferritic (duplex) stainless steel plate equivalent to S31200 25Cr duplex, with 450 MPa minimum proof strength and 640 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 80 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr23Ni2N S22353 Stainless Steel Plate Supplier
GB/T 4237 022Cr23Ni2N (S22353) is an austenitic-ferritic (lean duplex) stainless steel plate equivalent to 2202, with 450 MPa minimum proof strength and 650 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 60 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr23Ni4MoCuN S23043 Stainless Steel Plate Supplier
GB/T 4237 022Cr23Ni4MoCuN (S23043) is an austenitic-ferritic (lean duplex) stainless steel plate equivalent to 2304, with 400 MPa minimum proof strength and 600 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 60 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr25Ni7Mo4N S25073 Stainless Steel Plate Supplier
GB/T 4237 022Cr25Ni7Mo4N (S25073) is an austenitic-ferritic (super duplex) stainless steel plate equivalent to 2507, with 550 MPa minimum proof strength and 795 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 60 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr22Ni5Mo3N S22253 Stainless Steel Plate Supplier
GB/T 4237 022Cr22Ni5Mo3N (S22253) is an austenitic-ferritic (duplex) stainless steel plate equivalent to 2205 (S31803), with 450 MPa minimum proof strength and 620 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 80 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr23Ni5Mo3N S22053 Stainless Steel Plate Supplier
GB/T 4237 022Cr23Ni5Mo3N (S22053) is an austenitic-ferritic (duplex) stainless steel plate equivalent to 2205 (S32205), with 450 MPa minimum proof strength and 655 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 80 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr12Ni9Cu2NbTi S51290 Stainless Steel Plate Supplier
GB/T 4237 022Cr12Ni9Cu2NbTi (S51290) is a precipitation-hardening stainless steel plate equivalent to 455-type maraging PH, delivered solution treated. SHH STEEL supplies it hot rolled in 2 – 16 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More
GB/T 4237 Stainless Steel Products
Stainless Steel Sheets and Plates
SHH STEEL, a leading Stainless Steel Sheets and Plates exporter, produces and exports stainless steel sheets (0.3–6 mm) and plates (>6 mm) for marine, chemical, and structural applications. Our products, like 304 and 316L (ASTM A240), offer corrosion resistance and durability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for 316L stainless steel plates and custom solutions for your projects.