GB/T 4237 06Cr18Ni11Nb (S34778) stainless steel plate at SHH STEEL warehouse

GB/T 4237 06Cr18Ni11Nb S34778 Stainless Steel Plate Supplier

GB/T 4237 06Cr18Ni11Nb (S34778) is an austenitic stainless steel plate equivalent to 347, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 100 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.
Keywords
06Cr18Ni11Nb, S34778, 347 stainless plate, 0Cr18Ni11Nb, GB/T 4237 06Cr18Ni11Nb, 06Cr18Ni11Nb stainless steel plate, 06Cr18Ni11Nb plate, S34778 stainless steel, 06Cr18Ni11Nb S34778, 06Cr18Ni11Nb supplier
Equivalent Grades:
ASTM A240 Type 347, S34700 / EN 10088-2 X6CrNiNb18-10, 1.4550 / JIS G4304 SUS347 — Material Specification: GB/T 4237-2015 (06Cr18Ni11Nb, unified code S34778) — Delivery: ≥ 1 040 °C, water quench or other rapid cooling
Share:
Overview
Specification
Chemical Composition
Product Analysis
Stabilization
Mechanical Properties
Heat Treatment
Corrosion Resistance
Equivalent Grades
Welding & Fabrication
Applications
Grade Comparison
Surface & Processing
Dimensions
Testing & Certificates
Ordering
Mill Sourcing
FAQ
Conclusion

06Cr18Ni11Nb S34778 plate at a glance

06Cr18Ni11Nb is 347: niobium 10 × C to 1.00% stabilizes carbon. Niobium carbides are more stable than titanium carbides during welding, so 347 resists knife-line attack better and is the usual welding filler for 321 too.

Reading the designation: ’06’ gives the carbon level (C ≤0.08% in GB/T 4237), followed by Cr18 = about 18% chromium; Ni11 = about 11% nickel; Nb = niobium added. S34778 is the unified numeric code (ISC) used in GB/T 4237-2015. Older drawings and Chinese buyers may still write the pre-2007 name 0Cr18Ni11Nb.

SHH STEEL produces and exports austenitic stainless plate from China, works as a sales agent for leading stainless mills, and runs its own processing warehouse for cutting and surface finishing. 06Cr18Ni11Nb is part of our GB/T 4237 stainless plate range; for comparison, see our ASTM A240 Type 347 page.

GB/T 4237 06Cr18Ni11Nb specification details

Item GB/T 4237-2015 requirement / SHH STEEL supply
Standard GB/T 4237-2015 Hot rolled stainless steel plate, sheet and strip (current edition, replaces GB/T 4237-2007)
Grade / unified code 06Cr18Ni11Nb / S34778
Steel class Austenitic
Chemical composition Table 15 (heat analysis); product analysis per GB/T 222
Mechanical properties Table 20
Product forms Hot-rolled thick plate (3.0 – 200 mm in the standard), hot-rolled wide strip and cut plate (2.0 – 25.4 mm)
Our usual thickness range 3 – 100 mm
Delivery condition ≥ 1 040 °C, water quench or other rapid cooling
Surface Hot rolled, heat treated, pickled (No.1 / 1D) as standard; ground or polished by agreement
Density 7.93 g/cm³
Certificate EN 10204 3.1 mill certificate; 3.2 with third-party inspection on request

Sister grades on the same standard are listed under GB/T 4237; cold-rolled sheet of the same chemistry is ordered to GB/T 3280, and all our plate lines sit in stainless steel sheets and plates.

06Cr18Ni11Nb chemical composition (heat analysis)

Element 06Cr18Ni11Nb heat analysis, % (Table 15) Why it matters
C ≤ 0.08 Carbon. Low values protect welds from carbide precipitation; higher values add hot strength or hardenability.
Si ≤ 0.75 Silicon. Deoxidizer; in heat-resistant grades it builds a protective scale.
Mn ≤ 2.00 Manganese. Deoxidizer; in Mn-bearing grades it replaces nickel and keeps nitrogen in solution.
P ≤ 0.045 Phosphorus. Impurity, kept low for toughness and weld cracking resistance.
S ≤ 0.030 Sulfur. Impurity; low sulfur improves pitting resistance, hot workability and polishability.
Cr 17.00 – 19.00 Chromium. Forms the passive film; the main driver of corrosion and oxidation resistance.
Ni 9.00 – 13.00 Nickel. Stabilizes austenite, improves toughness and resistance to reducing acids.
Other Nb: 10 × C – 1.00 Stabilizing / special-element requirement of the standard
PREN (Cr + 3.3Mo + 16N) 17.0 – 18.0 (minimum – mid-range) Calculated from the limits above, not a requirement of GB/T 4237

Values are maximum unless a range is given. The mill reports the ladle (heat) analysis on the certificate; this is the figure to compare with Table 15.

Product analysis vs heat analysis

A check analysis drilled from the finished plate may differ slightly from the heat analysis. GB/T 4237 refers to GB/T 222 for the permitted deviations; the table applies them to the 06Cr18Ni11Nb limits. Deviations apply to one side of a range only, never to both sides in the same heat.

Element Heat analysis limit (%) Permitted deviation Product analysis limit (%)
C ≤ 0.08 ±0.01 ≤ 0.09
Si ≤ 0.75 ±0.05 ≤ 0.80
Mn ≤ 2.00 ±0.04 ≤ 2.04
P ≤ 0.045 +0.010 ≤ 0.055
S ≤ 0.030 +0.005 ≤ 0.035
Cr 17.00 – 19.00 ±0.20 16.80 – 19.20
Ni 9.00 – 13.00 ±0.10 (min) / ±0.15 (max) 8.90 – 13.15

Where the table says ‘by agreement’, the deviation is not tabulated for that content level and should be agreed in the contract, usually by reference to ASTM A480 Table A1.1.

How titanium or niobium stabilization works

In 06Cr18Ni11Nb the stabilizing element forms carbides that are more stable than chromium carbide, so chromium stays in solution even when the steel passes through 450–850 °C. The standard sets the minimum ratio: Nb: 10 × C – 1.00.

The ratio works only if carbon and nitrogen are measured and titanium or niobium is high enough. Check the certificate: for a 0.05% C heat, Ti ≥5×C means Ti ≥0.25%; many buyers ask for a margin above the minimum.

Compared with the low-carbon route (GB/T 4237 022Cr19Ni10 S30403 and GB/T 4237 022Cr17Ni12Mo2 S31603), stabilized grades keep more strength above 500 °C, which is why boiler and refinery designers still use them.

Mechanical properties of 06Cr18Ni11Nb plate

Property 06Cr18Ni11Nb (Table 20)
Proof strength Rp0.2, MPa ≥ 205
Tensile strength Rm, MPa ≥ 515
Elongation A, % ≥ 40
Hardness HBW ≤ 201
Hardness HRB ≤ 92
Hardness HV ≤ 210

Values apply to plate in the delivery heat-treated condition, tested transversely per GB/T 228.1. Hardness is checked by one method chosen by the mill.

How 06Cr18Ni11Nb plate is heat treated

Recommended heat treatment for 06Cr18Ni11Nb (GB/T 4237-2015 Annex C): ≥ 1 040 °C, water quench or other rapid cooling.

A stabilizing anneal at about 870–900 °C after welding can be added for parts that will see 450–850 °C service.

How 06Cr18Ni11Nb performs in corrosive service

Stabilized grades are bought for intergranular corrosion resistance after welding or after service in the 450–850 °C sensitization range. General corrosion resistance is similar to 304 (or 316 for Mo grades).

PREN of 06Cr18Ni11Nb from the GB/T 4237 limits: 17.0 – 18.0. PREN is a ranking tool for pitting in chlorides, not a guarantee; temperature, crevices, deposits and weld finish matter as much.

Intergranular corrosion: GB/T 4237-2015 Table 30 lists this grade for the GB/T 4334 Method E (Cu–CuSO4–H2SO4) test after sensitizing treatment, the stricter condition reserved for low-carbon and stabilized grades. Bent specimens must show no intergranular cracks.

If service is harsher than 06Cr18Ni11Nb can handle, the next step up in this batch is GB/T 4237 06Cr17Ni12Mo2Nb S31678.

06Cr18Ni11Nb equivalent grades: ASTM, EN, JIS

Standard system Equivalent / closest grade
China GB/T 4237-2015 06Cr18Ni11Nb (S34778)
Former Chinese name 0Cr18Ni11Nb
ASTM A240/A240M Type 347 / S34700
EN 10088-2 X6CrNiNb18-10 / 1.4550
JIS G4304 (hot rolled) SUS347
Common name 347

Equivalent grades are close in chemistry and properties but are never identical: limits on carbon, nitrogen and residual elements differ. For dual or multiple certification the heat must meet every standard named on the order, and we confirm that from the heat chemistry before quotation.

Related pages: ASTM A240 Type 347, ASME SA240 347, JIS G4305 SUS347, AISI 347. See also our ASTM A240/A240M and JIS G4305 plate lists.

Fabrication guidance

Weld stabilized grades with Nb-stabilized filler (ER347 / E347) — titanium does not transfer well across the arc, so ER321 is rarely used. For 316Ti use ER318 or ER316L.

Knife-line attack can occur in a narrow band next to the fusion line if the part sees 450–850 °C service after welding. If that is the case, ask for a stabilizing anneal (around 870–900 °C) in the procedure.

Cutting: we cut 06Cr18Ni11Nb by plasma (up to about 150 mm), laser (thin plate) or waterjet, and remove the heat-affected edge by machining where the drawing requires it.

Typical uses of GB/T 4237 06Cr18Ni11Nb

Where the stabilized chemistry pays off:

  • Petrochemical and synthetic fibre plants
  • Large boiler superheaters, reheaters and steam pipes (Annex B)
  • Nuclear power structures
  • Welded parts working at 400–800 °C

Buyers specifying 06Cr18Ni11Nb for these jobs often compare it with GB/T 4237 07Cr18Ni11Nb S34779 and GB/T 4237 06Cr17Ni12Mo2Nb S31678; the comparison table on this page shows the differences.

International grade pages for the alternatives mentioned above: ASTM A240 Type 347H, ASTM A240 Type 321, ASTM A240 Type 316Ti.

06Cr18Ni11Nb compared with related grades

The table compares 06Cr18Ni11Nb with the grades buyers most often weigh it against. Strength values are GB/T 4237-2015 minimums; PREN is calculated from the minimum chemistry.

Grade (GB/T 4237) Key chemistry, % PREN min Rp0.2 min, MPa Rm min, MPa
06Cr18Ni11Nb S34778 C ≤ 0.08, Cr 17.00 – 19.00, Ni 9.00 – 13.00 17.0 205 515
GB/T 4237 07Cr18Ni11Nb S34779 C 0.04 – 0.10, Cr 17.00 – 19.00, Ni 9.00 – 13.00 17.0 205 515
GB/T 4237 06Cr18Ni11Ti S32168 C ≤ 0.08, Cr 17.00 – 19.00, Ni 9.00 – 12.00, N ≤ 0.10 17.0 205 515
GB/T 4237 06Cr17Ni12Mo2Nb S31678 C ≤ 0.08, Cr 16.00 – 18.00, Ni 10.00 – 14.00, Mo 2.00 – 3.00, N ≤ 0.10 22.6 205 515

Nb-stabilized welds can hot crack in heavy sections; use ER347 with controlled ferrite (FN 3–8). Polishes better than 321.

Surface options and cut-to-size service

Finish Description Availability for this grade
No.1 / 1D Hot rolled, heat treated, pickled; the GB/T 4237 standard surface Standard
Shot-blasted + pickled Uniform matte for welded structures On request
No.4 / brushed Abrasive finish, grit 150–180 Warehouse processing, thin plate
HL (hairline) Long continuous lines, decorative Warehouse processing, thin plate
8K mirror Polished reflective finish Warehouse processing, limited sizes
2B / BA Cold-rolled finishes (ordered as GB/T 3280 sheet, not hot-rolled plate) Sheet only

Our warehouse cuts plate to size (plasma, laser, waterjet, saw), bevels weld edges, polishes and applies PVC protective film. Processed plate ships with the original mill heat number marked. Ask for cut pieces of other stainless steel products at the same time to consolidate freight.

Sizes, tolerances and weight

Dimension Typical supply
Thickness 3 – 100 mm
Width 1 000 / 1 219 / 1 250 / 1 500 / 1 800 / 2 000 mm; wider by mill order
Length 2 000 / 2 438 / 3 000 / 6 000 mm or cut to size
Flatness Per GB/T 4237; ≤15 mm per metre for plate up to 25 mm unless agreed tighter
Thickness tolerance Per the GB/T 4237 dimensional tolerance tables (normal or higher accuracy as ordered)
Edge Mill edge or cut edge

Weight: plate mass in kg/m² = thickness (mm) × density (7.93 g/cm³). A 10 mm 06Cr18Ni11Nb plate weighs about 79.3 kg/m²; a 1 500 × 6 000 × 10 mm plate about 714 kg.

Inspection, tests and mill certificates

  • Heat chemical analysis on every heat; product analysis by agreement
  • Tensile test (Rp0.2, Rm, A) per batch
  • Hardness test
  • Intergranular corrosion test, GB/T 4334 Method E (Table 30)
  • Ultrasonic testing (NB/T 47013.3 or ASTM A578) when specified
  • Positive material identification (PMI) on every plate leaving our warehouse
  • Visual and dimensional inspection; third-party inspection (SGS, BV, TÜV, Intertek) at the buyer’s request

Certificates follow EN 10204 3.1 as standard. Where plate is also certified to ASME SA240 or ASTM A240, both standards are shown on one certificate.

How to order

  • Standard and edition: GB/T 4237-2015
  • Grade and code: 06Cr18Ni11Nb (S34778); add the equivalent if dual certification is needed
  • Thickness × width × length, quantity in pieces or tonnes
  • Thickness tolerance class and flatness if tighter than standard
  • Surface finish and protective film
  • Tests beyond the standard (IGC, UT, impact, ferrite, PMI, grain size)
  • Certificate type (EN 10204 3.1 / 3.2) and inspection body
  • Marking, packing (wooden cases, steel pallets) and delivery terms

Send the list to SHH STEEL and we return a quotation with mill, lead time and stock options. Other grades from the same standard can be combined in one shipment; browse GB/T 4237 plate grades.

Supply chain and lead time

06Cr18Ni11Nb is a mainstream grade at Chinese stainless mills. We supply it from our own stock and processing warehouse, and by mill order from major producers such as TISCO and Baosteel Stainless, for which we act as a sales agent. Stock plate ships in about 1–2 weeks after cutting; mill orders typically take 30–60 days depending on thickness and rolling schedule.

Every plate is traceable to its heat number, and copies of the mill certificates stay on file for repeat orders and audits. The same mills also supply our ASTM A240, ASME SA240, JIS G4305 and AISI plate ranges, so mixed-standard orders can ship together.

FAQ

Is 347 better than 321?
For welded high-temperature parts, often yes. 347 (06Cr18Ni11Nb) uses Nb 10×C–1.00% instead of Ti, giving more stable carbides through welding, less knife-line attack and better surface finish. 321 is cheaper and more common.
What is the chemical composition of 06Cr18Ni11Nb?
Under GB/T 4237-2015 Table 15, 06Cr18Ni11Nb (S34778) has C ≤ 0.08, Cr 17.00 – 19.00, Ni 9.00 – 13.00; Nb: 10 × C – 1.00. Phosphorus is limited to ≤0.045% and sulfur to ≤0.030%.
What is the ASTM equivalent of 06Cr18Ni11Nb?
The closest equivalents of 06Cr18Ni11Nb (S34778) are Type 347 / S34700 in ASTM, X6CrNiNb18-10 / 1.4550 in EN, SUS347 in JIS (common name: 347). Chemistry limits differ slightly, so dual certification depends on the actual heat.
What are the mechanical properties of 06Cr18Ni11Nb plate?
GB/T 4237-2015 Table 20 requires for 06Cr18Ni11Nb: proof strength Rp0.2 ≥205 MPa, tensile strength ≥515 MPa and elongation ≥40%, hardness ≤201 HBW. Values apply to plate in the delivery heat-treated condition.
Is 06Cr18Ni11Nb stainless steel magnetic?
Not in the annealed condition. 06Cr18Ni11Nb is austenitic, so annealed plate is essentially non-magnetic; cold work can induce slight magnetism, mostly at cut and bent edges.
What thickness of 06Cr18Ni11Nb plate can you supply?
Under GB/T 4237 we supply 06Cr18Ni11Nb hot-rolled plate in 3 – 100 mm, widths up to 2 000 mm (wider by mill order), cut to size in our warehouse. Thinner material is cold-rolled sheet to GB/T 3280.

Conclusion

GB/T 4237 06Cr18Ni11Nb (S34778) is a stabilized austenitic plate grade, known internationally as 347. It is defined by Table 15 chemistry (C ≤ 0.08, Cr 17.00 – 19.00, Ni 9.00 – 13.00) and Table 20 properties of at least 205 MPa proof strength and 515 MPa tensile strength. Typical uses include petrochemical and synthetic fibre plants, large boiler superheaters, reheaters and steam pipes and nuclear power structures. Nb-stabilized welds can hot crack in heavy sections; use ER347 with controlled ferrite (FN 3–8).

Before ordering, state the standard edition, the grade name with its code, and any extra tests, so that the mill certificate matches your design documents. SHH STEEL supplies 06Cr18Ni11Nb plate from stock and by mill order, cut to size and finished in our own warehouse, with EN 10204 3.1 certificates. For related grades see GB/T 4237 07Cr18Ni11Nb S34779 and GB/T 4237 06Cr18Ni11Ti S32168, our GB/T 4237 category and the ASTM A240 Type 347 page. Send your sizes and quantities for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X