GB/T 4237 019Cr23Mo2Ti (S12361) stainless steel plate at SHH STEEL warehouse

GB/T 4237 019Cr23Mo2Ti S12361 Stainless Steel Plate Supplier

GB/T 4237 019Cr23Mo2Ti (S12361) is a ferritic stainless steel plate equivalent to 445J2, with 245 MPa minimum proof strength and 410 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 10 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.
Keywords
019Cr23Mo2Ti, S12361, SUS445J2, 445J2, GB/T 4237 019Cr23Mo2Ti, 019Cr23Mo2Ti stainless steel plate, 019Cr23Mo2Ti plate, S12361 stainless steel, 019Cr23Mo2Ti S12361, 019Cr23Mo2Ti supplier
Equivalent Grades:
JIS G4304 SUS445J2 — Material Specification: GB/T 4237-2015 (019Cr23Mo2Ti, unified code S12361) — Delivery: 850 – 1 050 °C, rapid cooling
Share:
Overview
Corrosion Resistance
Chemical Composition
Product Analysis
Mechanical Properties
Ferritic Behaviour
Equivalent Grades
Welding & Fabrication
Grade Comparison
Specification
Heat Treatment
Applications
Surface & Processing
Dimensions
Testing & Certificates
Mill Sourcing
Ordering
FAQ
Conclusion

GB/T 4237 019Cr23Mo2Ti: what it is and who uses it

019Cr23Mo2Ti is a 23% chromium ferritic with 1.50–2.50% molybdenum, matching the Japanese SUS445J2 class. Minimum PREN is about 26, above 316L, making it a ferritic option for building roofs and coastal cladding.

How to read the name: under GB/T 20878 the leading ‘019’ is the carbon code (here C ≤0.025%), then Cr23 = about 23% chromium; Mo2 = about 2% molybdenum; Ti = titanium added. S12361 is the unified numeric code (ISC) used in GB/T 4237-2015.

SHH STEEL produces and exports ferritic stainless plate from China, works as a sales agent for leading stainless mills, and runs its own processing warehouse for cutting and surface finishing. 019Cr23Mo2Ti is part of our GB/T 4237 stainless plate range; for comparison, see our ASTM A240 Type 444 page.

How 019Cr23Mo2Ti performs in corrosive service

Molybdenum and higher chromium bring ferritic grades up to 304–316L pitting resistance while keeping freedom from chloride stress corrosion cracking.

PREN of 019Cr23Mo2Ti from the GB/T 4237 limits: 25.9 – 29.1. PREN is a ranking tool for pitting in chlorides, not a guarantee; temperature, crevices, deposits and weld finish matter as much.

Intergranular corrosion testing of ferritic and martensitic plate is by agreement (GB/T 4334 or ASTM A763 practices).

Heat analysis limits for 019Cr23Mo2Ti

Element 019Cr23Mo2Ti heat analysis, % (Table 17) Why it matters
C ≤ 0.025 Carbon. Low values protect welds from carbide precipitation; higher values add hot strength or hardenability.
Si ≤ 1.00 Silicon. Deoxidizer; in heat-resistant grades it builds a protective scale.
Mn ≤ 1.00 Manganese. Deoxidizer; in Mn-bearing grades it replaces nickel and keeps nitrogen in solution.
P ≤ 0.040 Phosphorus. Impurity, kept low for toughness and weld cracking resistance.
S ≤ 0.030 Sulfur. Impurity; low sulfur improves pitting resistance, hot workability and polishability.
Cr 21.00 – 24.00 Chromium. Forms the passive film; the main driver of corrosion and oxidation resistance.
Mo 1.50 – 2.50 Molybdenum. Raises pitting and crevice resistance in chlorides (×3.3 in PREN).
Cu ≤ 0.60 Copper. Improves resistance to sulfuric acid and, in ferritics, general corrosion and formability.
N ≤ 0.025 Nitrogen. Strengthens, stabilizes austenite and adds pitting resistance (×16 in PREN).
Other Ti, Nb, Zr or their combination: 8 × (C+N) – 0.80 Stabilizing / special-element requirement of the standard
PREN (Cr + 3.3Mo + 16N) 25.9 – 29.1 (minimum – mid-range) Calculated from the limits above, not a requirement of GB/T 4237

Values are maximum unless a range is given. The mill reports the ladle (heat) analysis on the certificate; this is the figure to compare with Table 17.

Product analysis vs heat analysis

A check analysis drilled from the finished plate may differ slightly from the heat analysis. GB/T 4237 refers to GB/T 222 for the permitted deviations; the table applies them to the 019Cr23Mo2Ti limits. Deviations apply to one side of a range only, never to both sides in the same heat.

Element Heat analysis limit (%) Permitted deviation Product analysis limit (%)
C ≤ 0.025 +0.005 ≤ 0.030
Si ≤ 1.00 ±0.05 ≤ 1.05
Mn ≤ 1.00 ±0.03 ≤ 1.03
P ≤ 0.040 +0.005 ≤ 0.045
S ≤ 0.030 +0.005 ≤ 0.035
Cr 21.00 – 24.00 ±0.25 20.75 – 24.25
Mo 1.50 – 2.50 ±0.05 (min) / ±0.10 (max) 1.45 – 2.60
Cu ≤ 0.60 ±0.05 ≤ 0.65
N ≤ 0.025 ±0.01 ≤ 0.035

Where the table says ‘by agreement’, the deviation is not tabulated for that content level and should be agreed in the contract, usually by reference to ASTM A480 Table A1.1.

019Cr23Mo2Ti S12361 tensile and hardness requirements

Property 019Cr23Mo2Ti (Table 22)
Proof strength Rp0.2, MPa ≥ 245
Tensile strength Rm, MPa ≥ 410
Elongation A, % ≥ 20
Hardness HBW ≤ 217
Hardness HRB ≤ 96
Hardness HV ≤ 230
180° bend (cold) D=2a, no cracks on the outer surface

Values apply to plate in the delivery heat-treated condition, tested transversely per GB/T 228.1. Hardness is checked by one method chosen by the mill.

Living with a ferritic grade

019Cr23Mo2Ti is ferritic: it is magnetic, has lower thermal expansion and better thermal conductivity than austenitic steel, and is immune to chloride stress corrosion cracking. Those properties make it a good choice for heat exchangers, hot water tanks and exhaust parts.

The trade-off is toughness. Ferritic stainless has a ductile-brittle transition, and it moves to higher temperature with thickness and grain size. This is why ferritic plate is mostly thin; for sections above about 6 mm ask for Charpy data or bend in a warm shop.

Ferritic grades contain little or no nickel, so their price is far more stable than GB/T 4237 06Cr19Ni10 S30408 (304).

019Cr23Mo2Ti equivalent grades: ASTM, EN, JIS

Standard system Equivalent / closest grade
China GB/T 4237-2015 019Cr23Mo2Ti (S12361)
ASTM A240/A240M —
EN 10088-2 —
JIS G4304 (hot rolled) SUS445J2
Common name 445J2

Equivalent grades are close in chemistry and properties but are never identical: limits on carbon, nitrogen and residual elements differ. For dual or multiple certification the heat must meet every standard named on the order, and we confirm that from the heat chemistry before quotation.

Related pages: ASTM A240 Type 444, JIS G4305 SUS444. See also our ASTM A240/A240M and JIS G4305 plate lists.

Cutting, forming and welding 019Cr23Mo2Ti plate

Weld with ER316L, ER439Mo or a matching Mo-bearing ferritic filler. Shield the root with argon; nitrogen and carbon pick-up embrittle high-chromium ferritic welds.

Keep heat input low and avoid weaving; HAZ grain growth reduces toughness more than in austenitic grades.

Cutting: we cut 019Cr23Mo2Ti by plasma (up to about 150 mm), laser (thin plate) or waterjet, and remove the heat-affected edge by machining where the drawing requires it.

Comparison with sister grades

The table compares 019Cr23Mo2Ti with the grades buyers most often weigh it against. Strength values are GB/T 4237-2015 minimums; PREN is calculated from the minimum chemistry.

Grade (GB/T 4237) Key chemistry, % PREN min Rp0.2 min, MPa Rm min, MPa
019Cr23Mo2Ti S12361 C ≤ 0.025, Cr 21.00 – 24.00, Mo 1.50 – 2.50, N ≤ 0.025, Cu ≤ 0.60 25.9 245 410
GB/T 4237 019Cr23MoTi S12362 C ≤ 0.025, Cr 21.00 – 24.00, Mo 0.70 – 1.50, N ≤ 0.025, Cu ≤ 0.60 23.3 245 410
GB/T 4237 019Cr19Mo2NbTi S11972 C ≤ 0.025, Cr 17.50 – 19.50, Ni ≤ 1.00, Mo 1.75 – 2.50, N ≤ 0.035 23.3 275 415
GB/T 4237 019Cr21CuTi S12182 C ≤ 0.025, Cr 20.50 – 23.00, N ≤ 0.025, Cu 0.30 – 0.80 20.5 205 390

Mainly produced as sheet and coil; plate thickness is limited. Its sigma and 475 °C embrittlement risks rule out service above about 300 °C.

What the standard covers for this grade

Item GB/T 4237-2015 requirement / SHH STEEL supply
Standard GB/T 4237-2015 Hot rolled stainless steel plate, sheet and strip (current edition, replaces GB/T 4237-2007)
Grade / unified code 019Cr23Mo2Ti / S12361
Steel class Ferritic
Chemical composition Table 17 (heat analysis); product analysis per GB/T 222
Mechanical properties Table 22
Product forms Hot-rolled thick plate (3.0 – 200 mm in the standard), hot-rolled wide strip and cut plate (2.0 – 25.4 mm)
Our usual thickness range 2 – 10 mm
Delivery condition 850 – 1 050 °C, rapid cooling
Surface Hot rolled, heat treated, pickled (No.1 / 1D) as standard; ground or polished by agreement
Density 7.7 g/cm³
Certificate EN 10204 3.1 mill certificate; 3.2 with third-party inspection on request

Sister grades on the same standard are listed under GB/T 4237; cold-rolled sheet of the same chemistry is ordered to GB/T 3280, and all our plate lines sit in stainless steel sheets and plates.

How 019Cr23Mo2Ti plate is heat treated

Recommended heat treatment for 019Cr23Mo2Ti (GB/T 4237-2015 Annex C): 850 – 1 050 °C, rapid cooling.

Rapid cooling after annealing avoids sigma and 475 °C embrittlement in Mo-bearing high-Cr ferritics.

Applications of 019Cr23Mo2Ti plate

Typical uses:

  • Roofing and cladding in coastal or industrial atmospheres
  • Hot water tanks
  • Heat exchangers
  • Architectural panels

Buyers specifying 019Cr23Mo2Ti for these jobs often compare it with GB/T 4237 019Cr23MoTi S12362 and GB/T 4237 019Cr21CuTi S12182; the comparison table on this page shows the differences.

International grade pages for the alternatives mentioned above: JIS G4305 SUS443J1.

Other GB/T 4237 grades buyers request alongside it: GB/T 4237 019Cr18MoTi S11862, GB/T 4237 10Cr17 S11710, GB/T 4237 022Cr12 S11203, GB/T 4237 022Cr12Ni S11213, GB/T 4237 022Cr18Ti S11863.

Finishes and warehouse services

Finish Description Availability for this grade
No.1 / 1D Hot rolled, heat treated, pickled; the GB/T 4237 standard surface Standard
Shot-blasted + pickled Uniform matte for welded structures On request
No.4 / brushed Abrasive finish, grit 150–180 Warehouse processing, thin plate
HL (hairline) Long continuous lines, decorative Warehouse processing, thin plate
8K mirror Polished reflective finish Warehouse processing, limited sizes
2B / BA Cold-rolled finishes (ordered as GB/T 3280 sheet, not hot-rolled plate) Sheet only

Our warehouse cuts plate to size (plasma, laser, waterjet, saw), bevels weld edges, polishes and applies PVC protective film. Processed plate ships with the original mill heat number marked. Ask for cut pieces of other stainless steel products at the same time to consolidate freight.

019Cr23Mo2Ti plate sizes

Dimension Typical supply
Thickness 2 – 10 mm
Width 1 000 / 1 219 / 1 250 / 1 500 / 1 800 / 2 000 mm; wider by mill order
Length 2 000 / 2 438 / 3 000 / 6 000 mm or cut to size
Flatness Per GB/T 4237; ≤15 mm per metre for plate up to 25 mm unless agreed tighter
Thickness tolerance Per the GB/T 4237 dimensional tolerance tables (normal or higher accuracy as ordered)
Edge Mill edge or cut edge

Weight: plate mass in kg/m² = thickness (mm) × density (7.7 g/cm³). A 10 mm 019Cr23Mo2Ti plate weighs about 77.0 kg/m²; a 1 500 × 6 000 × 10 mm plate about 693 kg.

Testing and certification

  • Heat chemical analysis on every heat; product analysis by agreement
  • Tensile test (Rp0.2, Rm, A) per batch
  • Hardness test
  • 180° bend test
  • Ultrasonic testing (NB/T 47013.3 or ASTM A578) when specified
  • Positive material identification (PMI) on every plate leaving our warehouse
  • Visual and dimensional inspection; third-party inspection (SGS, BV, TÜV, Intertek) at the buyer’s request

Certificates follow EN 10204 3.1 as standard. Where plate is also certified to ASME SA240 or ASTM A240, both standards are shown on one certificate.

Supply chain and lead time

019Cr23Mo2Ti is produced by a small number of Chinese mills with the melting and heat treatment capability for it. We place mill orders for it through the producers we represent and do not usually hold it in stock. Expect about 45–90 days, with minimum quantities per thickness; we can combine small quantities into one rolling where the mill allows.

Every plate is traceable to its heat number, and copies of the mill certificates stay on file for repeat orders and audits. The same mills also supply our ASTM A240, ASME SA240, JIS G4305 and AISI plate ranges, so mixed-standard orders can ship together.

How to order

  • Standard and edition: GB/T 4237-2015
  • Grade and code: 019Cr23Mo2Ti (S12361); add the equivalent if dual certification is needed
  • Thickness × width × length, quantity in pieces or tonnes
  • Thickness tolerance class and flatness if tighter than standard
  • Surface finish and protective film
  • Tests beyond the standard (IGC, UT, impact, ferrite, PMI, grain size)
  • Certificate type (EN 10204 3.1 / 3.2) and inspection body
  • Marking, packing (wooden cases, steel pallets) and delivery terms

Send the list to SHH STEEL and we return a quotation with mill, lead time and stock options. Other grades from the same standard can be combined in one shipment; browse GB/T 4237 plate grades.

FAQ

What is 019Cr23Mo2Ti used for?
019Cr23Mo2Ti (S12361, SUS445J2 type) is used for roofing, coastal cladding and water tanks where 316L-level corrosion resistance and ferritic freedom from chloride SCC are wanted. Minimum PREN is about 26.
What is the chemical composition of 019Cr23Mo2Ti?
Under GB/T 4237-2015 Table 17, 019Cr23Mo2Ti (S12361) has C ≤ 0.025, Cr 21.00 – 24.00, Mo 1.50 – 2.50, N ≤ 0.025, Cu ≤ 0.60; Ti, Nb, Zr or their combination: 8 × (C+N) – 0.80. Phosphorus is limited to ≤0.040% and sulfur to ≤0.030%.
What is the ASTM equivalent of 019Cr23Mo2Ti?
The closest equivalents of 019Cr23Mo2Ti (S12361) are SUS445J2 in JIS (common name: 445J2). Chemistry limits differ slightly, so dual certification depends on the actual heat.
What are the mechanical properties of 019Cr23Mo2Ti plate?
GB/T 4237-2015 Table 22 requires for 019Cr23Mo2Ti: proof strength Rp0.2 ≥245 MPa, tensile strength ≥410 MPa and elongation ≥20%, hardness ≤217 HBW. Values apply to plate in the delivery heat-treated condition.
Is 019Cr23Mo2Ti stainless steel magnetic?
Yes. 019Cr23Mo2Ti is ferritic and is magnetic in all conditions.
What thickness of 019Cr23Mo2Ti plate can you supply?
Under GB/T 4237 we supply 019Cr23Mo2Ti hot-rolled plate in 2 – 10 mm, widths up to 2 000 mm (wider by mill order), cut to size in our warehouse. Thinner material is cold-rolled sheet to GB/T 3280.

Conclusion

GB/T 4237 019Cr23Mo2Ti (S12361) is a molybdenum or high-chromium ferritic plate grade, known internationally as 445J2. It is defined by Table 17 chemistry (C ≤ 0.025, Cr 21.00 – 24.00, Mo 1.50 – 2.50, N ≤ 0.025, Cu ≤ 0.60) and Table 22 properties of at least 245 MPa proof strength and 410 MPa tensile strength. Typical uses include roofing and cladding in coastal or industrial atmospheres, hot water tanks and heat exchangers. Mainly produced as sheet and coil; plate thickness is limited.

Before ordering, state the standard edition, the grade name with its code, and any extra tests, so that the mill certificate matches your design documents. SHH STEEL supplies 019Cr23Mo2Ti plate by mill order through the producers we represent, cut to size and finished in our own warehouse, with EN 10204 3.1 certificates. For related grades see GB/T 4237 019Cr23MoTi S12362 and GB/T 4237 019Cr19Mo2NbTi S11972, our GB/T 4237 category and the ASTM A240 Type 444 page. Send your sizes and quantities for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X