ISO 9328-2 13CrMoV12-10 Steel Plate | 13CrMoV12-10 Cr-Mo-V Pressure Vessel Plate | ISO 9328-2 Cr-Mo-V pressure vessel plate - SHH STEEL

ISO 9328-2 13CrMoV12-10 Steel Plate | 13CrMoV12-10 Cr-Mo-V Pressure Vessel Plate

ISO 9328-2 13CrMoV12-10 steel plate is a chromium-molybdenum-vanadium pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
Keywords
ISO 9328-2 13CrMoV12-10 plate, 13CrMoV12-10 pressure plate, Cr-Mo-V vessel plate, ISO 9328-2 Annex B, +QT pressure steel
Equivalent Grades:
EN 10028-2 12CrMoV12-10 (1.7767) (approx.)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ISO 9328-2 13CrMoV12-10 plate?

ISO 9328-2 13CrMoV12-10 is covered by the pressure-purpose flat-product specification ISO 9328-2:2018. The standard covers plate and strip and works together with ISO 9328-1:2018 general requirements. This enquiry page concerns plate, not a guarantee that every plate size or processing route is available.

13CrMoV12-10 is an Annex B alloy special steel. The visible ordering options identify +QT as an option under clause 5.2(s). The designation describes a nominal 3 % Cr–1 % Mo vanadium-bearing alloy. A related grade with a similar designation under another standard is not evidence of equal ISO chemistry, heat treatment or acceptance.

SHH STEEL handles enquiries within the ISO 9328-2 range and the Pressure Vessel Steel Plates family. We keep the specified ISO edition separate from familiar national-standard product names.

The ISO catalogue was checked on 12 November 2026 (Asia/Shanghai): the 2018 fourth edition remains Published, at stage 90.92 (to be revised). ISO/DIS 9328-2 is under development, not a published replacement. Reconfirm the edition when placing a later order.

Material specification for ISO 9328-2 13CrMoV12-10

Ordering item Basis
Standard ISO 9328-2:2018, Edition 4
General requirements ISO 9328-1:2018
Grade 13CrMoV12-10
Classification, clause 4.1 Alloy special steel
Grade table route Annex B
Product form Plate enquiry within the standard scope for plates and strip
Dimensions State nominal thickness, width, length and quantity; no verified grade thickness range is reproduced
Delivery and testing Confirm the Table B.2 usual condition; +QT is an ordering option under clause 5.2(s).
Inspection documents Specify the required document and traceability with the enquiry

Clause 5 requires purchaser information and treats supplementary options as order-stage decisions. Do not confuse the standard’s illustrative order dimensions with a grade-specific production range. The plate schedule and vessel material specification should accompany the enquiry.

EN 10028-2 comparison chemistry for ISO 9328-2 13CrMoV12-10 (not ISO Table B.1 transcription)

ISO 9328-2:2018 clause 6.3.1 places the cast-analysis requirements for 13CrMoV12-10 in Table B.1. The official 2018 preview does not include that table, and it is not transcribed here as an ISO normative row.

The following heat-analysis figures are EN 10028-2 comparison/reference data for EN 10028-2 12CrMoV12-10 (1.7767). They are shown because the two designations describe a similar alloy family. They are not ISO Table B.1 limits. A maximum is not a target addition. Confirm the official ISO Table B.1 row, the applicable notes and any product-analysis provisions of clause 6.3.2 and Table 1 before accepting a certificate.

Element Cast / heat analysis, mass %
C 0.10–0.15
Si ≤0.15
Mn 0.30–0.60
P ≤0.015
S ≤0.005
Al total Determined and reported
N ≤0.012
Cr 2.75–3.25
Cu ≤0.25
Mo 0.90–1.10
Nb ≤0.07
Ni ≤0.25
Ti ≤0.03
V 0.20–0.30
B ≤0.003
Ca ≤0.015

Product analysis must be assessed under the ISO product-analysis rules, not by silently widening these EN comparison limits. Intentional additions of unlisted elements remain an order-stage decision.

The EN comparison chromium range of 2.75–3.25 % matches the 12-10 designation class (about 3 % Cr). Peer supplier tables for 13CrMoV12-10 list a similar chromium and molybdenum window, with a looser carbon maximum (≤0.17 %) and a looser sulphur maximum than this EN row. The EN row is used here because it comes from a complete, consistent table; the ISO row may differ. EN 13CrMoV9-10 is a different 2.25 % Cr grade and is not this steel.

EN 10028-2 comparison mechanical properties for ISO 9328-2 13CrMoV12-10 (not ISO Table B.2 transcription)

ISO 9328-2:2018 clause 6.4.1 refers 13CrMoV12-10 mechanical acceptance to Table B.2 and to ISO 9328-1. That ISO grade-property table is not in the official 2018 preview, and it is not transcribed here as an ISO normative limit.

The following room-temperature and elevated-temperature values are EN 10028-2 comparison/reference data for the related grade EN 10028-2 12CrMoV12-10 (1.7767). They are offered because the two designations describe a similar alloy family. They must not be treated as ISO Table B.2 limits and must not be used as allowable design stresses. Confirm every acceptance value against the complete ISO 9328-2:2018 Table B.2 and the ordered edition before supply or design use.

Thickness bands below are EN table bands, not a stock list and not a claimed ISO grade thickness range. The usual delivery conditions in the EN table are EN conditions; the ISO usual condition is in Table B.2 and must be confirmed on the order.

Room-temperature tensile properties — EN 10028-2 comparison (transverse).

Nominal thickness t (mm) Usual delivery (EN Table 3) Yield ReH, min (MPa) Tensile Rm (MPa) Elongation A, min (%)
≤60 +NT 455 600–780 18
60 < t ≤ 150 +NT 435 590–770 18
150 < t ≤ 250 +QT 415 580–760 18

Impact energy KV — EN 10028-2 comparison.

Thickness applicability (EN Table 3) KV at −20 °C (J, min) KV at 0 °C (J, min) KV at +20 °C (J, min)
all listed bands 27 34 40

Minimum 0.2 % proof strength Rp0,2 at elevated temperature — EN 10028-2 comparison (MPa).

Nominal thickness t (mm) 50 °C 100 °C 150 °C 200 °C 250 °C 300 °C 350 °C 400 °C 450 °C 500 °C
≤60 410 395 380 375 370 365 362 360 350 –
60 < t ≤ 250 405 390 370 365 360 355 352 350 340 –

EN footnote g: a higher impact minimum may be agreed. The EN 13CrMoV9-10 table coincides with these mechanical cells; chemistry still differs.

No ASTM, JIS or GB property numbers have been substituted as ISO limits. Elevated-temperature values in a comparison table are not a universal maximum service temperature.

Delivery condition and ordering options for 13CrMoV12-10

Unless otherwise agreed, clause 6.2.1 requires supply in the usual condition given in Table B.2. Clause 5.2(s) allows the delivery condition +QT to be specified for 13CrMoV12-10. Confirm that option and the full Table B.2 row at enquiry and order. Do not assume an EN usual condition as the ISO default.

Clause 6.2.4 requires steels containing 2 % chromium or more to be supplied in a stress-relieved condition as a minimum. That minimum does not replace the ordered usual condition in Table B.2.

If untreated (+AR) delivery is agreed, clause 6.2.5 requires the processor to test pieces in the usual delivery condition indicated in Table B.2. Simulated heat-treatment tests do not discharge the processor from proving the specified properties in the finished, correctly heat-treated product. Mark untreated plate clearly.

Annex D of the standard contains heat-treatment information for the purchaser. Confirm the ISO usual condition, any agreed alternative, and any simulated post-weld or fabrication heat-treatment tests on the order.

Weldability and fabrication review for 13CrMoV12-10

Clause 6.7.1 describes the steels as suitable for welding processes in current use. This is not a qualified welding procedure for 13CrMoV12-10. The fabricator must establish consumables, preheat, interpass control, heat input and any post-weld heat treatment through the applicable procedure qualification and design requirements.

Clause 6.7.2 warns that excessive post-weld heat treatment can reduce mechanical properties. Tell SHH STEEL the intended treatment and discuss simulated heat-treated test pieces where they are required. This 3 % Cr–Mo–V grade needs a fabrication review of preheat and post-weld heat treatment appropriate to the chromium and vanadium design.

Base-plate certification is not proof of completed-weld or heat-affected-zone performance. Any required weld and HAZ toughness must be addressed by the fabrication qualification.

Dimensions, surface quality and inspection

Clause 6.8 refers dimensions and dimensional tolerances to ISO 9328-1. Surface condition, internal soundness, inspection, retesting and marking also refer to that general-requirements standard. This preview does not supply the full tolerance schedule; no numeric thickness deviation, flatness allowance or ultrasonic acceptance class is claimed.

State the required nominal dimensions, edge condition, dimensional acceptance, surface restrictions, internal-soundness examination and document type with the enquiry. Identification must remain traceable through cutting, packing and shipment. Confirm how test certificates and cut-piece identification will be supplied; dimensional availability remains subject to mill confirmation.

Applications and service limits of 13CrMoV12-10

13CrMoV12-10 may be considered for heavy-wall or elevated-temperature pressure-retaining plate, including thick vessel shells and related welded equipment, where the design specification selects this exact ISO grade. These are intended-use examples, not authorization for a particular pressure, temperature, wall thickness or fabrication code.

Elevated-temperature properties in a material specification or a comparison table are not a universal maximum service temperature. The designer must assess allowable stresses, creep where relevant, corrosion allowance and the governing pressure-equipment code. Grade selection remains an engineering decision, not a catalogue substitution.

Related product families on this site include EN 10028-2 and GB/T 713. Their certificates cannot replace the specified ISO delivery requirements without engineer approval.

Compare 13CrMoV12-10 with related ISO grades

Compare the following published ISO grades by their complete annex rows, delivery condition and project acceptance, not only by similar designations. These are related selections within the standard, not interchangeable materials. Other Annex B grades in this family are not linked here until those product pages are live.

ISO product Classification Review before a grade change
ISO 9328-2 13CrMo4-5 Alloy special steel, Annex A Lower chromium and molybdenum class, no vanadium design; different annex and property tables.
ISO 9328-2 16Mo3 Alloy special steel, Annex A Molybdenum grade without a 3 % chromium or vanadium design; different chemistry and mechanical tables.
ISO 9328-2 15NiCuMoNb5-6-4 Alloy special steel, Annex A Ni-Cu-Mo-Nb elevated-temperature grade; not a Cr-Mo-V substitute.

A similarly named Annex A and Annex B grade must remain a separate material identity. Do not assume equal chemistry, heat treatment or mechanical acceptance from a comparable designation.

Related grades and substitution limits for 13CrMoV12-10

The heading identifies a comparison topic, not a declaration of interchangeable material. No automatic foreign equivalent or dual certification is offered for 13CrMoV12-10.

Product / range Verified relationship or limitation Substitution control
EN 10028-2 12CrMoV12-10 (1.7767) Closest EN designation in the 3 % Cr–1 % Mo–V family. Not automatic identity of every ISO requirement. Engineer approval required; confirm chemistry, usual condition and mechanical tables.
EN 10028-2 10CrMo9-10 / EN 10028-2 13CrMo4-5 Related chromium-molybdenum vessel grades without this vanadium and chromium combination. Not substitutes for 13CrMoV12-10.

Complete specification review and engineer approval are required before substitution or dual-certification claims. General requirements, edition, options, inspection and project acceptance still need review.

Why choose SHH STEEL for 13CrMoV12-10

SHH STEEL supports specification-led pressure-plate purchasing rather than substitution by catalogue name.

  • We quote the requested ISO edition and grade separately from related national-standard products.
  • Delivery condition, fabrication heat treatment and supplementary test requests are reviewed before confirmation.
  • Comparison figures on this page are labelled as such; they are not used as unofficial ISO acceptance limits.
  • Inspection documentation and export packing are coordinated against the order.
  • Supply capability, lead time and any additional testing remain subject to quotation confirmation.

Enquiry and supply review for 13CrMoV12-10

Send the project material schedule for 13CrMoV12-10. SHH STEEL will review the enquiry and identify any clarification needed before confirming the supply route.

Enquiry item Information required
Material identity ISO 9328-2:2018 13CrMoV12-10; identify any proposed dual certification explicitly
Dimensions and quantity Nominal thickness, width, length, quantity and cutting drawings
Delivery condition Applicable usual condition, any agreed alternative, and untreated supply if requested
Acceptance values Complete ISO Table B.1 and Table B.2 requirements for the ordered edition; say if comparison values are for enquiry only
Inspection document Document type, traceability and any third-party attendance
Fabrication Forming, welding and intended post-weld heat treatment; any simulated heat-treatment tests
Destination Delivery place and any packing or marking restrictions

Missing numerical requirements on this comparison page are not waivers of the standard. Do not approve a substitution solely from this comparison content.

FAQ

Which edition applies to 13CrMoV12-10 here?
This page uses ISO 9328-2:2018, Edition 4. The ISO catalogue checked on 12 November 2026 (Asia/Shanghai) still lists it as Published, with revision planned and ISO/DIS 9328-2 under development.
What is the classification of 13CrMoV12-10?
Alloy special steel under clause 4.1. The applicable grade route is Annex B; its complete requirements and ISO 9328-1 general requirements must be used together.
Are chemistry and mechanical numbers ISO normative limits?
No. ISO Table B.1 and Table B.2 are not in the official preview and are not transcribed as ISO limits. Chemistry and mechanical figures on this page are EN 10028-2 comparison/reference data for 12CrMoV12-10, clearly labelled. Confirm the official ISO rows before supply or design use.
Can another standard or a similar designation replace it?
Not automatically. Related product families are comparison references only. Complete specification review and engineer approval are required before substitution or dual-certification claims.
What should I send for a quotation?
Send the ISO edition and grade, dimensions, quantity, delivery condition, complete ISO acceptance requirements, inspection-document type and planned fabrication heat treatment. Include agreed supplementary tests and destination. If comparison values are being used for enquiry only, say so. The complete ISO Table B.1 and Table B.2 row must be available for a technical supply commitment.

Request a quotation for ISO 9328-2 13CrMoV12-10 plate

Request a SHH STEEL quotation for ISO 9328-2:2018 13CrMoV12-10 plate. Send nominal thickness, width, length, quantity, destination and the project material specification.

Identify the delivery condition, complete ISO chemistry and mechanical acceptance requirements, required inspection document and any impact, internal-soundness or supplementary tests. Include forming, welding and intended post-weld heat treatment for technical review.

Availability, dimensions, processing, testing and lead time will be confirmed against the enquiry. Related grades are not treated as approved substitutes without engineer review.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X