EN 10088-2

Product Showcase

EN 10088-2 Stainless Steel Products

SHH STEEL offers EN 10088-2-compliant 304/316 stainless steel plates. EN 10088-2 specifies technical delivery conditions for hot/cold-rolled stainless steel plates, sheets, and strips for corrosion-resistant general purposes. Certified quality, competitive prices, customizable. Trust SHH STEEL!

EN 10088-2 X1CrNi25-21 (1.4335) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X1CrNi25-21 1.4335 Stainless Steel Plate

X1CrNi25-21 1.4335 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is a 25Cr-21Ni austenitic steel with very low carbon and silicon, used for nitric acid service. It is listed as a special grade and as hot rolled plate only. SHH STEEL supplies it through mill partners.
View More
EN 10088-2 X1NiCrMoCu31-27-4 (1.4563) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X1NiCrMoCu31-27-4 1.4563 Stainless Steel Plate

X1NiCrMoCu31-27-4 1.4563 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is a 31Ni-27Cr-3.5Mo-Cu austenitic steel for strong acids and chloride-contaminated process media, listed as a special grade and as hot rolled plate only. SHH STEEL supplies it through mill partners.
View More
EN 10088-2 X1CrNiMoCuN20-18-7 (1.4547) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X1CrNiMoCuN20-18-7 1.4547 Stainless Steel Plate

X1CrNiMoCuN20-18-7 1.4547 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is a 20Cr-18Ni austenitic steel with 6.0 – 7.0 % molybdenum, nitrogen and copper, for seawater and other chloride service, listed as a special grade. SHH STEEL supplies plate and sheet through mill partners.
View More
EN 10088-2 X1NiCrMoCuN25-20-7 (1.4529) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X1NiCrMoCuN25-20-7 1.4529 Stainless Steel Plate

X1NiCrMoCuN25-20-7 1.4529 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is a 25Ni-20Cr austenitic steel with 6.0 – 7.0 % molybdenum, nitrogen and copper, listed as a special grade and as hot rolled plate only. SHH STEEL supplies it through mill partners.
View More
EN 10088-2 X1NiCrMoCu25-20-5 (1.4539) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X1NiCrMoCu25-20-5 1.4539 Stainless Steel Plate

X1NiCrMoCu25-20-5 1.4539 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is the high-alloy 25Ni-20Cr austenitic steel of the 904L type, with 4.0 – 5.0 % molybdenum and copper for sulphuric and phosphoric acids. SHH STEEL supplies plate and sheet through mill partners.
View More
EN 10088-2 X6CrNiMoNb17-12-2 (1.4580) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X6CrNiMoNb17-12-2 1.4580 Stainless Steel Plate

X6CrNiMoNb17-12-2 1.4580 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is the niobium-stabilised 17Cr-12Ni-2Mo austenitic steel of the 316Cb type, listed as a special grade and as hot rolled plate only. SHH STEEL supplies it through mill partners.
View More
EN 10088-2 X6CrNiMoTi17-12-2 (1.4571) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X6CrNiMoTi17-12-2 1.4571 Stainless Steel Plate

X6CrNiMoTi17-12-2 1.4571 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is the titanium-stabilised 17Cr-12Ni-2Mo austenitic steel of the 316Ti type, resistant to intergranular corrosion after welding. SHH STEEL supplies hot rolled plate and cold rolled sheet through long-term mill partners.
View More
EN 10088-2 X2CrNiMoN17-13-5 (1.4439) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X2CrNiMoN17-13-5 1.4439 Stainless Steel Plate

X2CrNiMoN17-13-5 1.4439 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is a low-carbon, nitrogen-alloyed 17Cr-13Ni austenitic steel of the 317LMN type with 4.0 – 5.0 % molybdenum, for demanding chloride service. SHH STEEL supplies hot rolled plate and cold rolled sheet through mill partners.
View More
EN 10088-2 X2CrNiMo18-15-4 (1.4438) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X2CrNiMo18-15-4 1.4438 Stainless Steel Plate

X2CrNiMo18-15-4 1.4438 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is a low-carbon 18Cr-14Ni austenitic steel of the 317L type with 3.0 – 4.0 % molybdenum, listed by EN 10088-2 as a special grade. SHH STEEL supplies hot rolled plate and cold rolled sheet through mill partners.
View More
EN 10088-2 X3CrNiMo17-13-3 (1.4436) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X3CrNiMo17-13-3 1.4436 Stainless Steel Plate

X3CrNiMo17-13-3 1.4436 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is a 17Cr-12Ni austenitic steel of the 316 type with 2.50 – 3.00 % molybdenum, listed by EN 10088-2 as a special grade. SHH STEEL supplies hot rolled plate and cold rolled sheet through long-term mill partners.
View More
EN 10088-2 X2CrNiMo18-14-3 (1.4435) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X2CrNiMo18-14-3 1.4435 Stainless Steel Plate

X2CrNiMo18-14-3 1.4435 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is a low-carbon 18Cr-14Ni austenitic steel of the 316L type with 2.50 – 3.00 % molybdenum and more nickel than 1.4404. SHH STEEL supplies hot rolled plate and cold rolled sheet through long-term mill partners.
View More
EN 10088-2 X2CrNiMo17-12-3 (1.4432) stainless steel plate at SHH STEEL warehouse

EN 10088-2 X2CrNiMo17-12-3 1.4432 Stainless Steel Plate

X2CrNiMo17-12-3 1.4432 stainless steel plate is supplied to EN 10088-2, the European standard for stainless steel sheet/plate and strip for general purposes, covering chemistry, mechanical properties, finishes and tolerances. The grade is a low-carbon 17Cr-12Ni austenitic steel of the 316L type with 2.50 – 3.00 % molybdenum, higher than in 1.4404. SHH STEEL supplies hot rolled plate and cold rolled sheet through long-term mill partners.
View More

EN 10088-2 Stainless Steel Products

EN 10088-2 X1CrNiMoCuN24-22-8 1.4652 Stainless Steel Plate EN 10088-2 X4CrNi18-12 1.4303 Stainless Steel Plate EN 10088-2 X2CrNiMnMoCuN24-4-3-2 1.4662 Stainless Steel Plate EN 10088-2 X2CrNiMnMoN25-18-6-5 1.4565 Stainless Steel Plate
EN 10088-2 X2CrMnNiN21-5-1 1.4162 Stainless Steel Plate EN 10088-2 X7CrNiAl17-7 1.4568 Cold Rolled Stainless Steel Strip EN 10088-2 X5CrNiCuNb16-4 1.4542 Stainless Steel Plate EN 10088-2 X2CrNiMoCuWN25-7-4 1.4501 Stainless Steel Plate
EN 10088-2 X2CrNiMoCuN25-6-3 1.4507 Stainless Steel Plate EN 10088-2 X2CrNiMoN25-7-4 1.4410 Stainless Steel Plate EN 10088-2 X2CrNiMoN22-5-3 1.4462 Stainless Steel Plate EN 10088-2 X2CrNiN23-4 1.4362 Stainless Steel Plate
EN 10088-2 X1CrNi25-21 1.4335 Stainless Steel Plate EN 10088-2 X1NiCrMoCu31-27-4 1.4563 Stainless Steel Plate EN 10088-2 X1CrNiMoCuN20-18-7 1.4547 Stainless Steel Plate EN 10088-2 X1NiCrMoCuN25-20-7 1.4529 Stainless Steel Plate
EN 10088-2 X1NiCrMoCu25-20-5 1.4539 Stainless Steel Plate EN 10088-2 X6CrNiMoNb17-12-2 1.4580 Stainless Steel Plate EN 10088-2 X6CrNiMoTi17-12-2 1.4571 Stainless Steel Plate EN 10088-2 X2CrNiMoN17-13-5 1.4439 Stainless Steel Plate
EN 10088-2 X2CrNiMo18-15-4 1.4438 Stainless Steel Plate EN 10088-2 X3CrNiMo17-13-3 1.4436 Stainless Steel Plate EN 10088-2 X2CrNiMo18-14-3 1.4435 Stainless Steel Plate EN 10088-2 X2CrNiMo17-12-3 1.4432 Stainless Steel Plate
EN 10088-2 X2CrNiMoN17-11-2 1.4406 Stainless Steel Plate EN 10088-2 X2CrNiMo17-12-2 1.4404 Stainless Steel Plate EN 10088-2 X5CrNiMo17-12-2 1.4401 Stainless Steel Plate EN 10088-2 X6CrNiNb18-10 1.4550 Stainless Steel Plate
EN 10088-2 X6CrNiTi18-10 1.4541 Stainless Steel Plate EN 10088-2 X8CrNiS18-9 1.4305 Stainless Steel Plate EN 10088-2 X5CrNi18-10 1.4301 Stainless Steel Plate EN 10088-2 X2CrNiN18-10 1.4311 Stainless Steel Plate
EN 10088-2 X2CrNi19-11 1.4306 Stainless Steel Plate EN 10088-2 X2CrNi18-9 1.4307 Stainless Steel Plate EN 10088-2 X2CrNiN18-7 1.4318 Stainless Steel Plate EN 10088-2 X10CrNi18-8 1.4310 Cold Rolled Stainless Steel Strip
EN 10088-2 X4CrNiMo16-5-1 1.4418 Stainless Steel Plate EN 10088-2 X3CrNiMo13-4 1.4313 Stainless Steel Plate EN 10088-2 X50CrMoV15 1.4116 Stainless Steel Strip EN 10088-2 X46Cr13 1.4034 Stainless Steel Strip
EN 10088-2 X39Cr13 1.4031 Stainless Steel Strip EN 10088-2 X30Cr13 1.4028 Stainless Steel Plate EN 10088-2 X20Cr13 1.4021 Stainless Steel Plate EN 10088-2 X2CrMoTi29-4 1.4592 Cold Rolled Stainless Steel Strip
EN 10088-2 X12Cr13 1.4006 Stainless Steel Plate EN 10088-2 X2CrTi24 1.4613 Cold Rolled Stainless Steel Strip EN 10088-2 X2CrTi21 1.4611 Cold Rolled Stainless Steel Strip EN 10088-2 X2CrTiNb18 1.4509 Cold Rolled Stainless Steel Strip
EN 10088-2 X6CrMoNb17-1 1.4526 Cold Rolled Stainless Steel Strip EN 10088-2 X2CrMoTi18-2 1.4521 Stainless Steel Plate EN 10088-2 X2CrMoTi17-1 1.4513 Cold Rolled Stainless Steel Strip EN 10088-2 X2CrTi17 1.4520 Stainless Steel Plate
EN 10088-2 X3CrTi17 1.4510 Stainless Steel Plate EN 10088-2 X6Cr17 1.4016 Stainless Steel Plate EN 10088-2 X6Cr13 1.4000 Stainless Steel Plate EN 10088-2 X2CrTi12 1.4512 Stainless Steel Plate
EN 10088-2 X2CrNi12 1.4003 Stainless Steel Plate Supplier | 1.4003 Ferritic Plate
Stainless Steel Sheets and Plates

Stainless Steel Sheets and Plates

SHH STEEL, a leading Stainless Steel Sheets and Plates exporter, produces and exports stainless steel sheets (0.3–6 mm) and plates (>6 mm) for marine, chemical, and structural applications. Our products, like 304 and 316L (ASTM A240), offer corrosion resistance and durability. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for 316L stainless steel plates and custom solutions for your projects.

Stainless Steel Sheets and Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X