ISO 9328-2 19MnMoNi6-5 Steel Plate | 19MnMoNi6-5 Mn-Mo-Ni Pressure Vessel Plate | ISO 9328-2 Mn-Mo-Ni pressure vessel plate - SHH STEEL

ISO 9328-2 19MnMoNi6-5 Steel Plate | 19MnMoNi6-5 Mn-Mo-Ni Pressure Vessel Plate

ISO 9328-2 19MnMoNi6-5 steel plate is a manganese-molybdenum-nickel pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Alloy special steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
Keywords
ISO 9328-2 19MnMoNi6-5 plate, 19MnMoNi6-5 pressure plate, Mn-Mo-Ni vessel plate, ISO 9328-2 Annex B, nickel vessel steel
Equivalent Grades:
ISO / EN 20MnMoNi4-5 (approx.)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ISO 9328-2 19MnMoNi6-5 plate?

ISO 9328-2 19MnMoNi6-5 is covered by the pressure-purpose flat-product specification ISO 9328-2:2018. The standard covers plate and strip and works together with ISO 9328-1:2018 general requirements. This enquiry page concerns plate, not a guarantee that every plate size or processing route is available.

19MnMoNi6-5 is an Annex B alloy special steel. The 6-5 designation indicates a higher manganese class with a specified nickel addition. It is a separate Annex B grade from 19MnMoNi5-5 and from Annex A 20MnMoNi4-5. A related grade with a similar designation under another standard is not evidence of equal ISO chemistry, heat treatment or acceptance.

SHH STEEL handles enquiries within the ISO 9328-2 range and the Pressure Vessel Steel Plates family. We keep the specified ISO edition separate from familiar national-standard product names.

The ISO catalogue was checked on 12 November 2026 (Asia/Shanghai): the 2018 fourth edition remains Published, at stage 90.92 (to be revised). ISO/DIS 9328-2 is under development, not a published replacement. Reconfirm the edition when placing a later order.

Material specification for ISO 9328-2 19MnMoNi6-5

Ordering item Basis
Standard ISO 9328-2:2018, Edition 4
General requirements ISO 9328-1:2018
Grade 19MnMoNi6-5
Classification, clause 4.1 Alloy special steel
Grade table route Annex B
Product form Plate enquiry within the standard scope for plates and strip
Dimensions State nominal thickness, width, length and quantity; no verified grade thickness range is reproduced
Delivery and testing Confirm the grade-specific usual delivery condition in the complete ISO Table B.2; no default is assumed.
Inspection documents Specify the required document and traceability with the enquiry

Clause 5 requires purchaser information and treats supplementary options as order-stage decisions. Do not confuse the standard’s illustrative order dimensions with a grade-specific production range. The plate schedule and vessel material specification should accompany the enquiry.

Peer/supplier comparison chemistry for ISO 9328-2 19MnMoNi6-5 (not ISO Table B.1 transcription)

ISO 9328-2:2018 clause 6.3.1 places the cast-analysis requirements for 19MnMoNi6-5 in Table B.1. The official 2018 preview does not include that table, and it is not transcribed here as an ISO normative row.

The following heat-analysis figures are peer and supplier comparison data used for enquiry. They are not a transcription of ISO Table B.1. A maximum is not a target addition. The 2018 edition added a boron maximum of 0.0010 % in Table B.1 for this grade family (product-analysis boron 0.0015 % under Table 1, footnote b) and changed phosphorus and sulphur relative to the 2011 edition; the boron figure below follows that 2018 official note. Phosphorus, sulphur and the remaining element limits remain peer-comparison values. Confirm the complete official ISO Table B.1 row before accepting a certificate.

Peer tables for 19MnMoNi6-5 list Mn 1.15–1.50 %, Mo 0.45–0.60 %, Ni 0.40–0.70 %, Cr ≤0.20 % and V ≤0.020 %, with C ≤0.25 %. The nickel window is slightly tighter than the ISO Annex A 20MnMoNi4-5 nickel range of 0.40–0.80 %.

Element Cast / heat analysis, mass %
C ≤0.25
Si ≤0.40
Mn 1.15–1.50
P ≤0.025
S ≤0.025
Cr ≤0.20
Cu ≤0.40
Mo 0.45–0.60
Nb ≤0.020
Ni 0.40–0.70
Ti ≤0.030
V ≤0.020
B ≤0.0010

Product analysis for Annex B grades is controlled by ISO Table 1; for this grade family the Table B.1 maxima also apply to product analysis, except for the official boron product-analysis exception noted above. Do not treat the peer row as a waiver of the official table.

EN 10028-2 comparison mechanical properties for ISO 9328-2 19MnMoNi6-5 (not ISO Table B.2 transcription)

ISO 9328-2:2018 clause 6.4.1 refers 19MnMoNi6-5 mechanical acceptance to Table B.2 and to ISO 9328-1. That ISO grade-property table is not in the official 2018 preview, and it is not transcribed here as an ISO normative limit.

The following room-temperature and elevated-temperature values are EN 10028-2 comparison/reference data for the related grade EN 10028-2 20MnMoNi4-5 (1.6311), also published here as ISO 9328-2 20MnMoNi4-5. They are offered because the two designations describe a similar alloy family. They must not be treated as ISO Table B.2 limits and must not be used as allowable design stresses. Confirm every acceptance value against the complete ISO 9328-2:2018 Table B.2 and the ordered edition before supply or design use.

Thickness bands below are EN table bands, not a stock list and not a claimed ISO grade thickness range. The usual delivery conditions in the EN table are EN conditions; the ISO usual condition is in Table B.2 and must be confirmed on the order.

Room-temperature tensile properties — EN 10028-2 comparison (transverse).

Nominal thickness t (mm) Usual delivery (EN Table 3) Yield ReH, min (MPa) Tensile Rm (MPa) Elongation A, min (%)
≤40 +QT 470 590–750 18
40 < t ≤ 60 +QT 460 590–730 18
60 < t ≤ 100 +QT 450 570–710 18
100 < t ≤ 150 +QT 440 570–710 18
150 < t ≤ 250 +QT 400 560–700 18

Impact energy KV — EN 10028-2 comparison.

Thickness applicability (EN Table 3) KV at −20 °C (J, min) KV at 0 °C (J, min) KV at +20 °C (J, min)
all listed bands 27 40 50

Minimum 0.2 % proof strength Rp0,2 at elevated temperature — EN 10028-2 comparison (MPa).

Nominal thickness t (mm) 50 °C 100 °C 150 °C 200 °C 250 °C 300 °C 350 °C 400 °C 450 °C 500 °C
≤40 460 448 439 432 424 415 402 384 – –
40 < t ≤ 60 450 438 430 423 415 406 394 375 – –
60 < t ≤ 100 441 429 420 413 406 398 385 367 – –
100 < t ≤ 150 431 419 411 404 397 389 377 359 – –
150 < t ≤ 250 392 381 374 367 361 353 342 327 – –

Individual ISO Annex B grades in the 19MnMoNi family may have different Table B.2 rows; this EN table is a family comparison only.

No ASTM, JIS or GB property numbers have been substituted as ISO limits. Elevated-temperature values in a comparison table are not a universal maximum service temperature.

Delivery condition and ordering options for 19MnMoNi6-5

19MnMoNi6-5 is not one of the clause 6.2.3 grades for which +N, +AR or +QT must be named from that list. Clause 6.2.1 still requires supply in the usual condition given in Table B.2 unless otherwise agreed. Confirm that usual condition from the complete table; no default is assumed on this page.

If untreated (+AR) delivery is agreed, clause 6.2.5 requires the processor to test pieces in the usual delivery condition indicated in Table B.2. Simulated heat-treatment tests do not discharge the processor from proving the specified properties in the finished, correctly heat-treated product. Mark untreated plate clearly.

Annex D of the standard contains heat-treatment information for the purchaser. Confirm the ISO usual condition, any agreed alternative, and any simulated post-weld or fabrication heat-treatment tests on the order.

Weldability and fabrication review for 19MnMoNi6-5

Clause 6.7.1 describes the steels as suitable for welding processes in current use. This is not a qualified welding procedure for 19MnMoNi6-5. The fabricator must establish consumables, preheat, interpass control, heat input and any post-weld heat treatment through the applicable procedure qualification and design requirements.

Clause 6.7.2 warns that excessive post-weld heat treatment can reduce mechanical properties. Tell SHH STEEL the intended treatment and discuss simulated heat-treated test pieces where they are required. Nickel-bearing Mn-Mo vessel steels still need a qualified welding procedure written for the ordered grade; do not copy a procedure from a nickel-free Mn-Mo designation.

Base-plate certification is not proof of completed-weld or heat-affected-zone performance. Any required weld and HAZ toughness must be addressed by the fabrication qualification.

Dimensions, surface quality and inspection

Clause 6.8 refers dimensions and dimensional tolerances to ISO 9328-1. Surface condition, internal soundness, inspection, retesting and marking also refer to that general-requirements standard. This preview does not supply the full tolerance schedule; no numeric thickness deviation, flatness allowance or ultrasonic acceptance class is claimed.

State the required nominal dimensions, edge condition, dimensional acceptance, surface restrictions, internal-soundness examination and document type with the enquiry. Identification must remain traceable through cutting, packing and shipment. Confirm how test certificates and cut-piece identification will be supplied; dimensional availability remains subject to mill confirmation.

Applications and service limits of 19MnMoNi6-5

19MnMoNi6-5 may be considered for heavier pressure-retaining plate, including thick vessel components, where the design specification selects this exact ISO nickel-bearing Mn-Mo grade. These are intended-use examples, not authorization for a particular pressure, temperature or wall thickness.

Elevated-temperature properties in a material specification or a comparison table are not a universal maximum service temperature. The designer must assess allowable stresses, creep where relevant, corrosion allowance and the governing pressure-equipment code. Grade selection remains an engineering decision, not a catalogue substitution.

Related product families on this site include EN 10028-2 and GB/T 713. Their certificates cannot replace the specified ISO delivery requirements without engineer approval.

Compare 19MnMoNi6-5 with related ISO grades

Compare the following published ISO grades by their complete annex rows, delivery condition and project acceptance, not only by similar designations. These are related selections within the standard, not interchangeable materials. Other Annex B grades in this family are not linked here until those product pages are live.

ISO product Classification Review before a grade change
ISO 9328-2 20MnMoNi4-5 Alloy special steel, Annex A Related Mn-Mo-Ni designation on the Annex A route, with a verified ISO Table A.1 chemistry row.
ISO 9328-2 18MnMo4-5 Alloy special steel, Annex A Nickel-free manganese-molybdenum grade; not a nickel-bearing substitute.
ISO 9328-2 15NiCuMoNb5-6-4 Alloy special steel, Annex A Different nickel-copper-molybdenum-niobium design.

A similarly named Annex A and Annex B grade must remain a separate material identity. Do not assume equal chemistry, heat treatment or mechanical acceptance from a comparable designation.

Related grades and substitution limits for 19MnMoNi6-5

The heading identifies a comparison topic, not a declaration of interchangeable material. No automatic foreign equivalent or dual certification is offered for 19MnMoNi6-5.

Product / range Verified relationship or limitation Substitution control
EN 10028-2 20MnMoNi4-5 / ISO 9328-2 20MnMoNi4-5 Closest published Mn-Mo-Ni comparison grades on this site. Annex A alignment is stated in the ISO foreword for 20MnMoNi4-5, not for this Annex B grade. Not automatic equivalence; engineer approval required.

Complete specification review and engineer approval are required before substitution or dual-certification claims. General requirements, edition, options, inspection and project acceptance still need review.

Why choose SHH STEEL for 19MnMoNi6-5

SHH STEEL supports specification-led pressure-plate purchasing rather than substitution by catalogue name.

  • We quote the requested ISO edition and grade separately from related national-standard products.
  • Delivery condition, fabrication heat treatment and supplementary test requests are reviewed before confirmation.
  • Comparison figures on this page are labelled as such; they are not used as unofficial ISO acceptance limits.
  • Inspection documentation and export packing are coordinated against the order.
  • Supply capability, lead time and any additional testing remain subject to quotation confirmation.

Enquiry and supply review for 19MnMoNi6-5

Send the project material schedule for 19MnMoNi6-5. SHH STEEL will review the enquiry and identify any clarification needed before confirming the supply route.

Enquiry item Information required
Material identity ISO 9328-2:2018 19MnMoNi6-5; identify any proposed dual certification explicitly
Dimensions and quantity Nominal thickness, width, length, quantity and cutting drawings
Delivery condition Applicable usual condition, any agreed alternative, and untreated supply if requested
Acceptance values Complete ISO Table B.1 and Table B.2 requirements for the ordered edition; say if comparison values are for enquiry only
Inspection document Document type, traceability and any third-party attendance
Fabrication Forming, welding and intended post-weld heat treatment; any simulated heat-treatment tests
Destination Delivery place and any packing or marking restrictions

Missing numerical requirements on this comparison page are not waivers of the standard. Do not approve a substitution solely from this comparison content.

FAQ

Which edition applies to 19MnMoNi6-5 here?
This page uses ISO 9328-2:2018, Edition 4. The ISO catalogue checked on 12 November 2026 (Asia/Shanghai) still lists it as Published, with revision planned and ISO/DIS 9328-2 under development.
What is the classification of 19MnMoNi6-5?
Alloy special steel under clause 4.1. The applicable grade route is Annex B; its complete requirements and ISO 9328-1 general requirements must be used together.
Are chemistry and mechanical numbers ISO normative limits?
No. ISO Table B.1 and Table B.2 are not transcribed as ISO limits. Chemistry figures are labelled comparison or peer data. Mechanical figures are EN 10028-2 comparison/reference data for 20MnMoNi4-5. Confirm the official ISO rows before supply or design use.
Can another standard or a similar designation replace it?
Not automatically. Related product families are comparison references only. Complete specification review and engineer approval are required before substitution or dual-certification claims.
What should I send for a quotation?
Send the ISO edition and grade, dimensions, quantity, delivery condition, complete ISO acceptance requirements, inspection-document type and planned fabrication heat treatment. Include agreed supplementary tests and destination. If comparison values are being used for enquiry only, say so. The complete ISO Table B.1 and Table B.2 row must be available for a technical supply commitment.

Request a quotation for ISO 9328-2 19MnMoNi6-5 plate

Request a SHH STEEL quotation for ISO 9328-2:2018 19MnMoNi6-5 plate. Send nominal thickness, width, length, quantity, destination and the project material specification.

Identify the delivery condition, complete ISO chemistry and mechanical acceptance requirements, required inspection document and any impact, internal-soundness or supplementary tests. Include forming, welding and intended post-weld heat treatment for technical review.

Availability, dimensions, processing, testing and lead time will be confirmed against the enquiry. Related grades are not treated as approved substitutes without engineer review.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X