SHH STEEL offers GB/T 4237-compliant 304/316 stainless steel plates. GB/T 4237 specifies hot-rolled stainless steel plates, sheets, and strips for general applications. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GB/T 4237 022Cr19Ni16Mo5N S31723 Stainless Steel Plate Supplier
GB/T 4237 022Cr19Ni16Mo5N (S31723) is an austenitic stainless steel plate equivalent to 317LMN, with 240 MPa minimum proof strength and 550 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 120 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr19Ni13Mo4N S31753 Stainless Steel Plate Supplier
GB/T 4237 022Cr19Ni13Mo4N (S31753) is an austenitic stainless steel plate equivalent to 317LN, with 240 MPa minimum proof strength and 550 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 120 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr19Ni13Mo3 S31703 Stainless Steel Plate Supplier
GB/T 4237 022Cr19Ni13Mo3 (S31703) is an austenitic stainless steel plate equivalent to 317L, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 120 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 06Cr19Ni13Mo3 S31708 Stainless Steel Plate Supplier
GB/T 4237 06Cr19Ni13Mo3 (S31708) is an austenitic stainless steel plate equivalent to 317, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 120 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr25Ni22Mo2N S31053 Stainless Steel Plate Supplier
GB/T 4237 022Cr25Ni22Mo2N (S31053) is an austenitic stainless steel plate equivalent to 310MoLN, with 270 MPa minimum proof strength and 580 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 50 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 06Cr25Ni20 S31008 Stainless Steel Plate Supplier
GB/T 4237 06Cr25Ni20 (S31008) is an austenitic stainless steel plate equivalent to 310S, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 80 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 06Cr23Ni13 S30908 Stainless Steel Plate Supplier
GB/T 4237 06Cr23Ni13 (S30908) is an austenitic stainless steel plate equivalent to 309S, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 80 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 07Cr18Ni11Nb S34779 Stainless Steel Plate Supplier
GB/T 4237 07Cr18Ni11Nb (S34779) is an austenitic stainless steel plate equivalent to 347H, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 100 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 06Cr18Ni11Nb S34778 Stainless Steel Plate Supplier
GB/T 4237 06Cr18Ni11Nb (S34778) is an austenitic stainless steel plate equivalent to 347, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 100 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 07Cr19Ni11Ti S32169 Stainless Steel Plate Supplier
GB/T 4237 07Cr19Ni11Ti (S32169) is an austenitic stainless steel plate equivalent to 321H, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 100 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 06Cr18Ni11Ti S32168 Stainless Steel Plate Supplier
GB/T 4237 06Cr18Ni11Ti (S32168) is an austenitic stainless steel plate equivalent to 321, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 100 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 06Cr18Ni12Mo2Cu2 S31688 Stainless Steel Plate Supplier
GB/T 4237 06Cr18Ni12Mo2Cu2 (S31688) is an austenitic stainless steel plate equivalent to 316J1, with 205 MPa minimum proof strength and 520 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 120 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More
GB/T 4237 Stainless Steel Products
Stainless Steel Sheets and Plates
SHH STEEL, a leading Stainless Steel Sheets and Plates exporter, produces and exports stainless steel sheets (0.3–6 mm) and plates (>6 mm) for marine, chemical, and structural applications. Our products, like 304 and 316L (ASTM A240), offer corrosion resistance and durability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for 316L stainless steel plates and custom solutions for your projects.