GB/T 4237 022Cr19Ni16Mo5N (S31723) stainless steel plate at SHH STEEL warehouse

GB/T 4237 022Cr19Ni16Mo5N S31723 Stainless Steel Plate Supplier

GB/T 4237 022Cr19Ni16Mo5N (S31723) is an austenitic stainless steel plate equivalent to 317LMN, with 240 MPa minimum proof strength and 550 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 120 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.
Keywords
022Cr19Ni16Mo5N, S31723, 317LMN, 1.4439, GB/T 4237 022Cr19Ni16Mo5N, 022Cr19Ni16Mo5N stainless steel plate, 022Cr19Ni16Mo5N plate, S31723 stainless steel, 022Cr19Ni16Mo5N S31723, 022Cr19Ni16Mo5N supplier
Equivalent Grades:
ASTM A240 317LMN, S31726 / EN 10088-2 X2CrNiMoN17-13-5, 1.4439 — Material Specification: GB/T 4237-2015 (022Cr19Ni16Mo5N, unified code S31723) — Delivery: ≥ 1 040 °C, water quench or other rapid cooling
Share:
Overview
Chemical Composition
Product Analysis
Mechanical Properties
Corrosion Resistance
Equivalent Grades
Specification
Grade Comparison
Welding & Fabrication
Heat Treatment
Surface & Processing
Applications
Dimensions
Testing & Certificates
Mill Sourcing
Ordering
Why SHH STEEL
FAQ
Conclusion

GB/T 4237 022Cr19Ni16Mo5N: what it is and who uses it

022Cr19Ni16Mo5N is 317LMN: Mo 4.00–5.00%, Ni 13.50–17.50% and N 0.10–0.20%. It bridges 317L and the 6Mo super austenitics, with a minimum PREN of about 32.

How to read the name: under GB/T 20878 the leading ‘022’ is the carbon code (here C ≤0.030%), then Cr19 = about 19% chromium; Ni16 = about 16% nickel; Mo5 = about 5% molybdenum; N = nitrogen added. S31723 is the unified numeric code (ISC) used in GB/T 4237-2015.

SHH STEEL produces and exports austenitic stainless plate from China, works as a sales agent for leading stainless mills, and runs its own processing warehouse for cutting and surface finishing. 022Cr19Ni16Mo5N is part of our GB/T 4237 stainless plate range; for comparison, see our AISI 317LMN page.

022Cr19Ni16Mo5N chemical composition (heat analysis)

Element 022Cr19Ni16Mo5N heat analysis, % (Table 15) Why it matters
C ≤ 0.030 Carbon. Low values protect welds from carbide precipitation; higher values add hot strength or hardenability.
Si ≤ 0.75 Silicon. Deoxidizer; in heat-resistant grades it builds a protective scale.
Mn ≤ 2.00 Manganese. Deoxidizer; in Mn-bearing grades it replaces nickel and keeps nitrogen in solution.
P ≤ 0.045 Phosphorus. Impurity, kept low for toughness and weld cracking resistance.
S ≤ 0.030 Sulfur. Impurity; low sulfur improves pitting resistance, hot workability and polishability.
Cr 17.00 – 20.00 Chromium. Forms the passive film; the main driver of corrosion and oxidation resistance.
Ni 13.50 – 17.50 Nickel. Stabilizes austenite, improves toughness and resistance to reducing acids.
Mo 4.00 – 5.00 Molybdenum. Raises pitting and crevice resistance in chlorides (×3.3 in PREN).
N 0.10 – 0.20 Nitrogen. Strengthens, stabilizes austenite and adds pitting resistance (×16 in PREN).
PREN (Cr + 3.3Mo + 16N) 31.8 – 35.8 (minimum – mid-range) Calculated from the limits above, not a requirement of GB/T 4237

Values are maximum unless a range is given. The mill reports the ladle (heat) analysis on the certificate; this is the figure to compare with Table 15.

Product analysis vs heat analysis

A check analysis drilled from the finished plate may differ slightly from the heat analysis. GB/T 4237 refers to GB/T 222 for the permitted deviations; the table applies them to the 022Cr19Ni16Mo5N limits. Deviations apply to one side of a range only, never to both sides in the same heat.

Element Heat analysis limit (%) Permitted deviation Product analysis limit (%)
C ≤ 0.030 +0.005 ≤ 0.035
Si ≤ 0.75 ±0.05 ≤ 0.80
Mn ≤ 2.00 ±0.04 ≤ 2.04
P ≤ 0.045 +0.010 ≤ 0.055
S ≤ 0.030 +0.005 ≤ 0.035
Cr 17.00 – 20.00 ±0.20 16.80 – 20.20
Ni 13.50 – 17.50 ±0.15 13.35 – 17.65
Mo 4.00 – 5.00 ±0.10 3.90 – 5.10
N 0.10 – 0.20 ±0.01 (min) / ±0.02 (max) 0.09 – 0.22

Where the table says ‘by agreement’, the deviation is not tabulated for that content level and should be agreed in the contract, usually by reference to ASTM A480 Table A1.1.

Mechanical properties at room temperature

Property 022Cr19Ni16Mo5N (Table 20)
Proof strength Rp0.2, MPa ≥ 240
Tensile strength Rm, MPa ≥ 550
Elongation A, % ≥ 40
Hardness HBW ≤ 223
Hardness HRB ≤ 96
Hardness HV ≤ 225

Values apply to plate in the delivery heat-treated condition, tested transversely per GB/T 228.1. Hardness is checked by one method chosen by the mill.

Corrosion behaviour and intergranular corrosion tests

Molybdenum raises resistance to chlorides, sulfurous media and reducing acids. The low-carbon and nitrogen variants keep that resistance across welds.

PREN of 022Cr19Ni16Mo5N from the GB/T 4237 limits: 31.8 – 35.8. PREN is a ranking tool for pitting in chlorides, not a guarantee; temperature, crevices, deposits and weld finish matter as much.

Intergranular corrosion testing is not compulsory for this grade in GB/T 4237-2015; when required, the method (GB/T 4334, ASTM A262 or A923 for duplex) and acceptance are agreed in the order.

If service is harsher than 022Cr19Ni16Mo5N can handle, the next step up in this batch is GB/T 4237 015Cr20Ni18Mo6CuN S31252.

Cross-reference to other standards

Standard system Equivalent / closest grade
China GB/T 4237-2015 022Cr19Ni16Mo5N (S31723)
ASTM A240/A240M 317LMN / S31726
EN 10088-2 X2CrNiMoN17-13-5 / 1.4439
JIS G4304 (hot rolled) —
Common name 317LMN

Equivalent grades are close in chemistry and properties but are never identical: limits on carbon, nitrogen and residual elements differ. For dual or multiple certification the heat must meet every standard named on the order, and we confirm that from the heat chemistry before quotation.

Related pages: AISI 317LMN, AISI 317LM. See also our ASTM A240/A240M and JIS G4305 plate lists.

What the standard covers for this grade

Item GB/T 4237-2015 requirement / SHH STEEL supply
Standard GB/T 4237-2015 Hot rolled stainless steel plate, sheet and strip (current edition, replaces GB/T 4237-2007)
Grade / unified code 022Cr19Ni16Mo5N / S31723
Steel class Austenitic
Chemical composition Table 15 (heat analysis); product analysis per GB/T 222
Mechanical properties Table 20
Product forms Hot-rolled thick plate (3.0 – 200 mm in the standard), hot-rolled wide strip and cut plate (2.0 – 25.4 mm)
Our usual thickness range 3 – 120 mm (to 150 mm by mill order)
Delivery condition ≥ 1 040 °C, water quench or other rapid cooling
Surface Hot rolled, heat treated, pickled (No.1 / 1D) as standard; ground or polished by agreement
Density 8.0 g/cm³
Certificate EN 10204 3.1 mill certificate; 3.2 with third-party inspection on request

Sister grades on the same standard are listed under GB/T 4237; cold-rolled sheet of the same chemistry is ordered to GB/T 3280, and all our plate lines sit in stainless steel sheets and plates.

022Cr19Ni16Mo5N compared with related grades

The table compares 022Cr19Ni16Mo5N with the grades buyers most often weigh it against. Strength values are GB/T 4237-2015 minimums; PREN is calculated from the minimum chemistry.

Grade (GB/T 4237) Key chemistry, % PREN min Rp0.2 min, MPa Rm min, MPa
022Cr19Ni16Mo5N S31723 C ≤ 0.030, Cr 17.00 – 20.00, Ni 13.50 – 17.50, Mo 4.00 – 5.00, N 0.10 – 0.20 31.8 240 550
GB/T 4237 022Cr19Ni13Mo4N S31753 C ≤ 0.030, Cr 18.00 – 20.00, Ni 11.00 – 15.00, Mo 3.00 – 4.00, N 0.10 – 0.22 29.5 240 550
GB/T 4237 022Cr19Ni13Mo3 S31703 C ≤ 0.030, Cr 18.00 – 20.00, Ni 11.00 – 15.00, Mo 3.00 – 4.00, N ≤ 0.10 27.9 205 515
GB/T 4237 015Cr21Ni26Mo5Cu2 S31782 C ≤ 0.020, Cr 19.00 – 23.00, Ni 23.00 – 28.00, Mo 4.00 – 5.00, N ≤ 0.10, Cu 1.00 – 2.00 32.2 220 490
GB/T 4237 015Cr20Ni18Mo6CuN S31252 C ≤ 0.020, Cr 19.50 – 20.50, Ni 17.50 – 18.50, Mo 6.00 – 6.50, N 0.18 – 0.25, Cu 0.50 – 1.00 42.2 310 655

High Mo needs a high-alloy filler (ERNiCrMo-3 or -10 type) to keep weld pitting resistance. Plan lead time; this is a mill-order grade.

Welding and fabrication of 022Cr19Ni16Mo5N

Use ER316L/E316L filler, or ER317L when the weld must not be the weak point in chloride service. A small ferrite number (FN 3–10) in the weld metal prevents hot cracking.

Interpass ≤150 °C, no preheat, clean back purge with argon for root passes. Pickle and passivate after welding: heat tint lowers pitting resistance more in Mo grades than the weld itself.

Cutting: we cut 022Cr19Ni16Mo5N by plasma (up to about 150 mm), laser (thin plate) or waterjet, and remove the heat-affected edge by machining where the drawing requires it.

How 022Cr19Ni16Mo5N plate is heat treated

Recommended heat treatment for 022Cr19Ni16Mo5N (GB/T 4237-2015 Annex C): ≥ 1 040 °C, water quench or other rapid cooling.

Cool rapidly through 850–450 °C after annealing; slow cooling of thick Mo-bearing plate risks carbide and sigma precipitation.

Surface finish and processing

Finish Description Availability for this grade
No.1 / 1D Hot rolled, heat treated, pickled; the GB/T 4237 standard surface Standard
Shot-blasted + pickled Uniform matte for welded structures On request
No.4 / brushed Abrasive finish, grit 150–180 Warehouse processing, thin plate
HL (hairline) Long continuous lines, decorative Warehouse processing, thin plate
8K mirror Polished reflective finish Warehouse processing, limited sizes
2B / BA Cold-rolled finishes (ordered as GB/T 3280 sheet, not hot-rolled plate) Sheet only

Our warehouse cuts plate to size (plasma, laser, waterjet, saw), bevels weld edges, polishes and applies PVC protective film. Processed plate ships with the original mill heat number marked. Ask for cut pieces of other stainless steel products at the same time to consolidate freight.

Typical uses of GB/T 4237 022Cr19Ni16Mo5N

Where buyers specify it:

  • FGD absorbers and wet stacks
  • Pulp bleach plant equipment
  • Seawater-cooled condensers
  • Chemical tanks with chloride

Buyers specifying 022Cr19Ni16Mo5N for these jobs often compare it with GB/T 4237 022Cr19Ni13Mo4N S31753 and GB/T 4237 015Cr20Ni18Mo6CuN S31252; the comparison table on this page shows the differences.

International grade pages for the alternatives mentioned above: AISI 317L, ASTM A240 Type 317L, ASTM A240 Type 904L, AISI 254 SMO.

Sizes, tolerances and weight

Dimension Typical supply
Thickness 3 – 120 mm (to 150 mm by mill order)
Width 1 000 / 1 219 / 1 250 / 1 500 / 1 800 / 2 000 mm; wider by mill order
Length 2 000 / 2 438 / 3 000 / 6 000 mm or cut to size
Flatness Per GB/T 4237; ≤15 mm per metre for plate up to 25 mm unless agreed tighter
Thickness tolerance Per the GB/T 4237 dimensional tolerance tables (normal or higher accuracy as ordered)
Edge Mill edge or cut edge

Weight: plate mass in kg/m² = thickness (mm) × density (8.0 g/cm³). A 10 mm 022Cr19Ni16Mo5N plate weighs about 80.0 kg/m²; a 1 500 × 6 000 × 10 mm plate about 720 kg.

Inspection, tests and mill certificates

  • Heat chemical analysis on every heat; product analysis by agreement
  • Tensile test (Rp0.2, Rm, A) per batch
  • Hardness test
  • Ultrasonic testing (NB/T 47013.3 or ASTM A578) when specified
  • Positive material identification (PMI) on every plate leaving our warehouse
  • Visual and dimensional inspection; third-party inspection (SGS, BV, TÜV, Intertek) at the buyer’s request

Certificates follow EN 10204 3.1 as standard. Where plate is also certified to ASME SA240 or ASTM A240, both standards are shown on one certificate.

Where our plate comes from

022Cr19Ni16Mo5N is produced by a small number of Chinese mills with the melting and heat treatment capability for it. We place mill orders for it through the producers we represent and do not usually hold it in stock. Expect about 45–90 days, with minimum quantities per thickness; we can combine small quantities into one rolling where the mill allows.

Every plate is traceable to its heat number, and copies of the mill certificates stay on file for repeat orders and audits. The same mills also supply our ASTM A240, ASME SA240, JIS G4305 and AISI plate ranges, so mixed-standard orders can ship together.

How to order

  • Standard and edition: GB/T 4237-2015
  • Grade and code: 022Cr19Ni16Mo5N (S31723); add the equivalent if dual certification is needed
  • Thickness × width × length, quantity in pieces or tonnes
  • Thickness tolerance class and flatness if tighter than standard
  • Surface finish and protective film
  • Tests beyond the standard (IGC, UT, impact, ferrite, PMI, grain size)
  • Certificate type (EN 10204 3.1 / 3.2) and inspection body
  • Marking, packing (wooden cases, steel pallets) and delivery terms

Send the list to SHH STEEL and we return a quotation with mill, lead time and stock options. Other grades from the same standard can be combined in one shipment; browse GB/T 4237 plate grades.

Why buy from SHH STEEL

  • Mill-direct prices with our own export documentation
  • Own processing warehouse: cutting, bevelling, polishing, PVC film
  • PMI and dimensional check before packing
  • Mixed-grade shipments across our AISI stainless and GB/T plate ranges
  • Technical answers from people who read the standard, not just the price list

SHH STEEL has exported stainless and carbon steel plate to buyers in Asia, the Middle East, Africa, Europe and the Americas.

FAQ

What is 022Cr19Ni16Mo5N equivalent to?
022Cr19Ni16Mo5N (S31723) corresponds to ASTM 317LMN (S31726) and EN 1.4439 X2CrNiMoN17-13-5. GB/T 4237-2015 requires 240 MPa proof, 550 MPa tensile and 40% elongation.
What is the chemical composition of 022Cr19Ni16Mo5N?
Under GB/T 4237-2015 Table 15, 022Cr19Ni16Mo5N (S31723) has C ≤ 0.030, Cr 17.00 – 20.00, Ni 13.50 – 17.50, Mo 4.00 – 5.00, N 0.10 – 0.20. Phosphorus is limited to ≤0.045% and sulfur to ≤0.030%.
What are the mechanical properties of 022Cr19Ni16Mo5N plate?
GB/T 4237-2015 Table 20 requires for 022Cr19Ni16Mo5N: proof strength Rp0.2 ≥240 MPa, tensile strength ≥550 MPa and elongation ≥40%, hardness ≤223 HBW. Values apply to plate in the delivery heat-treated condition.
Is 022Cr19Ni16Mo5N stainless steel magnetic?
Not in the annealed condition. 022Cr19Ni16Mo5N is austenitic, so annealed plate is essentially non-magnetic; cold work can induce slight magnetism, mostly at cut and bent edges.
What thickness of 022Cr19Ni16Mo5N plate can you supply?
Under GB/T 4237 we supply 022Cr19Ni16Mo5N hot-rolled plate in 3 – 120 mm (to 150 mm by mill order), widths up to 2 000 mm (wider by mill order), cut to size in our warehouse. Thinner material is cold-rolled sheet to GB/T 3280.
What is the PREN of 022Cr19Ni16Mo5N?
Using PREN = Cr + 3.3Mo + 16N and the GB/T 4237-2015 limits, 022Cr19Ni16Mo5N has a PREN of about 31.8 at minimum chemistry and 35.8 at mid-range.

Conclusion

GB/T 4237 022Cr19Ni16Mo5N (S31723) is a molybdenum-bearing austenitic plate grade, known internationally as 317LMN. It is defined by Table 15 chemistry (C ≤ 0.030, Cr 17.00 – 20.00, Ni 13.50 – 17.50, Mo 4.00 – 5.00, N 0.10 – 0.20) and Table 20 properties of at least 240 MPa proof strength and 550 MPa tensile strength. Typical uses include fgd absorbers and wet stacks, pulp bleach plant equipment and seawater-cooled condensers. High Mo needs a high-alloy filler (ERNiCrMo-3 or -10 type) to keep weld pitting resistance.

Before ordering, state the standard edition, the grade name with its code, and any extra tests, so that the mill certificate matches your design documents. SHH STEEL supplies 022Cr19Ni16Mo5N plate by mill order through the producers we represent, cut to size and finished in our own warehouse, with EN 10204 3.1 certificates. For related grades see GB/T 4237 022Cr19Ni13Mo4N S31753 and GB/T 4237 022Cr19Ni13Mo3 S31703, our GB/T 4237 category and the AISI 317LMN page. Send your sizes and quantities for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X