EN 10028-5 P355ML1 TMCP low-temperature pressure vessel steel plate, −40 °C, 1.8832, SHH STEEL

EN 10028-5 P355ML1 Steel Plate | P355ML1 TMCP -40°C Vessel Plate

EN 10028-5 P355ML1 is European TMCP fine-grain low-temperature vessel plate, steel number 1.8832. Yield is 355 MPa at ≤16 mm. Impact is −40 °C. SHH STEEL supplies P355ML1 worldwide as a global steel mill sourcing partner.
Keywords
EN 10028-5 P355ML1, P355ML1, P355ML1 steel plate, 1.8832, P355ML1 TMCP -40°C, P355ML1 equivalent, P355ML1 supplier
Equivalent Grades:
EN 10028-5 P355ML1 / GB Q355D (TMCP struct near) — Material Specification: EN 10028-5 — Delivery: TMCP; -40℃ impact
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
TMCP -40°C Pressure-Vessel Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10028-5 P355ML1 Steel?

P355ML1 is the −40 °C TMCP quality in the P355 family of EN 10028-5. Buyers search EN 10028-5 P355ML1, P355ML1 steel plate, 1.8832, P355ML1 TMCP -40°C vessel plate and P355ML1 supplier. ML1 is the low-temperature letter set on a thermomechanically rolled route. This page is not P355M. M is room-temperature TMCP. This page is not P355ML2. ML2 is −50 °C. This page is not P355NL1. P355NL1 is EN 10028-3 normalized plate. This page is not S355ML. S355ML is EN 10025-4 structural steel.

Yield is 355 MPa at ≤16 mm. Tensile is 450–610 MPa. Steel number is 1.8832. Delivery is TMCP (M). Charpy is specified at −40 °C when the order follows ML1. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-5, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.

If a drawing says P355M, we will not ship P355ML1 and call 355 enough. If a drawing says P355NL1, we will not ship P355ML1 and call −40 °C automatic dual name unless both books are met. Dual marking with 16MnDR steel plate is possible only when chemistry, tensile, impact temperature and delivery all fit.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade EN 10028-5 P355ML1 Confirmed
Steel number 1.8832 Confirmed
Product specification EN 10028-5 + EN 10028-1 Applied
Steel type Weldable fine-grain, TMCP, −40 °C Confirmed
Usual delivery M thermomechanically rolled Confirmed
Yield idea 355 MPa at ≤16 mm Confirmed
Tensile 450–610 MPa at ≤16 mm Confirmed
Impact idea −40 °C Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates and carbon steel plates. Chinese −40 °C comparisons belong on GB/T 713.3. Normalized fine-grain sisters belong on EN 10028-3. Structural TMCP belongs on EN 10025-4.

Chemical Composition

Cast analysis follows EN 10028-5. Product analysis follows EN 10028-1 when ordered.

Cast Analysis and Product Analysis — EN 10028-5 P355ML1 (1.8832)

Element Cast Analysis (%) Product Analysis, when ordered (%)
Carbon (C), max 0.14 0.16
Silicon (Si), max 0.50 0.55
Manganese (Mn) 1.10 – 1.70 1.05 – 1.80
Phosphorus (P), max 0.020 0.025
Sulfur (S), max 0.008 0.010
Aluminum total (Al), min 0.020 0.015
Nitrogen (N), max 0.015 0.017
Chromium (Cr), max 0.30 0.35
Copper (Cu), max 0.30 0.35
Molybdenum (Mo), max 0.08 0.10
Nickel (Ni), max 0.50 0.55
Niobium (Nb), max 0.05 0.06
Titanium (Ti), max 0.05 0.06
Vanadium (V), max 0.10 0.12

Phosphorus and sulfur sit tighter than on P355M because ML1 is a toughness quality. Carbon stays low because TMCP plus −40 °C is the job. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search P355ML1 mechanical properties, P355ML1 impact and P355ML1 -40°C. Yield still falls with thickness. Impact is the ML1 item.

Tensile and Yield — EN 10028-5 P355ML1

Thickness (mm) Yield min (MPa) Tensile (MPa)
≤ 16 355 450 – 610
16 – 40 355 450 – 610
40 – 63 345 440 – 600
63 – 80 325 430 – 590
80 – 100 315 420 – 580
Density 7.85 g/cm³ 7.85 g/cm³

Elongation is typically 22% min on thinner plate. Charpy for ML1 is −40 °C. Energy is commonly 27 J average when the order follows the book. Location and orientation must be written. Do not assume ML2 −50 °C on this page.

Do not quote 355 MPa yield on an 80 mm plate. Do not treat −40 °C as permission to stamp 16MnDR steel plate or P355NL1 without checking both books.

Material Comparison

Grade Book What buyers search Swap?
EN 10028-5 P355M EN 10028-5 P355M steel plate No
EN 10028-5 P355ML1 EN 10028-5 P355ML1 steel plate This page
EN 10028-5 P355ML2 EN 10028-5 P355ML2 No
EN 10028-3 P355NL1 EN 10028-3 P355NL1 No
EN 10028-2 P355GH EN 10028-2 P355GH No
16MnDR steel plate GB/T 713.3 16MnDR No auto swap
SA662 Grade B SA-662 SA662 Gr.B No auto swap
SA841 Grade A Class 1 SA-841 SA841 Gr.A Cl.1 No auto swap
Q345R steel plate GB/T 713.2 Q345R No

Equivalent Material Grades

Designation Standard / region Notes
EN 10028-5 P355ML1 / 1.8832 EN 10028-5 Name on this page
P355M / 1.8821 EN 10028-5 Room-temp TMCP sister
P355ML2 / 1.8833 EN 10028-5 −50 °C TMCP sister
P355NL1 / 1.0566 EN 10028-3 Normalized −40 °C sister
16MnDR steel plate GB/T 713.3 Chinese −40 °C
SA662 Grade B SA-662 ASME low-temp carbon
SA516 Grade 70 SA-516 ASME carbon, impact extra
SA841 Grade A Class 1 SA-841 ASME TMCP vessel
SPV355 steel plate JIS G3115 Japanese vessel

TMCP -40°C Pressure-Vessel Service

Buyers pick P355ML1 when a PED file wants 355 MPa TMCP plate and Charpy at −40 °C. Search phrases such as P355ML1 -40°C, P355ML1 TMCP and 1.8832 steel plate all point here.

It is not a substitute for 09MnNiDR steel plate. That grade is −70 °C. It is not a substitute for 08Ni3DR steel plate. That grade is 3.5Ni. An ASME file should name SA-841 or SA-662 with a written −40 °C extra. Dual marking is possible only when both books are met.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

P355ML1 is killed TMCP fine-grain C-Mn vessel plate. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.

Qualify to the applicable code. Consumables must keep toughness at −40 °C. A procedure written for SA516 Grade 70 without an impact extra is not automatically valid. A nickel procedure written for SA203 Grade D is the wrong family. Heat input on TMCP plate should stay controlled so the rolled grain is not coarsened in the HAZ. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is thermomechanically rolled EN 10028-5 P355ML1 (M). This is not +N from EN 10028-3.

If the vessel will see PWHT, say so. Impact after simulated PWHT is worth naming on a −40 °C TMCP file. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists EN 10028-5 P355ML1; 1.8832; heat number; cast analysis; product analysis when ordered; tensile to the correct thickness column; M / TMCP; Charpy at −40 °C when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for P355ML1 TMCP -40°C vessel plate:

  • Thickness: commonly 6 mm – 80 mm, thicker by mill agreement
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Normalized −40 °C plate belongs on EN 10028-3 P355NL1. Structural TMCP belongs on EN 10025-4.

Tolerances

Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another table. Class A is the usual default. If the calculation used minimum thickness after corrosion, write the allowed minus. Do not apply ASTM A36 structural tolerances to a PED −40 °C TMCP plate without writing them. When dual-named against SA841 Grade A Class 1, write which thickness table governs.

Supplementary Requirements

Charpy details. Write −40 °C, joules, location and orientation. Do not write “impact as per EN 10028-5” and expect ML2.

Impact after simulated PWHT. When the vessel will be stress-relieved.

Product analysis. Especially P, S, Al and N.

NDE. EN 10160 or ASTM A435 / A578 as named.

Third-party. EN 10204 3.2 when written.

Applications

Industry Typical components
PED low-temp TMCP vessels EN 10028-5 P355ML1 shells at −40 °C
Storage tanks and drums P355ML1 courses
Dual-certified export P355ML1 / 16MnDR steel plate when both books fit
ASME comparison jobs P355ML1 next to SA841 Grade A Class 1

P355ML1 is the plate for a 355 MPa PED file that wants TMCP and −40 °C. It is the wrong plate for LNG inner tanks. That work belongs on 06Ni9DR steel plate. It is the wrong plate for −50 °C. That work is P355ML2.

Supply Capability

SHH STEEL sources EN 10028-5 P355ML1 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or TMCP route requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, thicker by mill agreement.

Processing: CNC or flame cutting, bevel, flattening, UT to EN 10160 or the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard TMCP about 45 days; simulated PWHT / 3.2 about 2 months.

Why Choose SHH STEEL

Experience on this grade is simple: keep the letters after P355. M, ML1 and ML2 are three different purchase orders. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices P355ML1 from first-line mills, reports 1.8832 chemistry, records TMCP, prints Charpy at −40 °C when ordered, and issues 3.1 as standard or 3.2 when specified.

We keep the grade on the order. P355ML1 is not P355M. P355ML1 is not P355ML2. P355ML1 is not P355NL1. P355ML1 is not Q345R steel plate. If the drawing says −50 °C, we will not ship ML1 and call minus forty close.

FAQ

What is P355ML1 steel plate?
P355ML1 is an EN 10028-5 TMCP fine-grain pressure-vessel plate, steel number 1.8832. Yield is 355 MPa at ≤16 mm and tensile is 450–610 MPa. ML1 means Charpy at −40 °C on a TMCP route. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
What is the equivalent of P355ML1?
Related comparisons are P355NL1, 16MnDR and SA-662 Grade B. Dual marking is possible only when both books are fully met.
How is P355ML1 different from P355M?
P355M is room-temperature TMCP. P355ML1 is −40 °C TMCP.
How is P355ML1 different from P355ML2?
ML2 is −50 °C. Do not ship ML1 against an ML2 drawing.
How is P355ML1 different from P355NL1?
P355NL1 is EN 10028-3 normalized plate. P355ML1 is EN 10028-5 TMCP plate. Same −40 °C idea, different rolling route.
Is P355ML1 the same as S355ML?
No. S355ML is EN 10025-4 structural TMCP steel. P355ML1 is EN 10028-5 pressure-vessel plate.
Can SHH STEEL ship P355ML1 to the USA, Europe or the Middle East?
Yes. SHH STEEL quotes FOB Shanghai and CIF to US West, US Gulf, Rotterdam, Jebel Ali, Singapore and other major ports.
What is the delivery time for P355ML1?
Ex-stock about 5–7 days when plate is in yard. Standard TMCP mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.
Can SHH STEEL issue EN 10204 3.2 for P355ML1?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged with SGS, TÜV, BV, ABS, CCS, DNV or the inspector named on the order.

Conclusion

EN 10028-5 P355ML1 Steel Plate is European TMCP fine-grain −40 °C pressure-vessel plate, steel number 1.8832, at the 355 MPa yield step and 450–610 MPa tensile at ≤16 mm. Whether the inquiry says EN 10028-5 P355ML1, 1.8832 or P355ML1 TMCP -40°C Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with P355ML1 chemistry, recorded TMCP, Charpy at −40 °C when ordered, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies EN 10028-5 P355ML1 TMCP -40°C Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.

Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.

EN 10028-5 P355ML1 Steel Plate, P355ML1 TMCP -40°C vessel plate, 1.8832, P355ML1 supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X