Product Showcase
GB/T 4237 Stainless Steel Products
SHH STEEL offers GB/T 4237-compliant 304/316 stainless steel plates. GB/T 4237 specifies hot-rolled stainless steel plates, sheets, and strips for general applications. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GB/T 4237 022Cr15NbTi S11573 Stainless Steel Plate Supplier
GB/T 4237 022Cr15NbTi (S11573) is a ferritic stainless steel plate equivalent to 429-type Nb+Ti, with 205 MPa minimum proof strength and 450 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 12 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr11NbTi S11173 Stainless Steel Plate Supplier
GB/T 4237 022Cr11NbTi (S11173) is a ferritic stainless steel plate equivalent to 409 (Nb+Ti) / S40930, with 170 MPa minimum proof strength and 380 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 12 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr11Ti S11163 Stainless Steel Plate Supplier
GB/T 4237 022Cr11Ti (S11163) is a ferritic stainless steel plate equivalent to 409L, with 170 MPa minimum proof strength and 380 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 12 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 019Cr21CuTi S12182 Stainless Steel Plate Supplier
GB/T 4237 019Cr21CuTi (S12182) is a ferritic stainless steel plate equivalent to 443, with 205 MPa minimum proof strength and 390 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 10 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 019Cr18CuNb S11882 Stainless Steel Plate Supplier
GB/T 4237 019Cr18CuNb (S11882) is a ferritic stainless steel plate equivalent to 430J1L, with 205 MPa minimum proof strength and 390 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 12 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 019Cr23MoTi S12362 Stainless Steel Plate Supplier
GB/T 4237 019Cr23MoTi (S12362) is a ferritic stainless steel plate equivalent to 445J1, with 245 MPa minimum proof strength and 410 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 10 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 019Cr23Mo2Ti S12361 Stainless Steel Plate Supplier
GB/T 4237 019Cr23Mo2Ti (S12361) is a ferritic stainless steel plate equivalent to 445J2, with 245 MPa minimum proof strength and 410 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 10 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 019Cr18MoTi S11862 Stainless Steel Plate Supplier
GB/T 4237 019Cr18MoTi (S11862) is a ferritic stainless steel plate equivalent to 436L, with 245 MPa minimum proof strength and 410 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 10 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr17NbTi S11763 Stainless Steel Plate Supplier
GB/T 4237 022Cr17NbTi (S11763) is a ferritic stainless steel plate equivalent to 439 (Nb+Ti), with 175 MPa minimum proof strength and 360 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 12 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 06Cr13Al S11348 Stainless Steel Plate Supplier
GB/T 4237 06Cr13Al (S11348) is a ferritic stainless steel plate equivalent to 405, with 170 MPa minimum proof strength and 415 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 12 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 019Cr19Mo2NbTi S11972 Stainless Steel Plate Supplier
GB/T 4237 019Cr19Mo2NbTi (S11972) is a ferritic stainless steel plate equivalent to 444, with 275 MPa minimum proof strength and 415 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 10 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More -
GB/T 4237 022Cr18Ti S11863 Stainless Steel Plate Supplier
GB/T 4237 022Cr18Ti (S11863) is a ferritic stainless steel plate equivalent to 439 / 430Ti, with 205 MPa minimum proof strength and 415 MPa tensile strength. SHH STEEL supplies it hot rolled in 2 – 12 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.View More
GB/T 4237 Stainless Steel Products
Stainless Steel Sheets and Plates
SHH STEEL, a leading Stainless Steel Sheets and Plates exporter, produces and exports stainless steel sheets (0.3–6 mm) and plates (>6 mm) for marine, chemical, and structural applications. Our products, like 304 and 316L (ASTM A240), offer corrosion resistance and durability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for 316L stainless steel plates and custom solutions for your projects.
Stainless Steel Sheets and Plates
X