EN 10088-2 X2CrNiMnMoCuN24-4-3-2 1.4662 Stainless Steel Plate at SHH STEEL warehouse

EN 10088-2 X2CrNiMnMoCuN24-4-3-2 1.4662 Stainless Steel Plate

EN 10088-2 X2CrNiMnMoCuN24-4-3-2 1.4662 Stainless Steel Plate: duplex grade to EN 10088-2, hot-rolled plate from stock in China. SHH STEEL supplies mill-direct material with EN 10204 3.1/3.2 certificates, third-party inspection and cutting to size.
Keywords
1.4662 stainless steel plate, 1.4662 plate, 1.4662 stainless plate supplier, EN 10088-2 1.4662, 1.4662 plate stock China
Equivalent Grades:
UNS S82441; GB/T 022Cr24Ni4Mn3Mo2CuN (S22493)
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Performance
Grade Selection
Heat Treatment
Surface Finishes
Tolerances
Stock
Equivalent Grades
Related Grades
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is EN 10088-2 X2CrNiMnMoCuN24-4-3-2 1.4662 Stainless Steel Plate?

Technical reviewer: Jack · Updated: 2026-10-21

Equivalent grades: 1.4662 X2CrNiMnMoCuN24-4-3-2 ≈ UNS S82441 ≈ GB/T 022Cr24Ni4Mn3Mo2CuN (S22493).

1.4662 X2CrNiMnMoCuN24-4-3-2 is a duplex grade. 1.4662 is a lean duplex steel with 24 % Cr, about 3.5 % Ni and 1.5 % Mo. Its PREN of about 33 is close to 1.4462, while its proof strength in thin gauges is higher than 1.4462 and its nickel and molybdenum costs are lower.

EN 10088-2 is the European standard for stainless steel sheet, plate and strip for general purposes. It defines the chemistry, the mechanical properties for each product form (C = cold-rolled strip, H = hot-rolled strip, P = hot-rolled plate) and the process routes that give each surface finish. Pressure-equipment plate is ordered to EN 10028-7 instead, which adds elevated-temperature properties.

This page sets out the EN 10088-2 requirements for 1.4662 X2CrNiMnMoCuN24-4-3-2 plate: specification summary, chemistry, mechanical properties, corrosion resistance, heat treatment, finishes and tolerances, current stock, equivalents, fabrication and testing. SHH STEEL supplies it mill-direct from China with EN 10204 3.1 certificates, optional third-party inspection and in-house cutting.

1.4662 X2CrNiMnMoCuN24-4-3-2 plate: specification summary

Item 1.4662 X2CrNiMnMoCuN24-4-3-2 data
Standard EN 10088-2:2014, stainless steels for general purposes – sheet/plate and strip
Product forms C = cold-rolled strip, H = hot-rolled strip, P = hot-rolled plate
Process routes / finishes 1C, 1E, 1D (hot rolled); 2D, 2B, 2R (cold rolled); special finishes by agreement
Typical thickness 0.5–6 mm cold rolled; 3–100 mm hot-rolled plate depending on grade
Dimensions and tolerances EN 10029 (plate), EN 10051 (hot-rolled strip and sheet), EN ISO 9445-1/-2 (cold rolled)
Required tests cast analysis, tensile test; corrosion test by agreement
Inspection documents EN 10204 3.1 or 3.2
Grade family duplex

Size range. Plate is produced on Steckel or reversing mills from about 5 mm up to 80–100 mm depending on grade, with widths of 1500–2500 mm and lengths up to 12 m; thinner plate of 3–12 mm is often cut from hot-rolled coil. Very heavy or wide plates, and plates with tight flatness, should be confirmed before ordering. 1.4662 X2CrNiMnMoCuN24-4-3-2 is a specialty grade made by a limited number of mills in campaign rolling. Stock covers the common sizes listed below; for project quantities or unusual sizes, plan for a mill campaign and reserve the heat early.

Chemical composition of 1.4662 X2CrNiMnMoCuN24-4-3-2 (EN 10088-2)

Element wt %
C 0.030 max
Si 0.70 max
Mn 2.5–4.0
P 0.035 max
S 0.005 max
Cr 23.0–25.0
Ni 3.0–4.5
Mo 1.0–2.0
Cu 0.10–0.80
N 0.20–0.30

Single values are maximums unless marked min. Ranges are heat (cast) analysis limits.

PREN check (Cr + 3.3 Mo + 16 N): about 29.5 at the specification minimums and about 33.0 at mid-range. Where corrosion resistance is critical, write a minimum PREN on the order and ask for the calculated value from the heat analysis on the certificate.

Mechanical properties of 1.4662 X2CrNiMnMoCuN24-4-3-2 plate

Product form / thickness Rp0.2 min, MPa Rm, MPa A min, % (transverse)
C, cold-rolled strip ≤ 6.4 mm 550 750–900 25
H, hot-rolled strip ≤ 13.5 mm 550 750–900 25
P, hot-rolled plate ≤ 50 mm 480 680–900 25

The minimum yield strength of 480 MPa is about 2.8 times the 170 MPa minimum of ASTM 316L. Designers use this to reduce thickness, but higher strength also means higher press loads and more springback. Mill values for production heats are usually well above the minimums; use certificate values when you calculate bending forces. Tension tests are taken in the direction stated in the standard; where a hardness limit is given, it is a maximum that confirms correct annealing.

Corrosion resistance of 1.4662 X2CrNiMnMoCuN24-4-3-2: PREN and limits

Duplex steels combine about half ferrite and half austenite after solution annealing. The structure gives about twice the yield strength of 304L/316L and much better resistance to chloride stress-corrosion cracking. The PREN (Cr + 3.3 Mo + 16 N) at the specification minimum is about 29.5; a mid-range heat is about 33.0, which places the grade relative to 304L (about 18), 316L (about 24) and 2205 (about 34).

The phase balance depends on correct solution annealing and fast cooling. Too low an annealing temperature or slow cooling can precipitate sigma, chi or chromium nitrides, which cut toughness and corrosion resistance without any visible sign. That is why project specifications add ASTM A923 Method A/B/C tests and a ferrite range. Duplex grades are not recommended for long service above about 300 °C, where 475 °C embrittlement of the ferrite begins.

How 1.4662 X2CrNiMnMoCuN24-4-3-2 compares with related grades

Grade Cr Ni Mo N PREN (min) YS / Rp0.2 min, MPa
1.4662 X2CrNiMnMoCuN24-4-3-2 23.0–25.0 3.0–4.5 1.0–2.0 0.20–0.30 29.5 480
UNS S82441 23.0–25.0 3.0–4.5 1.00–2.00 0.20–0.30 29.5 540
UNS S32003 19.5–22.5 3.0–4.0 1.50–2.00 0.14–0.20 26.7 485
UNS S32202 21.5–24.0 1.00–2.80 0.45 max 0.18–0.26 24.4 450
UNS S32900 23.0–28.0 2.0–5.0 1.00–2.00 — 26.3 485

Choose 1.4662 X2CrNiMnMoCuN24-4-3-2 when you need more strength and chloride stress-corrosion resistance than 316L at lower cost than super-austenitic or super-duplex grades. Do not use it for long-term service above about 300 °C or where full non-magnetic behaviour is required.

The table uses specification limits, not typical mill values, so it shows the guaranteed position of each grade. Final selection should also consider product availability in the thickness you need, welding consumables, and the inspection requirements of your project.

Heat treatment and delivery condition of 1.4662 X2CrNiMnMoCuN24-4-3-2

Heat treatment: 1000–1100 °C, water or air (rapid).

Rapid cooling from the solution-anneal temperature is essential to avoid sigma, chi and chromium nitrides in the 700–1000 °C range. Stress relieving in that range is not allowed; any hot forming must be followed by a full solution anneal and quench.

Surface finishes for 1.4662 X2CrNiMnMoCuN24-4-3-2 plate

EN 10088-2 identifies finishes by process route. 1D (hot rolled, heat treated, pickled) is the normal plate finish; 1E is mechanically descaled. Cold-rolled material is supplied as 2D (dull), 2B (skin passed) or 2R (bright annealed). Ground, brushed and polished finishes (1G, 2G, 2J, 2K) can be agreed. Specify the route code on the order because it fixes surface condition and the tolerance standard that applies.

Dimensions, tolerances and flatness

Tolerances depend on the product form: EN 10029 for quarto plate (thickness classes A, B, C, D and flatness classes N and S), EN 10051 for hot-rolled wide strip and sheet cut from it, and EN ISO 9445-1/-2 for cold-rolled material. State the tolerance class on the order; class B (all minus tolerance removed) is common for pressure and structural plate.

European ordering practice. An EN order gives the product form (C, H or P), the steel name or number, the process route code, the dimensions and the EN tolerance standard, and the inspection document type. Under the Pressure Equipment Directive, plate for pressure parts is normally ordered to EN 10028-7 or with a particular material appraisal, and the certificate is a 3.1 from a mill with an approved quality system or a 3.2 with third-party witness. Corrosion testing to EN ISO 3651-2 is applied only when ordered. Many buyers also add AD 2000 W2 or project-specific requirements, which should be quoted in full.

1.4662 X2CrNiMnMoCuN24-4-3-2 plate stock in China

Thickness (mm) Width (mm) Length (mm) Finish Approx. quantity Location
6 1500 / 2000 6000 1D 100+ t China
8 1500 / 2000 6000 1D 100+ t China
10 2000 6000 1D 100+ t China
12 2000 6000 1D 100+ t China
16 2000 / 2500 6000 1D 100+ t China
20 2000 / 2500 6000 / 8000 1D 100+ t China
30 2000 / 2500 6000 1D 100+ t China

Quantities are approximate and stock changes daily. Send your size list for current availability; other thicknesses, widths and cut sizes can be supplied from mill production.

Packing and logistics. Plate is bundled on steel or wooden skids with steel bands and edge protection, typically 3–8 t per bundle, and marked with heat and plate numbers. Cut pieces are crated. Heavy and wide plate ships in open-top or flat-rack containers or by break-bulk; we send loading photos with the shipping documents.

1.4662 X2CrNiMnMoCuN24-4-3-2 equivalents in other standards

Standard Designation Comment
ASTM / UNS UNS S82441 same alloy family and limits closely matched; compare each limit on the certificate
GB/T 022Cr24Ni4Mn3Mo2CuN (S22493) same alloy family and limits closely matched; compare each limit on the certificate

Equivalents are close, not identical. When a project names one standard, order to that standard or ask for multiple certification and check every limit on the certificate.

Related grades by alloy family

Duplex and lean duplex

Duplex grades with about twice the yield strength of 316L: A240 S32205, A240 S32304, A240 S32101, 1.4462 plate, 1.4362 plate.

Super duplex

PREN 40+ duplex grades for seawater and severe chlorides: A240 S32750, 1.4410 plate, 1.4501 plate, 1.4507 plate.

Austenitic

General-purpose austenitic grades for comparison: A240 S30400.

Same standard

Other grades in this standard: 1.4162 plate, 1.4565 plate, 1.4303 plate.

Applications, forming and welding of 1.4662 X2CrNiMnMoCuN24-4-3-2

Typical uses: storage tanks, chemical tankers, desalination and water treatment, pulp and paper, and structural parts.

Duplex sheet and plate need about 1.5–2 times the press force of 316L and show more springback. Cut by plasma, laser or waterjet and remove heat tint by pickling or grinding. For welding use a nickel-enriched duplex filler such as ER2209 (AWS A5.9), never an autogenous weld without filler. Keep the weld area clean and free of carbon-steel contamination, and pickle and passivate after welding where corrosion resistance matters.

Welding practice. Keep heat input in the range of about 0.5–2.5 kJ/mm and interpass temperature below about 150 °C. Too low a heat input gives a highly ferritic weld and HAZ; too high a heat input or slow cooling forms intermetallics. Use argon with 1–2 % nitrogen for GTAW where the specification allows, and back-purge root runs. Qualify the procedure with ferrite measurement and, where specified, A923 tests on the weld.

Certificates, testing and receiving inspection

Every delivery carries a mill certificate to EN 10088-1 and EN 10088-2 with heat analysis, tensile results and hardness, and the grade and standard as ordered. Supplementary tests we can arrange: ASTM A923 Methods A, B and C, ferrite count to ASTM E562, ASTM G48 pitting test, Charpy impact at the project temperature, and PMI on each plate. Third-party witness by SGS, BV, TÜV, DNV, ABS or LR is available with EN 10204 3.2 certificates.

On receipt, check marking and heat number against the certificate, measure thickness at several points and confirm the finish and edge condition before cutting.

Common mistakes when specifying 1.4662 X2CrNiMnMoCuN24-4-3-2

  • Ordering by UNS number only, without minimum N or PREN, and receiving a heat at the bottom of the range.
  • Assuming impact or ferrite requirements from one project apply to all; they come from the project specification, not the product standard.
  • Using 2205 design data for a lean duplex grade, or the reverse; strength and PREN differ.

Each of these can be avoided by writing the requirement into the purchase order and checking it on the certificate before the material is cut.

Sourcing 1.4662 X2CrNiMnMoCuN24-4-3-2: buyer concerns and SHH STEEL solutions

Concern How SHH STEEL handles it
Phase balance and intermetallics solution-anneal records checked; A923 and ferrite tests agreed before production
Low nitrogen at the bottom of the range minimum N and PREN written into the order and confirmed from the heat analysis
Small quantities across many sizes mixed thicknesses and grades combined in one shipment
Cutting and edge preparation in-house shearing, plasma, laser and waterjet cutting, bevelling
Delivery delays weekly production and shipping updates with photos

How to order 1.4662 X2CrNiMnMoCuN24-4-3-2 plate

State the standard and edition (EN 10088-2), the grade (1.4662 X2CrNiMnMoCuN24-4-3-2), thickness, width and length or coil, finish, quantity, tolerance class, any added chemistry limits, the supplementary tests and acceptance values from your specification, the certificate type and inspection agency, and packing. Send the list to SHH STEEL and we will reply with price, available stock and lead time.

FAQ

Is 1.4662 plate covered by EN 10088-2 or EN 10028-7?
EN 10088-2 covers general-purpose plate. For pressure equipment under the PED, order to EN 10028-7 where the grade is listed there, because it adds elevated-temperature proof-strength values.
Is 1.4662 X2CrNiMnMoCuN24-4-3-2 equivalent to UNS S82441?
They are the same alloy designation in different standards. Limits are closely matched, but always order to the standard named in your specification or ask for multiple certification.
What ferrite range should I specify for 1.4662 X2CrNiMnMoCuN24-4-3-2?
Use your project specification. Many specifications ask for 35–55 % ferrite measured to ASTM E562; the product standard itself does not set a range.
Can I order small quantities or cut sizes?
Yes. We combine mixed thicknesses and grades into one shipment and cut plate and sheet to size in our workshop.
Which certificates and tests can you provide?
Every order ships with a mill certificate (EN 10204 3.1 type) showing heat analysis and mechanical tests. Supplementary tests and 3.2 certificates with SGS, BV, TÜV or another agency are available by agreement.

Conclusion

1.4662 X2CrNiMnMoCuN24-4-3-2 plate should be ordered with the points the standard leaves open written into the contract: finish, tolerance class, any extra chemistry limits and the supplementary tests your application needs. With those fixed, stock material from China is a fast and reliable route.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X