Product Showcase
JIS G4305 Stainless Steel Products
SHH STEEL offers JIS G4305-compliant 304/316 stainless steel plates. JIS G4305 specifies cold-rolled stainless steel plates, sheets, and strips for general applications. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
JIS G4305 SUS631 Steel Plate | 631 Stainless Steel
JIS G4305 SUS631 is a semi-austenitic precipitation-hardening stainless steel sheet and plate with 16 – 18 % chromium, 6.5 – 7.75 % nickel and 0.75 – 1.5 % aluminium. It is formed when soft and hardened to 1 230 N/mm² by RH950. SHH STEEL supplies SUS631 mill-direct with JIS G4305 compliance. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS440A Steel Plate | 440A Stainless Steel
JIS G4305 SUS440A is a high-carbon martensitic stainless steel sheet and plate with 0.60 – 0.75 % carbon and 16 – 18 % chromium. It reaches at least 40 HRC after quenching and tempering. SHH STEEL supplies SUS440A in the annealed condition, mill-direct with JIS G4305 compliance and 3.1 certificates. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS447J1 Steel Plate | 447J1 Stainless Steel
JIS G4305 SUS447J1 is a super-ferritic stainless steel sheet and plate with 28.5 – 32 % chromium, 1.5 – 2.5 % molybdenum and very low carbon and nitrogen. JSSA rates its weather resistance comparable to titanium. SHH STEEL supplies SUS447J1 mill-direct with JIS G4305 compliance, subject to mill availability. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS445J1 Steel Plate | 445J1 Stainless Steel
JIS G4305 SUS445J1 is a high-chromium ferritic stainless steel sheet and plate with 21 – 24 % chromium and 0.7 – 1.5 % molybdenum. JSSA rates its corrosion and weather resistance equal to or better than SUS444. SHH STEEL supplies SUS445J1 mill-direct with JIS G4305 compliance, subject to mill availability. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS430LX Steel Plate | 430LX Stainless Steel
JIS G4305 SUS430LX is a low-carbon, titanium- or niobium-stabilised ferritic stainless steel sheet and plate with 16 – 19 % chromium. It forms and welds better than SUS430 and is used for appliance parts. SHH STEEL supplies SUS430LX mill-direct with JIS G4305 compliance and 3.1 certificates. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS327L1 Steel Plate | 327L1 Stainless Steel
JIS G4305 SUS327L1 is the 2507-type super-duplex stainless steel plate and sheet with 24 – 26 % chromium, 6 – 8 % nickel, 3 – 5 % molybdenum and 0.24 – 0.32 % nitrogen. It gives 550 N/mm² minimum proof stress. SHH STEEL supplies SUS327L1 plate mill-direct with JIS G4305 compliance. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS323L Steel Plate | 323L Stainless Steel
JIS G4305 SUS323L is a lean duplex stainless steel plate and sheet with 21.5 – 24.5 % chromium, 3 – 5.5 % nickel and 0.05 – 0.20 % nitrogen, the JIS counterpart of 2304. It gives 400 N/mm² minimum proof stress. SHH STEEL supplies SUS323L plate mill-direct with JIS G4305 compliance. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS890L Steel Plate | 890L Stainless Steel
JIS G4305 SUS890L is the 904L-type high-alloy austenitic stainless steel plate and sheet, with 23 – 28 % nickel, 19 – 23 % chromium, 4 – 5 % molybdenum and 1 – 2 % copper. It is chosen for sulphuric and phosphoric acid service. SHH STEEL supplies SUS890L plate mill-direct with JIS G4305 compliance. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS317J1 Steel Plate | 317J1 Stainless Steel
JIS G4305 SUS317J1 is a high-molybdenum austenitic stainless steel plate and sheet with 16 – 19 % chromium, 15 – 17 % nickel and 4 – 6 % molybdenum, above SUS317L in pitting resistance. SHH STEEL supplies SUS317J1 plate mill-direct with JIS G4305 compliance and 3.1 certificates, subject to mill availability. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS312L Steel Plate | 312L Stainless Steel
JIS G4305 SUS312L is a 6 % molybdenum super-austenitic stainless steel plate and sheet with 19 – 21 % chromium, 17.5 – 19.5 % nickel, 6 – 7 % molybdenum and 0.16 – 0.25 % nitrogen. It is used for seawater and chloride service. SHH STEEL supplies SUS312L plate mill-direct with JIS G4305 compliance. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS316LN Steel Plate | 316LN Stainless Steel
JIS G4305 SUS316LN is a low-carbon, nitrogen-alloyed molybdenum austenitic stainless steel plate and sheet with 16.5 – 18.5 % chromium, 2 – 3 % molybdenum and 0.12 – 0.22 % nitrogen. It gives 245 N/mm² minimum proof stress. SHH STEEL supplies SUS316LN plate mill-direct with JIS G4305 compliance and 3.1 certificates. Plates are supplied with JIS G0415 3.1 inspection documents.View More -
JIS G4305 SUS304LN Steel Plate | 304LN Stainless Steel
JIS G4305 SUS304LN is a low-carbon, nitrogen-alloyed austenitic stainless steel plate and sheet with 17 – 19 % chromium, 8.5 – 11.5 % nickel and 0.12 – 0.22 % nitrogen. It gives 245 N/mm² minimum proof stress with 304L-type weldability. SHH STEEL supplies SUS304LN plate mill-direct with JIS G4305 compliance. Plates are supplied with JIS G0415 3.1 inspection documents.View More
JIS G4305 Stainless Steel Products
Stainless Steel Sheets and Plates
SHH STEEL, a leading Stainless Steel Sheets and Plates exporter, produces and exports stainless steel sheets (0.3–6 mm) and plates (>6 mm) for marine, chemical, and structural applications. Our products, like 304 and 316L (ASTM A240), offer corrosion resistance and durability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for 316L stainless steel plates and custom solutions for your projects.
Stainless Steel Sheets and Plates
X