ISO 9328-2 PT450GH Steel Plate | PT450GH Elevated-Temp Pressure Plate | ISO 9328-2 elevated-temperature pressure vessel plate - SHH STEEL

ISO 9328-2 PT450GH Steel Plate | PT450GH Elevated-Temp Pressure Plate

ISO 9328-2 PT450GH steel plate is a non-alloy elevated-temperature pressure-equipment grade under ISO 9328-2:2018, Edition 4, Annex B. Non-alloy-quality steel identity and the ordered delivery condition must stay on the material order. SHH STEEL reviews plate dimensions, testing and inspection-document requirements before confirming supply. Grade names alone do not establish service suitability.
Keywords
ISO 9328-2 PT450GH plate, PT450GH pressure plate, ISO 9328-2 Annex B, carbon vessel plate, PT450GH steel plate
Equivalent Grades:
JIS G 3118 SGV450, JIS G 3103 SB450 (approx.)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ISO 9328-2 PT450GH plate?

ISO 9328-2 PT450GH is covered by the pressure-purpose flat-product specification ISO 9328-2:2018. The standard covers plate and strip and works together with ISO 9328-1:2018 general requirements. This enquiry page concerns plate, not a guarantee that every plate size or processing route is available.

PT450GH is an Annex B non-alloy-quality steel. The designation indicates a tensile-strength class around 450 MPa in the Annex B non-alloy group. Clause 6.2.3 requires the requested delivery condition to be specified at enquiry and order. A related grade with a similar designation under another standard is not evidence of equal ISO chemistry, heat treatment or acceptance.

SHH STEEL handles enquiries within the ISO 9328-2 range and the Pressure Vessel Steel Plates family. We keep the specified ISO edition separate from familiar national-standard product names.

The ISO catalogue was checked on 12 November 2026 (Asia/Shanghai): the 2018 fourth edition remains Published, at stage 90.92 (to be revised). ISO/DIS 9328-2 is under development, not a published replacement. Reconfirm the edition when placing a later order.

Material specification for ISO 9328-2 PT450GH

Ordering item Basis
Standard ISO 9328-2:2018, Edition 4
General requirements ISO 9328-1:2018
Grade PT450GH
Classification, clause 4.1 Non-alloy-quality steel
Grade table route Annex B
Product form Plate enquiry within the standard scope for plates and strip
Dimensions State nominal thickness, width, length and quantity; no verified grade thickness range is reproduced
Delivery and testing Specify the requested condition under clause 6.2.3; confirm grade-specific Table B.2 restrictions.
Inspection documents Specify the required document and traceability with the enquiry

Clause 5 requires purchaser information and treats supplementary options as order-stage decisions. Do not confuse the standard’s illustrative order dimensions with a grade-specific production range. The plate schedule and vessel material specification should accompany the enquiry.

JIS G 3118 comparison chemistry for ISO 9328-2 PT450GH (not ISO Table B.1 transcription)

ISO 9328-2:2018 clause 6.3.1 places the cast-analysis requirements for PT450GH in Table B.1. The official 2018 preview does not include that table, and it is not transcribed here as an ISO normative row.

The following heat-analysis figures are JIS G 3118 comparison/reference data for JIS G 3118 SGV450, a related carbon pressure-vessel grade in the same tensile-strength class. They are not ISO Table B.1 limits, and the thickness-dependent carbon columns are JIS columns, not an ISO thickness range. The 2018 ISO edition added a boron maximum of 0.0010 % for the PT grades in Table B.1 (product-analysis boron 0.0015 % under Table 1, footnote b); that official boron note is not a complete ISO chemistry row. Confirm the official ISO Table B.1 row before accepting a certificate.

Thickness, mm (JIS) C max, heat % Si, heat % Mn, heat % P max, % S max, %
6 to 12.5 0.24 0.15–0.40 0.85–1.20 0.020 0.020
over 12.5 to 50 0.26 0.15–0.40 0.85–1.20 0.020 0.020
over 50 to 100 0.28 0.15–0.40 0.85–1.20 0.020 0.020
over 100 to 200 0.29 0.15–0.40 0.85–1.20 0.020 0.020

Under the JIS comparison table, plates 12.5 mm and under may use a lower manganese range, and a carbon-manganese exchange rule may raise the manganese maximum up to 1.60 %. Those JIS options are not ISO options. Alloying elements not listed in the JIS row, if added, must be reported on the JIS certificate; that rule does not replace ISO Table B.1.

JIS G 3118 comparison mechanical properties for ISO 9328-2 PT450GH (not ISO Table B.2 transcription)

ISO 9328-2:2018 clause 6.4.1 refers PT450GH mechanical acceptance to Table B.2 and to ISO 9328-1. That ISO grade-property table is not in the official 2018 preview, and it is not transcribed here as an ISO normative limit.

The following values are JIS G 3118 comparison/reference data for JIS G 3118 SGV450, a related carbon pressure-vessel grade in the same tensile-strength class. They are not ISO Table B.2 limits and must not be used as allowable design stresses. Confirm every acceptance value against the complete ISO Table B.2 and the ordered edition.

Property (JIS G 3118 comparison) Requirement
Yield point or 0.2 % proof stress, min 245 N/mm²
Tensile strength 450–540 N/mm²
Elongation, 6 to 40 mm, No. 1A test piece, min 19 %
Elongation, over 50 to 200 mm, No. 10 test piece, min 23 %

JIS test pieces are transverse to the final rolling direction. Elongation adjustments for very thin or intermediate JIS test pieces are JIS rules, not ISO rules. Charpy, ultrasonic and other supplementary tests remain order-stage decisions.

No EN, ASTM or GB property numbers have been substituted as ISO limits. The JIS comparison tensile range is not an ISO thickness-banded table.

Delivery condition and ordering options for PT450GH

For PT450GH, clause 6.2.3 requires the requested delivery condition — normalized (+N), untreated (+AR) (see 6.2.5), or quenched and tempered (+QT) where applicable — to be specified at enquiry and order. A maximum carbon-equivalent value may be agreed for the PT grades under clause 6.3.3. Confirm the complete Table B.2 row; there is no automatic default assumed on this page.

If untreated (+AR) delivery is agreed, clause 6.2.5 requires the processor to test pieces in the usual delivery condition indicated in Table B.2. Simulated heat-treatment tests do not discharge the processor from proving the specified properties in the finished, correctly heat-treated product. Mark untreated plate clearly.

Annex D of the standard contains heat-treatment information for the purchaser. Confirm the ISO usual condition, any agreed alternative, and any simulated post-weld or fabrication heat-treatment tests on the order.

Weldability and fabrication review for PT450GH

Clause 6.7.1 describes the steels as suitable for welding processes in current use. This is not a qualified welding procedure for PT450GH. The fabricator must establish consumables, preheat, interpass control, heat input and any post-weld heat treatment through the applicable procedure qualification and design requirements.

Clause 6.7.2 warns that excessive post-weld heat treatment can reduce mechanical properties. Tell SHH STEEL the intended treatment and discuss simulated heat-treated test pieces where they are required. Treat this carbon pressure grade as a distinct ISO identity from similarly numbered JIS SGV or SB plates when writing the welding procedure.

Base-plate certification is not proof of completed-weld or heat-affected-zone performance. Any required weld and HAZ toughness must be addressed by the fabrication qualification.

Dimensions, surface quality and inspection

Clause 6.8 refers dimensions and dimensional tolerances to ISO 9328-1. Surface condition, internal soundness, inspection, retesting and marking also refer to that general-requirements standard. This preview does not supply the full tolerance schedule; no numeric thickness deviation, flatness allowance or ultrasonic acceptance class is claimed.

State the required nominal dimensions, edge condition, dimensional acceptance, surface restrictions, internal-soundness examination and document type with the enquiry. Identification must remain traceable through cutting, packing and shipment. Confirm how test certificates and cut-piece identification will be supplied; dimensional availability remains subject to mill confirmation.

Applications and service limits of PT450GH

PT450GH may be considered for pressure-retaining plate such as vessel shells, heads and welded equipment where the design specification selects this exact ISO non-alloy grade. These are intended-use examples, not authorization for a particular pressure, temperature or wall thickness.

Elevated-temperature properties in a material specification or a comparison table are not a universal maximum service temperature. The designer must assess allowable stresses, creep where relevant, corrosion allowance and the governing pressure-equipment code. Grade selection remains an engineering decision, not a catalogue substitution.

Related product families on this site include EN 10028-2 and GB/T 713. Their certificates cannot replace the specified ISO delivery requirements without engineer approval.

Compare PT450GH with related ISO grades

Compare the following published ISO grades by their complete annex rows, delivery condition and project acceptance, not only by similar designations. These are related selections within the standard, not interchangeable materials. Other Annex B grades in this family are not linked here until those product pages are live.

ISO product Classification Review before a grade change
ISO 9328-2 P265GH Non-alloy-quality steel, Annex A Annex A non-alloy route with a verified ISO Table A.1 chemistry row; different designation and annex.
ISO 9328-2 P295GH Non-alloy-quality steel, Annex A Higher Annex A yield class; not interchangeable with this Annex B PT grade.
ISO 9328-2 P355GH Non-alloy-quality steel, Annex A Higher Annex A yield class; confirm both complete annex rows before any comparison.

A similarly named Annex A and Annex B grade must remain a separate material identity. Do not assume equal chemistry, heat treatment or mechanical acceptance from a comparable designation.

Related grades and substitution limits for PT450GH

The heading identifies a comparison topic, not a declaration of interchangeable material. No automatic foreign equivalent or dual certification is offered for PT450GH.

Product / range Verified relationship or limitation Substitution control
JIS G 3118 SGV450 Related carbon pressure-vessel grade in the same tensile-strength class. JIS tables are comparison only. Not automatic equivalence; engineer approval required.
JIS G 3103 SB450 Related JIS boiler-plate designation in a similar tensile class. Different standard and acceptance route. Not a substitute for the ISO PT grade.

Complete specification review and engineer approval are required before substitution or dual-certification claims. General requirements, edition, options, inspection and project acceptance still need review.

Why choose SHH STEEL for PT450GH

SHH STEEL supports specification-led pressure-plate purchasing rather than substitution by catalogue name.

  • We quote the requested ISO edition and grade separately from related national-standard products.
  • Delivery condition, fabrication heat treatment and supplementary test requests are reviewed before confirmation.
  • Comparison figures on this page are labelled as such; they are not used as unofficial ISO acceptance limits.
  • Inspection documentation and export packing are coordinated against the order.
  • Supply capability, lead time and any additional testing remain subject to quotation confirmation.

Enquiry and supply review for PT450GH

Send the project material schedule for PT450GH. SHH STEEL will review the enquiry and identify any clarification needed before confirming the supply route.

Enquiry item Information required
Material identity ISO 9328-2:2018 PT450GH; identify any proposed dual certification explicitly
Dimensions and quantity Nominal thickness, width, length, quantity and cutting drawings
Delivery condition Applicable usual condition, any agreed alternative, and untreated supply if requested
Acceptance values Complete ISO Table B.1 and Table B.2 requirements for the ordered edition; say if comparison values are for enquiry only
Inspection document Document type, traceability and any third-party attendance
Fabrication Forming, welding and intended post-weld heat treatment; any simulated heat-treatment tests
Destination Delivery place and any packing or marking restrictions

Missing numerical requirements on this comparison page are not waivers of the standard. Do not approve a substitution solely from this comparison content.

FAQ

Which edition applies to PT450GH here?
This page uses ISO 9328-2:2018, Edition 4. The ISO catalogue checked on 12 November 2026 (Asia/Shanghai) still lists it as Published, with revision planned and ISO/DIS 9328-2 under development.
What is the classification of PT450GH?
Non-alloy-quality steel under clause 4.1. The applicable grade route is Annex B; its complete requirements and ISO 9328-1 general requirements must be used together.
Are chemistry and mechanical numbers ISO normative limits?
No. ISO Table B.1 and Table B.2 are not transcribed as ISO limits. Chemistry and mechanical figures on this page are JIS G 3118 comparison/reference data for SGV450, clearly labelled. Confirm the official ISO rows before supply or design use.
Can another standard or a similar designation replace it?
Not automatically. Related product families are comparison references only. Complete specification review and engineer approval are required before substitution or dual-certification claims.
What should I send for a quotation?
Send the ISO edition and grade, dimensions, quantity, delivery condition, complete ISO acceptance requirements, inspection-document type and planned fabrication heat treatment. Include agreed supplementary tests and destination. If comparison values are being used for enquiry only, say so. The complete ISO Table B.1 and Table B.2 row must be available for a technical supply commitment.

Request a quotation for ISO 9328-2 PT450GH plate

Request a SHH STEEL quotation for ISO 9328-2:2018 PT450GH plate. Send nominal thickness, width, length, quantity, destination and the project material specification.

Identify the delivery condition, complete ISO chemistry and mechanical acceptance requirements, required inspection document and any impact, internal-soundness or supplementary tests. Include forming, welding and intended post-weld heat treatment for technical review.

Availability, dimensions, processing, testing and lead time will be confirmed against the enquiry. Related grades are not treated as approved substitutes without engineer review.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X