EN 10088-2 X4CrNi18-12 1.4303 Stainless Steel Plate
What is EN 10088-2 X4CrNi18-12 1.4303 Stainless Steel Plate?
Equivalent grades: 1.4303 X4CrNi18-12 ≈ UNS S30500 ≈ GB/T 10Cr18Ni12 (S30510) ≈ JIS SUS305.
1.4303 X4CrNi18-12 is a austenitic grade. 1.4303 is a high-nickel 18-12 austenitic steel. The extra nickel lowers the work-hardening rate and keeps the austenite stable during cold forming, so it is used for deep drawing, spinning and cold heading, and where very low magnetic permeability after forming is needed.
EN 10088-2 is the European standard for stainless steel sheet, plate and strip for general purposes. It defines the chemistry, the mechanical properties for each product form (C = cold-rolled strip, H = hot-rolled strip, P = hot-rolled plate) and the process routes that give each surface finish. Pressure-equipment plate is ordered to EN 10028-7 instead, which adds elevated-temperature properties.
This page sets out the EN 10088-2 requirements for 1.4303 X4CrNi18-12 plate: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.
1.4303 X4CrNi18-12 plate: specification summary
| Item | 1.4303 X4CrNi18-12 data |
|---|---|
| Standard | EN 10088-2:2014, stainless steels for general purposes – sheet/plate and strip |
| Product forms | C = cold-rolled strip, H = hot-rolled strip, P = hot-rolled plate |
| Process routes / finishes | 1C, 1E, 1D (hot rolled); 2D, 2B, 2R (cold rolled); special finishes by agreement |
| Typical thickness | 0.5–6 mm cold rolled; 3–100 mm hot-rolled plate depending on grade |
| Dimensions and tolerances | EN 10029 (plate), EN 10051 (hot-rolled strip and sheet), EN ISO 9445-1/-2 (cold rolled) |
| Required tests | cast analysis, tensile test; corrosion test by agreement |
| Inspection documents | EN 10204 3.1 or 3.2 |
| Grade family | austenitic |
Size range. Plate is produced on Steckel or reversing mills from about 5 mm up to 80–100 mm depending on grade, with widths of 1500–2500 mm and lengths up to 12 m; thinner plate of 3–12 mm is often cut from hot-rolled coil. Very heavy or wide plates, and plates with tight flatness, should be confirmed before ordering. 1.4303 X4CrNi18-12 is produced regularly by several mills; common sizes are held in stock, and other sizes are rolled in the mill’s scheduled campaigns for the grade.
Chemical composition of 1.4303 X4CrNi18-12 (EN 10088-2)
| Element | wt % |
|---|---|
| C | 0.06 max |
| Si | 1.00 max |
| Mn | 2.00 max |
| P | 0.045 max |
| S | 0.015 max |
| Cr | 17.0–19.0 |
| Ni | 11.0–13.0 |
| N | 0.11 max |
Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.
PREN check (Cr + 3.3 Mo + 16 N): about 17.0 at the specification minimums and about 18.9 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.
Mechanical properties of 1.4303 X4CrNi18-12 plate
| Product form / thickness | Rp0.2 min, MPa | Rm, MPa | A min, % (transverse) |
|---|---|---|---|
| C, cold-rolled strip ≤ 8 mm | 220 | 500–650 | 45 |
| H, hot-rolled strip ≤ 13.5 mm | 220 | 500–650 | 45 |
| P, hot-rolled plate ≤ 75 mm | 220 | 500–650 | 45 |
The minimum yield strength of 220 MPa is about 1.3 times the 170 MPa minimum of ASTM 316L. Annealed austenitic and 200-series material work-hardens quickly, so cold-formed parts are stronger than these minimums. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.
Corrosion resistance of 1.4303 X4CrNi18-12: PREN and limits
Austenitic stainless steels are non-hardenable by heat treatment, tough down to cryogenic temperatures and easy to form and weld. Corrosion resistance rises with chromium, molybdenum and nitrogen; the PREN of this grade at the specification minimum is about 17.0. Low-carbon (L) and stabilised versions protect welds against intergranular corrosion.
Austenitic grades are prone to chloride stress-corrosion cracking above about 60 °C in chloride environments. Where that risk exists, duplex or super-austenitic grades are the usual upgrade. Cold work raises strength but also makes some grades slightly magnetic.
How 1.4303 X4CrNi18-12 compares with related grades
| Grade | Cr | Ni | Mo | N | PREN (min) | YS / Rp0.2 min, MPa |
|---|---|---|---|---|---|---|
| 1.4303 X4CrNi18-12 | 17.0–19.0 | 11.0–13.0 | — | 0.11 max | 17.0 | 220 |
| UNS S31050 | 24.0–26.0 | 20.5–23.5 | 1.60–2.60 | 0.09–0.15 | 30.7 | 270 |
| UNS S31050 | 24.0–26.0 | 20.5–23.5 | 1.60–2.60 | 0.09–0.15 | 30.7 | 270 |
| 06Cr19Ni10 (S30408) | 17.5–19.5 | 8–10.5 | — | 0.1 max | 17.5 | 205 |
| 022Cr19Ni10 (S30403) | 17.5–19.5 | 8–12 | — | 0.1 max | 17.5 | 180 |
Choose 1.4303 X4CrNi18-12 for general corrosion resistance with easy forming and welding. In warm chloride environments consider a molybdenum-bearing or duplex grade instead.
The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.
Heat treatment and delivery condition of 1.4303 X4CrNi18-12
Heat treatment: 1000–1100 °C, water or air (rapid).
Austenitic grades are solution annealed and cooled rapidly to keep carbides in solution. They cannot be hardened by heat treatment, only by cold work.
Surface finishes for 1.4303 X4CrNi18-12 plate
EN 10088-2 identifies finishes by process route. 1D (hot rolled, heat treated, pickled) is the normal plate finish; 1E is mechanically descaled. Cold-rolled material is supplied as 2D (dull), 2B (skin passed) or 2R (bright annealed). Ground, brushed and polished finishes (1G, 2G, 2J, 2K) can be agreed. Specify the route code on the order because it fixes surface condition and the tolerance standard that applies.
Dimensions, tolerances and flatness
Tolerances depend on the product form: EN 10029 for quarto plate (thickness classes A, B, C, D and flatness classes N and S), EN 10051 for hot-rolled wide strip and sheet cut from it, and EN ISO 9445-1/-2 for cold-rolled material. State the tolerance class on the order; class B (all minus tolerance removed) is common for pressure and structural plate.
European ordering practice. An EN order gives the product form (C, H or P), the steel name or number, the process route code, the dimensions and the EN tolerance standard, and the inspection document type. Under the Pressure Equipment Directive, plate for pressure parts is normally ordered to EN 10028-7 or with a particular material appraisal, and the certificate is a 3.1 from a mill with an approved quality system or a 3.2 with third-party witness. Corrosion testing to EN ISO 3651-2 is applied only when ordered. Many buyers also add AD 2000 W2 or project-specific requirements, which should be quoted in full.
1.4303 X4CrNi18-12 plate stock in China
| Thickness (mm) | Width (mm) | Length (mm) | Finish | Approx. quantity | Location |
|---|---|---|---|---|---|
| 6 | 1500 / 2000 | 6000 | 1D | 200+ t | China |
| 8 | 1500 / 2000 | 6000 | 1D | 200+ t | China |
| 10 | 2000 | 6000 | 1D | 100+ t | China |
| 12 | 2000 | 6000 | 1D | 100+ t | China |
| 16 | 2000 / 2500 | 6000 | 1D | 100+ t | China |
| 20 | 2000 / 2500 | 6000 / 8000 | 1D | 100+ t | China |
| 30 | 2000 / 2500 | 6000 | 1D | 100+ t | China |
Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.
Packing and logistics. Plate is bundled on steel or wooden skids with steel bands and edge protection, typically 3–8 t per bundle, and marked with heat and plate numbers. Cut pieces are crated. Heavy and wide plate ships in open-top or flat-rack containers or by break-bulk; we send loading photos with the shipping documents.
1.4303 X4CrNi18-12 equivalents in other standards
| Standard | Designation | Comment |
|---|---|---|
| ASTM / UNS | UNS S30500 | same alloy family and limits closely matched; compare each limit on the certificate |
| GB/T | 10Cr18Ni12 (S30510) | same alloy family and limits closely matched; compare each limit on the certificate |
| JIS | SUS305 | same alloy family and limits closely matched; compare each limit on the certificate |
Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.
Related grades by alloy family
Austenitic
General-purpose austenitic grades for comparison: A240 S30400, A240 S30403, A240 S31600, A240 S31603, A240 S30500, A240 S32100, A240 S30100, 1.4301 plate, 1.4307 plate.
Same standard
Other grades in this standard: 1.4162 plate, 1.4565 plate, 1.4662 plate.
Applications, forming and welding of 1.4303 X4CrNi18-12
Typical uses: deep-drawn and spun parts, cold-headed fasteners, electronic and instrument housings, and non-magnetic components.
Austenitic sheet and plate form and weld easily. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use an ER308L, ER316L or ER347 filler matching the grade (AWS A5.9). Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.
Welding practice. Austenitic sheet is welded with GTAW, GMAW, SMAW or laser without preheat. Keep the interpass temperature below about 150 °C, use back-purging on corrosion-critical joints and pickle afterwards. Low-carbon or stabilised grades avoid sensitisation; standard-carbon grades used at temperature may need a solution anneal after heavy welding.
Certificates, testing and receiving inspection
Every delivery carries a mill certificate to EN 10088-1 and EN 10088-2 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: intergranular corrosion testing (ASTM A262 Practice E or EN ISO 3651-2 / GB/T 4334), PMI and surface inspection. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.
On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.
Common mistakes when specifying 1.4303 X4CrNi18-12
- Mixing L and standard-carbon grades in welded equipment.
- Leaving out the finish and film side for visible parts.
- Using the grade in warm chlorides where stress-corrosion cracking is likely.
Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.
Sourcing 1.4303 X4CrNi18-12: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Mixed-up 304/316 or L/non-L grades | PMI and heat-number tracking for every sheet |
| Surface scratches on finished sheet | PVC film, interleaving paper and wooden-case packing |
| Small quantities across many sizes | mixed thicknesses and grades combined in one shipment |
| Cutting and edge preparation | in-house shearing, plasma, laser and waterjet cutting, bevelling |
| Delivery delays | weekly production and shipping updates with photos |
How to order 1.4303 X4CrNi18-12 plate
State the standard and edition (EN 10088-2), the grade (1.4303 X4CrNi18-12), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.
FAQ
-
Is 1.4303 plate covered by EN 10088-2 or EN 10028-7?
- EN 10088-2 covers general-purpose plate. For pressure equipment under the PED, order to EN 10028-7 where the grade is listed there, because it adds elevated-temperature proof-strength values.
-
Is 1.4303 X4CrNi18-12 equivalent to UNS S30500?
- They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
-
Is 1.4303 X4CrNi18-12 magnetic?
- It is essentially non-magnetic when annealed; cold work can make it slightly magnetic.
-
Can I order small quantities or cut sizes?
- Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
-
Which certificates and tests can you provide?
- Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.
Conclusion
1.4303 X4CrNi18-12 plate should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.