JIS G3115 SPV315 pressure vessel steel plate, yield 315 MPa, as-rolled or normalized plate, SHH STEEL

JIS G3115 SPV315 Steel Plate | SPV315 Pressure Vessel Plate

JIS G3115 SPV315 / SPV 315 is weldable pressure-vessel plate for intermediate-temperature service. Yield is 315 MPa at 6–50 mm. Tensile is 490–610 MPa. SHH STEEL supplies SPV315 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
Keywords
JIS G3115 SPV315, SPV315, SPV 315, JISG3115 SPV315, SPV315 steel plate, intermediate temperature vessel plate, SPV315 supplier
Equivalent Grades:
JIS G3115 SPV315 / EN 10028-2 P295GH (near) / ASTM A515 Gr 65 (near) / GB Q295R (near) — Material Specification: JIS G3115 — Delivery: As-rolled (AR); Normalized (N) by agreement
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
How the Six JIS G3115 Grades Differ
Material Comparison
Intermediate-Temperature Vessel Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is JIS G3115 SPV315 Steel ?

IS G3115 SPV315, also written SPV 315, JISG3115 SPV315 and SPV315 steel plate, is a weldable pressure-vessel plate under JIS G3115. The standard title is Steel plates for pressure vessels for intermediate temperature service. SPV315 is the second strength step in that book. Yield is 315 MPa at 6–50 mm. Tensile is 490–610 MPa. Thickness may run to 150 mm. Usual delivery is as-rolled, with normalize allowed. TMCP or QT is allowed by agreement. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade. Plate is produced to JIS G3115 and shipped to buyers in the USA, Europe, Middle East, Southeast Asia, Latin America, Africa and East Asia.

A purchase order that only says “SPV plate” is incomplete. Write JIS G3115 SPV315. Do not ship SPV235 against an SPV315 drawing. Do not ship SPV355 against an SPV315 drawing. Do not ship SA516 Gr.70 and call it SPV315 because tensile looks close.

JIS G3115 is not a low-temperature vessel book. Low-temperature Japanese plate belongs under JIS G3126. It is not boiler plate under JIS G3103 SB. It is not ordinary structural plate under JIS G3106. Intermediate-temperature service means the plate is intended for pressure vessels and high-pressure equipment that are not specified for high-temperature or low-temperature service under other JIS books.

This page is not DIN 17100 St52-3. It is not SA285 Gr.C. It is not QT alloy under ASME SA387 or ASME SA543.

Company scope: global steel mill sourcing partner – SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade JIS G3115 SPV315 / SPV 315 Confirmed
Product Specification JIS G3115:2022 Applied
Service idea Intermediate-temperature pressure vessels Confirmed
Steel type Killed, weldable plate Confirmed
Usual delivery As-rolled; N allowed; TMCP / QT by agreement Confirmed
Yield idea 315 MPa at 6–50 mm Confirmed
Tensile 490–610 MPa Confirmed
Thickness 6–150 mm Confirm mill
Supply role Global steel mill sourcing partner SHH STEEL
Markets Americas, Europe, Middle East, Africa, Asia FOB / CIF as ordered
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates and carbon steel plates. ASME comparisons belong on ASME SA516 and ASME SA285, not as automatic substitutes.

Chemical Composition

JIS G3115 SPV315 / SPV 315 heat analysis is given in JIS G3115 Table 3. Product analysis is not printed as a second official column in that table. When a destination file asks for product analysis, SHH STEEL applies the usual JIS check-analysis practice (JIS G0321 style): finished-plate chemistry is allowed a small extra tolerance over heat analysis. Write “heat + product analysis” on the order if both are required.

Heat Analysis and Product Analysis — JIS G3115 SPV315

Element Heat Analysis (JIS G3115 Table 3) (%) Product Analysis, when ordered (%)
Carbon (C), max 0.18 0.20
Silicon (Si), max 0.55 0.60
Manganese (Mn), max 1.60 1.70
Phosphorus (P), max 0.020 0.025
Sulfur (S), max 0.020 0.025

Other elements may be added for deoxidation or grain practice. For TMCP or QT SPV315, carbon equivalent and Pcm limits from JIS G3115 also apply. Do not treat an SPV235 heat as SPV315. Do not treat an SPV355 heat as SPV315. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.

Mechanical Properties

Yield starts at 315 MPa at 6–50 mm and falls as thickness rises.

Tensile and Yield — JIS G3115 SPV315

Thickness (mm) Yield min (MPa) Tensile (MPa)
6 – 50 315 490 – 610
50 – 100 295 490 – 610
100 – 150 275 490 – 610
Density 7.85 g/cm³ 7.85 g/cm³

Elongation depends on thickness and specimen type. Bend testing is specified. Charpy energy for SPV315 is commonly 0 °C, average 47 J, individual 27 J. Write the test temperature if the destination file wants something other than the JIS default.

Do not quote 315 MPa yield on a 120 mm plate. Do not treat 490–610 MPa tensile as permission to stamp SA516 Gr.70, SA516 Gr.65 or SA299 Gr.A.

How the Six JIS G3115 Grades Differ

Grade Yield idea (thin) Tensile Usual route
SPV235 235 MPa 400–510 AR / N
SPV315 315 MPa 490–610 AR / N; TMCP or QT by agreement
SPV355 355 MPa 520–640 AR / N; TMCP or QT by agreement
SPV410 410 MPa 550–670 TMCP first
SPV450 450 MPa 570–700 QT first
SPV490 490 MPa 610–740 QT first

Same book. Different strength and different heat-treatment default. SHH STEEL will not ship SPV315 against an SPV410 TMCP drawing.

Material Comparison

Grade Route Strength idea Swap?
JIS G3115 SPV235 Intermediate-temp vessel 235 / 400–510 No
JIS G3115 SPV315 Intermediate-temp vessel 315 / 490–610 This page
JIS G3115 SPV355 Intermediate-temp vessel 355 / 520–640 No
SA516 Gr.60 ASME carbon vessel 220 / 415–550 No
SA516 Gr.70 ASME carbon vessel 260 / 485–620 No
SA285 Gr.C ASME carbon vessel 205 / 380–515 No
ASTM A36 steel plate Structural Not a vessel book No

SA203 Gr.A, SA515 Gr.60 and SA662 Gr.A are also vessel plates. None of them is SPV315.

Intermediate-Temperature Vessel Service

JIS G3115 SPV315 / SPV 315 is selected for welded pressure vessels, tanks and high-pressure equipment that still name the Japanese intermediate-temperature book at the 315 MPa step. It sits between SPV235 and SPV355. It is not automatically an ASME Section VIII plate. If the vessel is ASME, the drawing should name an ASME or ASTM grade such as SA516 Gr.70, SA516 Gr.65 or SA285 Gr.C.

SHH STEEL supplies this plate to fabricators in the United States, Europe, the Middle East, Latin America, Africa and Asia. It is not nickel low-temp plate like SA203 Gr.D or SA203 Gr.E. It is not QT Ni-Cr-Mo like SA543 Type B Cl.1. It is not Cr-Mo like SA387 Gr.22 Cl.2. Stainless inquiries belong on ASME SA240 or ASTM A240.

Weldability

SPV315 is killed C-Mn vessel plate at the 315 MPa step. Welding is production welding, and Code welding when the equipment is a vessel.

Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the 490–610 MPa tensile band, not a SA387 Gr.12 Cl.2 Cr-Mo procedure and not a QT procedure from SA517 Gr.F. When TMCP or QT is used, Ceq and Pcm from JIS G3115 must stay inside the table. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is as-rolled JIS G3115 SPV315 / SPV 315 plate. Normalize is allowed when the order names it. TMCP or QT is allowed by agreement and must be written on the purchase order. Those routes are not assumed.

If the vessel will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the QT route used on SA738 Gr.B or SA737 Gr.C. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.

The certificate lists JIS G3115 SPV315 (and SPV 315 if requested); heat number; heat analysis; product analysis when ordered; tensile results to the correct thickness column; delivery condition; impact at the named temperature; Ceq / Pcm when TMCP or QT is used. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to SA516 Gr.70 is not automatic.

Dimensions

Usual supply range from SHH STEEL for SPV315 pressure vessel plate:

  • Thickness: commonly 6 mm – 150 mm. Confirm any request above 150 mm against mill capability
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm
  • Cut-to-length plates and nest sizes inside those limits

Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.

Tolerances

Dimensional limits follow the mill rolling standard named on the order. Do not apply ASTM A36/A36M structural tolerances to a JIS vessel plate without writing them. UT to JIS, EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.

Supplementary Requirements

Most export JIS G3115 SPV315 / SPV 315 orders add extras. SHH STEEL does not assume them.

Charpy details. Temperature, energy, location and orientation. JIS default is commonly 0 °C.

Product analysis. Add this when the destination file wants finished-plate chemistry, not only ladle chemistry.

Ceq / Pcm. Required when TMCP or QT is selected.

Simulated PWHT. When the equipment will be stress-relieved.

NDE. UT per the named method.

Z-direction / through-thickness testing. When the drawing names Z15 / Z25 / Z35.

Third-party. EN 10204 3.2, with inspectors arranged for US, European, Middle East, Latin American or Asian documentation packages.

Equivalent Material Grades

These names are project-comparison grades. They are not automatic substitutes.

Designation Standard / region Notes
JIS G3115 SPV315 / SPV 315 JIS G3115 Name on this page
SPV235 JIS G3115 Lower step
SPV355 JIS G3115 Higher step
SA516 Gr.70 SA-516 Related carbon vessel, different yield
SA516 Gr.65 SA-516 / A516 Related vessel family
ASTM A516 A516 family Related vessel family
ASME SA515 SA-515 family Intermediate/high-temp carbon
ASME SA285 SA-285 family Lower-strength vessel family

ASME SA662 is not SPV315.

Applications

Industry Typical components
Intermediate-temperature vessels JIS G3115 SPV315 shells and SPV 315 plates
Tanks and process steelwork SPV315 courses
Dual-certified export SPV315 plate from SHH STEEL when the drawing keeps the JIS name
Fabrication SPV315 cut to nest sizes

Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.B, A516 Grade 70, SA533 Type C Cl.2, SA517 Gr.P, SA738 Gr.C.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN and JIS steel to buyers outside a single region. Origin is mill-direct, China origin. Inquiry packages are written for fabricators and EPC buyers, not only for East Asia.

SHH STEEL has supplied steel plates to:

  • North America: USA, Mexico
  • South America: Argentina, Peru and other South American ports
  • Central America: El Salvador
  • Europe: Spain, Netherlands, Germany and surrounding ports
  • Middle East: UAE, Saudi Arabia and nearby Gulf ports
  • Africa: South Africa
  • South / Southeast Asia: India, Thailand, Singapore, Vietnam, Philippines
  • East Asia: Japan, Korea

Typical trade terms:

  • FOB Shanghai
  • CIF Houston
  • CIF Rotterdam
  • CIF Jebel Ali
  • Other CIF / CFR ports on request, including Manzanillo, Callao, Buenos Aires, Barcelona, Durban, Laem Chabang, Ho Chi Minh, Manila, Mumbai, Yokohama and Busan

Typical lead time for JIS G3115 SPV315 / SPV 315:

  • Ex-stock / ready plate: about 5–7 days after order confirmation, subject to actual warehouse size and cutting
  • Mill rolling, standard as-rolled or normalize: about 45 days
  • TMCP / QT, simulated PWHT, 3.2 hold or extra NDE: about 2 months

Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading for US, Mexican, European, Middle East, Japanese or Korean documentation packages. Packing is seaworthy, with edge protection and marking in English as specified on the order.

If the buyer actually needs SPV410 TMCP or SPV490 QT, say so on the inquiry. If the buyer needs a PED / 3.2 file, say so on the inquiry. Do not assume a domestic Chinese certificate format will pass at destination.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS steel to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia. On JIS G3115 SPV315 / SPV 315 that means mill pricing, SPV315 chemistry reported as heat analysis and as product analysis when ordered, recorded delivery condition, tensile results to the correct thickness column, 315 MPa yield in the thin band, 3.1 as standard and 3.2 when specified. Trade terms include FOB Shanghai and CIF Houston / Rotterdam / Jebel Ali.

We keep the grade on the order. SPV315 is not SPV235. SPV315 is not SPV355. SPV315 is not SPV410. SPV315 is not SA516 Gr.70. SPV315 is not SA387 Gr.22 Cl.2. JIS G3115 is not JIS G3103 and not JIS G3126. If the drawing names 355 MPa, we will not ship SPV315 and call it close.

Company scope: global steel mill sourcing partner – SHH STEEL.

FAQ

What is SPV315 steel plate?
SPV315 is a JIS G3115 weldable pressure-vessel plate for intermediate-temperature service. Yield is 315 MPa at 6–50 mm and tensile is 490–610 MPa. Buyers also write SPV 315, JISG3115 SPV315 and SPV315 steel plate. SHH STEEL supplies this plate as a global steel mill sourcing partner.
Does JIS G3115 give product analysis for SPV315?
JIS G3115 Table 3 is heat analysis. Product analysis is added when the order names it, using usual JIS check-analysis practice. SHH STEEL reports both when written on the purchase order.
What is the equivalent of SPV315?
Strength is often compared with SA516 Grade 70. Dual marking is possible only when chemistry, tensile and impact all fit the named ASME or ASTM edition.
How is SPV315 different from SPV235 and SPV355?
SPV235 yield is 235 MPa and tensile is 400–510 MPa. SPV315 yield is 315 MPa and tensile is 490–610 MPa. SPV355 yield is 355 MPa and tensile is 520–640 MPa.
Is SPV315 a low-temperature plate?
No. JIS G3115 is intermediate-temperature service. Low-temperature Japanese plate belongs under JIS G3126.
Can SHH STEEL ship JIS G3115 SPV315 to Mexico, South America or Southeast Asia?
Yes. SHH STEEL has supplied plates to Mexico, Argentina, El Salvador, Peru, Spain, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea, as well as the USA, Europe and the Middle East.
What is the delivery time for SPV315?
Ex-stock about 5–7 days. Standard mill rolling about 45 days. TMCP / QT, simulated PWHT or 3.2 inspection about 2 months.
Can SHH STEEL issue EN 10204 3.2 for SPV315?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged when written on the order.

Conclusion

JIS G3115 SPV315 Steel Plate, also searched as SPV 315, JISG3115 SPV315 and SPV315 steel plate, is weldable pressure-vessel plate under JIS G3115 for intermediate-temperature service at the 315 MPa yield step, 490–610 MPa tensile, thickness to 150 mm. Whether the inquiry says JIS G3115 SPV315, SPV 315 or SPV315 Pressure Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with SPV315 chemistry, heat and product analysis when ordered, recorded delivery condition, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies JIS G3115 SPV315 / SPV315 Pressure Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.

Contact SHH STEEL for mill rolling, stock inquiry, normalize, TMCP / QT by agreement, impact testing, 3.2 inspection or a quotation.

JIS G3115 SPV315 Steel Plate, SPV 315, JISG3115 SPV315, intermediate temperature vessel plate, SPV315 supplier, global steel mill sourcing partner SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X