Product Showcase
EN 10028-7 Stainless Steel Products
SHH STEEL offers EN 10028-7-compliant 304/316 stainless steel plates. EN 10028-7 specifies technical delivery conditions for flat stainless steel products, including creep-resistant austenitic steels, for pressure purposes. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
EN 10028-7 X8NiCrAlTi32-21 1.4959 Pressure Vessel Stainless Plate
EN 10028-7 X8NiCrAlTi32-21 (1.4959) is a creep-resisting austenitic steel for high-temperature pressure parts for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 170 MPa and Rm 500 – 750 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X5NiCrAlTi31-20 1.4958 Pressure Vessel Stainless Plate
EN 10028-7 X5NiCrAlTi31-20 (1.4958) is a creep-resisting austenitic steel for high-temperature pressure parts for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 170 MPa and Rm 500 – 750 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X8CrNiNb16-13 1.4961 Pressure Vessel Stainless Plate
EN 10028-7 X8CrNiNb16-13 (1.4961) is a creep-resisting austenitic steel for high-temperature pressure parts for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 200 MPa and Rm 510 – 690 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X3CrNiMoBN17-13-3 1.4910 Pressure Vessel Stainless Plate
EN 10028-7 X3CrNiMoBN17-13-3 (1.4910) is a creep-resisting austenitic steel for high-temperature pressure parts for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 260 MPa and Rm 550 – 750 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X6CrNiTiB18-10 1.4941 Pressure Vessel Stainless Plate
EN 10028-7 X6CrNiTiB18-10 (1.4941) is a creep-resisting austenitic steel for high-temperature pressure parts for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 200 MPa and Rm 490 – 690 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X6CrNi25-20 1.4951 Pressure Vessel Stainless Plate
EN 10028-7 X6CrNi25-20 (1.4951) is a creep-resisting austenitic steel for high-temperature pressure parts for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 200 MPa and Rm 510 – 710 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X6CrNi23-13 1.4950 Pressure Vessel Stainless Plate
EN 10028-7 X6CrNi23-13 (1.4950) is a creep-resisting austenitic steel for high-temperature pressure parts for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 200 MPa and Rm 510 – 710 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X6CrNi18-10 1.4948 Pressure Vessel Stainless Plate
EN 10028-7 X6CrNi18-10 (1.4948) is a creep-resisting austenitic steel for high-temperature pressure parts for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 190 MPa and Rm 510 – 710 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X2CrNiMoCuWN25-7-4 1.4501 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiMoCuWN25-7-4 (1.4501) is an austenitic-ferritic (duplex) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 530 MPa and Rm 730 – 930 MPa (Table 10). SHH STEEL supplies it up to 50 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X2CrNiMoCuN25-6-3 1.4507 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiMoCuN25-6-3 (1.4507) is an austenitic-ferritic (duplex) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 490 MPa and Rm 690 – 890 MPa (Table 10). SHH STEEL supplies it up to 50 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X2CrNiMoN25-7-4 1.4410 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiMoN25-7-4 (1.4410) is an austenitic-ferritic (duplex) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 530 MPa and Rm 730 – 930 MPa (Table 10). SHH STEEL supplies it up to 50 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X2CrNiMoN22-5-3 1.4462 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiMoN22-5-3 (1.4462) is an austenitic-ferritic (duplex) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 460 MPa and Rm 640 – 840 MPa (Table 10). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More
EN 10028-7 Stainless Steel Products
Stainless Steel Sheets and Plates
SHH STEEL, a leading Stainless Steel Sheets and Plates exporter, produces and exports stainless steel sheets (0.3–6 mm) and plates (>6 mm) for marine, chemical, and structural applications. Our products, like 304 and 316L (ASTM A240), offer corrosion resistance and durability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for 316L stainless steel plates and custom solutions for your projects.
Stainless Steel Sheets and Plates
X