EN 10028-5 P355ML2 Steel Plate | P355ML2 TMCP -50°C Vessel Plate
What is EN 10028-5 P355ML2 Steel?
P355ML2 is the −50 °C TMCP quality in the P355 family of EN 10028-5. Buyers search EN 10028-5 P355ML2, P355ML2 steel plate, 1.8833, P355ML2 TMCP -50°C vessel plate and P355ML2 supplier. ML2 is colder than ML1. This page is not P355M. M is room-temperature TMCP. This page is not P355ML1. ML1 is −40 °C. This page is not P355NL2. P355NL2 is EN 10028-3 normalized plate. This page is not S355ML. S355ML is EN 10025-4 structural steel.
Yield is 355 MPa at ≤16 mm. Tensile is 450–610 MPa. Steel number is 1.8833. Delivery is TMCP (M). Charpy is specified at −50 °C when the order follows ML2. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-5, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.
If a drawing says P355ML1, we will not ship P355ML2 and call colder automatically better without the buyer writing the name. If a drawing says −50 °C, we will not ship ML1 and call minus forty close. Dual marking with 15MnNiNbDR steel plate is possible only when both books are fully met.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | EN 10028-5 P355ML2 | Confirmed |
| Steel number | 1.8833 | Confirmed |
| Product specification | EN 10028-5 + EN 10028-1 | Applied |
| Steel type | Weldable fine-grain, TMCP, −50 °C | Confirmed |
| Usual delivery | M thermomechanically rolled | Confirmed |
| Yield idea | 355 MPa at ≤16 mm | Confirmed |
| Tensile | 450–610 MPa at ≤16 mm | Confirmed |
| Impact idea | −50 °C | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates and carbon steel plates. Chinese low-temperature comparisons belong on GB/T 713.3. Normalized fine-grain sisters belong on EN 10028-3. Structural TMCP belongs on EN 10025-4.
Chemical Composition
Cast analysis follows EN 10028-5. Product analysis follows EN 10028-1 when ordered.
Cast Analysis and Product Analysis — EN 10028-5 P355ML2 (1.8833)
| Element | Cast Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), max | 0.14 | 0.16 |
| Silicon (Si), max | 0.50 | 0.55 |
| Manganese (Mn) | 1.10 – 1.70 | 1.05 – 1.80 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.008 | 0.010 |
| Aluminum total (Al), min | 0.020 | 0.015 |
| Nitrogen (N), max | 0.015 | 0.017 |
| Chromium (Cr), max | 0.30 | 0.35 |
| Copper (Cu), max | 0.30 | 0.35 |
| Molybdenum (Mo), max | 0.08 | 0.10 |
| Nickel (Ni), max | 0.50 | 0.55 |
| Niobium (Nb), max | 0.05 | 0.06 |
| Titanium (Ti), max | 0.05 | 0.06 |
| Vanadium (V), max | 0.10 | 0.12 |
Phosphorus and sulfur stay tight because ML2 is a colder toughness quality than P355M. Carbon stays low because TMCP plus −50 °C is the job. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.
Mechanical Propertie
Buyers search P355ML2 mechanical properties, P355ML2 impact and P355ML2 -50°C. Yield still falls with thickness. Impact is the ML2 item.
Tensile and Yield — EN 10028-5 P355ML2
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) |
|---|---|---|
| ≤ 16 | 355 | 450 – 610 |
| 16 – 40 | 355 | 450 – 610 |
| 40 – 63 | 345 | 440 – 600 |
| 63 – 80 | 325 | 430 – 590 |
| 80 – 100 | 315 | 420 – 580 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Elongation is typically 22% min on thinner plate. Charpy for ML2 is −50 °C. Energy is commonly 27 J average when the order follows the book. Location and orientation must be written. Do not assume ML1 −40 °C is enough for an ML2 drawing.
Do not quote 355 MPa yield on an 80 mm plate. Do not treat −50 °C as permission to stamp 15MnNiNbDR steel plate or P355NL2 without checking both books.
Material Comparison
| Grade | Book | What buyers search | Swap? |
|---|---|---|---|
| EN 10028-5 P355M | EN 10028-5 | P355M steel plate | No |
| EN 10028-5 P355ML1 | EN 10028-5 | P355ML1 steel plate | No |
| EN 10028-5 P355ML2 | EN 10028-5 | P355ML2 steel plate | This page |
| EN 10028-3 P355NL2 | EN 10028-3 | P355NL2 | No |
| EN 10028-2 P355GH | EN 10028-2 | P355GH | No |
| 15MnNiNbDR steel plate | GB/T 713.3 | 15MnNiNbDR | No auto swap |
| 16MnDR steel plate | GB/T 713.3 | 16MnDR | No |
| SA662 Grade C | SA-662 | SA662 Gr.C | No auto swap |
| SA841 Grade A Class 1 | SA-841 | SA841 Gr.A Cl.1 | No auto swap |
Equivalent Material Grades
| Designation | Standard / region | Notes |
|---|---|---|
| EN 10028-5 P355ML2 / 1.8833 | EN 10028-5 | Name on this page |
| P355ML1 / 1.8832 | EN 10028-5 | −40 °C TMCP sister |
| P355M / 1.8821 | EN 10028-5 | Room-temp TMCP sister |
| P355NL2 / 1.1106 | EN 10028-3 | Normalized −50 °C sister |
| 15MnNiNbDR steel plate | GB/T 713.3 | Chinese −50 °C Nb |
| 16MnDR steel plate | GB/T 713.3 | Chinese −40 °C |
| SA662 Grade C | SA-662 | ASME low-temp carbon |
| SA841 Grade A Class 1 | SA-841 | ASME TMCP vessel |
| 09MnNiDR steel plate | GB/T 713.3 | 0.5Ni −70 °C |
TMCP -50°C Pressure-Vessel Service
Buyers pick P355ML2 when a PED file wants 355 MPa TMCP plate and Charpy at −50 °C. Search phrases such as P355ML2 -50°C, P355ML2 TMCP and 1.8833 steel plate all point here.
It is not a substitute for 09MnNiDR steel plate. That grade is −70 °C. It is not a substitute for 08Ni3DR steel plate. That grade is 3.5Ni. It is not LNG inner-tank plate. That work belongs on 06Ni9DR steel plate. An ASME file should name SA-841 or SA-662 with a written −50 °C extra. Dual marking is possible only when both books are met.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.
Weldability
P355ML2 is killed TMCP fine-grain C-Mn vessel plate. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.
Qualify to the applicable code. Consumables must keep toughness at −50 °C, not only at −40 °C. A procedure written for SA516 Grade 70 without an impact extra is not automatically valid. A nickel procedure written for SA203 Grade D is the wrong family. Heat input on TMCP plate should stay controlled so the rolled grain is not coarsened in the HAZ. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is thermomechanically rolled EN 10028-5 P355ML2 (M). This is not +N from EN 10028-3.
If the vessel will see PWHT, say so. Impact after simulated PWHT is worth naming on a −50 °C TMCP file. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists EN 10028-5 P355ML2; 1.8833; heat number; cast analysis; product analysis when ordered; tensile to the correct thickness column; M / TMCP; Charpy at −50 °C when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for P355ML2 TMCP -50°C vessel plate:
- Thickness: commonly 6 mm – 80 mm, thicker by mill agreement
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
Normalized −50 °C plate belongs on EN 10028-3 P355NL2. Structural TMCP belongs on EN 10025-4.
Tolerances
Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another table. Class A is the usual default. If the calculation used minimum thickness after corrosion, write the allowed minus. Do not apply ASTM A36 structural tolerances to a PED −50 °C TMCP plate without writing them. When dual-named against SA841 Grade A Class 1, write which thickness table governs.
Supplementary Requirements
Charpy details. Write −50 °C, joules, location and orientation. Do not write “impact as per EN 10028-5” and expect the mill to guess ML2.
Impact after simulated PWHT. When the vessel will be stress-relieved.
Product analysis. Especially P, S, Al and N.
NDE. EN 10160 or ASTM A435 / A578 as named.
Third-party. EN 10204 3.2 when written.
Applications
| Industry | Typical components |
|---|---|
| PED low-temp TMCP vessels | EN 10028-5 P355ML2 shells at −50 °C |
| Cold-service storage tanks | P355ML2 courses |
| Dual-certified export | P355ML2 / 15MnNiNbDR steel plate when both books fit |
| ASME comparison jobs | P355ML2 next to SA841 Grade A Class 1 |
P355ML2 is the plate for a 355 MPa PED file that wants TMCP and −50 °C. It is the wrong plate for LNG inner tanks. That work belongs on 06Ni9DR steel plate. It is the wrong plate for −40 °C only. That work is P355ML1.
Supply Capability
SHH STEEL sources EN 10028-5 P355ML2 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or TMCP route requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, thicker by mill agreement.
Processing: CNC or flame cutting, bevel, flattening, UT to EN 10160 or the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days; standard TMCP about 45 days; simulated PWHT / 3.2 about 2 months.
Why Choose SHH STEEL
Experience on this grade is simple: keep the letters after P355. M, ML1 and ML2 are three different purchase orders. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices P355ML2 from first-line mills, reports 1.8833 chemistry, records TMCP, prints Charpy at −50 °C when ordered, and issues 3.1 as standard or 3.2 when specified.
We keep the grade on the order. P355ML2 is not P355M. P355ML2 is not P355ML1. P355ML2 is not P355NL2. P355ML2 is not Q345R steel plate. If the drawing says −40 °C, we will not ship ML2 and call colder automatically better without the buyer writing the name.
FAQ
-
What is P355ML2 steel plate?
- P355ML2 is an EN 10028-5 TMCP fine-grain pressure-vessel plate, steel number 1.8833. Yield is 355 MPa at ≤16 mm and tensile is 450–610 MPa. ML2 means Charpy at −50 °C on a TMCP route. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
What is the equivalent of P355ML2?
- Related comparisons are P355NL2, 15MnNiNbDR and SA-662 Grade C. Dual marking is possible only when both books are fully met.
-
How is P355ML2 different from P355ML1?
- ML1 is −40 °C. ML2 is −50 °C. Same yield step, different impact temperature.
-
How is P355ML2 different from P355M?
- P355M is room-temperature TMCP. P355ML2 is −50 °C TMCP.
-
How is P355ML2 different from P355NL2?
- P355NL2 is EN 10028-3 normalized plate. P355ML2 is EN 10028-5 TMCP plate. Same −50 °C idea, different rolling route.
-
Is P355ML2 the same as S355ML?
- No. S355ML is EN 10025-4 structural TMCP steel. P355ML2 is EN 10028-5 pressure-vessel plate.
Conclusion
EN 10028-5 P355ML2 Steel Plate is European TMCP fine-grain −50 °C pressure-vessel plate, steel number 1.8833, at the 355 MPa yield step and 450–610 MPa tensile at ≤16 mm. Whether the inquiry says EN 10028-5 P355ML2, 1.8833 or P355ML2 TMCP -50°C Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with P355ML2 chemistry, recorded TMCP, Charpy at −50 °C when ordered, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies EN 10028-5 P355ML2 TMCP -50°C Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.
Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.
EN 10028-5 P355ML2 Steel Plate, P355ML2 TMCP -50°C vessel plate, 1.8833, P355ML2 supplier, SHH STEEL