GB/T 4237 022Cr19Ni13Mo3 (S31703) stainless steel plate at SHH STEEL warehouse

GB/T 4237 022Cr19Ni13Mo3 S31703 Stainless Steel Plate Supplier

GB/T 4237 022Cr19Ni13Mo3 (S31703) is an austenitic stainless steel plate equivalent to 317L, with 205 MPa minimum proof strength and 515 MPa tensile strength. SHH STEEL supplies it hot rolled in 3 – 120 mm, No.1 finish or polished, cut to size, with heat and product analysis on EN 10204 3.1 certificates.
Keywords
022Cr19Ni13Mo3, S31703, 317L, 00Cr19Ni13Mo3, GB/T 4237 022Cr19Ni13Mo3, 022Cr19Ni13Mo3 stainless steel plate, 022Cr19Ni13Mo3 plate, S31703 stainless steel, 022Cr19Ni13Mo3 S31703, 022Cr19Ni13Mo3 supplier
Equivalent Grades:
ASTM A240 Type 317L, S31703 / EN 10088-2 X2CrNiMo18-15-4, 1.4438 / JIS G4304 SUS317L — Material Specification: GB/T 4237-2015 (022Cr19Ni13Mo3, unified code S31703) — Delivery: ≥ 1 040 °C, water quench or other rapid cooling
Share:
Overview
Chemical Composition
Product Analysis
Mechanical Properties
Corrosion Resistance
Equivalent Grades
Specification
Grade Comparison
Welding & Fabrication
Heat Treatment
Surface & Processing
Applications
Dimensions
Testing & Certificates
Mill Sourcing
Ordering
Why SHH STEEL
FAQ
Conclusion

GB/T 4237 022Cr19Ni13Mo3: what it is and who uses it

022Cr19Ni13Mo3 is 317L, the standard ‘next step up’ from 316L in FGD absorbers, pulp bleaching and chemical plants. Carbon ≤0.030% with Mo 3.00–4.00% gives weld-safe corrosion resistance at a moderate premium.

Reading the designation: ‘022’ gives the carbon level (C ≤0.030% in GB/T 4237), followed by Cr19 = about 19% chromium; Ni13 = about 13% nickel; Mo3 = about 3% molybdenum. S31703 is the unified numeric code (ISC) used in GB/T 4237-2015. Older drawings and Chinese buyers may still write the pre-2007 name 00Cr19Ni13Mo3.

SHH STEEL produces and exports austenitic stainless plate from China, works as a sales agent for leading stainless mills, and runs its own processing warehouse for cutting and surface finishing. 022Cr19Ni13Mo3 is part of our GB/T 4237 stainless plate range; for comparison, see our ASTM A240 Type 317L page.

Heat analysis limits for 022Cr19Ni13Mo3

Element 022Cr19Ni13Mo3 heat analysis, % (Table 15) Why it matters
C ≤ 0.030 Carbon. Low values protect welds from carbide precipitation; higher values add hot strength or hardenability.
Si ≤ 0.75 Silicon. Deoxidizer; in heat-resistant grades it builds a protective scale.
Mn ≤ 2.00 Manganese. Deoxidizer; in Mn-bearing grades it replaces nickel and keeps nitrogen in solution.
P ≤ 0.045 Phosphorus. Impurity, kept low for toughness and weld cracking resistance.
S ≤ 0.030 Sulfur. Impurity; low sulfur improves pitting resistance, hot workability and polishability.
Cr 18.00 – 20.00 Chromium. Forms the passive film; the main driver of corrosion and oxidation resistance.
Ni 11.00 – 15.00 Nickel. Stabilizes austenite, improves toughness and resistance to reducing acids.
Mo 3.00 – 4.00 Molybdenum. Raises pitting and crevice resistance in chlorides (×3.3 in PREN).
N ≤ 0.10 Nitrogen. Strengthens, stabilizes austenite and adds pitting resistance (×16 in PREN).
PREN (Cr + 3.3Mo + 16N) 27.9 – 30.5 (minimum – mid-range) Calculated from the limits above, not a requirement of GB/T 4237

Values are maximum unless a range is given. The mill reports the ladle (heat) analysis on the certificate; this is the figure to compare with Table 15.

Check analysis of 022Cr19Ni13Mo3 plate

A check analysis drilled from the finished plate may differ slightly from the heat analysis. GB/T 4237 refers to GB/T 222 for the permitted deviations; the table applies them to the 022Cr19Ni13Mo3 limits. Deviations apply to one side of a range only, never to both sides in the same heat.

Element Heat analysis limit (%) Permitted deviation Product analysis limit (%)
C ≤ 0.030 +0.005 ≤ 0.035
Si ≤ 0.75 ±0.05 ≤ 0.80
Mn ≤ 2.00 ±0.04 ≤ 2.04
P ≤ 0.045 +0.010 ≤ 0.055
S ≤ 0.030 +0.005 ≤ 0.035
Cr 18.00 – 20.00 ±0.20 17.80 – 20.20
Ni 11.00 – 15.00 ±0.15 10.85 – 15.15
Mo 3.00 – 4.00 ±0.10 2.90 – 4.10
N ≤ 0.10 ±0.01 ≤ 0.11

Where the table says ‘by agreement’, the deviation is not tabulated for that content level and should be agreed in the contract, usually by reference to ASTM A480 Table A1.1.

022Cr19Ni13Mo3 S31703 tensile and hardness requirements

Property 022Cr19Ni13Mo3 (Table 20)
Proof strength Rp0.2, MPa ≥ 205
Tensile strength Rm, MPa ≥ 515
Elongation A, % ≥ 40
Hardness HBW ≤ 217
Hardness HRB ≤ 95
Hardness HV ≤ 220

Values apply to plate in the delivery heat-treated condition, tested transversely per GB/T 228.1. Hardness is checked by one method chosen by the mill.

Corrosion resistance and PREN of 022Cr19Ni13Mo3

Molybdenum raises resistance to chlorides, sulfurous media and reducing acids. The low-carbon and nitrogen variants keep that resistance across welds.

PREN of 022Cr19Ni13Mo3 from the GB/T 4237 limits: 27.9 – 30.5. PREN is a ranking tool for pitting in chlorides, not a guarantee; temperature, crevices, deposits and weld finish matter as much.

Intergranular corrosion: GB/T 4237-2015 Table 30 lists this grade for the GB/T 4334 Method E (Cu–CuSO4–H2SO4) test after sensitizing treatment, the stricter condition reserved for low-carbon and stabilized grades. Bent specimens must show no intergranular cracks.

If service is harsher than 022Cr19Ni13Mo3 can handle, the next step up in this batch is GB/T 4237 022Cr19Ni16Mo5N S31723.

Cross-reference to other standards

Standard system Equivalent / closest grade
China GB/T 4237-2015 022Cr19Ni13Mo3 (S31703)
Former Chinese name 00Cr19Ni13Mo3
ASTM A240/A240M Type 317L / S31703
EN 10088-2 X2CrNiMo18-15-4 / 1.4438
JIS G4304 (hot rolled) SUS317L
Common name 317L

Equivalent grades are close in chemistry and properties but are never identical: limits on carbon, nitrogen and residual elements differ. For dual or multiple certification the heat must meet every standard named on the order, and we confirm that from the heat chemistry before quotation.

Related pages: ASTM A240 Type 317L, ASME SA240 317L, JIS G4305 SUS317L, AISI 317L. See also our ASTM A240/A240M and JIS G4305 plate lists.

What the standard covers for this grade

Item GB/T 4237-2015 requirement / SHH STEEL supply
Standard GB/T 4237-2015 Hot rolled stainless steel plate, sheet and strip (current edition, replaces GB/T 4237-2007)
Grade / unified code 022Cr19Ni13Mo3 / S31703
Steel class Austenitic
Chemical composition Table 15 (heat analysis); product analysis per GB/T 222
Mechanical properties Table 20
Product forms Hot-rolled thick plate (3.0 – 200 mm in the standard), hot-rolled wide strip and cut plate (2.0 – 25.4 mm)
Our usual thickness range 3 – 120 mm (to 150 mm by mill order)
Delivery condition ≥ 1 040 °C, water quench or other rapid cooling
Surface Hot rolled, heat treated, pickled (No.1 / 1D) as standard; ground or polished by agreement
Density 8.0 g/cm³
Certificate EN 10204 3.1 mill certificate; 3.2 with third-party inspection on request

Sister grades on the same standard are listed under GB/T 4237; cold-rolled sheet of the same chemistry is ordered to GB/T 3280, and all our plate lines sit in stainless steel sheets and plates.

Choosing between 022Cr19Ni13Mo3 and its neighbours

The table compares 022Cr19Ni13Mo3 with the grades buyers most often weigh it against. Strength values are GB/T 4237-2015 minimums; PREN is calculated from the minimum chemistry.

Grade (GB/T 4237) Key chemistry, % PREN min Rp0.2 min, MPa Rm min, MPa
022Cr19Ni13Mo3 S31703 C ≤ 0.030, Cr 18.00 – 20.00, Ni 11.00 – 15.00, Mo 3.00 – 4.00, N ≤ 0.10 27.9 205 515
GB/T 4237 06Cr19Ni13Mo3 S31708 C ≤ 0.08, Cr 18.00 – 20.00, Ni 11.00 – 15.00, Mo 3.00 – 4.00, N ≤ 0.10 27.9 205 515
GB/T 4237 022Cr17Ni12Mo2 S31603 C ≤ 0.030, Cr 16.00 – 18.00, Ni 10.00 – 14.00, Mo 2.00 – 3.00, N ≤ 0.10 22.6 180 485
GB/T 4237 022Cr19Ni13Mo4N S31753 C ≤ 0.030, Cr 18.00 – 20.00, Ni 11.00 – 15.00, Mo 3.00 – 4.00, N 0.10 – 0.22 29.5 240 550
GB/T 4237 022Cr19Ni16Mo5N S31723 C ≤ 0.030, Cr 17.00 – 20.00, Ni 13.50 – 17.50, Mo 4.00 – 5.00, N 0.10 – 0.20 31.8 240 550
GB/T 4237 015Cr21Ni26Mo5Cu2 S31782 C ≤ 0.020, Cr 19.00 – 23.00, Ni 23.00 – 28.00, Mo 4.00 – 5.00, N ≤ 0.10, Cu 1.00 – 2.00 32.2 220 490

Weld 317L with an over-alloyed filler (ER317L at least, often ER385 or a Ni-base filler in severe FGD service) because weld metal loses pitting resistance through Mo segregation. Table 30 lists it for the sensitized Cu-CuSO4 test.

Fabrication guidance

Use ER316L/E316L filler, or ER317L when the weld must not be the weak point in chloride service. A small ferrite number (FN 3–10) in the weld metal prevents hot cracking.

Interpass ≤150 °C, no preheat, clean back purge with argon for root passes. Pickle and passivate after welding: heat tint lowers pitting resistance more in Mo grades than the weld itself.

Cutting: we cut 022Cr19Ni13Mo3 by plasma (up to about 150 mm), laser (thin plate) or waterjet, and remove the heat-affected edge by machining where the drawing requires it.

Heat treatment and delivery condition

Recommended heat treatment for 022Cr19Ni13Mo3 (GB/T 4237-2015 Annex C): ≥ 1 040 °C, water quench or other rapid cooling.

Cool rapidly through 850–450 °C after annealing; slow cooling of thick Mo-bearing plate risks carbide and sigma precipitation.

Finishes and warehouse services

Finish Description Availability for this grade
No.1 / 1D Hot rolled, heat treated, pickled; the GB/T 4237 standard surface Standard
Shot-blasted + pickled Uniform matte for welded structures On request
No.4 / brushed Abrasive finish, grit 150–180 Warehouse processing, thin plate
HL (hairline) Long continuous lines, decorative Warehouse processing, thin plate
8K mirror Polished reflective finish Warehouse processing, limited sizes
2B / BA Cold-rolled finishes (ordered as GB/T 3280 sheet, not hot-rolled plate) Sheet only

Our warehouse cuts plate to size (plasma, laser, waterjet, saw), bevels weld edges, polishes and applies PVC protective film. Processed plate ships with the original mill heat number marked. Ask for cut pieces of other stainless steel products at the same time to consolidate freight.

Applications of 022Cr19Ni13Mo3 plate

Where buyers specify it:

  • FGD absorber walls and outlet ducts
  • Pulp bleach washers and towers
  • Chemical and petrochemical vessels
  • Textile dyeing equipment
  • Condensers and heat exchangers

Buyers specifying 022Cr19Ni13Mo3 for these jobs often compare it with GB/T 4237 06Cr19Ni13Mo3 S31708 and GB/T 4237 015Cr21Ni26Mo5Cu2 S31782; the comparison table on this page shows the differences.

International grade pages for the alternatives mentioned above: ASTM A240 Type 317, ASTM A240 Type 316L, AISI 317LMN, ASTM A240 Type 904L.

Sizes, tolerances and weight

Dimension Typical supply
Thickness 3 – 120 mm (to 150 mm by mill order)
Width 1 000 / 1 219 / 1 250 / 1 500 / 1 800 / 2 000 mm; wider by mill order
Length 2 000 / 2 438 / 3 000 / 6 000 mm or cut to size
Flatness Per GB/T 4237; ≤15 mm per metre for plate up to 25 mm unless agreed tighter
Thickness tolerance Per the GB/T 4237 dimensional tolerance tables (normal or higher accuracy as ordered)
Edge Mill edge or cut edge

Weight: plate mass in kg/m² = thickness (mm) × density (8.0 g/cm³). A 10 mm 022Cr19Ni13Mo3 plate weighs about 80.0 kg/m²; a 1 500 × 6 000 × 10 mm plate about 720 kg.

Testing and certification

  • Heat chemical analysis on every heat; product analysis by agreement
  • Tensile test (Rp0.2, Rm, A) per batch
  • Hardness test
  • Intergranular corrosion test, GB/T 4334 Method E (Table 30)
  • Ultrasonic testing (NB/T 47013.3 or ASTM A578) when specified
  • Positive material identification (PMI) on every plate leaving our warehouse
  • Visual and dimensional inspection; third-party inspection (SGS, BV, TÜV, Intertek) at the buyer’s request

Certificates follow EN 10204 3.1 as standard. Where plate is also certified to ASME SA240 or ASTM A240, both standards are shown on one certificate.

Supply chain and lead time

022Cr19Ni13Mo3 is a mainstream grade at Chinese stainless mills. We supply it from our own stock and processing warehouse, and by mill order from major producers such as TISCO and Baosteel Stainless, for which we act as a sales agent. Stock plate ships in about 1–2 weeks after cutting; mill orders typically take 30–60 days depending on thickness and rolling schedule.

Every plate is traceable to its heat number, and copies of the mill certificates stay on file for repeat orders and audits. The same mills also supply our ASTM A240, ASME SA240, JIS G4305 and AISI plate ranges, so mixed-standard orders can ship together.

What to put on a 022Cr19Ni13Mo3 purchase order

  • Standard and edition: GB/T 4237-2015
  • Grade and code: 022Cr19Ni13Mo3 (S31703); add the equivalent if dual certification is needed
  • Thickness × width × length, quantity in pieces or tonnes
  • Thickness tolerance class and flatness if tighter than standard
  • Surface finish and protective film
  • Tests beyond the standard (IGC, UT, impact, ferrite, PMI, grain size)
  • Certificate type (EN 10204 3.1 / 3.2) and inspection body
  • Marking, packing (wooden cases, steel pallets) and delivery terms

Send the list to SHH STEEL and we return a quotation with mill, lead time and stock options. Other grades from the same standard can be combined in one shipment; browse GB/T 4237 plate grades.

Why buy from SHH STEEL

  • Mill-direct prices with our own export documentation
  • Own processing warehouse: cutting, bevelling, polishing, PVC film
  • PMI and dimensional check before packing
  • Mixed-grade shipments across our AISI stainless and GB/T plate ranges
  • Technical answers from people who read the standard, not just the price list

SHH STEEL has exported stainless and carbon steel plate to buyers in Asia, the Middle East, Africa, Europe and the Americas.

FAQ

What is the PREN of 317L?
Using GB/T 4237-2015 limits for 022Cr19Ni13Mo3 (Cr 18–20%, Mo 3–4%), PREN = Cr + 3.3Mo + 16N is about 27.9 at minimum chemistry and about 30.5 at mid-range, compared with roughly 23–26 for 316L.
What is the chemical composition of 022Cr19Ni13Mo3?
Under GB/T 4237-2015 Table 15, 022Cr19Ni13Mo3 (S31703) has C ≤ 0.030, Cr 18.00 – 20.00, Ni 11.00 – 15.00, Mo 3.00 – 4.00, N ≤ 0.10. Phosphorus is limited to ≤0.045% and sulfur to ≤0.030%.
What is the ASTM equivalent of 022Cr19Ni13Mo3?
The closest equivalents of 022Cr19Ni13Mo3 (S31703) are Type 317L / S31703 in ASTM, X2CrNiMo18-15-4 / 1.4438 in EN, SUS317L in JIS (common name: 317L). Chemistry limits differ slightly, so dual certification depends on the actual heat.
What are the mechanical properties of 022Cr19Ni13Mo3 plate?
GB/T 4237-2015 Table 20 requires for 022Cr19Ni13Mo3: proof strength Rp0.2 ≥205 MPa, tensile strength ≥515 MPa and elongation ≥40%, hardness ≤217 HBW. Values apply to plate in the delivery heat-treated condition.
Is 022Cr19Ni13Mo3 stainless steel magnetic?
Not in the annealed condition. 022Cr19Ni13Mo3 is austenitic, so annealed plate is essentially non-magnetic; cold work can induce slight magnetism, mostly at cut and bent edges.
What thickness of 022Cr19Ni13Mo3 plate can you supply?
Under GB/T 4237 we supply 022Cr19Ni13Mo3 hot-rolled plate in 3 – 120 mm (to 150 mm by mill order), widths up to 2 000 mm (wider by mill order), cut to size in our warehouse. Thinner material is cold-rolled sheet to GB/T 3280.

Conclusion

GB/T 4237 022Cr19Ni13Mo3 (S31703) is a molybdenum-bearing austenitic plate grade, known internationally as 317L. It is defined by Table 15 chemistry (C ≤ 0.030, Cr 18.00 – 20.00, Ni 11.00 – 15.00, Mo 3.00 – 4.00, N ≤ 0.10) and Table 20 properties of at least 205 MPa proof strength and 515 MPa tensile strength. Typical uses include fgd absorber walls and outlet ducts, pulp bleach washers and towers and chemical and petrochemical vessels. Weld 317L with an over-alloyed filler (ER317L at least, often ER385 or a Ni-base filler in severe FGD service) because weld metal loses pitting resistance through Mo segregation.

Before ordering, state the standard edition, the grade name with its code, and any extra tests, so that the mill certificate matches your design documents. SHH STEEL supplies 022Cr19Ni13Mo3 plate from stock and by mill order, cut to size and finished in our own warehouse, with EN 10204 3.1 certificates. For related grades see GB/T 4237 06Cr19Ni13Mo3 S31708 and GB/T 4237 022Cr17Ni12Mo2 S31603, our GB/T 4237 category and the ASTM A240 Type 317L page. Send your sizes and quantities for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *