GB/T 4237 019Cr18CuNb S11882 Stainless Steel Plate Supplier
What is GB/T 4237 019Cr18CuNb (S11882) stainless steel plate?
019Cr18CuNb is a copper-bearing Nb-stabilized ferritic similar to JIS SUS430J1L: Cr 16–20%, Cu 0.30–0.80%, C ≤0.025%. Copper improves general corrosion resistance and formability, so it is used for appliance and automotive parts that once took 304.
How to read the name: under GB/T 20878 the leading ‘019’ is the carbon code (here C ≤0.025%), then Cr18 = about 18% chromium; Cu = copper added; Nb = niobium added. S11882 is the unified numeric code (ISC) used in GB/T 4237-2015.
SHH STEEL produces and exports ferritic stainless plate from China, works as a sales agent for leading stainless mills, and runs its own processing warehouse for cutting and surface finishing. 019Cr18CuNb is part of our GB/T 4237 stainless plate range; for comparison, see our JIS G4305 SUS430J1 page.
Chemical composition of 019Cr18CuNb S11882
| Element | 019Cr18CuNb heat analysis, % (Table 17) | Why it matters |
|---|---|---|
| C | ≤ 0.025 | Carbon. Low values protect welds from carbide precipitation; higher values add hot strength or hardenability. |
| Si | ≤ 1.00 | Silicon. Deoxidizer; in heat-resistant grades it builds a protective scale. |
| Mn | ≤ 1.00 | Manganese. Deoxidizer; in Mn-bearing grades it replaces nickel and keeps nitrogen in solution. |
| P | ≤ 0.040 | Phosphorus. Impurity, kept low for toughness and weld cracking resistance. |
| S | ≤ 0.030 | Sulfur. Impurity; low sulfur improves pitting resistance, hot workability and polishability. |
| Cr | 16.00 – 20.00 | Chromium. Forms the passive film; the main driver of corrosion and oxidation resistance. |
| Ni | ≤ 0.60 | Nickel. Stabilizes austenite, improves toughness and resistance to reducing acids. |
| Cu | 0.30 – 0.80 | Copper. Improves resistance to sulfuric acid and, in ferritics, general corrosion and formability. |
| N | ≤ 0.025 | Nitrogen. Strengthens, stabilizes austenite and adds pitting resistance (×16 in PREN). |
| Other | Nb: 8 × (C+N) – 0.8 | Stabilizing / special-element requirement of the standard |
| PREN (Cr + 3.3Mo + 16N) | 16.0 – 18.0 (minimum – mid-range) | Calculated from the limits above, not a requirement of GB/T 4237 |
Values are maximum unless a range is given. The mill reports the ladle (heat) analysis on the certificate; this is the figure to compare with Table 17.
Product (check) analysis tolerances
A check analysis drilled from the finished plate may differ slightly from the heat analysis. GB/T 4237 refers to GB/T 222 for the permitted deviations; the table applies them to the 019Cr18CuNb limits. Deviations apply to one side of a range only, never to both sides in the same heat.
| Element | Heat analysis limit (%) | Permitted deviation | Product analysis limit (%) |
|---|---|---|---|
| C | ≤ 0.025 | +0.005 | ≤ 0.030 |
| Si | ≤ 1.00 | ±0.05 | ≤ 1.05 |
| Mn | ≤ 1.00 | ±0.03 | ≤ 1.03 |
| P | ≤ 0.040 | +0.005 | ≤ 0.045 |
| S | ≤ 0.030 | +0.005 | ≤ 0.035 |
| Cr | 16.00 – 20.00 | ±0.20 | 15.80 – 20.20 |
| Ni | ≤ 0.60 | ±0.03 | ≤ 0.63 |
| Cu | 0.30 – 0.80 | ±0.03 (min) / ±0.05 (max) | 0.27 – 0.85 |
| N | ≤ 0.025 | ±0.01 | ≤ 0.035 |
Where the table says ‘by agreement’, the deviation is not tabulated for that content level and should be agreed in the contract, usually by reference to ASTM A480 Table A1.1.
Mechanical properties at room temperature
| Property | 019Cr18CuNb (Table 22) |
|---|---|
| Proof strength Rp0.2, MPa | ≥ 205 |
| Tensile strength Rm, MPa | ≥ 390 |
| Elongation A, % | ≥ 22 |
| Hardness HBW | ≤ 192 |
| Hardness HRB | ≤ 90 |
| Hardness HV | ≤ 200 |
| 180° bend (cold) | D=2a, no cracks on the outer surface |
Values apply to plate in the delivery heat-treated condition, tested transversely per GB/T 228.1. Hardness is checked by one method chosen by the mill.
Specification summary
| Item | GB/T 4237-2015 requirement / SHH STEEL supply |
|---|---|
| Standard | GB/T 4237-2015 Hot rolled stainless steel plate, sheet and strip (current edition, replaces GB/T 4237-2007) |
| Grade / unified code | 019Cr18CuNb / S11882 |
| Steel class | Ferritic |
| Chemical composition | Table 17 (heat analysis); product analysis per GB/T 222 |
| Mechanical properties | Table 22 |
| Product forms | Hot-rolled thick plate (3.0 – 200 mm in the standard), hot-rolled wide strip and cut plate (2.0 – 25.4 mm) |
| Our usual thickness range | 2 – 12 mm |
| Delivery condition | 800 – 1 050 °C, rapid cooling |
| Surface | Hot rolled, heat treated, pickled (No.1 / 1D) as standard; ground or polished by agreement |
| Density | 7.7 g/cm³ |
| Certificate | EN 10204 3.1 mill certificate; 3.2 with third-party inspection on request |
Sister grades on the same standard are listed under GB/T 4237; cold-rolled sheet of the same chemistry is ordered to GB/T 3280, and all our plate lines sit in stainless steel sheets and plates.
Living with a ferritic grade
019Cr18CuNb is ferritic: it is magnetic, has lower thermal expansion and better thermal conductivity than austenitic steel, and is immune to chloride stress corrosion cracking. Those properties make it a good choice for heat exchangers, hot water tanks and exhaust parts.
The trade-off is toughness. Ferritic stainless has a ductile-brittle transition, and it moves to higher temperature with thickness and grain size. This is why ferritic plate is mostly thin; for sections above about 6 mm ask for Charpy data or bend in a warm shop.
Ferritic grades contain little or no nickel, so their price is far more stable than GB/T 4237 06Cr19Ni10 S30408 (304).
019Cr18CuNb equivalent grades: ASTM, EN, JIS
| Standard system | Equivalent / closest grade |
|---|---|
| China GB/T 4237-2015 | 019Cr18CuNb (S11882) |
| ASTM A240/A240M | — |
| EN 10088-2 | — |
| JIS G4304 (hot rolled) | SUS430J1L |
| Common name | 430J1L |
Equivalent grades are close in chemistry and properties but are never identical: limits on carbon, nitrogen and residual elements differ. For dual or multiple certification the heat must meet every standard named on the order, and we confirm that from the heat chemistry before quotation.
Related pages: JIS G4305 SUS430J1, AISI 430. See also our ASTM A240/A240M and JIS G4305 plate lists.
019Cr18CuNb compared with related grades
The table compares 019Cr18CuNb with the grades buyers most often weigh it against. Strength values are GB/T 4237-2015 minimums; PREN is calculated from the minimum chemistry.
| Grade (GB/T 4237) | Key chemistry, % | PREN min | Rp0.2 min, MPa | Rm min, MPa |
|---|---|---|---|---|
| 019Cr18CuNb S11882 | C ≤ 0.025, Cr 16.00 – 20.00, Ni ≤ 0.60, N ≤ 0.025, Cu 0.30 – 0.80 | 16.0 | 205 | 390 |
| GB/T 4237 019Cr21CuTi S12182 | C ≤ 0.025, Cr 20.50 – 23.00, N ≤ 0.025, Cu 0.30 – 0.80 | 20.5 | 205 | 390 |
| GB/T 4237 022Cr17NbTi S11763 | C ≤ 0.030, Cr 16.00 – 19.00 | 16.0 | 175 | 360 |
| GB/T 4237 10Cr17 S11710 | C ≤ 0.12, Cr 16.00 – 18.00, Ni ≤ 0.75 | 16.0 | 205 | 420 |
Copper-bearing ferritics are mostly made as cold-rolled sheet; hot-rolled plate under GB/T 4237 is thin (around 3–6 mm) and by mill order.
Corrosion resistance and PREN of 019Cr18CuNb
17–18% chromium ferritics resist indoor and mild outdoor atmospheres, foods and nitric acid. They are immune to chloride stress corrosion cracking but pit more easily than 304.
PREN of 019Cr18CuNb from the GB/T 4237 limits: 16.0 – 18.0. PREN is a ranking tool for pitting in chlorides, not a guarantee; temperature, crevices, deposits and weld finish matter as much.
Intergranular corrosion testing of ferritic and martensitic plate is by agreement (GB/T 4334 or ASTM A763 practices).
If service is harsher than 019Cr18CuNb can handle, the next step up in this batch is GB/T 4237 019Cr21CuTi S12182.
Welding and fabrication of 019Cr18CuNb
Stabilized 17–18% Cr ferritics weld much better than 430: use ER430Ti/ER439 or ER308L/309L filler. Low heat input and fast travel limit grain coarsening.
Plain 10Cr17 (430) needs a preheat of about 150–200 °C on thick sections and, ideally, a post-weld anneal at 760–820 °C to restore ductility and corrosion resistance.
Cutting: we cut 019Cr18CuNb by plasma (up to about 150 mm), laser (thin plate) or waterjet, and remove the heat-affected edge by machining where the drawing requires it.
How 019Cr18CuNb plate is heat treated
Recommended heat treatment for 019Cr18CuNb (GB/T 4237-2015 Annex C): 800 – 1 050 °C, rapid cooling.
Avoid holding ferritic plate at 400–550 °C (475 °C embrittlement) and do not overheat above about 950 °C, which coarsens grain.
Where this plate goes
Typical uses:
- Kitchen appliances and sinks
- Automotive exhaust and trim
- Building interior panels
- Electrical cabinets
Buyers specifying 019Cr18CuNb for these jobs often compare it with GB/T 4237 019Cr21CuTi S12182 and GB/T 4237 10Cr17 S11710; the comparison table on this page shows the differences.
International grade pages for the alternatives mentioned above: JIS G4305 SUS443J1, ASTM A240 Type 439, ASTM A240 Type 430.
Surface finish and processing
| Finish | Description | Availability for this grade |
|---|---|---|
| No.1 / 1D | Hot rolled, heat treated, pickled; the GB/T 4237 standard surface | Standard |
| Shot-blasted + pickled | Uniform matte for welded structures | On request |
| No.4 / brushed | Abrasive finish, grit 150–180 | Warehouse processing, thin plate |
| HL (hairline) | Long continuous lines, decorative | Warehouse processing, thin plate |
| 8K mirror | Polished reflective finish | Warehouse processing, limited sizes |
| 2B / BA | Cold-rolled finishes (ordered as GB/T 3280 sheet, not hot-rolled plate) | Sheet only |
Our warehouse cuts plate to size (plasma, laser, waterjet, saw), bevels weld edges, polishes and applies PVC protective film. Processed plate ships with the original mill heat number marked. Ask for cut pieces of other stainless steel products at the same time to consolidate freight.
Dimensions and plate weight
| Dimension | Typical supply |
|---|---|
| Thickness | 2 – 12 mm |
| Width | 1 000 / 1 219 / 1 250 / 1 500 / 1 800 / 2 000 mm; wider by mill order |
| Length | 2 000 / 2 438 / 3 000 / 6 000 mm or cut to size |
| Flatness | Per GB/T 4237; ≤15 mm per metre for plate up to 25 mm unless agreed tighter |
| Thickness tolerance | Per the GB/T 4237 dimensional tolerance tables (normal or higher accuracy as ordered) |
| Edge | Mill edge or cut edge |
Weight: plate mass in kg/m² = thickness (mm) × density (7.7 g/cm³). A 10 mm 019Cr18CuNb plate weighs about 77.0 kg/m²; a 1 500 × 6 000 × 10 mm plate about 693 kg.
Testing and certification
- Heat chemical analysis on every heat; product analysis by agreement
- Tensile test (Rp0.2, Rm, A) per batch
- Hardness test
- 180° bend test
- Ultrasonic testing (NB/T 47013.3 or ASTM A578) when specified
- Positive material identification (PMI) on every plate leaving our warehouse
- Visual and dimensional inspection; third-party inspection (SGS, BV, TÜV, Intertek) at the buyer’s request
Certificates follow EN 10204 3.1 as standard. Where plate is also certified to ASME SA240 or ASTM A240, both standards are shown on one certificate.
What to put on a 019Cr18CuNb purchase order
- Standard and edition: GB/T 4237-2015
- Grade and code: 019Cr18CuNb (S11882); add the equivalent if dual certification is needed
- Thickness × width × length, quantity in pieces or tonnes
- Thickness tolerance class and flatness if tighter than standard
- Surface finish and protective film
- Tests beyond the standard (IGC, UT, impact, ferrite, PMI, grain size)
- Certificate type (EN 10204 3.1 / 3.2) and inspection body
- Marking, packing (wooden cases, steel pallets) and delivery terms
Send the list to SHH STEEL and we return a quotation with mill, lead time and stock options. Other grades from the same standard can be combined in one shipment; browse GB/T 4237 plate grades.
Where our plate comes from
019Cr18CuNb is produced by a small number of Chinese mills with the melting and heat treatment capability for it. We place mill orders for it through the producers we represent and do not usually hold it in stock. Expect about 45–90 days, with minimum quantities per thickness; we can combine small quantities into one rolling where the mill allows.
Every plate is traceable to its heat number, and copies of the mill certificates stay on file for repeat orders and audits. The same mills also supply our ASTM A240, ASME SA240, JIS G4305 and AISI plate ranges, so mixed-standard orders can ship together.
What SHH STEEL adds
- Mill-direct prices with our own export documentation
- Own processing warehouse: cutting, bevelling, polishing, PVC film
- PMI and dimensional check before packing
- Mixed-grade shipments across our AISI stainless and GB/T plate ranges
- Technical answers from people who read the standard, not just the price list
SHH STEEL has exported stainless and carbon steel plate to buyers in Asia, the Middle East, Africa, Europe and the Americas.
FAQ
-
What is 019Cr18CuNb?
- 019Cr18CuNb (S11882) is a low-C, Nb-stabilized 18Cr ferritic with 0.30–0.80% copper, similar to JIS SUS430J1L. GB/T 4237-2015 gives 205 MPa proof, 390 MPa tensile and 22% elongation minimum.
-
What is the chemical composition of 019Cr18CuNb?
- Under GB/T 4237-2015 Table 17, 019Cr18CuNb (S11882) has C ≤ 0.025, Cr 16.00 – 20.00, Ni ≤ 0.60, N ≤ 0.025, Cu 0.30 – 0.80; Nb: 8 × (C+N) – 0.8. Phosphorus is limited to ≤0.040% and sulfur to ≤0.030%.
-
What is the ASTM equivalent of 019Cr18CuNb?
- The closest equivalents of 019Cr18CuNb (S11882) are SUS430J1L in JIS (common name: 430J1L). Chemistry limits differ slightly, so dual certification depends on the actual heat.
-
What are the mechanical properties of 019Cr18CuNb plate?
- GB/T 4237-2015 Table 22 requires for 019Cr18CuNb: proof strength Rp0.2 ≥205 MPa, tensile strength ≥390 MPa and elongation ≥22%, hardness ≤192 HBW. Values apply to plate in the delivery heat-treated condition.
-
Is 019Cr18CuNb stainless steel magnetic?
- Yes. 019Cr18CuNb is ferritic and is magnetic in all conditions.
-
What thickness of 019Cr18CuNb plate can you supply?
- Under GB/T 4237 we supply 019Cr18CuNb hot-rolled plate in 2 – 12 mm, widths up to 2 000 mm (wider by mill order), cut to size in our warehouse. Thinner material is cold-rolled sheet to GB/T 3280.
Conclusion
GB/T 4237 019Cr18CuNb (S11882) is a 17–18% chromium ferritic plate grade, known internationally as 430J1L. It is defined by Table 17 chemistry (C ≤ 0.025, Cr 16.00 – 20.00, Ni ≤ 0.60, N ≤ 0.025, Cu 0.30 – 0.80) and Table 22 properties of at least 205 MPa proof strength and 390 MPa tensile strength. Typical uses include kitchen appliances and sinks, automotive exhaust and trim and building interior panels. Copper-bearing ferritics are mostly made as cold-rolled sheet; hot-rolled plate under GB/T 4237 is thin (around 3–6 mm) and by mill order.
Before ordering, state the standard edition, the grade name with its code, and any extra tests, so that the mill certificate matches your design documents. SHH STEEL supplies 019Cr18CuNb plate by mill order through the producers we represent, cut to size and finished in our own warehouse, with EN 10204 3.1 certificates. For related grades see GB/T 4237 019Cr21CuTi S12182 and GB/T 4237 022Cr17NbTi S11763, our GB/T 4237 category and the JIS G4305 SUS430J1 page. Send your sizes and quantities for a quotation.